• Title/Summary/Keyword: 단일구조 지르코니아 크라운

Search Result 7, Processing Time 0.024 seconds

Effect of additional firing process after sintering of monolithic zirconia crown on marginal and internal fitness (단일구조 지르코니아 크라운의 소결 후 추가 소성 과정이 변연 및 내면 적합도에 미치는 영향)

  • Shin, Mi-Sun;Lee, Hyeonjong
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.57 no.4
    • /
    • pp.321-327
    • /
    • 2019
  • Purpose: To evaluate an effect of additional firing process after sintering of monolithic zirconia crown on marginal and internal fit through three-dimensional analysis. Materials and methods: Ten monolithic zirconia crowns were fabricated using titanium abutment model. Monolithic zirconia crowns were designed, milled, and sintered as a control group, and additional firing with coloring was performed as a test group. Three dimensional analysis were performed by using triple-scan protocol, and cross-section analysis on mesio-distal and disto-lingual section was evaluated to measure marginal and internal fitness. Then, three-dimensional surface difference on between two groups was evaluated (${\alpha}=.05$). Results: There was statistically significant difference between the control group ($32.0{\pm}24.3{\mu}m$) and the test group ($17.0{\pm}10.8{\mu}m$) in the mesial axial wall (P < .02) and the control group ($60.2{\pm}24.3{\mu}m$) and the test group ($71.8{\pm}21.5{\mu}m$) in the distal axial wall (P < .01). There was no statistically significant difference at the remaining point. Conclusion: There was no statistical significance on the deviation of inner surface of crown according to firing number, and the results of both group were considered clinically acceptable.

The effect of reduced thickness in different regions on the fracture resistance of monolithic zirconia crowns (다양한 부위에서의 감소된 두께가 지르코니아 크라운의 파절 저항에 미치는 영향)

  • Abukabbos, Layla;Park, Je Uk;Lee, Wonsup
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.60 no.2
    • /
    • pp.135-142
    • /
    • 2022
  • Purpose. This study aims to evaluate the combined effect of reduced thickness in different regions on the fracture resistance of monolithic zirconia crowns. Materials and methods. Seven nickel-chromium dies were generated from a 3D model of mandibular first molar using the digital scanner with the following geometries: 1.5 mm occlusal reduction, 1.0 mm deep chamfer. Based on the abutment model, Zirconia blocks (Luxen Zirconia) were selected to fabricate Sixty-three zirconia crowns with occlusal thicknesses of 0.3 mm, 0.5 mm, and 1.5 mm, and different axial thicknesses of 0.3 mm, 0.5 mm, and 1.0 mm. All crowns were cemented by resin cement. Next, the crowns were subjected to load-to-fracture test until fracture using an electronic universal testing machine. In addition, fracture patterns were observed with a scanning electron microscope (SEM). Two-way ANOVA and the Tuckey HSD test for post hoc analysis were used for statistical analysis (P < .05). Results. The mean values of fracture resistancerecorded was higher than the average biting force in the posterior region. The two-way ANOVA showed that the occlusal and axial thickness affected the fracture resistance significantly (P < .05). However, the effect of axial thickness on fracture resistance did not show a statistical difference when thicker than 0.5 mm. The observed failure modes were partial or complete fracture depending on the severity of crack propagation. Conclusion. Within the limitations of the present study, the CAD-CAM monolithic zirconia crown with extremely reduced thickness showed adequate fracture resistance to withstand occlusal load in molar regions. In addition, both occlusal and axial thickness affected the fracture resistance of the zirconia crown and showed different results as combined.

Full mouth rehabilitation using zirconia crown in severe worn dentition: a case report (마모가 심한 환자에서 지르코니아 크라운을 이용하여 전악 수복한 증례)

  • Park, Jung-Hyun;Sohn, Sang-Hyuk;Cho, Sung-Am
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.32 no.3
    • /
    • pp.202-208
    • /
    • 2016
  • The progressive attrition of teeth is a normal process by aging. However, excessive tooth wear with decreased vertical dimension of occlusion and collapse of occlusal plane may cause pathologic pulpal condition, occlusal disharmony and functional disorders. In this case, a patient with severely worn dentition was treated. Diagnostic wax-up was performed at the increased vertical dimension. After evaluation of provisional restorations for 12 weeks, final restorations were fabricated with zirconia crown and routine clinical assessments were made. Esthetically and functionally satisfactory results were obtained.

Implant-supported prosthetic rehabilitation for the edentulous maxilla using the additive manufacturing technology: A case report (레이저 적층 제조 기술을 이용한 상악 무치악 환자의 임플란트 고정성 보철 수복 증례)

  • Kim, Hee-Kyung
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.56 no.2
    • /
    • pp.173-178
    • /
    • 2018
  • The direct metal laser sintering (DMLS) technique would be promising for the full-arch implant-supported restorations due to reduced cost and manufacturing time without potential human errors and casting defects. The aims of this case report were to describe the successful outcome of an implant-supported fixed dental prosthesis in the edentulous maxilla by using the DMLS technology and computer-aided design and computer-aided manufacturing (CAD/CAM) monolithic zirconia crowns, and to describe its clinical implications. A healthy 51-year-old Korean woman visited Seoul National University Dental Hospital and she was in need of a rehabilitation of her entire maxilla due to severe tooth mobility. In this case, all maxillary teeth were extracted and an implant-supported fixed dental prosthesis was fabricated that involved a cobalt-chromium (Co-Cr) framework with the DMLS technique and CAD/CAM monolithic zirconia crowns. Six months after delivery, no distinct mechanical and biological complications were detected and the prosthesis exhibited satisfactory esthetics and function. In this case report, with the DMLS system, the three-dimensional printed prosthesis was created without additional manual tooling and thus, reliable accuracy and passive fit were obtained.

Dental application of glass-ceramic materials for aesthetic restoration (심미수복을 위한 글라스-세라믹 재료의 치과 응용)

  • Bae, Tae Sung
    • The Journal of the Korean dental association
    • /
    • v.58 no.7
    • /
    • pp.435-442
    • /
    • 2020
  • Porcelain is the first ceramic material to be introduced into dentistry. Porcelain jacket crown was introduced by Dr. Charles H Land in 1886, which was an excellent aesthetic dental restoration but has not been widely used due to high firing shrinkage and low tensile strength. Then metal-ceramic system, which combines the esthetic properties of ceramics and the mechanical properties of metals, was introduced and nowadays it is still used in dental clinical field. However, the metal-ceramic system has shown some problems, such as increased lightness by reflection of light at opaque layer, shadow beneath the gingival line due to the block-out of light by metal coping, exposure of metal in margin part, bond failure between metal and porcelain, oxidation of metal coping during firing the porcelain, etc. Recently, along with the advance of fabrication methods of dental ceramics, the all-ceramic restorations with high esthetic and mechanical properties has increased and gradually replaced metal-ceramic restorations. Especially, CAD/CAM technology has opened a new era in fabricating the dental ceramic restorations. This overview will take a look at the past, present and future possibility of the dental ceramic materials.

  • PDF

Full mouth rehabilitation in a patient with partial mandibulectomy using CAD/CAM zirconia framework and monolithic zirconia (하악골 부분절제술 시행한 환자에서 CAD/CAM Zirconia Framework와 Monolithic Zirconia를 이용한 전악 수복 증례)

  • Ma, Bo-Young;Park, Hongju;Im, Yeong-Gwan;Park, Chan;Shin, Jin-Ho;Lim, Hyun-Pil
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.55 no.3
    • /
    • pp.279-285
    • /
    • 2017
  • Defects due to mandibulectomy often cause hard and soft tissue loss and result in esthetic problems and functional disorders such as mastication, swallowing, and pronunciation. After the mandibular reconstruction, several complications including loss of alveolar bone can cause limitations in maintenance or supporting of removable prosthesis. For these patients, implant-supported fixed restorations have been an appropriate prosthetic restorative method. In this case report, we report the patient who underwent mandibulectomy and mandibular reconstruction owing to oral cancer, and then restored the current dentition functionally and aesthetically by applying zirconia frameworks and monolithic zirconia crowns by computer-aided design and computer-aided manufacturing.

A Making of Aesthetic Dental restorations with Nano Hybrid Ceramic material by CAD/CAM System (치과 CAD/CAM용 Nano Hybrid Ceranic 소재를 이용한 심미 치과보철물의 제작)

  • Choi, Beom-jin
    • Journal of the Korean Academy of Esthetic Dentistry
    • /
    • v.25 no.2
    • /
    • pp.98-108
    • /
    • 2016
  • In recent days, perhaps the biggest driver in new material development is the desire to improve restorations esthetics compared to the traditional metal substructure based ceramics or all-ceramic restorations. Each material type performs differently regarding strength, toughness, effectiveness of machining and the final preparation of the material prior to placement. For example, glass ceramics are typically weaker materials which limits its use to single-unit restorations. On the other hand, zirconia has a high fracture toughness which enables multi-unit restorations. This material requires a long time sintering procedure which excludes its use for fast chair side production. Hybrid ceramic material developed for CAD/CAM system is contained improved nano ceramic elements. This new material, called a Resin Nano Hybrid Ceramic is unique in durability of function and aesthetic base compositions. The new nano-hybrid ceramic material is not a composite resin. It is also not a pure ceramic. The material is a mixture of both and consists of nano-ceramic fillers. Like a composite, the material is not brittle and is fracture resistant. Like a glass ceramic, the material has excellent polish retention for lasting esthetics. The material is easily machined by chair side or in a dental lab side, could be an useful restorative option.