• 제목/요약/키워드: 금속사출성형

검색결과 55건 처리시간 0.031초

금속분말 사출성형된 순-구리의 미세조직에 미치는 고온 소결조건의 영향 (Effect of High-Temperature Sintering Condition on Microstructure Evolution of Pure-Cu Subjected to Metal Injection Molding)

  • 한다인;수하르토노 트리;김동주;이은혜;김종하;고영건
    • 소성∙가공
    • /
    • 제31권4호
    • /
    • pp.240-245
    • /
    • 2022
  • In this study, to achieve good electrical conductivity of a charging terminal component in electric vehicles, we investigated the microstructure evolution of pure-Cu subjected to metal injection molding by controlling the sintering variables, such as temperature and time. Thus, three samples were sintered at temperatures ranging from 1000 ℃ to 1050 ℃ near to the melting temperature of 1085 ℃ for 1 and 10 h after thermal evaporation of binder at 730 ℃. Both procedures were made using a unified furnace under Ar+H2 gas with high purity. The structural observation displayed that the grain size as well as the compactness (a reciprocal of porosity) increased simultaneously as temperature and time increased. This gave rise to high thermal conductivity of 90% IACS together with high density, which was mainly attributed to decrease in fractions of grain boundaries and micro-pores working as effective scattering center for electron movement.

Feedstock 종류에 따른 금속분말사출성형 유동특성 분석을 위한 실험적 연구 (An Experimental Study on Rheological Characteristics of Metal Injection Molding by Feedstock Material)

  • 정무철;허영무;신광호;윤길상;장성호;이정원
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.57-61
    • /
    • 2009
  • In recently industry, with the miniaturization and high-precision of machine part, the development of mold manufacturing technology for mass production is accompanied by the development of new industrial field such as IT, NT and BT. The metal injection molding(MIM) process combines the well-known thermoplastic injection and powder metallurgy technologies to manufacture small parts for IT, NT, BT industrial. In this study, the bar type MIM mold with a 800um thickness is made for influence of feedstock material and injection parameter through an experiment.

  • PDF

금속 염 첨가 방법을 이용하여 사출성형된 텅스텐 중합금의 소결거동 (Sintering Behavior of the Injection Molded W-Ni-Fe Heavy Alloy by Addition of Metallic Stat)

  • 김대건;류성수;김은표;이정근;김영도;문인형
    • 한국분말재료학회지
    • /
    • 제6권4호
    • /
    • pp.294-300
    • /
    • 1999
  • This study was carried out to investigate the possibility whether Metal Injection Molding (MIM) process could be applied to 95wt.%W-3.5wt.%Ni-1.5wt.%Fe heavy alloy in order to obtain an intricate shape. Methylcellulose was used in the injection molding for binder. $FeCl_2-4H_2O$ was added in solvent substituting Fe powder and $FeCl_2$ was doped on W-Ni premixed powder. When $FeCl_2-4H_2O$ was added in solvent, the binder separation occurred for injection molding so that the matrix content was changed. Such problem was solved when $FeCl_2$ was doped. In this study. the debinding process did not affect residual carbon content. The sintered microsouctures as addition methods of Fe element and the sintering temperature from $1420^{\circ}C$ to $1470^{\circ}C$, which are around the temperature of liquid phase formation, were observed.

  • PDF

DMLS 금형강의 미세 절삭가공 특성 분석 (Analysis on the Characteristics of Micro Cutting Process for DMLS Mold Material)

  • 윤길상;김건희;이정원;김종덕
    • 한국산학기술학회:학술대회논문집
    • /
    • 한국산학기술학회 2011년도 추계학술논문집 2부
    • /
    • pp.518-520
    • /
    • 2011
  • 금속분말 쾌속조형법의 한 종류인 DMLS 공정은 사출성형품의 균일한 냉각이 가능한 3차원 냉각시스템을 포함한 코어, 캐비티 제작이 가능하다. 그러나, 코어 및 캐비티 내 미세형상의 경우 DMLS로 제작하기에는 난해하므로 별도 미세 절삭가공을 통해 제작할 필요가 있다. 따라서, 본 연구에서는 DMLS금형강 소재의 미세 절삭가공 특성을 분석하고자 하였으며, 이를 위하여 HIP 공정 적용 전 후 DMLS금형강 소재를 대상으로 미세 절삭가공 실험을 수행하고 버 발생 및 공구마모 경향을 분석하였다. 실험 결과 HIP 적용 전 시편이 강도 및 조직측면에서 미세 절삭가공에 상대적으로 유리함을 확인할 수 있었다.

  • PDF

기계적 합금방법으로 제조한 극초미세 조직의 W-Cu 복합분말의 금속사출성형 연구 (Metal Injection Molding of Nanostructured W-Cu Composite Powders Prepared by Mechanical Alloying)

  • 김진천
    • 한국분말재료학회지
    • /
    • 제5권2호
    • /
    • pp.145-153
    • /
    • 1998
  • W-Cu alloy is attractive to thermal managing materials in microelectronic devices because of its good thermal properties. The metal injection molding (MIM) of W-Cu systems can satisfy the need for mass production of the complex shaped W-Cu parts in semiconductor devices. In this study, the application of MIM process of the mechanically alloyed (MA) W-Cu composite powders, which had higher sinterability were investigated. The MA W-Cu powders and reduction treated (RT) powders were injected by using of the multicomponent binder system. The multi-stage debinding cycles were adopted in $N_2$ and $H_2$ atmosphere. The isostatic repressing treatment was carried out in order to improve the relative density of brown parts. The brown part of RT W-Cu composite powder sintered at 110$0^{\circ}C$ had shown the higher sinterability compared to that of MA powder. The relative sintered density of all specimens increased to 96% by sintering at 120$0^{\circ}C$ for 1 hour. The relationship between green density and the sintering behavior of MA W-Cu composite powder was analyzed and discussed on the basis of the nanostructured characteristics of the MA W-Cu composite powder.

  • PDF

금속사출성형을 이용한 STS 316L 밸브피팅 제작에 대한 연구 (A Study of STS 316L Threaded Elbow Fitting Fabrication by Metal Injection Molding)

  • 김재영;김성조;정성택;안석영
    • 소성∙가공
    • /
    • 제24권2호
    • /
    • pp.121-129
    • /
    • 2015
  • A net-shape forming of small and complex-shaped metal parts by metal injection molding (MIM) has economic advantages in mass production, especially for STS 316L valve fitting. STS 316L offers excellent corrosion resistance, but it has poor machinability, which is a limitation in using it for a cost-effective production where both forging and machining are employed. Simulation and experimental analysis were performed to develop a MIM STS 316L 90° elbow fitting minimizing trial and error. A Taguchi method was used to determine which input parameter was the most sensitive to possible defects (e.g. sink mark depth) during the injection molding. The final prototype was successfully built. The results indicate that the simulation tool can be used during the design process to minimize trial and error, but the final adjustment of parameters based on field experience is essential.

금속사출성형을 위한 W-10wt.%Cu 분말의 제조에 관한 연구 (Fabrication of W-10wt.%Cu Powder for the Application of Metal Injection Molding)

  • 김순욱;손찬현;김영도;문인형
    • 한국분말재료학회지
    • /
    • 제8권4호
    • /
    • pp.245-252
    • /
    • 2001
  • Recent remarkable progress in the semiconductor industry has promoted smaller size of semiconductor chips and increased amounts of heat generation. So, the demand for a substrate material to meet both the characteristics of thermal expansion coefficient and heat radiation has been on the increase. Under such conditions, tungsten(W)-copper(Cu) has been proposed as materials to meet both of the above characteristics. In the present study, the W-10wt.%Cu powders were synthesised by the mixing and hydrogen reduction of the starting mixture materials such as W-Cu, $W-CuCl_2$and $WO_3-CuCl_2$ in order to obtain the full densification. The W-10wt.%Cu produced by hydrogen reduction showed the higher interparticle friction than the simple mixed W-10wt%Cu because of the W agglomerates. In the dilatometric analysis the W-10wt.%Cu prepared from the $W-CuCl_2$was largely shrank by heating up $1400^{\circ}C$ at the constant heating rate of $5^{\circ}C$/min. The possibility of application of metal injection molding (MIM) was also investigated for mass production of the complex shaped W-Cu parts in semiconductor devices. The relationship between the temperature of molding die and the pressure of injection molding was analyzed and the heating up stage of 120-$290^{\circ}C$ in the debinding process was controlled for the most suitable MIM condition.

  • PDF

금속분말 사출성형된 Ti-6Al-4V 합금의 미세조직 및 기계적 물성 (Microstructure and Mechanical Properties of Ti-6Al-4V Alloy Processed by Metal Injection Molding)

  • 김민준;백승훈;윤동근;이은혜;김종하;고영건
    • 소성∙가공
    • /
    • 제29권5호
    • /
    • pp.251-256
    • /
    • 2020
  • The purpose of this study is to investigate the effect of sintering condition on the microstructure evolution and tensile properties of the Ti-6Al-4V alloy sample processed by metal injection molding (MIM) in terms of the sizes of the alpha morphology and pore found in the matrix. For this purpose, a series of MIM were conducted on this sample at various sintering temperatures ranging from 1173 to 1373 K for three hours followed by furnace cooling, observed by the scanning electron microscopy. The microstructures sintered in this study showed that, with increasing sintering temperature over beta transus temperature, the transformation of the equiaxed alpha into transformed beta was attained while the size of pores would tend to decrease. Thus, the strength remained unchanged significantly in the tension while ductility increased to some extent as sintering temperature increased. Such mechanical behavior would be explained in relation to the microstructure evolution of the Ti-6Al-4V sample via the MIM.

W-Cu의 마이크로 금속분말사출성형 (Micro Metal Powder Injection Molding in the W-Cu System)

  • 김순욱;양주환;박순섭;김영도;문인형
    • 한국분말재료학회지
    • /
    • 제9권4호
    • /
    • pp.267-272
    • /
    • 2002
  • The production of micro components is one of the leading technologies in the fields of information and communiation, medical and biotechnology, and micro sensor and micro actuator system. Microfabrication (micromachining) techniques such as X-ray lithography, electroforming, micromolding and excimer laser ablation are used for the production of micro components out of silicon, polymer and a limited number of pure metals or binary alloys. However, since the first development of microfabrication technologies there have been demands for the cost-effective replication in large scale series as well as the extended range of available material. One such promising process is micro powder injection molding (PIM), which inherits the advantages of the conventional PIM technology, such as low production cost, shape complexity, applicability to many materials, applicability to many materials, and good tolerance. This paper reports on a fundamental investigation of the application of W-Cu powder to micro metal injection molding (MIM), especially in view of achieving a good filling and a safe removal of a micro mold conducted in the experiment. It is absolutely legitimate and meaningful, at the present state of the technique, to continue developing the micro MIM towards production processes for micro components.

플라즈마 공정으로 구상화된 티타늄 분말과 금속사출성형 공정을 이용한 치과용 부품 제조 (Preparation of Metal Injection Molded Dental Components using Spheroidized Ti Powders by Plasma Process)

  • 곽지나;양상선;윤중열;김주용;박성진;김현승;김용진;박용호
    • 한국분말재료학회지
    • /
    • 제20권6호
    • /
    • pp.467-473
    • /
    • 2013
  • This research presents a preparation method of dental components by metal injection molding process (MIM process) using titanium scrap. About $20{\mu}m$ sized spherical titanium powders for MIM process were successfully prepared by a novel dehydrogenation and spheroidization method using in-situ radio frequency thermal plasma treatment. The effects of MIM process parameters on the mechanical and biological properties of dental components were investigated and the optimum condition was obtained. After sintering at $1250^{\circ}C$ for 1 hour in vacuum, the hardness and the tensile strength of MIMed titanium components were 289 Hv and 584 MPa, respectively. Prepared titanium dental components were not cytotoxic and they showed a good cell proliferation property.