Cho, Chul-Min;Kim, Jang Jay Ho;Lee, Doo-Sung;Kim, Tae-Kyun
Journal of the Korea institute for structural maintenance and inspection
/
v.21
no.3
/
pp.1-8
/
2017
An experimental study is needed a reinforcing method for seismic load to apply for RC structures because a lot of earthquakes have frequently happened in the world and those also collapsed infrastructures or damaged human lives. The reinforcing effect of PolyUrea (PU) appeared to be excellent under blast and impact about RC structures. In this study, Stiff Type PolyUrea (STPU) had developed by manipulating the ratio of the components of prepolymer and hardener of PU. And the durability performance evaluation of STPU for deterioration and chemical resistance has been performed. Acid environmental exposure test and ultraviolet (UV) exposure test have been performed as the durability performance evaluation for STPU. Concrete carbonation exposure test and freezing and thawing test for concrete coated with STPU have been performed. The experimental result showed that STPU has high resisting capacity and durability in all tests. Therefore, STPU would be used as seismic reinforcement materials.
Journal of the Korea institute for structural maintenance and inspection
/
v.17
no.6
/
pp.145-152
/
2013
As a typical construction material, concrete has been used in building all kinds of structures since the late $19^{th}$ century. Although it was recognized to secure durability as long as the regulations on design and construction have been reasonably complied, the trends of life-shortening and deterioration have frequently occurred due to all kinds of the external effects that have been experienced during the procedures of using the structures. To make matters even worse, deterioration of the concrete structures according to deterioration can not be controlled any more. Finally, the reality is that repair and maintenance are necessary in the maintenance aspect of the concrete structure. In this study, CRM(Chemical Resistance of Laminating Reinforcement Method), which had been developed to reinforce the surface of concrete and specially improve chemical resistance performance, has been applied to enhance the existing repairing and maintenance method. Therefore, the result has been drawn with comparison and analysis of the specimens applied with the general repairing and maintenance method and CRM through a variety of durability test in this study. With the result of the test, durability of the specimen applied with CRM has been more improved than the existing repairing and maintenance method, which is judged as because of the laminating effect due to reinforcement of epoxy impregnated of alkali-resistance fiber and double layered fiber reinforced seat.
Journal of the Korea Academia-Industrial cooperation Society
/
v.18
no.11
/
pp.130-137
/
2017
To maintain traffic safety during the target lifetime of bridges, it is essential to secure an appropriate maintenance budget and allocate that budget appropriately. This paper proposes a reasonable budget allocation system that considers various impact factors to improve the conventional budget allocation method simply considering the bridge scale. The maintenance action rate model and the unit cost model based on the prior maintenance history were developed to allocate appropriately the bridge maintenance budget for the total bridges of the management organization with the target management level. A method to determine the optimal budget allocation ratio for each management subject was proposed and case analysis was conducted using the proposed model. Proper budget allocation was made considering the bridge types, current safety level, and service life as well as the bridge size as an impact factor of the budget allocation of the bridge. The developed method can prevent budget waste and provide a rational basis for budget allocation by implementing the rational budget distribution.
최근 강구조물의 건설이 지속적으로 증가되어 왔다. 또한 강구조물의 유지관리 및 안전성에 대한 관심이 급증하고 있다. 시설물의 안전성 확보는 대형사고의 사전 예방, 공용 중 갑작스런 가동 중지에 의하여 발생되는 비용증가를 사전에 차단 할 수 있다는 점에서 그 중요성은 매우 크다고 할 수 있다. 또한 각종 구조물은 열악한 사용조건, 고온, 고압, 고속, 대형화됨에 따라 일단 사고가 발생 했을 경우 대형사고의 위험이 예상되므로, 제작시 검사의 강화뿐만이 아니라 공용 중 구조물의 안전성을 진단 할 수 있는 모니터링 체계의 확립이 필요한 시점이다. 현재 국내에서 강구조물들의 균열 모니터링 시스템에 관한 연구는 매우 미흡한 실정이며, 현재 사용되고 있는 비파괴검사 방법은 UT와 RT등이다. 이러한 방법들은 많은 시간과 경비가 소요되며 또한 거대구조물 혹은 사람의 접근이 어려운 곳에는 적용하기가 힘들다. 또한 주기적인 검사 작업으로 인한 막대한 시간과 비용의 손실이 발생되고 있으며 초기 결함을 조기에 인지하지 못함으로써 적절한 보수 보강 대책이 이루어지지 않아 보수 보강 비용의 증대를 초래한다. 더욱이, 결함이 진전된 이후에도 이것을 인지하지 못하여 적절한 대응을 하지 않는다면 대형사고로 이어질 수도 있다. 따라서 강구조물에 대한 효율적인 유지관리가 가능하고, 초기결함으로부터 균열이 진전하여 붕괴되는 사고를 미연에 방지하며 초기에 보수보강 작업을 수행함으로써 보수보강 비용도 절감 할 수 있는 모니터링 시스템의 개발이 요구되고 있다. 이러한 모니터링 시스템의 개발은 기술적 측면에서 강구조물의 효율적인 유지 관리 노하우를 얻을 수 있으며 경제 산업적 측면에서는 보수 보강 비용 및 불필요한 주기적 점검 비용을 절감 할 수 있다. 이 연구에서는 전위차법을 이용하여 강구조물의 필렛 용접부에서의 균열진전양상을 파악하고 정량화를 통해 필렛용접부의 잔여수명을 예측하였다.
This paper presents experimental investigations about compressive strength and durability of reinforced concrete compressive members repaired using ductile fiber reinforced cementitious composite (DFRCC) and carbon fiber sheet through freezing and thawing test. Total 24 RC specimens of 100x100x400mm size were tested by compressive strength test and freezing and thawing test by KS F 2456. The specimens were reinforced using 4D10 steels and repaired on 4 sides expect on top cycle. Test results showed that the specimens repaired using fiber carbon sheet revealed about 5% higher values of the compressive strength compared than the cases of DFRCC motar. On the other hand, the resurts did not showed meaningful differences in the aspect of durability. For further research, considerations of the steel interference effect and real old specimens such as taken from real deteriorated structures are needed to be tested after repairing with DFRCC and carbon fiber sheet.
This paper presents experimental investigations about flexural strength and durability of reinforced concrete beams repaired using ductile fiber reinforced cementitious composite (DFRCC) and carbon fiber sheet through freezing and thawing test. Total 14 RC beams of $100{\times}100{\times}400mm$ size were tested by 3-point bending and freezing and thawing test by KS F 2456. The beams were reinforced using 3D10 steels on both the tensile and compressive sides, and repaired on 3 sides expect on top cycle. Test results showed that the beams repaired using fiber carbon sheet revealed about 15% higher values of flexural strength compared than the cases of DFRCC motar. On the other hand, the results did not showed meaningful differences in the aspect of durability. For further research, consideration of the steel interference effect and real old specimens such as taken from real deteriorated structures are needed to be tested after repairing with DFRCC and carbon fiber sheet.
Even though the cost associated with the repair and rehabilitation of existing structures are rapidly increasing, vast number of the repaired and rehabilitated structures do not function properly as expected during their remaining service lives. This paper focused on the flexural behavior of reinforced concrete slabs repaired and reinforced by PS strand and polymer mortar in the tension face. The slabs have the size of 700${\times}120{\times}$2200 m and 700${\times}120{\times}$1300 mm. Variables of experiment were space of strengthening, chipping, the number of strand, the kind of mortar in this experimental study. Attention is concentrated upon overall bending capacity, deflection, ductility and failure mode of repaired and reinforced slabs. Test results show that deflection of repaired and reinforced slabs reduced to approximately $40 \%$ comparison to standard slabs. Boundary cracking of chipping slab started ultimate load afterward. Concrete-mortar interface cracked 64.5 kN in repaired slab with AP mortar and 36.0 kN in repaired slab with general polymer mortar. Reinforcement effect increased with reducing space of strand. Also, Reinforcement effects are more by strand than by polymer mortar.
Journal of the Korea institute for structural maintenance and inspection
/
v.10
no.1
/
pp.183-189
/
2006
When RC structures are repaired or strengthened using FRP, it is required to cure for some Period under certain air temperature and then it is hopeful to avoid detrimental action caused by external vibration sources during that period. Therefore, an effect of repeated loading during Carbon Fiber Sheet(CFS) strengthening Process on the strengthening efficiency is studied through an experiment for a number of RC beams. Experimental results showed that the curing time of 24 hours without any repeated loading after CFS attachment were recommended for 1 ply strengthening, and 12 hours for 2 plies strengthening.
Journal of the Korea institute for structural maintenance and inspection
/
v.13
no.6
s.58
/
pp.115-125
/
2009
In these days, carbon fiber-reinforced polymers (CFRP) have been widely used for retrofitting and/or strengthening structural elements. However, there are not enough test data to predict the long-term performance of the retrofitted structures exposed to freeze-thawing cycles. This paper presents the results of experimental program undertaken to investigate the effects of freeze-thawing cycling (from-18 to $4^{\circ}C) on the behavior and failure characteristics of reinforced concrete (RC) beams strengthened in shear with CFRP sheet and plate using acoustic emission (AE) technique.
Journal of the Korea institute for structural maintenance and inspection
/
v.18
no.4
/
pp.50-58
/
2014
Due to the cost burden of new construction, the necessity of repair and retrofitting of aged structures is sharply increasing as the domain of repair and retrofitting construction is expanding. Because of the necessity, new technologies for repair and retrofitting are continuously studied in Korea and foreign countries. Steel adhesive method, fiber reinforced plastic (FRP) surface adhesive method, and external prestressing method are used to perform the repair and retrofitting works in Korea. In order to consider a repair method using steel mesh reinforced cement mortar (SMCM), 3-point flexural member test was conducted considering repair area and layer number of SMCM. Five types of specimens including ordinary reinforced concrete (RC) specimen with dimensions of $1400{\times}500{\times}200$ (mm) were cast for testing the deflection measurement, a LVDT was installed at the top center of the specimens. Also, a steel strain gauge and a concrete strain gauge were placed at the center of the specimens. A steel strain gauge was also installed on the shear reinforcement. The 3 point flexural member test results showed that the maximum load of SMCM reinforced specimen was higher than that of basic RC specimen in all of the load-displacement curves. Also, the results showed that, when the whole lower part of the basic RC specimen was reinforced, the maximum load and strain were 1.18 and 1.37 times higher than that of the basic RC specimen, respectively. Each specimen showed a slightly different failure behavior where the difference of the results was caused by the difference in the adhesive level between SMCM and RC. Particularly, in SM-B1 specimen, SMCM spalled off during the experiment. This failure behavior showed that the adhesive performance for RC must be improved in order to utilize SMCM as repair and retrofitting material.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.