  • In this paper, fatigue tests were carried out at stress test levels of 461 MPa, 441 MPa, and 431 MPa by using smooth specimen of$2_{1/4}$ Cr-1 Mo steel with the stress ratio(R) of 0.05. The initiation, growth and coalescense process of the major cracks and sub-cracks among the fatigue cracks on the smooth specimen are investigated and measured under each stress level at a constant cycle ratio by the replica technique with optical microscope. Some of the important results are as follows: In spite of the difference of stress levels, the major crack data gather into a small band in the curve of surface crack length and crack depth against cycle ratio N/Nf. The sub-crack data, however, deviate from the band of the major crack. The growth rates, da/dN, of major and sub-crack plotted against the stress intensity factor range, ${\Delta}K$, have the tendency to be compressed on a relatively small band. But it is more effective to predict fatigue life through major cracks. The propagation behavior of surface microcracks on the smooth specimens coincides with that of the specimen having an artificial small surface defect or through crack.

  • PDF

$2_{1/4}$ Cr-1 Mo강의 평활재상의 미소한 표면피로균열의 성장특성 (Propagation Characteristics of Fatigue Microcracks on Smooth Specimen of $2_{1/4}$ Cr-1 Mo Steel)

  • 서창민;우병철;장희락
    • 한국해양공학회지
    • /
    • 제4권2호
    • /
    • pp.250-250
    • /
    • 1990
  • In this paper, fatigue tests were carried out at stress test levels of 461 MPa, 441 MPa, and 431 MPa by using smooth specimen of$2_{1/4}$ Cr-1 Mo steel with the stress ratio(R) of 0.05. The initiation, growth and coalescense process of the major cracks and sub-cracks among the fatigue cracks on the smooth specimen are investigated and measured under each stress level at a constant cycle ratio by the replica technique with optical microscope. Some of the important results are as follows: In spite of the difference of stress levels, the major crack data gather into a small band in the curve of surface crack length and crack depth against cycle ratio N/Nf. The sub-crack data, however, deviate from the band of the major crack. The growth rates, da/dN, of major and sub-crack plotted against the stress intensity factor range, ${\Delta}K$, have the tendency to be compressed on a relatively small band. But it is more effective to predict fatigue life through major cracks. The propagation behavior of surface microcracks on the smooth specimens coincides with that of the specimen having an artificial small surface defect or through crack.

시간과 공간적 특성에 따른 축구 패스 성공률 분석: 2018 러시아 월드컵 대회 자료를 중심으로 (Influences on Time and Spatial Characteristics of Soccer Pass Success Rate: A Case Study of the 2018 World Cup in Russia)

  • 이승훈;김영훈
    • 디지털융복합연구
    • /
    • 제19권1호
    • /
    • pp.475-483
    • /
    • 2021
  • 이 연구는 2018 FIFA 러시아 월드컵 영상자료에서 수집한 2차 가공 데이터와 공식기록을 비교 및 활용하여 패스 정확도의 시간적, 공간적 특성을 규명 하는데 목적이 있었다. 이를 위해 총 128경기를 대상으로 경기결과, 패스 시간, 패스 위치에 따른 패스성공률을 반복측정 이원변량분석을 활용해 검증했다. 연구결과 승패 집단 간 패스성공률의 차이는 나타나지 않았으며, 패스시간 및 위치에 대한 상호작용효과도 발견되지 않았다. 패스시간에 따른 패스성공률은 전반전이 후반전에 비해 높게나왔으며, 15~30분 지점인 전반 중반(79.2%)과 60~75분 지점인 후반 중반(77.9%)에서 가장 높은 성공률을 보였다. 패스지역에 따른 패스성공률은 수비-미드필드지역(83.9%), 미드필드-공격지역(81.7%), 수비지역(70.6%), 공격지역(61.1%)순으로 나타났다. 결론적으로 월드컵 경기의 상대적 경쟁의 강도가 높은 특성에 따라 승패 팀의 패스성공률의 차이가 나타나지 않았다고 판단되며, 향후 다양한 매개변수를 적용해 승패 요소 보다는 경기내용 자체를 분석하기 위한 후속 연구가 필요하다.