Search Result 293, Processing Time 0.026 seconds

Evaluation of Residual Stress on Pipe Welded Joints Using Laser Interferometry (레이저 간섭계를 이용한 배관 용접부 잔류응력 평가)

  • Chang, Ho-Seob;Na, Man-Gyun;Kim, Koung-Suk
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.34 no.1
    • /
    • pp.18-22
    • /
    • 2014
  • Residual stresses that occur during the welding process, are the main cause of failure and defects in welded structures. This paper, presents the use of an electronic processing laser speckle interferometer to measure the residual stress of a welded pipe for a nuclear power plant. A tensile testing machine was used to evaluate a welded pipe that failed in compression. The inform plane deformation and modulus of elasticity of the base metal and welds were measured using an interferometer. Varying the load on the welded pipe had a larger effect on the deformation of the base metal the other properties of the base metal and welds. The elastic moduli of the base metal and weld of the welded pipe were 202.46 and 212.14 GPa, respectively, the residual stress was measured to be 6.29 MPa.

Trend of the welding technology for surface modification (표면개질을 위한 오버레이용접 기술개발 현황)

  • 백응률
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 1998.11a
    • /
    • pp.19-20
    • /
    • 1998
  • 오버레이용접에 의한 표면개질기술(Weld Surfacing or Hardfacing Technology)은 내식성, 내 마모성, 또는 내열성을 갖는 합금의 용접재료를 모재 표면에 균일하게 용착(오버레이:Ovedayer)시킴으로써 목적하는 재료의 표면성질을 향상시키는 표면처리의 한 방법이으로써 1922년 Stoody가 Steel Tube에 Cr합금 분말을 충진한 용접봉을 제조하여 석유시추용 회전드릴의 선단 표면을 오버 레이 용접시켜 내마모성을 획기적으로 개선시킴으로써 이루어 졌다. 초기 오버레이 용접기술은 발전설비I 제철설비I 시벤트설비, 그리고 제지설비 등 주로 설비 부품들의 표면부 내마모성을 개선시키는 방향으로 주로 연구 개발이 이루어졌으나, 기술개발의 진전으로 탈황설비 둥의 표면부 내식성 향상, 연속주조롤 표면부의 내산화성, 내열피로성, 내마모 성 향상 둥을 위해 점차 산업전반에 널리 이용되고 있으며, 설비의 고도화 및 장수명화가 요구되 면서 본 기술의 중요성 또한 점차 부각되고 있다. 그림 1은 연강의 모재 위에 셀프쉴드플럭스코어드와이어(Self-Shield Flux Cored Wire:SS-FCW, 이하 55-FCW라 기술함)를 사용하여 오버레이 용접올 하는 장면을 도식적으로 나 타낸 것이다. 모재와 전극재인 용접봉(S5-FCW) 사이에서 아크가 발생되고, 아크열에 의해서 용접 봉 및 모재 일부가 용융되면서 모재 표면에 새로운 오버레이 표면층이 형성된다. 통상 오버레이 층의 1층 두께는 2-6mm 내외이며, 단층 혹은 다충 오버레이를 자유롭게 실시한다. 오버레이층의 물성은 아크열에 의한 모재로의 용입정도에 따라 1층부에서는 모재의 영향을 크게 받지만 오버레 이충 수가 증가된 3층부에서 부터는 전적으로 용접봉의 성분에 좌우된다. 사진 1은 연강(55-41)의 모재위에 크롬탄화물이 다량 함유된 고크롬 탄화물형 내마모재가 오버 레이된 내마모 복합강판 (wear plate)의 단면 미세조직 사진으로써 모재부와 오버레이충을 함께 보여주고 있다. 모재와 오버레이 충간의 경계면은 모재 일부가 용융된 후 웅고하면서 형성됨으로 인해서 도금이나 용사층과는 달리 매우 견고하게 결합되어 있다. 따라서 계면부의 탈락이라는 문 제점은 거의 없어 심한 응력을 받는 기계구조물 및 부품에도 본 기술은 널리 적용되고 있다. 그리고 사진 1에서 알 수 있는 바와 같이 모재와는 전혀 상이한 재료를 자유로이 선택하여 표면 유효층 일부만 오버레이시키며I 주조 및 단조가 불가능한 재료까지도 표면부에 오버레이 시킴으로 서 부품 및 설비의 제조에 있어 재료비의 절감과 제품의 수명이 획기적으로 개선될 수 있다. 그리고 최근에는 도금 빛 용사 둥과 같은 표면처리를 할 경우임의 소재 표면에 도금 및 용 사에 용이한 재료를 오버레이용접시킨 후 표면처리를 함으로써 보다 고품질의 표면층을 얻기위한 시도가 이루어지고 있다. 따라서 국내, 외의 오버레이 용접기술의 적용현황 및 대표적인 적용사례, 오버레이 용접기술 및 용접재료의 개발현황 둥을 중심으로 살펴봄으로서 아직 국내에서는 널리 알려지지 않은 본 기 술의 활용을 넓이고자 한다.

  • PDF

Friction Welding of Ni-Base ODS Alloy Prepared by Mechanical Alloying (기계적 합금법으로 제조된 Ni기 산화물 분산강화 합금의 마찰압접에 관한 연구)

  • 강지훈;박성계;김지순;권영순
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 1994.10b
    • /
    • pp.15-15
    • /
    • 1994
  • M MA ODS 합금의 보다 폭넓용 실용확훌 위해 크게 요구되고 있는 적정 접합기술 개발의 한 방안£로, 마찰압접(Friction Welding) 방법의 가능성옳 조사하기 위하여 마찰압력과 시간, 마 찰 후 접촉압력(Upset Pressure) 풍을 다양하게 변화시켜 접합체톨 제조한 후, 접합체 강도에 대한 인장시험과 접합계연의 결합 및 미세구조에 대한 현미경 관찰, EDS에 의한 원소분석, 접 합이옴부의 경도분포와 파단면 분석 풍율 행하였다. 실험에 사용된 모재는 기계적 합금법으로 제조된 Inca사의 Ni기 MA 754 합금이었으며, 직경 l 10 mm, 길이 50 mm로 가공한 후, 아세통£로 초음파 세척하여 접합에 사용하였다. 접합온 브 레이크식 마찰압접기틀 사용하여 행하였으며, 회전시험편의 회전수는 2400 rpm이었A며, 다른 한쪽의 고정시험편과의 마찰압력 및 마찰시간온 각각 50 - 500 MPa과 1-5초로, 또한 업셋압 력도 50 - 600 MPa로 변화시켰다. 이때 업셋압력은 모든 시편에 대해 일정하게 6초동안 가하 였다. 얻어진 접합체는 각 압접조건 당 2개 이상의 접합시험편에 대해 상온 인장강도톨 측정하 였으며, 파단이 일어난 위치를 확인한 후 파면에 대한 분석율 주사전자현미경(SEM)과 에너지 분산형 분광분석기mDS)릎 사용하여 행하였다. 컵합이옴부의 첩합성올 확인하기 위하여, 접합 체를 접합변에 수직으로 절단, 연마한 후 광학현미경과 SEM, EDS 퉁으로 관찰, 분석하여 접 합부의 형상과 결합형성 여부, 접합계면의 미세조직 퉁옳 조사하였다. 또한 마찰압접에 따론 모재와 접합계연부의 경도분포훌 접합이옴부로부터 모재쪽으로 일정 간격율 두어 마이크로 비 커스 경도기로 측정, 조사하였다. 이상의 설험 결과, 다옴과 같온 결론옳 얻었다. ( (1) 접합체 강도가 모채 강도의 95% 이상이 되는 양호한 렵합체흩 얻기 위한 마찰압력 조건 온, 2400 rpm의 회전속도와 6초의 업셋압력 유지시간에서 마찰압력과 업셋압력, 그리고 마찰시 간이 각각 400 MPa 이상과 500 MPa 이상,2초입율 확인하였다. ( (2) 컵합이옴부의 관찰 결과, 모든 마찰압접 조건에서 컵합이옴부는, 기폰 모재의 texture 조직 을 유지하고 있는 모재부 영역(영역 ill)과 첩합계면부에 인접하여 업셋압력이 주어질 때 단조 효과에 의해 계연 외부로 metal flow가 일어나면서 형성된 영역 II, 매우 미세한 결정립으로 구성된 중앙부의 영역 1 로 이투어져 있옴융 확인하였다. ( (3) 최적접합조건이 충족되지 않온 경우, 접합부의 영역 I 에서 관찰된 void와 균열, 불균일한 접합계면 통의 접합결함에 Al과 Y. Ti 퉁£로 구성된 산화물률이 용집되어 있옴을 확인하였 다-( (4) 접합체의 파단 양상온 크게 접합부 파단과 모재부 파단, 이률의 혼합형 파단i로 나눌수 있었다. 모재부 파단의 경우, 파단면이 매끄럽고 파변상의 결정립도 매우 미세하였으며, 산확물 의 용집도 찾아보기 어려웠 나, 접합부 파단의 경우에는 파변의 굴곡이 비교척 심하고 연성 입계파괴의 형태를 보였£며, 결정립도 모채부 파단의 경우에 비해 조대하였다. 조대하였다.

  • PDF

Solid State Joining of Iron and Steels (철강재료의 고상접합기술)

  • 김영섭;권영각;장래웅
    • Journal of Welding and Joining
    • /
    • v.10 no.2
    • /
    • pp.1-10
    • /
    • 1992
  • 저탄소강은 일반적으로 용접성이 우수하지만 완전한 접합 강도와 용접부에서의 결함을 방지하기 위해서는 많은 주위가 필요하다. 용접부의 기계적 성질은 그 미세구조에 따라 좌우되는데, 이 구조는 모재의 화학조성, 용접 조건 그리고 후열처리에 의하여 결정이 된다. 이와 같이 용융용 접에 의한 저탄소강의 접합부는 저탄소함량으로 응고 균열에 대한 저항이 높다. 그러나 탄소의 함량이 증가하므로서 용접성은 저하하여, 0.3% 이상에서 용접부는 과열, 과냉, 저온 균열과 porosity에 취약하게 된다. 구조용강애 있어서는 용접성에 대한 일반적인 기준이 없으므로 이 러한 재료는 모재와 용접부의 기계적 성질, 고온 및 저온 균열성, 열간 및 냉각가공성등을 고려 하게 된다. 그러나 가장 중요한 것은 용접부의 신뢰도이다. 탄소강과 저합금강에 있어서 용접은 높은 강도를 얻을 수 있어야 하며 접합부에서 모재의 원래의 특성을 유지하여야 하고 결함이 없어야 할 것이다. 이와 같은 결함은 모재의 융접 이하에서 접합을 실시하는 고상접합으로 충 분히 억제할 수가 있다. 고상접합에서는 근본적인 미세조직의 결정화도 피할 수 있으며 고온균 일과 같은 결함의 위험도 배제할 수 있다. 고상접합은 용융용접과는 달리 모재를 용융시키지 않고 고체상태에서 접합을 하는데, 신금속 및 신소재의 개발과 첨단산업의 발달로 고상접합 기 술이 크게 각광을 받고 발전하게 되었다. 이와 같은 접합기술의 발전으로 기존의 용접으로는 접합이 불가한 소재, 용접기술의 적용이 곤란한 복잡한 형상, 복합기능 소재, 고품질 및 고정밀 성이 요구되는 소재등이 접합이 가능하게 되었다. 이러한 접합기술로는 brazing, 확산접합, 마찰 용접 등이 주로 많이 이용되고 있다. Brazing은 융점이 낮은 filler metal이 모재의 사이에서 용 융상태로 유입되어 냉각되면서 접합되는 방식이고 확산접합은 모재의 접합계면에서 원자의 상호 확산으로 접합을 하게 된다. 한편 마찰용접은 계면에서 회전에 의한 마찰열고 접합하는 방식 이다. 본 기술해설에서는 이러한 고상접합 기술을 이용한 철강재료의 접합에 대하여 고찰하도록 하겠다.

  • PDF

Residual Stress Measurement of Flat Welded Specimen by Electronic Speckle Pattern Interferometry (전자처리스페클패턴 간섭법을 이용한 평판 용접시험편의 잔류응력 측정)

  • Chang, Ho-Seob;Kim, Dong-Soo;Jung, Hyun-Chul;Kim, Kyung-Suk
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.32 no.2
    • /
    • pp.149-154
    • /
    • 2012
  • The size and distribution of welding residual stress and welding deformation in welding structures have an effect on various sorts of damage like brittle failure, fatigue failure and stress corrosion cracking. So, research for this problem is necessary continuously. In this study, non-destructive technique using laser electronic speckle pattern interferometry, plate of welding specimen according to the external load on the entire behavior of residual stress are presented measurement techniques. Once, welding specimen force tensile loading, using electronic speckle pattern interferometry is measured. welding specimen of base metal and weld zone measure strain from measured result, this using measure elastic modulus. In this study, electronic speckle pattern interferometry use weld zone and base metal parts of the strain differences using were presented in residual stress calculated value, This residual stress value were calculated by numerical calculation. Consequently, weld zone of modulus high approximately 3.7 fold beside base metal and this measured approximately 8.46 MPa.

The Study on the Corrosion Characteristics of STS 304 Pipeline Steel Weldment for Gas Cooling & Heating System (가스 냉온수기용 STS 304 배관 용접부의 부식특성에 관한 연구)

  • Kim, Hwan-Sik;Lim, Uh-Joh
    • Journal of the Korean Institute of Gas
    • /
    • v.11 no.2 s.35
    • /
    • pp.31-36
    • /
    • 2007
  • In order to study on the corrosion characteristics of STS 304 pipeline steel weldment for gas cooling & heating system. the electrochemical polarization test and corrosion test by impressed potential in 0.5M $H_2SO_4+0.01M$ KSCN solution was carried out. Also, SEM and hardness of welding zone was measured. And then passive behavior, corrosion behavior by the impressed potential and SEM aspect and hardness behavior of base metal(BM) and heat affected zone(HAZ) for STS 304 pipe were investigated. The main results are as follows: 1) The critical anodic current density of heat affected zone(HAZ) is drained more highly than that of base metal(BM), and primary passive potential of HAZ become higher than that of BM. 2) The passive current density of TUE is drained more highly than that of BM, and passive region of BM become bigger than that of HAZ. 3) By the impressed potential, the current density of HAZ is drained more than that of BM.

  • PDF

Study on Hydrogen Embrittlement for API 5L X65 Steel Using Small Punch Test I : Base Metal (소형펀치 시험을 이용한 API 5L X65 강의 수소취화에 관한 연구 I : 모재부)

  • Jang, Sang-Yup;Yoon, Kee-Bong
    • Journal of Energy Engineering
    • /
    • v.18 no.1
    • /
    • pp.49-55
    • /
    • 2009
  • Occurrence of hydrogen embrittlement could be one of the main obstacles for using structural equipment under hydrogen environment. It is required to develop assessment methods of hydrogen embrittlement for the metals used in production, storage, transmission and application utilities of hydrogen. The most probable method of hydrogen mass transmission is using existing natural gas pipeline. Base or weld part of the pipeline can be damaged by mixed gas of hydrogen in the pipeline. In this study small punch (SP) testing was employed to evaluate the hydrogen embrittlement behavior for a line pipe steel (API X65) with electrochemically hydrogen charged specimens. Results showed that the SP test can be a good candidate test method for hydrogen damage evaluation method. Strength of steel is known to be decreased with the level of hydrogen charging. However, for API X65 steel base metal need in this study, the effect of hydrogen to strength was not significant. It can be negligible regardless of the hydrogen contents in the steel. With this test different strength levels with various hydrogen charging conditions were observed. It can also be anticipated that more sensitive evaluation of material behavior be obtainable by the SP test method.

주증기관의 균열성장 수명평가 사례 연구

  • 백운봉;이해무;박종서;윤기봉
    • Proceedings of the Korean Institute of Industrial Safety Conference
    • /
    • 2001.11a
    • /
    • pp.364-369
    • /
    • 2001
  • 고온 고압 산업용 설비의 경우, 대부분 균열이 용접부위에서 가장 먼저 발생하여 성장한다(1). 그러나 용접부라고 하지만 장기간 사용에 의한 사용재 균열성장은 엄밀히 말하면 용접부와 모재부 사이의 열영향부이며 열영향부 중에서도 ICHAZ(Intercritical heat affected zone)에서 발생하는 TYPE IV균열/sup (1)/이라 하겠다 따라서 용접부 균열에 대한 파괴거동을 연구하는 것은 고온고압 산업용 설비의 잔여 수명을 평가하는데 매우 중요하다.(중략)

  • PDF

Metallurgical Structures and Mechanical Properties in Weldments of Dissimilar Cr-Mo Steels (Cr-Mo계 이종재질간 용접부의 미세조직 및 기계적성질)

  • 지병하;김정태;박화순
    • Proceedings of the KWS Conference
    • /
    • 1996.10a
    • /
    • pp.42-44
    • /
    • 1996
  • 이종재료인 2$\frac{1}{4}$Cr-1Mo강과 12Cr-1Mo-V계 강의 용접부의 용접성에 대하여 모재계열의 용접재료와 Inconel계의 용접재료를 사용하여 야금학적인 관점으로부터 미세조직적 특성 및 기계적성질을 중심으로 검토하였다. 그 결과를 요약하면 다음과 같다. (1) 본 연구의 실험범위에 의하면, 내부결함, 균열 등의 용접결함을 발생하지 않는 양호한 용접부를 얻을 수 가 있었다. (2) 광학현미경을 이용한 미세조직의 관찰에 의하면, Inconel계의 용접재료를 제외한 모재계열의 용접재료를 사용하였을 경우, 용융경계부 근방에서 연속 또는 불연속적인 백색의 밴드상이 형성되었다. (3)백색밴드상의 형성부는 인장변형에 의하여 국부적인 수축변형을 일으키나, 파단은 2$\frac{1}{4}$Cr-1Mo강의 모재에서 발생하였으며, 거시적인 인장성질에는 영향을 미치지 않았다.

  • PDF

A Parametric Study on the Strength of Single-Lap Bonded Joints of Carbon Composite and Aluminum (탄소 복합재-알루미늄 단일겹침 접착 체결부의 강도에 관한 인자연구)

  • Kim, Tae-Hwan;Seong, Myeong-Su;Choi, Jin-Ho;Kweon, Jin-Hwe
    • Composites Research
    • /
    • v.20 no.5
    • /
    • pp.34-42
    • /
    • 2007
  • Strength and failure of adhesively bonded carbon composite-to-aluminum single-lap joints were studied by experiment. The main objective of this study is to investigate the effect of various parameters such as curing pressure for bonding, overlap lengths, and adherend thickness on the failure loads and modes of the bonded Joints with dissimilar materials. Experimental results show that the bonding pressure for composite-to-aluminum dissimilar materials should be 4 atm at the lowest. Failure load of the joints increases as the overlap length increases, but the strength (failure load divided by bonded area) decreases rapidly after the overlap width-to-length ratio is greater than 1. When the adherend thickness increase to double, bonding strength increase $12{\sim}55%$. Major failure mode of the joints is the delamination in the composite laminate and the location of delamination goes deeper into the laminates as the bonding pressure and overlap length increase.