열교환기용 BAS111합금 고주파유도용접관에서 인발조건이 기계적 특성에 미치는 영향 (Effects of Drawing Parameters on Mechanical Properties in High Frequency Induction Welded Tubes of BAS111 Alloy for Heat-exchangers)

  • 국진선;김낙찬;송중근;전동태
    • Journal of Welding and Joining
    • /
    • 제22권4호
    • /
    • pp.65-72
    • /
    • 2004
  • The aim of this study is to investigate the optimum drawing parameter for BAS111 welded tubes. The BAS111 aluminium alloy tubes with 25.4mm in external diameter and 1.5mm in thickness for heat-exchangers were manufactured by high frequency induction welding with the V shaped convergence angle 6.8$^{\circ}$ and power input 50㎾. With increasing the reduction of area (1.6, 5.8, 11.5, 14.2, 18.5, 22.5%) by drawing, tensile strength was increased and elongation was decreased. With increasing the reduction of area by drawing, hardness in weld metal increased rapidly, while that of base metal increased slowly. In the specimen with the outer diameter smaller than 22mm, hardness of weld metal was higher than that of base metal. The optimum drawing parameter of area reduction was estimated about 15% because of the work hardening of welds.

고주파 유도가열된 조선용 강판의 기계적 특성 연구 (A Study on the Mechanical Properties of Heated Plates by Induction Heating System)

  • 현충민;이명수;조시훈;장태원
    • Journal of Welding and Joining
    • /
    • 제32권1호
    • /
    • pp.47-52
    • /
    • 2014
  • Due to of high intensity, lower noise and easy controllability of the heat, induction heating system became well known. Induction heating method has been suggested as substitute for the gas heat source and adopted in the automation of curved hull forming system. In this study, an investigation was accomplished to find the effects on the change of material properties when the induction heating was applied on the mild steel plate. Plates were heated using weaving method to get sufficiently heat affected zone and then cooled with water or in the air. The mechanical properties of the heated plate were evaluated. As results, the tensile test, impact test and microstructures satisfied the class rule.

직렬공진 PWM인버터를 이용한 전자간절유도가열 열유체 에너지시스템과 그 성능평가 (Electromagnetic Indirect Induction Fluid Heating System using Series Resonant PWM Inverter and Its Performance Evaluations)

  • 김용주;김기환;신대철
    • 전력전자학회논문지
    • /
    • 제7권1호
    • /
    • pp.48-54
    • /
    • 2002
  • 본 논문에서는 간접 유도가열 되는 DPH시스템과 주파수 범위가 20kHz에서 50kHz사이에서 작동되는 전압형 직렬공진 고주파인버터를 이용하여 열 기체를 발생시키는 전압형 공진형 인버터에 관하여 설명하였다. 얇은 스텐레스 판재가 서로 스폿 용접되어 연결되어 있고 미세한 많은 구멍을 갖고있는 적층형 충진발열테로 특수하게 설계된 유도 가열기는 외부에 워크 코일로 감겨져 있는 불소수지계의 절연용기 안에 삽입되어 있다. 이 워크 코일은 공진형 인버터와 연결되어 있으며 유도가열기를 통해 흐르는 관 유체를 1단가열부에서 저압의 포화증기를 2단가열부에서 열방사성 증발유체를 생성하는 본 DPH시스템의 성능 및 효용성을 실용적인 측면에서 논의하고 평가 할 것이다.

고주파 유도가열을 이용한 선상가열 시 각 변형 예측에 관한 연구 (A study on the prediction of the angular distortion in line heating with high frequency induction heating)

  • 박동환;진형국;박성식;신상범
    • Journal of Welding and Joining
    • /
    • 제33권1호
    • /
    • pp.80-86
    • /
    • 2015
  • The purpose of this study is to establish the predictive method of the angular distortion caused by the line heating process with high frequency induction heating. In order to do it, the heat input model for the high frequency induction heating system was established through comparing the temperature evaluation results obtained by both FEA and experiment. The critical heating conditions to prevent the degradation of the work piece with various thicknesses were identified by FEA and microstructure test results. Under the critical heating conditions, the extensive line heating tests were performed. According to the test results, it was found that the angular distortion behavior of the heated plates could be defined as the function of heat intensity and the rigidity of heated plate. In addition, it was clarified that the angular distortion strongly depended on the size of test specimen such as the length and the width of the heated plate. Based on these results, the predictive equation for the angular distortion was established with the function of heat intensity, bending rigidity and size of heated plate.

국부가열용 고주파 유도가열 특성에 관한 연구 (A Study on Characteristic of High Frequency Induction Heating for Local Heating)

  • 진형국;이동주;신상범
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2010년도 춘계학술발표대회 초록집
    • /
    • pp.60-60
    • /
    • 2010
  • Since the curved hull plate was made by a series of manufacturing process including cold bending, manual local heating and correction work, the accuracy of curved plate strongly depends on the proficiency of worker. So the demands on the automatic local heating system for curved hull plate have continuously increased and the various researches relevant to it have been performed. Generally, the heat sources used for local heating were flame and induction heat. In terms of initial cost, flame heating is in a better favorable position than induction heating. However, from the viewpoint of the control of heat, induction heating has more advantage. So the various researches related to apply the induction heating to the automatic forming system has been performed. The purpose of this study is to establish the proper capacity of high frequency induction heating system for forming the curved hull plate. In order to do it, the proper coil shape for local heating was designed and the efficiency of induction heating system was determined by comparing of temperature results obtained by FEA and experiment. With the results, the extensive FEA was performed to identify the effect of heated plate dimension, cooling method and the capacity of induction heating system on the amount of heat loss introduced by induction heating. Based on the results, the proper capacity of high frequency induction heating system was proposed.

  • PDF

고주파유도용접된 열교환기용 BAS121합금튜브의 기계적 특성에 미치는 인발조건의 영향 (Effects of Drawing Parameters on Mechanical Properties of BAS121 Alloy Tubes for Heat-exchangers by High Frequency Induction Welding)

  • 한상우;김병일;이현우;전우용;국진선
    • 한국재료학회지
    • /
    • 제14권12호
    • /
    • pp.851-856
    • /
    • 2004
  • The aim of this study is to investigate the optimum drawing parameter for BAS121 welded tubes. The BAS121 aluminium alloy tubes with 25 mm in external diameter and 1.3 mm in thickness for heat-exchangers were manufactured by high frequency induction welding with the V shaped convergence angle $6.5^{\circ}$ and power input 55 kW. With increasing the reduction of area ($13,\;21\%$) by drawing, tensile strength was increased and elongation was decreased. With increasing the reduction of area by drawing, hardness in weld metal increased rapidly, while that of base metal increased slowly. In the specimen with the outer diameter smaller than 22 mm, hardness of weld metal was higher than that of base metal. The optimum drawing parameter of area reduction in BAS121 alloys was estimated about $13\%$ because of the work hardening of welds.

Ag-Cu-Zn-Cd 계 용가재를 이용한 Bronze 소결체/강의 브레이징 접합부 특성 평가 (Characteristics of Brazed Joint of Sintered Bronze/steel Using Ag-Cu-Zn Type Filler Materials)

  • 이정훈;이창희
    • Journal of Welding and Joining
    • /
    • 제17권3호
    • /
    • pp.79-89
    • /
    • 1999
  • The study was carried out to examine in more detail metallurgical and mechanical properties of brazed joints of diamond cutting wheel. In this work, shank(mild steel) and sintered bronze-base tips were brazed with three different filler materials(W-40, BAgl and BAg3S). The machine used in this work was a high frequency induction brazing equipment. The joint thickness, porosities and microstructure of brazed joints with brazing variables(brazing temperature, holding time) were evaluated with OLM, SEM, EDS and XRD. Bending(torque) test was also performed to evaluate strength of brazed joints. Further wetting test was performed in a vacuum furnace in order to evaluate the wettability of filler metals on base metals9shank and tips). The brazing temperature had a strong influence on the joint strength and the optimum brazing temperature range was about $700~850^{\circ}C$ for the bronze/steel combinations. The strength of the brazed joint was found to be influenced by the three factors : degree of reaction region, porosity content, joint thickness. The reaction region was formed in the bronze-base tip adjacent to the joint. The reaction region resulted in a bad influence on the strength due to the formation of Cu5.6Sn, CuZn4, $\beta(CuZn)$ and CdAg, etc. Porosities increased as brazing variables(brazing temperature, holding time) increased, and the brazed joints with porosities of less than about 3-5% had an optimum strength for the bronze-base tip.