  • In this paper, fatigue tests were carried out at stress test levels of 461 MPa, 441 MPa, and 431 MPa by using smooth specimen of$2_{1/4}$ Cr-1 Mo steel with the stress ratio(R) of 0.05. The initiation, growth and coalescense process of the major cracks and sub-cracks among the fatigue cracks on the smooth specimen are investigated and measured under each stress level at a constant cycle ratio by the replica technique with optical microscope. Some of the important results are as follows: In spite of the difference of stress levels, the major crack data gather into a small band in the curve of surface crack length and crack depth against cycle ratio N/Nf. The sub-crack data, however, deviate from the band of the major crack. The growth rates, da/dN, of major and sub-crack plotted against the stress intensity factor range, ${\Delta}K$, have the tendency to be compressed on a relatively small band. But it is more effective to predict fatigue life through major cracks. The propagation behavior of surface microcracks on the smooth specimens coincides with that of the specimen having an artificial small surface defect or through crack.

  • PDF

Propagation Characteristics of Fatigue Microcracks on Smooth Specimen of $2_{1/4}$ Cr-1 Mo Steel ($2_{1/4}$ Cr-1 Mo강의 평활재상의 미소한 표면피로균열의 성장특성)

  • Suh, Chang-Min;Woo, Byung-Chul;Jang, Hui-Rak
    • Journal of Ocean Engineering and Technology
    • /
    • v.4 no.2
    • /
    • pp.250-250
    • /
    • 1990
  • In this paper, fatigue tests were carried out at stress test levels of 461 MPa, 441 MPa, and 431 MPa by using smooth specimen of$2_{1/4}$ Cr-1 Mo steel with the stress ratio(R) of 0.05. The initiation, growth and coalescense process of the major cracks and sub-cracks among the fatigue cracks on the smooth specimen are investigated and measured under each stress level at a constant cycle ratio by the replica technique with optical microscope. Some of the important results are as follows: In spite of the difference of stress levels, the major crack data gather into a small band in the curve of surface crack length and crack depth against cycle ratio N/Nf. The sub-crack data, however, deviate from the band of the major crack. The growth rates, da/dN, of major and sub-crack plotted against the stress intensity factor range, ${\Delta}K$, have the tendency to be compressed on a relatively small band. But it is more effective to predict fatigue life through major cracks. The propagation behavior of surface microcracks on the smooth specimens coincides with that of the specimen having an artificial small surface defect or through crack.

Influences on Time and Spatial Characteristics of Soccer Pass Success Rate: A Case Study of the 2018 World Cup in Russia (시간과 공간적 특성에 따른 축구 패스 성공률 분석: 2018 러시아 월드컵 대회 자료를 중심으로)

  • Lee, Seung-Hun;Kim, Young-Hoon
    • Journal of Digital Convergence
    • /
    • v.19 no.1
    • /
    • pp.475-483
    • /
    • 2021
  • The purpose of this study is to identify the temporal and spatial characteristics of pass accuracy by utilizing the second processing data and official records collected from the 2018 FIFA World Cup Russia video data. For a total of 128 games, the success rate of passes based on the results of the game, passing time, and passing position was two-way ANOVA with repeated measure. The results showed no difference between winning and losing groups, and no interaction effects were found for passing time and location. The difference in passing time was high in the first half, with the highest success rate in the middle of the first half (79.2%) and the middle of the second half (77.9%) in the 15~30 minutes and the 60~75 minutes. Pass success rates were in the order of defense-midfield area (83.9%), midfield-attack area (81.7%), defense area (70.6%) and attack area (61.1%). In conclusion, there was no difference in the passing success rate of the winning and losing teams depending on the characteristics of the relative competitive strength of the World Cup games, and it is believed that follow-up research is needed to analyze the game contents rather than the factors of the winning and losing in the future.