• Title/Summary/Keyword: 불소수지

Search Result 45, Processing Time 0.035 seconds

Radiation-Induced Graft Copolymerization of 2-hydroxyethyl-methacrylate and Styrene onto Polytetrafluoroethylene (불소수지 필름에 2-Hydroxyethyl methacrylate와 스틸렌의 방사선 그라프트 공중합)

  • Nho, Young-Chang;Garnett, J.L.;Dworjanyn, P.A.;Jin, Joon-Ha
    • Applied Chemistry for Engineering
    • /
    • v.3 no.3
    • /
    • pp.491-498
    • /
    • 1992
  • Graft polymerization of 2-hydroxyethyl methacrylate(HEMA) and styrene, from both their binary and unitary systems, onto polytetrafluoroethylene(PTFE) film was investigated by means of the simultaneous ${\gamma}-ray$ induced method. The effect of various parameters such as monomer concentration, dose rate, absorbed dose, HEMA/styrene feed ratios and the type of diluent on the extent of grafting in unitary and binary systems was studied. It was observed that when unitary HEMA was used for grafting, the grafting extent was very slight, whereas when comonomers were used, a good grafting yield could be obtained. Inclusion of sulfuric acid in the monomer solution resulted in enhanced grafting yields.

  • PDF

Investigation into the Thermal Stability of Fluoropolymer Coating for Heat-Resistant Application (내열성 불소수지 코팅막의 열 안정성에 관한 연구)

  • Cho, Hey-Jin;Ryu, Ju-Hwan;Byun, Doo-Jin;Choi, Kil-Yeong
    • Polymer(Korea)
    • /
    • v.29 no.1
    • /
    • pp.96-101
    • /
    • 2005
  • Fluoropolymer of PTFE and PFA etc. is a heat resistance polymeric material that it is known as that maximum continuous use temperature reaches for 260 $^{\circ}C$. It was observed that these polymers had the enough thermal stability so enough that it was kept by thermal aging of 280 $^{\circ}C$/7 weeks too in this study. However, such thermal stability means that bulk material property is kept such as mechanical strength, melting point and initial pyrolysis temperature etc. If these polymers are evaluate by coating property such as surface contact angle, surface morphology, surface scratch, thing that heat resistance is not enough was confirmed in this study. Thermal aging of flouropolymer coating was achieved by gear aging oven that the exchange rate of air was controlled, and the analysis results were indicating serious damage of surface morphology and adhesive strength on metal substrate.

Surface Modification of Poly(tetrafluoroethylene) (PTFE) Membranes (PTFE 막의 표면 개질 방법)

  • Jun Kyu Jang;Chaewon Youn;Ho Bum Park
    • Membrane Journal
    • /
    • v.33 no.1
    • /
    • pp.1-12
    • /
    • 2023
  • In this review, surface modification methods of hydrophobic poly(tetrafluoroethylene) (PTFE) membrane are introduced and their improved hydrophilicity results are discussed. Fluoropolymer based membranes, represented by PTFE membranes have been used in various membrane separation processes, including membrane distillation, oil separation and gas separation. However, despite excellent physical properties such as chemical resistance, heat resistance and high mechanical strength, the strong hydrophobicity of PTFE membrane surface has become a challenging factor in expanding its membrane separation application. To improve the separation performance of PTFE membranes, wet chemical, hydrophilic coating, plasma, irradiation and atomic layer deposition are applied, modifying the surface property of PTFE membranes while maintaining their inherent properties.

Influence of usage environment from camping cooking utensils on migration of hazardous metals (사용 환경에 따른 캠핑용 조리 기구로부터 유해금속 용출의 변화)

  • Lee, Jin-hee;Kim, Ji-Yeon;Park, Ye-Seul;Park, Sang-Gyu;Lee, Jae-Ho;Yoon, Jong-Ho;Kim, Gyung-Tae;Han, Gi-Dong
    • Food Science and Preservation
    • /
    • v.24 no.8
    • /
    • pp.1094-1102
    • /
    • 2017
  • Hazardous metals leaching experiment was carried out in accordance with various usage environments for camping cooking utensils distributed in the market. There was a significant difference in the degree of migration for lead, arsenic, cadmium and nickel defending on the solvent and how to use, although they were all appropriate for criteria. In general, the migrated amount of aluminum was increased in acidic condition, and the migrated amount of arsenic was increased in salty condition. Physical scratches increased the overall release of hazardous metals from the portable pots and pans for camping in all solvents. Especially, in 0.5% citric acid solution, cadmium was migrated by physical scratch in stainless steel and hard aluminum pots and pans. The longer the leaching time, the higher the migration of aluminum in acid condition and arsenic in basic condition. From these results, it is desirable to use the cooking utensil for camping without being exposed to strong acidic or basic solution and scratches in order to reduce the migration of hazardous metals from them.

다양한 흡착제에 의한 지하수 중의 불소제거 특성

  • Park, Hyeon-Ju;Jeong, Jin-Hwa;Song, Myeong-Gi;Na, Chun-Gi
    • Proceedings of the Korean Environmental Sciences Society Conference
    • /
    • 2008.11a
    • /
    • pp.423-427
    • /
    • 2008
  • 지하수 중에 함유된 불소이온을 제거하기 위한 흡착제로 상용의 음이온교환수지(PA), 란탄산화물(La) 및 수산화아파타이트(HAp)를 선정하고 각각의 흡착특성을 회분식 실험을 통해 검토하였다. 그 결과를 요약하면 다음과 같다. 1) PA, La 및 HAp의 불소흡착은 Fruendlich isodtherm model 및 Pseudo-second-order kinetics model과 일치하는 거동을 보였다. 2) D-R model로부터 구한 흡착에너지는 9.66$\sim$12.90 kJ/mol로 이온교환메커니즘을 나타내는 흡착에너지 6$\sim$16 kJ/mol의 범위에 속하였다. 3) Van't Hoff 식에 이용하여 구한 ${\Delta}H^{\circ}$${\Delta}G^{\circ}$값은 각각 3.40$\sim$89.28 kJ/mol과 -12.26$\sim$-13.76 kJ/mol의 범위를 보여 모두 흡착과정이 발열반응이며 자발적으로 일어나는 조건임을 알 수 있었다. 4) PA는 pH 6$\sim$8인 중성영역에서 가장 높은 불소 제거율을 보였으며, La과 HAp는 산성영역으로 갈수록 불소 제거율이 증가하는 특성을 나타내었다. 5) 불소에 대한 흡착선택성은 La$\geq$HAp>PA 순으로 높았으며, La의 경우 불소를 제외한 모든 음이온에 대한 흡착능이 없을 정도로 불소에 대한 흡착 특이성을 보였다.

  • PDF

A Study on the Tribological Characteristics of a Frying Pan Coated with PTFE and Nano-Diamond (나노다이아몬드가 첨가된 프라이팬 불소수지코팅의 Tribological 특성 연구)

  • Lee, Jin-Ho;Kim, Hyun-Soo;Yoon, Han-Ki;Kim, Tae-Gyu
    • Journal of Ocean Engineering and Technology
    • /
    • v.23 no.6
    • /
    • pp.99-104
    • /
    • 2009
  • PTFE has good mechanical and chemical stability at a wide range of temperatures and demonstrates a low friction coefficient value. PTFE is being used for self-lubricating parts in industry. But it shows a high wear rate. Thus, PTFE and nano-diamond powder were mixed into a composite and the wear properties of a PTFE coating layer on Al6061 was investigated. A ball-on-disk type of wear tester was used under a dry condition and different temperatures of oil. After the wear test, the wear track wasexamined by optical microscope. The PTFE-diamond showed the lowest friction coefficient (0.02) of all the lubricants in the experiments. The friction coefficient was shown to be directly related to the diamond powder in the PTFE coating. Adhesion estimations were performed by a scratch test, which is mainly used for coatings. The critical load between the coating and substrate was defined through analyses of the friction load, normal load curve, and acoustic emissions, along with optical microscope observations. The scratch test results showed that an import item (SWISS) gave the highest critical load values.