• Title/Summary/Keyword: 블라스트 표면처리

Search Result 11, Processing Time 0.024 seconds

Effect of Blast Cleaning on Fatigue Behavior of Non-load-carrying Fillet Welded Cruciform Joints (블라스트 표면처리가 하중비전달형 십자필렛 용접이음의 피로거동에 미치는 영향)

  • Kim, In Tae;Jung, Young Soo;Kim, Kwang Jin;Lee, Dong Uk
    • Journal of Korean Society of Steel Construction
    • /
    • v.21 no.1
    • /
    • pp.55-62
    • /
    • 2009
  • Blast cleaning has been applied in steel bridges for cleaning forged surface and increasing adhesive property of applied coating systems. Blasting is the operation of cleaning or preparing a surface by forcible propelling a stream of abrasive metals against it. Blast cleaning may improve surface geometry and induce compressive residual stress, and eventually may increase fatigue life of weld joints. In this paper, fatigue tests were carried out on three types of non-load-carrying fillet welded cruciform joints, as-welded joints, blast-treated joints, and stress-relieved joints after blasting, in order to investigate effect of blast cleaning on fatigue behavior of the weld joints. By Blast cleaning, the weld toe radius was increased by 29% and compressive residual stress was induced near weld toes. Blast cleaning increased fatigue life and fatigue endurance limit of the weld joints. When the applied stress ranges decreased, the increment in fatigue life became larger. About a 150% increase in fatigue limit could be realized by using blast cleaning.

Improving Fatigue Strength of Weld Joints by Blast Cleaning used in Painting Steel Bridge (강교 도장용 블라스트 표면처리에 의한 용접이음의 피로강도 향상)

  • Kim, In-Tae;Jung, Young-Soo;Lee, Dong-Uk
    • Journal of Korean Society of Steel Construction
    • /
    • v.23 no.2
    • /
    • pp.137-146
    • /
    • 2011
  • In the fabrication of steel bridges, blast cleaning prior to painting is carried out on the steel members to clean the forged surface and to increase the adhesive property of the applied painting systems. The effect of blast cleaning on the fatigue strength improvement of the weld joints, however, is not clear. In this study, Almen strips and steel specimens were blast-treated, conforming to ten types of blast-cleaning conditions deducted from the blast-cleaning conditions of seven steel structure fabrication companies. The arc height, roughness, hardness, and compressive residual stress were measured before and after the implementation of the ten blast-cleaning methods, and the relationship between the blast conditions and the measured values was studied. The geometry of the weld toe and the compressive residual stress near the weld toe were also measured before and after the blast cleaning of the butt-welded joints, and fatigue tests were carried out on the butt weld joints. The test results showed that blast cleaning significantly increases the fatigue strength and limit.

The Effect of Blast Cleaning for Steel Bridge Painting on Fatigue Behavior of Out-of-Plane Gusset Welded Joints (강교 도장용 블라스트 처리가 면외거셋 용접이음의 피로거동에 미치는 영향)

  • Kim, In Tae;Le, Van Phuoc Nhan;Kim, Kwang Jin;Lee, Dong Uk
    • Journal of Korean Society of Steel Construction
    • /
    • v.20 no.5
    • /
    • pp.583-590
    • /
    • 2008
  • Blasting has been applied in newly-built steel structures for cleaning forged surfaces and increasing the adhesive property of applied painting systems. However, the effect of the blast cleaning on fatigue behavior of welded joints is not clear. In this paper, fatigue tests were carried out on out-of-plane gusset welded joints and the effect of the blast cleaning on the fatigue behavior was studied. The curvature radius at the weld toe of the surface-treated specimens by using the blast method is larger than that of as-welded specimens. By the blast cleaning compressive residual stresses were induced into weld toes. The experimental results showed that the fatigue life of surface-treated specimens is longer than that of as-welded specimens, even though the fatigue life of surface-treated specimens and that of as-welded specimens are not clearly different in the high stress range. About a 160% increase in fatigue limit could be realized by using blast cleaning.

Improvement of Blast Efficiency by Correlation Analysis of Impella Blast and Steel Balls for Surface Treatment of Steel Bridges (강교 보수도장의 표면처리를 위한 임펠라 블라스트와 스틸볼의 상관관계 분석을 통한 블라스트 효율 향상)

  • Chang, Byoung Ha;Jang, Dong Wook;Seo, Myoung Kook;Lee, Ho Yeon;Park, Jae Hyun
    • Journal of Drive and Control
    • /
    • v.19 no.1
    • /
    • pp.8-15
    • /
    • 2022
  • The demand for the re-painting of steel bridges is increasing, but surface treatment is still centered on human resources for on-site re-painting processes. Worker safety accidents continue to occur because the work is performed in a narrow space. Recently, PS balls with excellent surface treatment have been used for blasting, but the working environment is poor due to the large amount of dust generated. In this study, an effective surface treatment method using impeller blasting equipment was developed. The correlation between steel ball size, impeller rotation speed, and exposure time was studied to optimize the efficiency of the surface treatment.

Increase heat dissipation efficiency of Al plate according to surface roughness treatment by sandpaper or sandblast (사포, 샌드블라스트로 표면 거칠기 처리에 따른 알루미늄 판의 방열 효율 증대)

  • Lee, Dong-Hee;Lee, Jong-Hyeon
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.20 no.1
    • /
    • pp.170-178
    • /
    • 2019
  • Recently, as the interest in energy savings has increased, there has been increasing use of LED lighting, which is an eco-friendly device that replaces high energy consuming fluorescent lamps and incandescent lamps. In the case of a high output LED, however, the life time is shortened due to deterioration caused by heat generation. As a solution to this problem, this paper evaluated the LED life extension effect by increasing the convective heat transfer coefficient of the heat sink surface for LED packaging. A roughing process was carried out using sandpaper and sand blasting. The changes in surface roughness and surface area after each surface treatment process were evaluated quantitatively and the convective heat transfer coefficient was measured. When sandblasting and sandpaper were used to roughen the aluminum surface, a higher convection heat transfer coefficient was obtained compared to the untreated case, and a high heat dissipation efficiency of 82.76% was obtained in the sandblast treatment. Therefore, it is expected that the application of heat dissipation to the heat sink will extend the lifetime of the LED significantly and economically by increasing the heat efficiency.

알루미늄 표면처리를 통한 발수 특성 개발

  • Byeon, Eun-Yeon;Lee, Seung-Hun;Kim, Jong-Guk;Kim, Yang-Do;Kim, Do-Geun
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2012.11a
    • /
    • pp.185-185
    • /
    • 2012
  • 최근 자연모사를 이용한 연구가 다양한 분야에 적용되고 있다. 특히 연 잎의 표면에서 나타나는 초발수 특성이 마이크로 나노 크기의 구조와 표면에너지를 제어하는 에피큐티클 왁스에 기인하다는 것이 밝혀지면서 이를 응용한 연구가 진행되고 있다. 본 연구는 알루미늄 표면처리로 마이크로와 나노 구조물을 형성하고 그 위에 발수 특성을 가진 물질을 증착하여, 발수성을 가지는 표면을 개발하였다. 알루미늄 표면에 마이크로 크기의 알루미나($Al_2O_3$) 분말을 이용한 블라스트(blast) 공정으로 표면에 마이크로 구조를 형성하고, Linear Ion Source(LIS)를 적용한 Ar 이온빔 에칭으로 나노 구조를 형성하였다. FE-SEM 분석을 통해 수~수십 마이크로 구조 위에 나노 크기의 구조가 형성 된 것을 관찰하였다. 마이크로 나노 구조가 형성된 알루미늄의 표면에너지를 낮추기 위해 trimethylsilane(TMS) 및 Ar을 이용한 플라즈마처리로 표면에 기능성 코팅막을 형성하였다. 그 결과 TMS 발수 코팅하기 전에 비해 표면에너지가 $99.75mJ/m^2$에서 $9.05mJ/m^2$으로 급격히 낮아지고 접촉각 값이 $123^{\circ}$로 향상된 것을 확인하였다.

  • PDF

연 잎 구조를 응용한 금속 표면의 발수 특성 개발

  • Byeon, Eun-Yeon;Lee, Seung-Hun;Kim, Jong-Guk;Kim, Yang-Do;Kim, Do-Geun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.167-167
    • /
    • 2013
  • 최근 발수 특성은 자동차 표면, 건축 구조물, 가전제품 및 모바일 기기 등 여러 분야에서 사용되고 점차 그 필요성이 대두되고 있다. 이러한 발수성의 표면은 연 잎이나 곤충의 날개, 도마뱀의 발바닥 등 자연계의 여러 곳에서 관찰 할 수 있다. 특히 연 잎의 표면에서 나타나는 초발수 특성이 마이크로와 나노 크기의 돌기 구조와 표피 왁스 성분에 기인한다는 것이 밝혀지면서 이를 응용한 다양한 연구가 진행되고 있다. 본 연구에서는 물리적인 표면처리로 마이크로와 나노 구조물을 형성하고 그 위에 표면에너지를 낮출 수 있는 물질을 증착하여, 발수 특성을 가지는 표면을 개발하였다. 알루미늄 표면에 마이크로 크기의 알루미나(Al2O3) 분말을 이용한 블라스트(blast) 공정으로 마이크로 구조를 형성하고, 선형 이온 소스(LIS)를 이용한 Ar 이온 빔 에칭으로 나노 구조를 형성하였다. FE-SEM 분석을 통해 수~수십 마이크로 구조 위에 나노 크기의 구조가 형성 된 것을 관찰하였다. 마이크로와 나노 구조가 형성된 알루미늄의 표면에너지를 낮추기 위해 trimethylsilane (TMS) 및 Ar을 이용한 플라즈마처리로 표면에 기능성 코팅막을 형성하였다. 그 결과 TMS처리 전에 비해 표면에너지가 99.75 mJ/m2에서 9.05 mJ/m2으로 급격히 낮아지고 접촉각이 $54^{\circ}$에서 $123^{\circ}$로 향상되었다.

  • PDF

An Evaluation of Slip Coefficient in High Strength Bolt Joint using Zn/Al Metal Spray Corrosion Resistance Method (Zn/Al 금속용사 방식공법을 적용한 고력볼트 접합부의 미끄럼계수 평가)

  • Kim, Tae-Soo;Lee, Han-Seung;Tae, Sung-Ho;Ahn, Hyun-Jin;Oh, Sang-Hoon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.11 no.5
    • /
    • pp.114-122
    • /
    • 2007
  • In high strength bolted joints, the corrosion of base material causes the reduction of slip resistance of the joints. In this study, tensile tests on slip-critical joints utilizing Zn/Al metal spraying corrosion resistance method were carried out in order to prevent the corrosion and meet the required mechanical characteristics of joints. In addition, slip coefficient and surface roughness were calculated. The key parameters were surface finishing condition and thickness of coating with the identical geometry in all specimens. From the results, it is found that the slip coefficient of the joints with coated finish after sand blast treatment as well as those of non-coated joints with only sand blast treatment were similar or superior to 0.45, which is a specification criteria of slip coefficient in friction-typed joints.

Evaluation of Deterioration Propagation Life of Steel Bridge Paints According to Surface Treatment Methods and Heavy-Duty Painting Types (표면처리방법에 따른 강교용 일반중방식도장계의 열화진행수명 평가)

  • Kim, Gi-Hyeok;Jeong, Young-Soo;Ahn, Jin-Hee;Kim, In-Tae
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.25 no.1
    • /
    • pp.75-84
    • /
    • 2021
  • In this study, to evaluate deterioration propagation life and deterioration curve of the shop painted and field re-painted steel bridges, accelerated corrosion tests were carried out on 4 types of heavy-duty painting systems with different surface treatments. The surface treatments prior to painting were examined by hand tool(SSPC SP-2), power tool(SP-3,) or blast cleaning(SP-10) considering shop painting and field re-painting. The paint deterioration curves for each painting system and surface treatment were evaluated based on corrosion propagation from the initial paint defects. From the test results, the paint deterioration life of shop painted and field re-painted system was evaluated and compared by using corrosivity categories and durability performance evaluation of structural steel. The deterioration propagation life of shop and field paint was estimated in 18 to 21 years and 5.3 to 8.0 years with atmospheric corrosion category C4.

Cavitation Erosion Behavior in Seawater of Shot Peened Gray Cast Iron (쇼트피닝 처리된 회주철의 해수 내 캐비테이션 침식 손상 거동)

  • Park, Il-Cho;Kim, Seong-Jong
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.111-111
    • /
    • 2017
  • 쇼트피닝 기술은 크게 피로강도 향상을 위한 쇼트피닝(shot peening), 재료의 청정 및 도장 품질 향상을 위한 쇼트블라스트(shot blast) 그리고 쇼트피닝 시 판재의 변형되는 성질을 이용한 핀포밍(peen forming) 등으로 구분할 수 있다. 그 중 본 연구에서는 해양산업 분야에서 널리 사용되는 회주철의 효과적인 내구성 향상을 위해 쇼트피닝 기술을 적용하였다. 그러나 쇼트피닝 기술 적용에 있어서 가장 중요한 것은 제품의 균일성, 정확성, 신뢰성을 확보하기 위해 쇼트피닝 강도를 제어하는 여러 가지 변수들에 대하여 최적 상태를 유지하는 것이다. 따라서 회주철에 대한 최적 쇼트피닝 분사조건 규명작업은 반드시 쇼트피닝 가공 전에 수반되어야만 한다. 그 일환으로 실험은 쇼트피닝 분사시간과 분사압력을 변수로 하여 회주철 표면에 적용하였으며, 기계적 특성 평가를 통해 최적의 쇼트피닝 조건을 규명하고자 하였다. 쇼트피닝 분사조건에 따른 회주철의 내구성을 평가하기 위해 캐비테이션 실험을 실시하였으며, 경도 측정, 횡단면 관찰 및 표면의 3D 현미경 관찰 등을 통해 기계적 특성을 분석하였다. 캐비테이션 실험은 ASTM G32 규정에 의거하여 천연해수 내 $30^{\circ}C$에서 $50{\mu}m$의 진폭으로 실시하였다. 실험 후에는 주사전자현미경으로 손상표면을 관찰하였으며, 손상 정도를 비교하기 위해 무게 감소량을 계측하여 상호 비교/분석하였다.

  • PDF