• 제목/요약/키워드: 스커핑 수명

검색결과 6건 처리시간 0.019초

윤활환경에 따라 발생하는 소성변형량과 저주기 피로물성을 이용한 스커핑 수명 예측 (The Prediction of Scuffing Life due to Plastic Deformation and Low-cycle Fatigue Properties Under Various Lubricated Conditions)

  • 김병주;이영제
    • Tribology and Lubricants
    • /
    • 제14권4호
    • /
    • pp.7-14
    • /
    • 1998
  • A correlation between the low-cycle fatigue life and the scuffing-failure life is demonstrated using the plastic strain increment in boundary lubricated sliding. Loadings proportional to hardness with three different lubricated conditions were used to evaluate the plastic strain increments. As the results of scuffing tests using vacuum pump oils in nitrogen gas, plastic strain increment shows 0.0062, and in the mineral oils and commercial engine oils in air, plastic strain increments show 0.0042 and 0.00092. Those are very useful to describe quantitatively the real lubricated sliding conditions, and are very effective to find the relation between the low-cycle fatigue life and the scuffing-failure life.

윤활조건에 따른 미끄럼표면의 소성변형량에 의한 스커핑수명 연구 (A Study on Scuffing Life by the Plastic Strain on Sliding Surfaces under Miscellaneous Lubricated Conditions)

  • 김병주;이영제
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1998년도 제28회 추계학술대회
    • /
    • pp.91-99
    • /
    • 1998
  • A correlation between the low-cycle fatigue life and the scuffing-failure life is demonstrated using the plastic strain in boundary lubricated sliding. Loadings proportional to hardness with three different lubricated conditions were used to evaluate the plastic strain. As the results of scuffing tests using vacuum pump oils in nitrogen gas, plastic strain shows 0.0062, and In the mineral oils and commercial engine oils in air, plastic strain show 0.0042 and 0.00092. Those are very useful to describe quantitatively the real lubricated sliding conditions, and are very effective to find the relation between the low-cycle fatigue life and the scuffing life.

  • PDF

다양한 박막을 증착한 디젤 엔진용 피스톤링과 실린더 블록의 마찰 마멸 및 스커핑 수명 평가 (Friction, Wear and Scuffing Life of Piston Rings With Several Coating for Low Friction Diesel Enging)

  • 안태식;조대현;정순오;이영제
    • Tribology and Lubricants
    • /
    • 제23권4호
    • /
    • pp.170-174
    • /
    • 2007
  • Wear and scuffing tests were conducted using friction and wear measurement of piston rings and cylinder blocks in low friction diesel engine. The frictional forces, wear amounts and cycles to scuffing in boundary lubricated sliding condition were measured using the reciprocating wear tester. The cylinder blocks were used as reciprocating specimens, and the piston rings with several coatings were used as fixed pin. Several coatings were used such as DLC, TiN, Cr-ceramic and TiAlN in order to improve the tribological characteristics. From the tests wear volume of piston ring surfaces applied various coatings were compared. During the tests coefficients of friction were monitored. Test results showed that DLC coatings showed good tribological properties. TiN and Cr-ceramic coated rings showed good wear resistance properties but produced high friction.

나노다이아몬드를 첨가한 오일의 트라이볼로지 특성 및 이에 미치는 표면 경도의 영향 (Tribological Characteristics of Paraffin Liquid Oil with Nanodiamond and Effects of Surface Hardness on Wear Properties)

  • 이규선;김현수;이정훈;박태희;이정석;이영제
    • Tribology and Lubricants
    • /
    • 제27권6호
    • /
    • pp.321-325
    • /
    • 2011
  • Nanodiamond was dispersed in paraffin liquid oil to investigate the effects of nanodiamond at the marginally lubricated condition. Scuffing test and immediate loading sliding wear test were conducted using the fabricated nanodiamond oil. As a result, dispersion of nanodiamond in oil leads to increase in scuffing life, and nanodiamond contents affects the scuffing life. In case of immediate loading sliding wear test, the result was different according to hardness of specimen. If hardness of specimen was low, abrasion of nanodiamond occurred actively. If hardness of specimen was increased, however, nanodiamond can act as a spacer or rolling between contacting surfaces.

스퍼 기어의 진동 신호와 비 유막 두께(Specific Film Thickness)의 상관관계에 관한 실험적 연구 (Experimental Investigation to Establish Correlation Between Specific Film Thickness and Vibration Signals in Spur Gear System)

  • 김종식;;이상권
    • 대한기계학회논문집A
    • /
    • 제38권9호
    • /
    • pp.1005-1012
    • /
    • 2014
  • 기어의 구동은 여러 기계요소에서 동력전달을 가능하게 해주는 가장 중요한 요소이다. 이러한 기어 접촉면에서의 상태는 마모, 재료의 변형 그리고 윤활 상태에 따라 크게 좌우되며, 이러한 상태 변화는 기어의 수명에 큰 영향을 준다. 따라서, 이러한 상태 진단에 대한 해법은 원활한 구동을 위한 필수요소이다. 기어의 상태 변화는 연마 마모(Abrasive wear), 점식 (Pitting), 스커핑(Scuffing), 스폴링(Spalling) 등을 유발하며, 이러한 마모들은 기어로부터 발생하는 진동 레벨을 상승시킨다. 본 연구에서는 스퍼 기어를 장착한 기어 박스를 이용한 실험적 연구를 통해 기어의 표면 피로 마모를 평가하기 위해 진동 신호로부터 구해진 통계적 변수들과 Stribeck Curve 와의 상관관계를 검증하였다.

누설 레일리 표면파를 이용한 TiN 코팅 부재의 특성평가 (Characterization of TiN Layered Substrate using Leaky Rayleigh Surface Wave)

  • 권성덕;김학준;송성진
    • 비파괴검사학회지
    • /
    • 제26권1호
    • /
    • pp.7-11
    • /
    • 2006
  • 기계부품의 세라믹 코팅 층은 사용 중 그 표면특성이 변하므로 잔류수명 예측과 신뢰성 확보를 위해 비파괴적으로 세라믹 코팅 층의 특성을 평가하는 것은 매우 중요하다. 이를 위해 본 인구는 AISI 1045 강과 오스테나이트 스테인리스 304 강 모재위에 매우 얇은 TiN 세라믹 층을 코팅한 시편에 내하여 누설 레일리(Rayleigh) 표면파를 이용한 TiN 코팅부재의 특성평가를 시도하였다. 후방복사 측정기법으로 코팅 층 내의 표면파의 전파특성이 평가되었고 표면 거칠기, 코팅 층 두께, 마모조긴 둥이 다양한 시편들에 대해 후방복사 프로파일이 측정되었다. 후방복사 프로파일의 정점각과 크기는 시편의 조건들에 따라 민감하게 변하였고, 정점각의 증가는 코팅 층 접합 강도의 저하로 설명되었다. 결과들은 후방복사 기법을 이용한 표면파의 분산성 평가가 코팅 층의 특성 평가에 매우 유용함을 보여주었다.