  • Diamond grit was coated with Ti by RF Sputtering to investigate the effect of coated diamond particles on performance of diamond impregnated saw. Coated and uncoated powders were separately mixed with 70Co-30W(wt %) powders by conventional milling technique. Hot pressing was carried out to make specimens. The wear test were carried out with these two types of diamond impregnated specimens. It was demonstrated that Ti coating was effective in improving the ability of grit retention and thus enhanced the tribological performance of diamond tool.

  • PDF

실험계획법에 의한 화인세라믹스 원통래핑의 최적화에 관한 연구

  • 최민식;김정두
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1992.10a
    • /
    • pp.145-150
    • /
    • 1992
  • 화인세라믹의 우수한 공학적 특성으로 인한 최근의 이용가치 증대와 더불어 세라믹의 고정도 가공에 대한 관심이 높아지고 있다. 다이아몬드휠을 이용한 연삭이나 다이아몬드 공구를 이용한 선삭에 의해 세라믹의 고정도 표면생성을 실현시키고자 하는 연구가 활발히 진행되고는 있으나 아직 미흡한 상태에 있다. 따라서 전통적으로 고정도 표면생성에 널리 용되어 온 래핑에 의한 표면다듬질이 현재 행하여지고 있는 일반적인 방법이다. 본 연구에서는 화인세라믹의 고정도 표면생성을 위한 원통래핑 공정의 최적화 방법으로 실험계획법의 한 응용분야인 반응표면분석법을 이용하였으며 그 결과, 적은 재료와 시간으로 능률적이고 체계적인 실험 및 통계적인 분석을 통해서 원통세라믹의 고정도 표면생성을 위한 최적래핑조건을 찾아내었다.

마이크로 선반에서의 절삭성 평가

  • 김재건;정종운;고태조;김희술
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2004.05a
    • /
    • pp.256-256
    • /
    • 2004
  • Micro/Meso 기계적 가공은 기존 MEMS 공정에서 제작할 수 없었던 높은 세장비(aspect ratio)를 가지는 제품을 가공할 수 있을 뿐만 아니라 보다 높은 가공 정밀도를 획득할 수 있다. 따라서, 미소 부품에 대한 마이크로/매소 단위의 미세 절삭 가공을 위해서는 공간적 측면과 에너지 소비, 정밀도 측면에서 효율적인 시스템을 구성하기 위해서 마이크로 머시닝 전용 기계가 요구된다. 이에 본 연구에서는 '마이크로 팩토리' 의 기본 공작기계인 마이크로 선반을 개발하여 초정밀 미소 절삭에 대한 연구를 진행 중에 있다.(중략)

  • PDF

Effect of Ti Coated Diamond Grit on Performance of Diamond Tool (티타늄 코팅된 다이아몬드 지립이 다이아몬드 공구의 성능에 미치는 영향)

  • 임동필;임대순;민언기;임종관
    • Tribology and Lubricants
    • /
    • v.13 no.3
    • /
    • pp.102-107
    • /
    • 1997
  • Diamond grit was coated with Ti by RF Sputtering to investigate the effect of coated diamond particles on performance of diamond impregnated saw. Coated and uncoated powders were separately mixed with 70Co-30W powders by conventional milling technique. Hot pressing was carried out to make specimens. The wear test were carried out with these two types of diamond impregnated specimens. It was demonstrated that Ti coating was effective in improving the ability of grit retention and thus enhanced the tribological performance of diamond tool.

Cutting Force Prediction in Single Point Diamond Turning (정밀 선삭 가공 과정의 절삭력 예측모델)

  • 윤영식
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.17 no.6
    • /
    • pp.1456-1464
    • /
    • 1993
  • The achievable machining accuracy depends upon the level of the micro-engineering, and the dimensional tolerances in the order of 10 nm and surface roughness in the order of 1 nm are the accuracy targets to achieved today. Such requirements cannot be satisfied by the conventional machining processes. Single point diamond turning is one of the new techniques which can produce the parts with such accuracy limits. The aims of this thesis are to get a better understanding of the complex cutting forces. A cutting model for describing the influence of cutting conditions (cutting speed, feedrate and depth of cut), material properties of the workpiece and tool geometry has been proposed after estimating the two cutting force models-the Recht model and the Dautzenberg model. The experiments with Al-alloy workpieces, which have been carried out in order to estimate the models, show that the proposed model in this thesis is better than the two models. As the depth of cut and feedrate are increased in the operations settings (depth of cut 8-100$\mu{m}$, feedrate 8-140$\mu{m}$/rev, and cutting speed 8 m/sec), the relation of dimensionless cutting forces from experiments are similar to the proposed model. With the undeformed chip area of $30-80{\times}10^{2}$\mu{m}^2$, the experimental cutting forces accord with the force prediction.

금속중간층을 이용한 나노결정질 다이아몬드 박막 코팅

  • Na, Bong-Gwon;Myeong, Jae-U;Gang, Chan-Hyeong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.99-99
    • /
    • 2013
  • 나노결정질 다이아몬드(Nanocrystalline Diamond: NCD) 박막은 고경도와 낮은 마찰계수를 가지고 있어 초경합금이나 고속도강과 같은 절삭공구 위에 코팅하여 공구의 성능 향상을 도모하려는 노력이 있어 왔다. 그러나 NCD 박막의 잔류응력이 크고, 초경합금과 철계 금속에 NCD가 증착되지 않는다는 문제점이 있다. 따라서 잔류응력 완화와 다이아몬드 핵생성을 위하여 제3의 중간층 재료가 필요하다. 본 연구에서는 W과 Ti을 중간층으로 하여 초경합금(WC-Co)과 고속도강(SKH51)에 NCD 박막을 코팅하고 기계적 특성을 비교하였다. 초경합금 또는 고속도강기판 위에 W 또는 Ti 중간층을 DC magnetron sputter를 이용해 각 1 ${\mu}m$의 두께로 증착하고 그 위에 MPCVD (Microwave Plasma Chemical Vapor Deposition)를 이용해 NCD 박막을 2${\mu}m$의 두께로 코팅하였다. FESEM을 이용하여 표면과 단면의 형상을 관찰하였고, XRD와 Raman spectroscopy를 통해 NCD 박막의 결정성을 확인하였다. 그리고 tribology test를 실시하여 코팅된 박막의 내마모성을 비교하였으며, Rockwell C indentation test를 이용하여 밀착력을 비교하였다. 초경합금에 적용 시, W이 Ti보다 중간층으로서 더 우수한 것으로 나타났으며 이는 열팽창계수 차이에 의한 잔류응력의 차이에 의한 것으로 여겨진다. 중간층 두께에 따른 박막의 기계적 특성 변화를 알아보기 위해 W 중간층의 두께를 1, 2, 4 ${\mu}m$로 변화를 주었다. 중간층 두께가 2 ${\mu}m$ 이상일 때 박막의 밀착력이 증가되는 것으로 나타났다. 고속도강 위에 같은 방법으로 1 ${\mu}m$의 W 또는 Ti 중간층 위에 2 ${\mu}m$의 NCD 박막을 코팅한 시편들은 초경합금에 코팅한 것과 달리 두 시편 모두 낮은 밀착력을 나타내었다. 열팽창계수 차이에 의한 잔류응력을 완화하기 위해 고속도강에 W/Ti 복합박막을 중간층으로 Ti, W순으로 각각 1 ${\mu}m$ 두께로 증착 후 그 위에 NCD 박막을 2 ${\mu}m$ 두께로 코팅 한 후 특성을 비교하였다. Ti/W 복합 중간층 위에 코팅된 NCD 박막의 밀착력이 W 혹은 Ti 단일 중간층에 코팅된 박막에 비해 우수한 것으로 나타났다. 그러나 실제 공구에 적용하기에는 박막의 밀착력 개선이 요구되며 이를 위해서 더 연구가 필요하다.

  • PDF

Wear Mwarsurement of Single Crystal Diamond Tool Using Image Processing (영상처리를 이용한 초정밀가공용 다이아몬드 공구의 마멸 측정)

  • 양민양
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1996.04a
    • /
    • pp.135-139
    • /
    • 1996
  • In this a paper, a new method to measure the wear of the single crystal diamond(SCD) tool using image processing is presented. To increase resoultion, high magnifying lens is used and to enlarge the measurement field of view, a image region matching method is applied. The shape of SCD tool is modeled by mathematical analysis. Cutting edge chipping and wear are calculated by the model. This method is proved to be efficient in detecting a few micron of wear and cutting edge loss by chipping along the whole cutting edge.

  • PDF

A Study on the Precision Cutting Characteristics by the Diamond Tool on the Cutting Distance (다이아몬드 공구의 절삭거리에 따른 정밀가공 특성 연구)

  • Yu, Ki-Hyun;Cheong, Chin-Yong
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.7 no.5
    • /
    • pp.127-133
    • /
    • 1998
  • This research intends to gain the sight for the qualitative characteristics of precision cutting by using the CNC lathe with a mono-crystal diamond(MCD) and a poly-crystal diamond(PCD) tool on the cutting distance. In case of an MCD tool, as the cutting distance increases, the surface roughness becomes worse and the standard deviation of surface roughness is small. In case of a PCD tool, as the cutting distance increases, the surface roughness becomes stable with a large standard deviation. The cutting force ratio(Ft/Fn) decreases as the nose radius increases and the decreasing ratio becomes larger for small nose radius.

  • PDF