Synthesis of Na-A type Zeolite From Melting Slag (소각재 용융슬래그를 이용한 제올라이트 Na-A의 합성)

  • Jang Young-Nam;Chae Soo-Chuu;Bae In-Kook;Ryou Kyung-Won
    • Journal of the Mineralogical Society of Korea
    • /
    • v.18 no.1
    • /
    • pp.11-17
    • /
    • 2005
  • Na-A zeolite were synthesized from melting slag of the incinerated ash by the alkaline activation processes. The experiments were performed in stainless steel vessels, with continuous stirring during the reaction periods. The silica-rich solution, a starting material, which was the waste of crystal growth factory, contains 5.7 wt% SiO₂ and 3.2 wt% Na₂O. And NaAlO₂ was made by the reaction of aluminium dross and NaOH solution and its molar ratios were Na₂O/Al₂O₃= 1.2 and H₂O/Na₂O=9. During the residence time of 7∼8 h at 80℃, the mixing of the silica-rich solution, NaAlO₂ and melting slag yields the production of homogeneous Na-A zeolite. The optimal reactant composition in molar ratio of Na₂O:Al₂O₃:SiO₂ was 1.3∼l.4 : 0.8∼0.9 : 2 and mixing ratio of solution and slag was 1/7∼10 (g/cc). Synthesized Na-A zeolite has cubic form uniformly and its size ranges about 1 ㎛. Ca/sup 2+/ ion exchange capacity of the Na-A was about 180∼210 meq/100g, corresponding approximately 80% to the commercial detergent builder.