Property Optimization of Ni/CGO Cermet Anodes (Ni/CGO Cermet Anode의 특성 최적화)

  • 최종혁;김남진;이덕열
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.12 no.1
    • /
    • pp.94-102
    • /
    • 1999
  • Ni/CGO cermets were fabricated as the anode for SOFC which uses CGO as the electrolyte. And their electrical conductivity, electrochemical reactivity, and thermal expansion coefficient were optimized through the variation of NiO/CGO particle size ration and their composition. The electrical conductivity of the cermet was increased abruptly at a certain Ni content and the percolation concentration was decreased with the decreasing particle size ratio. Anodic overpotential was also decreased with the decreasing particle size ratio. For a fixed ratio it showed a minimum value at 50 wt.%. Thermal expansion coefficient was increased monotonically with increasing Ni contents, however it did not depend on the size ratio. With three properties taken into account, the cermet of particle size ration of 0.03 and composition of 50 wt.% was judged to be optimal as the anode.

  • PDF

Formation of a Core/Rim Structure in Ti(C, N)-based Cermets (Ti(C, N)계 써메트의 유심구조 형성거동)

  • Kim, Suk-Hwan
    • Journal of Powder Materials
    • /
    • v.13 no.1 s.54
    • /
    • pp.10-17
    • /
    • 2006
  • Model experiment was introduced to obtain the formation of a core/rim structure by only liquid phase reaction in Ti(C, N)-based cermet alloys. Infiltrated Ti(C, N)-Ni, $MO_2C-Ni$, and TaC-Ni cermets were bonded to sandwiched specimen by heat treatment $1450^{\circ}C$ for 5hr. With nitrogen addition, both (Ti, Mo) (C, N) and (Ti, Ta) (C, N) rim structure was nucleated around comer of cuboidal Ti(C, N) core. However, equilibrium shapes of(Ti, Mo) (C, N) and (Ti, Ta) (C, N) rim were different possibly due to the effect of interface energy. The core/rim and rim! binder interfaces were parallel to each other with TaC addition, while rotated to each other with $MO_2C$ addition.

Effect of VC Addition on the Microstructure & Mechanical Properties of Ti(CN)-based Cermet (VC 첨가가 Ti(CN)계 써메트의 미세구조 및 기계적 성질에 미치는 영향)

  • 안성용;강신후
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.12
    • /
    • pp.1316-1322
    • /
    • 1998
  • The amount of VC and C/N ratio in Ti(CN) was varied to investigate the effect of VC addition on the mi-crostructural change in Ti(CN)-Ni system. As the amount of VC addition increases in Ti(C0.7N0.3)-20Ni sys-tem a complete solid solution was observed in Ti(C0.7N0.3)-20Ni-25VC system. It implies that the ratio of the dissolution rates of Ti(C0.7N0.3)to that of VC is nearly 2:1 at the sintering conditions used in this study. It was found from the experiments that the system composed of the Ti(C0.7N0.3) phase exhibits a rimless structure and relatively small amount of solid solution. That is among Ti(C0.7N0.3) phase exhibits a rimless structure and relatively small amount of solid solution. This is among Ti(C1-xNx) phases the dissolution rate of Ti(C0.3N0.7) is the lowest. Also fracture toughness(KIC) of the cermet was measured by indentation method. Attentions were paid to crack propagation path to look for a dominant fracture mode and to cor-relate it with fracture toughness values. The fracture toughness was relatively high with the addition of VC content. But the addition of a large VC content reduced the overall toughness of the cermet. This result is explained with the difference in fracture mode.