• Title/Summary/Keyword: 균열성장거동

Search Result 240, Processing Time 0.022 seconds

Effects of Strain Hardening Exponents on the Retardation of Fatigue Crack Propagation (가공경화지수가 피로균열 지연거동에 끼치는 영향)

  • 김상철;강동명
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.14 no.5
    • /
    • pp.1193-1199
    • /
    • 1990
  • Effects of strain hardening exponents on the behavior of fatigue crack propagation are experimentally investigated. The retardation effect of fatigue crack propagation after single overloading is investigated in relation to strain hardening exponent and crack closure. A relationship between crack opening ratio and strain hardening exponents is inspected through an examination of the crack closure behavior. An empirical equation relating retardation effect of fatigue crack propagation after single overloading, percent peak load and strain hardening exponent of materials is proposed.

Numerical analysis of rock behavior with crack model implementation (균열모형을 이용한 암석거동의 수치해석)

  • 전석원
    • Tunnel and Underground Space
    • /
    • v.9 no.1
    • /
    • pp.56-63
    • /
    • 1999
  • Rock behaves in a complex way due to the discontinuities. To describe the complicated failure and deformation behavior of rock, many researches were focused on the development of crack models. This study discusses the validity of the sliding and shear crack model to systematically fractured rock, i.e. coal. The model was also implemented into a numerical analysis. For that, a finite element program was modified in several ways. To describe the transverse isotropy in two-dimensional analysis, the stress-strain relationship was modified for the direction of the axis of symmetry. Also, the changes of the effective elastic moduli according to the crack growth were calculated. A simple example of two-dimensional laboratory uniaxial compression test was analyzed. The results coincided with the observations obtained from the laboratory tests.

  • PDF

Fracture Behavior of Aged 15Cr-5Ni Stainless Steel (15Cr-5Ni 스테인리스강의 파괴 거동)

  • Chu, M.C.;Saito, K.;Tubota, M.;Ando, K.
    • Journal of Power System Engineering
    • /
    • v.6 no.1
    • /
    • pp.61-67
    • /
    • 2002
  • 15Cr-5Ni 석출강화 스테인리스강 3종류의 피로균열 발생과 성장 특성 및 파괴인성에 대하여 노치함수로서 연구하였다. 3종류강의 열처리 조건은 $482\;^{\circ}C,\;579\;^{\circ}C$$621\;^{\circ}C$이다. $621\;^{\circ}C$에서 4시간동안 열처리한 시험편 C는 약 $280\;MPa\;\sqrt{m}$의 가장 높은 파괴인성을 보였으며, 3종류에서 피로균열 성장이 가장 늦었다. $482\;^{\circ}C$에서 1시간 열처리한 시험편 A에서, 피로균열발생한계, ${\Delta}k{\rho}$, 는 노치반경0.3 mm에서 약 $280\;MPa\;\sqrt{m}$의 가장 높은 값을 보였다. 시험편 A는 시험편 B와 C보다 피로균열 성장이 빨랐지만, 피로균열 발생이 늦었다. 예 하중에 의한 노치선단의 압축잔류응력은 노치 시험편의 피로강도 향상에 유용한 방법이었다.

  • PDF

A Fructure Mechanics Analysis on the Crack in the Variable Thickness Plate Having Fillet (필렛을 갖는 변후부재의 균열에 대한 파괴역학적 연구)

  • 양원호;최용식;조명래
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.15 no.5
    • /
    • pp.1433-1438
    • /
    • 1991
  • 본 연구에서는 팔렛을 갖는 유한폭 변후판재 내의 모드 Ⅰ균열에 대하여 3차 원 유한요소법으로 응력확대계수를 수치해석하였다.

Behaviour of Fatigue Crack Propagation under Mixed Mode(I+II) with variation of Angle and Crack Length (혼합모드(I+II)하에서 각도와 균열길이 변화를 갖는 피로균열 전파 거동)

  • 정의효
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.9 no.5
    • /
    • pp.73-79
    • /
    • 2000
  • The applications of fracture mechanics have traditionally concentrated on cracks loaded by tensile stresses, and growing under an opening or mode I mechanism. However, many cases of failures occur from growth of cracks subjected to mixed mode loading. Several criteria have been proposed regarding the crack growth direction under mixed mode loadings. This paper is aimed at investigation of fatigue crack growth behaviour under mixed mode(I+II) with variation of angle and pre-crack length in two dimensional branched type precrack. Especially the direction of fatigue crack propagation was predicted and effective stress intensity factor was calculated by finite element analysis(FEA. In this paper, the maximum tangential stress(MTS) criterion was used to predict crack growth direction. Not only experiment but also finite element analysis was carried out and the theoretical predictions were compared with experimental results.

  • PDF

Propagation of Crack in Concrete Subjected to Dynamic Loading (동적하중(動的荷重)을 받는 콘크리트의 구열(龜裂)성장)

  • Kang, Sung Hoo;Kim, Woo
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.8 no.2
    • /
    • pp.135-145
    • /
    • 1988
  • This study deals with the prediction of crack propagation in concrete mortar subjected to static and dynamic load. Total 54 CLWL-DCB(Crack-line-loaded-double-cantilever beam) concrete mortar specimens were tested to measure crack growth using ASTM 561-80. Main variables were sand to cement ratio and water to cement ratio. The resulting load(P)-COD(Crack Opening Displacement; $2V_1$) curves and COD-CTOD (Crack Tip Opening Displacement; $2V_2$) curves were analyzed to calculate effective crack length and physical crack length by way of ASTM 561-80 proposed. Replica crack length were also obtained directly during the test. The differences in crack propagation between under static load and under dynamic load were investigated.

  • PDF

An Experimental Study on the Growth Behavior of Multi-Surface-Cracks in Type 304 Stainless Steel at Elevated Temperature (고온하 304 스테인리스철의 표면규열의 성장거동에 관한 실험적 연구)

  • 서창민;신형섭;황남성;정대윤
    • Journal of Ocean Engineering and Technology
    • /
    • v.9 no.1
    • /
    • pp.63-72
    • /
    • 1995
  • The crack which is discovered in various structures and machine elements is multi-cracks. Multi-cracks may cause serious problems because they grow individually, and coalesce into one and it leads to fracture. Fatigue tests have been carried out to study the growth and coalescence behavior of multi-surface-cracks initiated at the semicircular surface notch in type 304 stainless steel at elevated temperature. The results are as follows; When multi-surface-cracks are lying on the surface of material, the major surface crack has greater influence on the fatigue life than the subcracks. The aspect ratio of multi-surface-cracks is lower than that of single crack because of the interaction and coalescence of surface cracks. Crack growth shape turns to semiellipse from the semicircle notch. After coalescence, the surface crack length increases rapidly, and it leads to fracture. Further, the slope transition of Paris law was found in the da/dN-$\Delta$K$_1$ plots.

  • PDF

Initiation and Propagation Behaviors of Micro-Surface-Fatigue Cracks under In-Plane Tension Fatigue Tests (引張 軸荷重 疲勞 에 의한 微小表面 균열 의 發생 . 成長擧動)

  • 서창민
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.9 no.1
    • /
    • pp.1-9
    • /
    • 1985
  • In-plane tension fatigue tests (R = 0.05) were carried out to investigate the initiation and propagation behaviors of micro-surface-fatigue cracks on smooth surfaces of a mild steel. Also, the investigations of saturated cyclic strain which can be obtained by the fatigue tests have been made via the cyclic strain intensity factor, .DELTA. $K_{\epsilon}$/, for the purpose of unifying two approaches of the study of fatigue; the one approach is based on the fracture mechanics concept and the other on lowcycle fatigue concept. Some of the results are as follows; The growth rate, d(2a)/dN, of small cracks cannot be represented by one straight line as a function of .DELTA.K for various of the nominal stress range, .DELTA..sigma., and is higher than that of a larger through crack. The rearrangement of the d(2a)/dN by .DELTA..epsilon..root..pi.s( = .DELTA. $K_{\epsilon}$/) with the stress range .DELTA..epsilon. in .DELTA.K replaced by .DELTA..epsilon., strain range, gives one straight line of the .DELTA. $K_{\epsilon}$-d(2a)/dN relation for various values of stress range .DELTA.$_{\epsilon}$../.X>../.

An Experimental on the Evalution of Fatigue Crack Propagation of Carbon Steel (탄소강의 피로균열 진전거동 평가에 관한 실험적 연구)

  • 김희송;안병욱
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.13 no.5
    • /
    • pp.938-946
    • /
    • 1989
  • Using the CT specimen of carbon steel(SM45C), we estimated the fatigue crack propagation behavior in stable crack propagation range. Furthermore the fatigue crack propagation rate, Acoustic Emission(AE) count rate, and fractography characteristics were also compared among others. The following results were confirmed by experimental observation. Near-threshold stress intensity factor range(.DELTA. $K_{th}$) is influenced by stress ratio but not at the upper limit of stable crack propagation range. As stress intensity factor range(.DELTA.K) and(or) stress amplitude increase (s), both crack propagation rate(da/dN) and AE count rate(dn/dN) increase. Effective stress intensity factor range(.DELTA. $K_{off}$) determined from the crack closure point measurement by AE method is useful for the evaluation of fatigue crack propagation rate. Fractography in stable crack propagation range showed striation, and agreed with the crack propagation rate obtained either by experiment of by the results of microscopic measurements.s.