• 제목/요약/키워드: 마멸특성

검색결과 268건 처리시간 0.026초

고크롬 롤의 수명과 마멸특성에 관한 연구 (A Study on the Wear Characteristics and Lifetime Of High Chromium Roll)

  • 김문경;김순경;전언찬
    • 한국정밀공학회지
    • /
    • 제14권2호
    • /
    • pp.58-65
    • /
    • 1997
  • Work rolls used in cold rolling mills must have outstanding wear resistance and very little plastic defor- mation. Thus, these rolls require a higher surface hardness and harding to a greater depth. To meet these requirements, the rolls, in general, have basic chemical composition of 0.7 to 1.0% carbon and 1.0 to 5.0% Cr(chromium), plus a small amounts of special elements, and are subjected to intensive water quenching and tempering at low temperature to provide a surface hardness of over 90 shore. This test results are as follows. Deflection and fracture load of 5% Cr material are than those of 3% Cr material and show flat curve from surface to subsurface. It will be clear that 5% Cr work roll has a superior resisti- bility against wear and abrasion comparing with 3% Cr work roll. The improvement of wear and abrasion in 5% Cr work roll will be achieved by the large amount of wpheroidal carbide. In grindability and polish, 5% Cr work roll will be a little inferior comparing with 3% Cr work roll.

  • PDF

탄소섬유 에폭시 복합재료의 절삭(밀링) 특성 (Cutting(Milling) Characteristics of Carbon Fiber/Epoxy Composites)

  • 김기수;이대길;곽윤근
    • 대한기계학회논문집
    • /
    • 제14권1호
    • /
    • pp.37-42
    • /
    • 1990
  • 본 연구에서는 수직 밀링에서 탄소섬유 에폭시 복합재료를 절삭할 경우 절삭 조건에 따른 공구마멸 형태를 조사하였으며, 여유면 마멸량을 측정하여 Taylor 지수를 구하였다. 또한 절삭조건 및 측정 방향에 따른 표면거칠기를 조사하여 탄소섬유 에 폭시 복합재료의 가공특성을 조사하였다.

Power 서보 실린더의 피스톤 헤드용 AlBC의 마멸 특성 (Wear Characteristics of AlBC for Piston Head of Power Servo Cylinder)

  • 조연상;박흥식
    • Tribology and Lubricants
    • /
    • 제27권2호
    • /
    • pp.65-70
    • /
    • 2011
  • The power servo cylinder for driving accurately turbine stop valve of an atomic power plant is necessary to do turn-over owing to a leakage of oil and a structure problem, especially, it of a power plant be in demand a high quality standard depends entirely on import. There are much problem that the AlBC be to used as a material of piston head in cylinder are caused by wear. Therefore, it is necessary to examine friction characteristics of it. In this study, wear test experiments was carried out with AlBC and SCM440, using reciprocating friction tester of pin on disk. This result was shown that the wear mechanism of AlBC on working condition is adhesive wear and the maximum temperature of infra redray thermal image of frictional surface show over 2 mm from contact surface of pin and disk.

공해방지를 위한 강구조물의 도장용 샌드블라스트 장치에 관한 연구 (Study on the Sandblast Machine in Painting of Steel Structures for Environmental Pollution Prevention)

  • 임우조;황태호;이진열
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1996년도 제23회 학술대회
    • /
    • pp.47-52
    • /
    • 1996
  • 본 연구에서는 각종 강구조물의 도장전 샌드블리스트 작업에 다른 공해를 방지하기 위해, 모래-물의 2상류를 분사할 수 있는 샌드블라스트 장치를 제작하여, 2상류 분사에 따른 마멸-부식(wear-corrosion)특성과 slurry erosion에 의한 anchor pattern 및 침식-마멸거동을 고찰하고, 물에 의한 강구조물의 부식방지를 위한 부식억제제가 강구조물의 도막에 미치는 방식특성을 구명함으로써 공해방지, 부식손상 및 산업의 국제경쟁력 향상에 기여하고자 한다.

  • PDF

단섬유 보강 복합재료의 트라이볼로지 특성 (Tribological characteristics of short fiber reinforced composites)

  • 윤재륜
    • 대한기계학회논문집
    • /
    • 제12권6호
    • /
    • pp.1238-1245
    • /
    • 1988
  • 본 연구에서는 단섬유가 첨가된 복합재료의 마찰 및 마멸특성에 대하여 보고 하고자 하며, 최근 공업용 고분자(engineering plastic)로 중오시되고 있는 PAI를 모 재로 하여 탄소섬유(graphite fiber), 유리섬유(glass fiber), TiO$_{2}$ 등이 첨가된 복합재료의 트라이볼로지(tribology) 특성에 대하여 고찰하고자 한다. 본 연구에서 사용된 복합재료에 포함된 단섬유들은 일정한 배열방향이 없이 마구잡이로 분포되어 있으며, 섬유특성에 따라 마멸메카니즘에 큰 차이가 있음을 본 연구 결과를 통하여 알 수 있다.

SiO2 나노 콜로이드 첨가량에 따른 질화규소의 트라이볼러지 (Tribology of Si3N4 Ceramics Depending on Amount of Added SiO2 Nanocolloid)

  • 남기우;정영규;황석환;김종순;문창권
    • 대한기계학회논문집A
    • /
    • 제35권3호
    • /
    • pp.267-272
    • /
    • 2011
  • 본 연구는 $SiO_2$ 나노 콜로이드 첨가량에 따르는 $Si_3N_4$ 세라믹스의 마멸 특성을 평가하였다. 시험 편은 35 MPa, 2123 K의 질소 가스 분위기 1시간동안 소결하였다. 마멸 시험은 링 블록 시험기를 사용 하였으며, 시험 조건은 직경 35 mm인 링의 회전속도50 rpm, 하중 9.8 N, 실험중의 대기 온도 293 K이 었다. 세라믹스의 마멸계수는 약 1.0, 마멸손실은 약 0.02 mm이었다. 본 연구에 사용된 시험편 중에서 1.3 wt% $SiO_2$ 나노 콜로이드가 첨가된 시험편은 가장 낮은 마멸계수와 마멸 손실을 나타내어, 최상의 마멸 저항성을 나타내었다. 이것은 가장 높은 비커스 경도와 굽힘 강도를 나타내었다. 마멸계수는 경도 와 굽힘 강도에 역비례 관계를 보였다.

자동차 섀시 시스템에 유입되는 먼지입자에 의한 고무-씨일 부품의 마멸특성 -PART II: 먼지유입에 따른 고무-씨일의 마멸특성- (Wear Characteristics of Rubber-Seal for Inflow of Dust Particles in Automobile Chassis System -PART II: The Influence of Dust Particle Inflow on Wear Characteristics of Rubber-Seal-)

  • 이영제;정순오;원태영;김기훈;김대성
    • Tribology and Lubricants
    • /
    • 제25권4호
    • /
    • pp.261-264
    • /
    • 2009
  • Environmental factors affect parts of the automobile. When dust particles are embedded, specially, friction and wear of the rubber-seal in automobile chassis system are increased. Increase in friction and wear leads to weakness of component and reduction of mechanical life. In this study, the wear characteristics of rubber-seal for inflow of dust particles are investigated. Silica($SiO_2$) and alumina($Al_2O_3$) particles are used as a dust particle because these particles are main elements of dust particles. The sliding wear tester are used for investigate the wear characteristics of rubber-seal. If the single dust particle($SiO_2$) is embedded in the rubber-seal component, the influence of dust particle size is more than that of inflow rate on the wear characteristics of rubber-seal. If the mixed dust particles are embedded in the rubber-seal component, the wear rate is increased as the rate of alumina that has a bigger hardness is increased. If the mixed dust particles that have different hardness are embedded in the rubber-seal component, the influence of particle size is more than that of particle hardness.

힌지재료의 부식특성 및 찰과마멸 거동 (Behaviour of the Fretting Wear and Corrosion Characteristics on a Hinge Material)

  • 곽남인;임우조;이종락
    • 한국가스학회지
    • /
    • 제3권3호
    • /
    • pp.39-44
    • /
    • 1999
  • 일반강구조물로 많이 사용되고 있는 SM20C, BsC3 및 STC4H에 대하여, 여러 가지 부식환경(지하수($6,000{\Omega}{\cdot}cm$), $0.5\%\;H_2SO_4$$0.5\%HNO_3$)침지하에서의 부식특성 및 건조상태에서의 찰과마멸특성실험에 의한 이종금속간의 찰과마멸특성을 고찰하였다. 침지시험의 경우, 이들 금속의 전위값은 $HNO_3$, 지하수, $H_2SO_4$ 순으로 크게 나타났으며, BsC3을 제외한 동재금속보다 이종금속의 전위가 높았다. 동종재인 SM20C의 마멸은 회전측의 경우가 이동측보다 약 1.9배 증가하였으며, 이는 마찰력에 의한 표면경화가 그 원인인 것으로 추측된다.

  • PDF

머신비전을 이용한 밸브어셈블리의 3차원 마멸특성 분석 (3D Wear Analysis of Valve Assemblies by Using the Machine Vision)

  • 박창우;정성종
    • 대한기계학회논문집A
    • /
    • 제30권5호
    • /
    • pp.496-504
    • /
    • 2006
  • Wear of engine valves and seat inserts is a major factor affecting engine performance. In order to improve quality and life of valve assemblies, wear mechanism and 3-D surface topography should be analyzed according to operating conditions of the engine. After developing an engine simulator that generates valve speed up to 90Hz and temperature up to $900^{\circ}C$ as well as controls test load, wear experiments have been conducted for two different engine speeds as 10Hz and 25Hz. In order to observe the wear characteristics and monitor surface conditions of the valve assemblies, a cost-effective 3-D wear analysis system based on the shape from focus(SFF) and machine vision has been fabricated in this paper. 3-D surface topography of the valve assemblies has been analyzed to understand the wear behavior according to operating conditions of the engine. Consequently, wear volume of the valve assemblies is quantized by using the developed 3-D wear analysis system.

오스템퍼링한 구상점연주철의 부식환경중의 마멸특성에 관한 연구 (A Study on the Wear Characteristics of Austempered Ductile Cast Iron in Corrosive Environments)

  • 강명순;전태옥;박흥식;진동규
    • 한국해양공학회지
    • /
    • 제2권2호
    • /
    • pp.87-95
    • /
    • 1988
  • This paper is studied to know corrowive wear characteristics of austempered ductile cast ironin corrosive environments against mating SM45C hardened two test pieces in distilled water and NaCl aqueous solution. The corrosive wear mechanism was investigated by scanning electron microscopy and retained austenite volume fraction was investigated by X-ray diffractometer. The experimental result show that the corrosive wear characteristics depend largely on the $\textrm{Fe(OH)}_{3}$which is influenced by the critical sliding distance $L_{cr}$ and $L_{cr}$ shorted with increasing NaCl concentration. It was found that the carbides in matrix have a significant effect on their corrosive wear resisance and the fine acicular bainite showed corrosive wear resistance stronger than that of the coarse acicular and platelet bainite. From above results the model of corrosive wear mechanism in corrosive environments is proposed.

  • PDF