• 제목/요약/키워드: 알칼리 실리카 반응

검색결과 68건 처리시간 0.022초

쇄석골재의 알칼리-실리카 반응에 관한 실험적 연구 (제3보 : 무해골재 치환량 및 포졸란물질이 알칼리-실리카 반응에 미치는 영향) (An Experimental Study on the Alkali-Silica Reaction of Crushed Stones (Part 3 : The Influence of the Innocuous Aggregate Content and Pozzolanic Materials to the Alkali-Silica Reaction))

  • 이양수;정재동;노재호;조일호;윤재환;이영수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1994년도 봄 학술발표회 논문집
    • /
    • pp.169-173
    • /
    • 1994
  • Recently, the use of crushed stones is increased due to the shortage of natural aggregates. In the previous papers of part 1 and 2, we got the conclusions that some of crushed stones have the characteristic of alkali-silica reaction(ASR). And these reactions are influenced by the amount and type of alkali in cement. The purpose of this paper is how to prepare for the prevention against alkali-silica reaction. As a solution of problems, we have conducted the experiments of two methods. One was the replacement of innocuous aggregates instead of reactive aggregates, the other was the addition of various pozzolanic materials. As a result, we found that the expansion by alkali-silica reaction in mortar bar could be effectively decredsed by upper methods.

  • PDF

붕규산 유리 분말을 혼입한 차폐용 콘크리트의 알칼리 실리카 반응에 의한 팽창 실험 (An Experimental Study on Alkali-Silica Reaction due to Neutron Shielding Concrete Containing Borosilicate Glass Powder)

  • 장보길;김지현;정철우
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 춘계 학술논문 발표대회
    • /
    • pp.160-161
    • /
    • 2015
  • Borosilicate glass can be used for improving neutron shielding of concrete. The well known expansion of borosilicate glass caused by expansion of mortar bar was can cause serious damage to the concrete. In this research, borosilicate glass was powdered to reduce the particle size similar to that of cement, and 20% cement replacement set was reduced expansion rate about 30%. But aggregate replacement set was damaged because of Alkali-Silica Reaction expansion.

  • PDF

잔골재용 폐유리의 표면개질이 모르타르의 역학적 특성 및 알칼리 실리카 반응에 미치는 영향 (Effect of Surface Modification of Waste Glass for Fine Aggregate on the Mechanical Properties and Alkali Silica Reaction of Mortar)

  • 손민재;김규용;이상규;사수이;유하민;남정수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2020년도 가을 학술논문 발표대회
    • /
    • pp.23-24
    • /
    • 2020
  • In this study, effect of surface modification of waste glass for fine aggregates on the mechanical properties and alkali silica reaction of mortar was analyzed. As a result, it was confirmed that the incorporation of waste glass fine aggregate decreases the mechanical properties of the mortar and increase the alkali silica reaction expansion. On the other hand, the surface modification of the waste glass fine aggregate is effective in improving this problem. However, unlike green and brown waste glass, it is judged that an additional experiment to determine the cause is necessary for white waste glass where alkali silica reactive expansion occurs extremely.

  • PDF

폐유리 잔골재가 고강도 모르타르의 역학적 특성 및 알칼리-실리카 반응(ASR), ASR 후, 잔류 역학적 특성에 미치는 영향 (Effect of Waste Glass Fine Aggregate on Mechanical Properites and Alkali-Silica Reaction(ASR), After ASR Residual Mechanical Properties of High Strength Mortar)

  • 유하민;김규용;손민재;사수이;이예찬;남정수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2020년도 가을 학술논문 발표대회
    • /
    • pp.31-32
    • /
    • 2020
  • This study measured the mechanical performance and residual strength of high strength/normal strength mortar mixed with waste glass fine aggregate after alkali-silica reaction and alkali-silica reaction. As a result, the effect of improving the slip phenomenon of the waste glass fine aggregate in the high-strength mortar was not significant, but rather the amount of ASR was increased.

  • PDF

폐유리 잔골재 대체율이 물시멘트비가 다른 모르타르의 역학적 특성 및 알칼리 -실리카 반응에 미치는 영향 - (Effect of the replacement rates of Waste Glass Fine Aggregate on the Mechanical Properties and Alkali - Silica Reaction of Mortars with different W/C Ratio -)

  • 유하민;김규용;남정수;손민재;사수이;이예찬
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2020년도 봄 학술논문 발표대회
    • /
    • pp.195-196
    • /
    • 2020
  • This study evaluated the mechanical properties and alkali silica reaction of mortar according to the mixing ratio of waste glass. As a result, as the mixing ratio of the waste glass increased, the compressive and flexible strength of the mortar decreased due to the slip of aggregate, and the alkali-silica reaction(ASR) increased. So, it is considered that research is needed to prevent slip and ASR of the waste glass aggregate in order to use the waste glass as a fine aggregate for concrete.

  • PDF

지오폴리머 모르타르의 알칼리-실리카반응에 관한 연구 (A Study on the Alkali-Silica Reaction of Geopolymer Mortar)

  • 김성훈;김영수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 추계 학술논문 발표대회
    • /
    • pp.7-8
    • /
    • 2015
  • The purpose of this study is to investigate the expansion of alkali-activated geopolymer mortar containing reactive aggregate due to alkali-silica reaction. In addition, this study is particularly concerned with the behavior of these alkaline materials in the presence of reactive aggregates. The test method included expansion measurement of the mortar bar specimens and geopolymer compressive strength test. Major results that alkali-activated geopolymer mortars showed expansion due to the alkali-silica reaction. geopolymer mortars is safety for the expansion exhibited less than 0.2% at 14 day.

  • PDF

폐유리 분말을 혼입한 유리 콘크리트의 역학적 특성에 관한 실험적 연구 (Experimental Study on the Mechanical Properties of Glass Concrete with Powdered Waste Glasses)

  • 배수호;정영수
    • 콘크리트학회논문집
    • /
    • 제13권1호
    • /
    • pp.54-61
    • /
    • 2001
  • 천연자원 보존의 일환으로서 폐타이어, 폐플라스틱 재료 등에 대한 재활용 연구가 활발히 진행되고 있다. 따라서 본 연구의 목적은 폐유리를 시멘트 대체재료로서 개발하기 위한 것이다. 이를 위하여, 먼저 보통강도 및 고강도 콘크리트 각각에 대해서 폐유리 분말의 혼입률을 변화시킨 콘크리트를 제조한 다음 그것의 압축강도 시험을 통하여 폐유리 분말의 최적 혼입률을 도출하였다. 또한, 최적 혼입률에 의하여 제작된 보통강도 및 고강도 콘크리트 각각에 대해서 압축, 인장 및 휨강도와 탄성적 성질 등 역학적 특성을 구명하였다. 한편, 시멘트 속의 알칼리와 폐유리 속에 다량 함유된 실리카 성분은 서로 반응하려는 경향이 있기 때문에, 현재 모프타르봉 시험 방법(KS F 2546)에 의한 알칼리.실리카 반응 시험을 진행하고 있다. 본 실험연구 결과로부터 폐유리 분말을 혼입한 콘크리트는 실리카흄 콘크리트보다 작업성은 다소 우수하며, 강도특성은 유사한 것으로 나타나, 폐유리 분말에 대해서 경제적이고 환경친화적인 콘크리트 혼화재로서의 가능성을 입증하였다.

사문석으로부터 제올라이트 A의 합성 (Synthesis of zeolite A from serpentine)

  • 김동진;정헌생;이재천;김인회;이자현
    • 한국결정성장학회지
    • /
    • 제10권1호
    • /
    • pp.73-79
    • /
    • 2000
  • 마그네슘 함수 규산염인 사문석을 염산처리하여 얻은 다공성의 침출잔사인 비정질 실리카를 제올라이트 A합성을 위한 실리카 원료로 사용하였다. 제올라이트 A는 사문석 침출잔사인 다공성 실리카와 알루미늄원인 수산화 알루미늄을 각각 수산화나트륨에 혼합 용해하여 대기압하에서 수열반응에 의하여 합성하였으며 최적합성조건은 반응온도 $80^{\circ}C$, 반응시간 2시간 그리고 $Na_2O/SiO_2$몰비 1.5이었다. 또한 제올라이트의 결정화속도는 반응온도 및 알칼리도가 높을수록 빨리 일어나지만 반응온도 $80^{\circ}C$, 반응시간 120분 이상인 실험조건에서는 hydroxysodalite 제올라이트가 생성되었다.

  • PDF