필렛용접에서의 결함발생 원인 분석 및 저감 방안 (An Analysis of the Cause of Porosity Generation and Reduction Plan in Fillet Welding)

  • 최기영;김영필;김경주;김대순;배상득
    • 대한조선학회 특별논문집
    • /
    • 대한조선학회 2006년도 특별논문집
    • /
    • pp.128-133
    • /
    • 2006
  • Generally, porosity which was formed by pyrolysis of the primer is usually generated in the weld metal in respect of increase of the welding speed. in order to analyze the cause of porosity generation, this study was performed using FCAW(flux cored arc welding) process for three kinds of inorganic.zinc primer. in addition the evaluation by influence of welding method on porosity generation is conducted to compare between FCAW and MAG(metal active gas) welding with the same inorganic zinc primer. As the result of this investigation, not only primer of lower organic binder and zinc but also FCAW process than MAG in fillet welding have been verified the excellent resistance to the porosity generation for horizontal fillet welding.

  • PDF

미끄럼 표면 도막두께변수에 따른 고력볼트 장기축력 예측 (Estimation of Long Term Clamping Force of High Strength Bolts By Coating Thickness Parameters of Slip Faying Surfaces)

  • 나환선;이현주;류재용;최성모
    • 복합신소재구조학회 논문집
    • /
    • 제3권1호
    • /
    • pp.8-15
    • /
    • 2012
  • 고력볼트의 초기 체결력은 미끄럼표면조건에 따라, 일정시간이 경과될 때까지, 축력저하가 발생한다. 이 연구는 미끄럼접합부 표면에 도장이 되어있는 경우, 도장의 크리프현상에 따른 축력저하에 관한 예측 모델을 찾는 것이다. 이 실험연구 범위는 무기질 아연 프라이머로 도포된 볼트접합부의 장기축력저하에 한정한다. 실험에 적용된 볼트종류는 다크로 도포된 토크쉬어 볼트이다. 대상 표면의 도막 두께는 각각 96, 168, $226{\mu}m$ 이었다. 도막두께가 증가될수록, 초기 체결이후 축력이완율은 도막의 크리프 때문에 10%에서 18%로 증가되었다. 장기축력예측을 위한 정량적인 모델은 도막두께에 따른 크리프 스트레인과 경과된 시간사이에 회귀분석 결과로 얻어진다. 이 실험연구를 통해 미끄럼표면 도막의 크리프 거동특성을 알 수 있다면, 일정시간 경과후 고력볼트 체결력은 초기 체결력으로부터 구할 수 있다. 본 실험결과를 근거로 각 도막두께에 대한 장기축력이완이후의 고력볼트 체결력에 관한 정량적인 수식을 제안하였다.