급냉 제강 슬래그 치환 고성능 그라우트의 유동특성 (Fluidity Properties of the Rapidly-Chilled Steel Slag Replacement High-Performance Grout)

  • 이건영;이건철;최중구;박헌일
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.110-111
    • /
    • 2014
  • Amount of slag which is a recycled aggregate that be produced as a industrial by-product from steel production process is increasing. But there is few suggestions for usage of slag except for shaft furnace slag and studies for utilizing this are lacked. In this study, it reviews flow characteristics according to replacement ratio of rapid cooling steelmaking slag from the perspective of rheology. Replacement ratio of ps ball is used by replacing 40, 45, 50% for each binder mass.

  • PDF

팽창재 및 플라이애쉬를 이용하는 수중불분리 모르터의 특성 (Properties of Undispersed Underwater Mortar Using the Expansive Additives and Fly Ash)

  • 한천구;이대주;이광설;한일영;권지훈;유홍종
    • 콘크리트학회지
    • /
    • 제10권6호
    • /
    • pp.223-231
    • /
    • 1998
  • 종래의 시멘트 모르터 그라우트 방식에 의한 제자리 콘크리트 말뚝은 시공후 자기수축 및 건조수축 등에 의하여 말뚝의 내력이 저하하고, 지하수에 의하여 재료분리가 발생하며, 많은 단위시멘트량에 의한 비경제성 등이 문제시되고 있다. 그러므로 본 연구는 팽창제 및 플라이애쉬 등 각종 혼화재료를 이용한 제자리 콘크리트 말뚝용 고성능 시멘트 모르터의 역학적 성질이 분석되었다. 실험결과 팽창재 혼입율이 증가함에 따라 유동성은 감소하고, 공기량은 증가하며, 응결시간은 지연되고 압축강도는 7일에서는 감소하나 28일 및 91일 재령인 경우는 팽창제혼입율 5%에서 약간 상승하는 것으로 나타났다. 플라이애쉬치환율이 증가함에 따라 유동성은 양호해지고, 공기량은 증가하며, 응결시간은 지연되고 압축강도는 약간 감소하였다. 또한 길이변화특성은 팽창재혼입율이 증가할수록 크게 팽창하고, 플라이애쉬치환율이 증가할수록 수축은 작은 것으로 나타났다.