• Title/Summary/Keyword: 공작물 제거율

Search Result 2, Processing Time 0.014 seconds

Machining Characteristics of WEDM due to Electrical Conductivity of Dielectric (방전액의 전도율의 변화에 따른 와이어방전가공의 가공특성)

  • Kim, Chang-Ho;Kang, Jae-Won
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.15 no.6
    • /
    • pp.15-21
    • /
    • 2006
  • This work deals with the electrical conductivity of dielectric on output parameters such as metal removal rate and surface roughness value of a carbon steel(SM25C) and sintered carbides cut by wire electrical discharge machining (WEDM). Dielectric has several functions like insulation, ionization, cooling, the removal of waste metal particles. The presence of minute metal particles(debris) in spark gap contaminates and lowers the breakdown strength of dielectric. And it is considered that too much debris in spark gap is generally believed to be the cause of arcing. Experimental results show that increases of cobalt amount in carbides affects the metal removal rate and worsens the surface quality as a greater quantity of solidified metal deposits on the eroded surface. Lower electrical conductivity of the dielectric results in a lower metal removal rate because the gap between wire electrode and workpiece reduced. Especially, the surface characteristics of rough-cut workpiece and wire electrode were analyzed too. Debris were analyzed also through scanning electron microscopy(SEM) and surface roughness tester. Micro cracks and some of electrode material are found on the workpiece surface by energy dispersive spectrometer(EDS).

Die Sinking Electrical Discharge Machining of SiC/AI Metal Matix Composite (탄화규소/알루미늄 금속계 복합재료의 형상방전가공)

  • 왕덕현
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.7 no.1
    • /
    • pp.34-40
    • /
    • 1998
  • Conductive metal matrix composite(MMC) material of 30% silicon carbide particulated based on aluminum matrix was machined by die sinking electrical discharge machining(EDM) process according to different current and duty factor for reverse polarity of electrode. Material removal rate(MRR) was examined by process under various operation conditions. The surface morphology was evaluated by surface roughness parameter and scanning electron microscopy(SEM) research. The MRR was suddenly increased over 11 ampere of current, and it was slightly changed over 0.3 of duty factor. The maximum surface roughness of EDMed surface was affected by the duty factor. The SEM photograghs of EDMed surface showed wide recast distribution region of melting materials as increased of current and duty factor.

  • PDF