The Effect on the Kind of Alkali-Activator of Cement ZERO Mortar (알칼리 활성화제 종류가 시멘트 ZERO 모르타르에 미치는 영향)

  • Ryu, Gum-Sung;Kang, Hyun-Jin;Ko, Kyung-Taek;Kang, Su-Tae;Kim, Sung-Wook;Lee, Jang-Hwa
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.397-398
    • /
    • 2009
  • Recently, the research about alkaline activity concrete is being progressed actively. In this paper, the effect of many kinds of alkaline activation to fly ash based cement zero mortar is examined.

  • PDF

Influence of varying cement types and abutment heights on pull-off force of zirconia restorations (시멘트의 종류 및 임플란트 지대주 높이가 지르코니아 수복물의 제거력에 미치는 영향)

  • Yeong-Jun Jung;Yu-Lee Kim;Ji-Hye Jung;Nae-Un Kang;Hyun-Jun Kong
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.40 no.2
    • /
    • pp.64-71
    • /
    • 2024
  • Purpose: The purpose of this study is to evaluate Ti-base abutment's three different heights and three different cement types on the pull-off force of zirconia-based restorations. Materials and Methods: A total of 90 fixture lab analogs were embedded in auto polymerizing resin bloack. 90 Ti-base abutments heights of 3 mm, 5 mm, 7 mm were scanned and zirconia restoration were prepared from scanned files. Zirconia restoration were cemented with three different types of cements (temporary, semi-permanent, permanent) following manufacturer's instructions. All 90 specimens were placed and tested in a universal testing machine for pull-out testing. Retention was measured by recording the force at load drop. Statistical analysis was performed using Kruskal-Wallis test for detecting whether there are any statistical significance along cement types or abutment heights. After that, Mann-Whitney test was used for figuring out differences regarding abutment height and the comparison between 3 cements. Results: Temp bond showed significantly lower pull-off force compared to Fujicem regardless of any abutment height. However, there were significant differences between Cem-implant and Fujicem in abutment height of 3 mm and 7 mm, but there was no significant difference in 5 mm. Temp bond and Cem-implant had significant differences only in abutment height of 5 mm. Conclusion: Although Ti-base abutment height did not influenced zirconia restorations' retentiveness, cement types showed significant differences.

Physical Properies of Polymer Cement Mortar Using Ground FRP Wastes (분쇄된 FRP 폐기물을 사용한 폴리머 시멘트 모르타르의 물성)

  • 이병기;이범재;황의환;노재성
    • Magazine of the Korea Concrete Institute
    • /
    • v.10 no.5
    • /
    • pp.217-225
    • /
    • 1998
  • 분쇄한 FRP(Fiver-Reinforced Plastics) 폐기물을 사용한 폴리머 모르타르의 물성에 고나하여 조사하였다. 분쇄한 FRP 폐기물을 시멘트 모르타르의 세골재로 재활용하기 위하여 세골재에 대하여 0~50wt% 치환.사용하였고, FRP 폐기물의 사용으로 나타나는 강도 저하현상을 보완하기 위하여 3종류 폴리머 혼화제의 첨가량을 변화시켜 각종 공시체를 제작하였다. 폴리머 혼화제로서는 styrene-bytadiene rubber(SBR) 라텍스, polyacrylic ester(PAE) 에멀젼 및 ethylene-vinyl acetate(EVA)에멀젼을 사용하였다. 분쇄한 FRP 폐기물을 사용한 시멘트 모르타르에 폴리머 혼화제를 첨가하여 만든 폴리머 시멘트 모르타르는 폴리머 혼화제를 첨가하지 않은 모르타르보다 압축 및 휨강도가 크게 증가하였다. 폴리머 시멘트비 10wt%에서 세골재 대용으로 분쇄한 FRP 폐기물의 적정 치환량은 20wt%로 나타났다. 8$0^{\circ}C$에서 가열양생하여 제조한 폴리머 시멘트 모르타르는 폴리머 시멘트비 10wt%이하에서 표준양생한 모르타르보다 강도가 저하되었다. 폴리머 시멘트 포르타르의 흡수율은 폴리머 시멘트비가 증가함에 따라 크게 감소하였다.

A Study on the Improvement of Adhesion in Tension and Flexure of Polymer Cement Mortar Depending on Various Test Methods (시험방법에 따른 폴리머 시멘트 모르타르의 인장 및 휨접착강도 개선에 관한 연구)

  • Jo, Young-Kug
    • Journal of the Korea Institute of Building Construction
    • /
    • v.19 no.1
    • /
    • pp.47-57
    • /
    • 2019
  • The purpose of this study is to evaluate the improvement effect of adhesion in tension and flexure of polymer cement mortars that have widely used as a repair-reinforcement material in construction field according to adding of polymer dispersions depending on different three types test methods. From the test results, the adhesion performance is improved with a raise in polymer-cement ratio irrespective of the type of polymer. The maximums of A type adhesion in tension, B type adhesion in tension and adhesion in flexure show 1.90 times, 2.17 times and 1.83 times, respectively that of plain cement mortar. The relative strength ratios, B type adhesion in tension and adhesion in flexure of polymer cement mortars to tensile and flexural strengths of plain mortar respectively are in ranges of 50.1% to 101.7% and 73.8% to 132.9% compared to 46.9% of plain mortar. It is apparent that polymer cement mortars with EVA and polymer cement ratios of 10% to 15% are recommended considering its adhesion performance and cost as a repair-reinforcement material in construction field.

Effect of Temperature and Aging on the Relationship Between Dynamic and Static Elastic Modulus of Concrete (온도와 재령이 콘크리트의 동탄성계수와 정 탄성계수의 상관관계에 미치는 영향)

  • 한상훈;김진근;박우선;김동현
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.6
    • /
    • pp.610-618
    • /
    • 2001
  • This paper investigates the relationships between dynamic elastic modulus and static elastic modulus or compressive strength according to curing temperature, aging, and cement type. Based on this investigation, the new model of the relationships we proposed. Impact echo method estimates the resonant frequency of specimens and uniaxial compression test measures the static elastic modulus and compressive strength. Type I and V cement concretes, which have the water-cement ratios of 0.40 and 0.50, are cured under the isothermal curing temperatures of 10, 23, and 50$\^{C}$ Cement type and aging have no large influence on the relationship between dynamic and static elastic modulus, but the ratio of dynamic and static elastic modulus comes close to 1 as temperature increases. Initial chord elastic modulus which is calculated at lower strain level of stress-strain curve, has the similar value to dynamic elastic modulus. The relationship between dynamic elastic modulus and compressive strength has the same tendency as the relationship between dynamic and static elastic modulus according to cement type, temperature and aging. The proposcd relationship equations between dynamic elastic modulus and static elastic modulus or compressive strength properly estimates the variation of relationships according to cement type md temperature.

Evaluation on Rear Fracture Reduction and Crack Properties of Cement Composites with High-Velocity Projectile Impact by Fiber Types (섬유 종류에 따른 시멘트복합체의 고속 비상체 충격에 대한 배면파괴저감 및 균열특성 평가)

  • Han, Sang-Hyu;Kim, Gyu-Yong;Kim, Hong-Seop;Kim, Jung-Hyun;Nam, Jeong-Soo
    • Journal of the Korea Concrete Institute
    • /
    • v.27 no.2
    • /
    • pp.157-167
    • /
    • 2015
  • Cement composites subjected to high-velocity projectile shows local failure and it can be suppressed by improvement of flexural toughness with reinforcement of fiber. Therefore, researches on impact resistance performance of cement composites are in progress and a number of types of fiber reinforcement are being developed. Since bonding properties of fiber with matrix, specific surface area and numbers of fiber are different by fiber reinforcement type, mechanical properties of fiber reinforced cement composites and improvement of impact resistance performance need to be considered. In this study, improvement of flexural toughness and failure reduction effect by impact of high-velocity projectile have been evaluated according to fiber type by mixing steel fiber, polyamide, nylon and polyethylene which are have different shape and mechanical properties. As results, flexural toughness was improved by redistribution of stress and crack prevention with bridge effect of reinforced fibers, and scabbing by high-velocity impact was suppressed. Since it is possible to decrease scabbing limit thickness from impact energy, thickness can be thinner when it is applied to protection. Scabbing of steel fiber reinforced cement composites was occurred and it was observed that desquamation of partial fragment was suppressed by adhesion between fiber and matrix. Scabbing by high-velocity impact of synthetic fiber reinforced cement composites was decreased by microcrack, impact wave neutralization and energy dispersion with a large number of fibers.

Colorimetric Analysis of Preformed Zirconia Anterior Crowns for Esthetic Restoration (심미수복용 기성 지르코니아 크라운의 색조 평가)

  • Lee, Changkeun;Park, Kibong;Yang, Yeonmi;Lee, Daewoo;Kim, Jaegon
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.46 no.3
    • /
    • pp.318-327
    • /
    • 2019
  • The purpose of this study was to identify which combination of zirconia crowns and cements is most similar in color to the maxillary primary incisors by varying the color of zirconia crowns, crown thickness, and shade of cements. Prefabricated zirconia crowns in 3 shades and crowns fabricated using 6 types of zirconia blocks were used in this study. These were filled with A2-shade or translucent-shade resin cement and the $L^*$, $a^*$, and $b^*$ values were calculated using a spectrophotometer. The color differences between the natural teeth and the zirconia crowns were assessed. The shade of the final restoration was more similar to that of the natural teeth using A2-shade than translucent-shade resin cement. Application of A2-shade cement to a 0.5-mm-thick crown fabricated from a smile series 2 zirconia block resulted in the color most similar to that of the natural teeth. A2-shade resin cement is recommended for zirconia crown restoration in anterior primary teeth compared to TR-shade resin cement for more esthetic restoration. Since restorations with Nu-smile zirconia crowns were not esthetically favorable in terms of shade, improvement of the shade characteristics of the product or development of a new kind of zirconia crown is required.

Shear Behavior Characteristics of Joint according to Strain-Hardening Cement Composite Types (시멘트 복합체 종류에 따른 접합부의 전단거동특성)

  • Nam, Sang-Hyun;Jeon, Esther;Yun, Hyun-Do;Choi, Ki-Sun;You, Young-Chan;Kim, Keung-Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2010.05a
    • /
    • pp.27-28
    • /
    • 2010
  • This paper discusses behavior of Joint with strain hardening cement composites(SHCC). The main variables considered include the type of cement composites(mortar, SHCC with hybrid fiber) and shape and space of reinforcement. As the result of the tests, for the same reinforcement detail, SHCC specimen showed better overall behavior(stress, ductile, multiple cracking) than mortar specimen.

  • PDF

Equations Evaluation for and Shear Behavior Characteristics of Joint according to Cement Composite Types (시멘트 복합체 종류에 따른 접합부의 전단거동 및 산정식 평가)

  • Jeon, Esther;Yun, Hyun-Do;Lee, Young-Oh;Kim, Sun-Woo;Ryu, Seung-Hyun
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2010.05a
    • /
    • pp.97-98
    • /
    • 2010
  • This paper discusses shear behavior of Joint with premix mortar and strain hardening cement composites(SHCC) with PVA and PE fibers. The main variables considered include the type of cement composites(premixed mortar, SHCC with hybrid fiber) and reinforcement. It was evaluated that shear load had a good accordance with the test and equation result.

  • PDF

기술연구 - Clinker free 콘크리트의 기초성상에 관한 연구

  • Lee, Jong-Yeol
    • Cement
    • /
    • s.192
    • /
    • pp.39-47
    • /
    • 2011
  • 최근 온실가스 감축과 기후변화 그리고 녹색성장에 대한 관심증대와 더불어 시멘트 분야의 연구 생산분야는 천연자원 사용량을 줄이고, 소성공정을 도입하지 않은 새로운 개념의 무기바인더가 다시 고개를 들고 있다. 다른 용어로는 비소성, 무시멘트 등으로 표현되기도 하는데, 광의의 개념으로 보면 알칼리 활성화제를 사용한 비소성 무기결합재인 지오폴리머가 바로 그것이다. 지오폴리머 결합재는 1957년 우크라이나의 토목공학회에서 개발한 알칼리 활성 슬래그시멘트에 기원을 두고 있고, 1970년대 말 프랑스의 다비도비치에 의해 지오폴리머라는 용어가 처음 사용되기 시작했다. 알칼리 활성 무기결합재(Alkali-activated inorganic binder)의 정의이다. Alkali-activated inorganic binder는 원래는 결합능력이 없던 재료에 대해서 Alkali-activating 용액을 첨가했을 때, 시멘트처럼 결합능력을 가지게 되는 모든 종류의 결합시스템을 말한다. 국내에도 이미 2000년 초부터 지오폴리머의 개념을 도입한 제품이 상업화되어 오랫동안 품질검증을 거쳐 안정성이 확인되고 있다. 최근에 다시 전남대가 그 동안의 연구성과를 발 빠르게 중소기업에 기술 이전하여 소위 무시멘트 시대에 진입하는 분위기이다. 지난 9월 동아에스텍(주)과 조인트벤처 설립을 위해 손을 잡았고, 사업화가 곧 진행될 것으로 보인다. 이를 계기로 국내에도 무시멘트회사가 본격적으로 등장하게 된 것이다. 따라서 본 고는 무시멘트의 개념을 잘 표현한 문헌으로 일본콘크리트공학 연차논문집, 2010년 1월호를 번역 요약 발췌한 것이다.

  • PDF