• Title/Summary/Keyword: 결함길이

Search Result 202, Processing Time 0.026 seconds

A Study on Measurement of Internal Defects of Pressure Vessel by Digital Shearography(II) (전자 전단 간섭법을 이용한 압력용기의 내부결함 측정에 관한 연구(II) (전자 전단 간섭법을 이용한 압력용기의 내부결함 검출 시스템의 오차 분석))

  • Kang, Young-June;Park, Nak-Kyu;Ryu, Won-Jae;Kim, Dong-Woo
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.22 no.4
    • /
    • pp.402-410
    • /
    • 2002
  • Recently the necessity of study on optical measuring method using laser to detect the pipeline's defect in nuclear facilities, chemical industries and power plants has been increased. Because laser light can be delivered to a remote area without any difficulties, the application of laser in many industries can solve several difficulties from the limitation of access in danger area and reduce the risks of workers. Therefore, we applied a new experimental technique to the measurement of internal defects in pressure vessels with the combination of shearography and image processing technique and detected the internal cracks of pressure vessels in the former paper. In this paper, we used the same optical system as in the former study and found the optimum shearing magnitude by comparing the real length of specimen with experimental results. A variety of conditions were applied to certify the validity of this method. Actually, several specimens which have different lengths and depths were used in this experiment under the three diverse pressure. Consequently, we have carried out this experiment to determine the limit of measurement ability with analyzing errors.

Electromigration Characteristics in Al-1%Si hin Film Interconnections for Microelectronic Devices (극소전자 디바이스를 위한 Al-1%Si 박막배선에서의 electromigration 특성)

  • 박영식;김진영
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 1995.06a
    • /
    • pp.48-49
    • /
    • 1995
  • 전자소자의 축소화에 따라 electromigration은 점차 반도체 디바이스의 주요 결함 원 인으로 부각되고 있다. 본 실험은 현재 배선 재료로 널리 사용되고 있는 Al-1%Si 금속박막 배선의 electromigration에 대한 온도 및 배선길이 의존성에 관하여 연구하였다. ppLCC(pplastic Leaded Chipp Carrier) ppackage된 ppSG(8000$\AA$)/SiO2(1000$\AA$)/Al-1%Si(7000 $\AA$)/SiO2(5000$\AA$)/pp-typpe Si(100)의 보호막처리된 시편과 Al-1%Si/SiO2(5000$\AA$)/pp-typpe Si(100)의 보호막처리되지 않은 시편등을 standard pphotolithograpphy 공정을 이용하여 각각 제작하였다. 선폭 3$mu extrm{m}$, 길이 100, 400, 800, 1600$\mu\textrm{m}$의 등의 Al-1%Si 박막배선구조를 사용하 였다. 가속화실험을 위해 인가된 D.C 전류밀도는 4.5$\times$106A/cm2이었고 실온에서 10$0^{\circ}C$까지 의 분위기 온도에서 electromigration를 실행하였다. 박막배선길이에 따른 MTF(Mean Time-to-Failure)는 임계길이 이상에서 포화되는 경향을 보이며 임계길이는 Al-1%Si 박막 배선에서 분위기온도에 따라 길이 400$\mu\textrm{m}$과 800$\mu\textrm{m}$범위에서 나타났다. 각 시편에서 electromigration에 대한 활성화에너지도 MTF의 특성과 유사하게 임계길이 이상에서 포화 되는 특성을 타나내었다.

  • PDF

A Study of the Detection for Underclad Cracks of Nuclear Pressure Vessel (원자력 압력용기의 피복하부 결함검출에 대한 고찰(II))

  • Park, C.S.;Kang, K.W.
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.13 no.2
    • /
    • pp.31-39
    • /
    • 1993
  • It has not been performed to inspect the underclad cracking of nuclear pressure vessel in Korea since there is no code requirements for inspection. However, underclad cracks in nuclear pressure vessels have been reported since the early 1970s. The aim of this experiment is to find the suitable ultrasonic inspection techniques for underclad cracking. The various transducers, for example $70_{\backprime}$ refracted longitudinal wave, 50/70 multibeam, SLIC-40, SLIC-50, are used in this investigation. Experiments on prescreening blocks and a demonstration block under the same condition as in the nuclear power pressure vessels show that the $70_{\backprime}$ refracted longitudinal wave method is the best one for the length evaluation and also gives a good signal pattern for detection of the crack, while the 50/70 multibeam transducer is more effective for the detection of underclad cracking. On the other hand, the SLIC-50 transducer using M-SPOT(Satellite Pulse Observation Technique) and M-PET (Peak-Echo Technique) methods is the most effective one for the depth of underclad crack estimation.

  • PDF

Study on Buckling Instability of Expansion Tube using Finite Element Method (유한요소법을 이용한 팽창튜브의 좌굴불안전성에 관한 연구)

  • Choi, Won-Mok;Kwon, Tae-Su;Jung, Hyun-Sung
    • Journal of the Korean Society for Railway
    • /
    • v.13 no.2
    • /
    • pp.147-151
    • /
    • 2010
  • Since the kinetic energy is dissipated through plastic deformation energy generated in expanding process of the tube by a die. In order to successfully absorb the kinetic energy there should be no buckling in the expansion tube during expanding process. The buckling instability of the expansion tubes is affected by the initial boundary conditions, tube thickness and length. In this study, the effects of the tube thickness except length and initial boundary condition on the buckling instability are studied using a finite element method. In addition, Analysis procedure for nonlinear post-buckling analysis of expansion tube is established. There are three kinds of finite element analysis procedures for buckling analysis of expansion tube, quasi-static analysis, linear buckling analysis and nonlinear post-buckling analysis. The effect of the geometry imperfections defined as linear superimposition of buckling modes is considered in the nonlinear post-buckling analysis. The results of finite element analysis indicate that the buckling load increase with increase of thickness of tube and geometry imperfection. Finial buckling shapes are changed with respect to the geometry imperfection.

Assessment of Composite Cylinder Flaw for Compressed Natural Gas Vehicles (압축천연가스자동차용 복합재료용기의 외피손상결함 평가)

  • Kim, Young-Seob;Kim, Lae-Hyun;Yang, Dong-Ju
    • Proceedings of the Korea Society for Energy Engineering kosee Conference
    • /
    • 2010.04a
    • /
    • pp.43-43
    • /
    • 2010
  • 국내에 천연가스버스가 보급된 이래 5차례의 용기파열 사고가 발생하였는데 그중 2005년 8월 전주 덕진충전소에서 발생한 용기파열사고는 CNG용기의 라이너를 감싸고 있는 복합재료가 손상되어 발생한 사고로 보고되었다. 복합재료용기의 외피손상이 원인이 되어 발생한 사고사례는 해외에서 약 13건이 보고되었다. CNG용기 외피손상은 용기룰 고정하는 스트랩과 밀접한 관련이 있다. 용기고정이 불완전하면 슬립이 발생하고 이는 복합재의 손상으로 이어진다. 본 연구에서는 ISO 19078, CGA C6.4 등 국제코드의 규정을 고려하여 국내에서 제조된 Type 2, 3, 4 용기와 외국에서 생산된 Type 3 용기를 대상으로 결함깊이, 길이, 넓이에 따른 복합재료 결함 내구성시험을 수행하여 CNG용기의 내구성능을 평가하였고, 시험과 동일한 조건으로 복합재료 손상결함 조건을 컴퓨터로 전산모사하여 시험결과의 타당성과 유효성을 비교 검증하였다. 실험결과, Type 2 용기의 경우, 11,250회의 최소반복가압 회수를 충족하였으나 외피손상부와 반복가압에 따른 실제누출부위가 일치하지 않아 실험조건을 달리한 추가실험이 요구되었다. Type 3 용기의 경우에는 복합재 결함부위와 누수부위가 일치된 시험용기의 수는 67%정도로, 복합재료 용기의 수명을 저하시키는 원인으로 라이너와 외피손상이 서로 밀접한 관련이 있음을 확인하였다. Type 4 용기는 국제기준에서 요구하는 반복횟수를 만족하였고, 손상깊이 0.75mm와 1.25mm에서 반복가압회수가 60,000회 이상이 되어도 누설이 발생되지 않았다. 이는 라이너의 재질이 폴리머로서 균일한데다 탄소섬유 복합재료층 위에 유리섬유 복합재료 층이 1.5mm 정도 추가로 적층되어 있어서 3등급의 손상결함(결함깊이 1.25mm)에서도 구조 층이 전혀 손상되지 않은 것으로 판단되며, 이는 Type 2 용기의 강재라이너나 Type 3의 알루미늄 라이너와 비교하여 Type 4 용기의 폴리에틸렌 라이너의 물성이 반복성능이 탁월함을 확인할 수 있었다.

  • PDF

Determination of an Test Condition for IR Thermography to Inspect a Wall-Thinning Defect in Nuclear Piping Components (원전 배관 감육 결함 검사를 위한 IR 열화상시험 조건 결정)

  • Kim, Jin-Weon;Yun, Won-Kyung;Jung, Hyun-Chul;Kim, Kyeong-Suk
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.32 no.1
    • /
    • pp.12-19
    • /
    • 2012
  • This study conducted infrared (IR) thermography tests using pipe and plate specimens with artificial wall-thinning defects to find an optimal condition for IR thermography test on the wall-thinned nuclear piping components. In the experiment halogen lamp was used to heat the specimens. The distance between the specimen and the lamp and the intensity of halogen lamp were regarded as experimental parameter. When the distance was set to 1~2 m and the lamp intensity was above 60 % of full power, a single scanning of IR thermography detected all artificial wall-thinning defects, whose minimum dimension was $2{\Theta}=90^{\circ}$, d/t=0.5, and $L/D_o=0.25$, within the pipe of 500 mm in length. Regardless of the distance between the specimen and the lamp, the image of wall-thinning defect in IR thermography became distinctive as the intensity of halogen lamp increased. The detectability of IR thermography was similar for both plate and pipe specimens, but the optimal test condition for IR thermography depended on the type of specimen.

Electromigration Characteristics in AI-1%Si Thin Film Interconnections for Microelectronic Devices (극소전자 디바이스를 위한 AI-1%Si 박막배선에서의 Electromigration 특성)

  • 박영식;김진영
    • Journal of the Korean Vacuum Society
    • /
    • v.4 no.3
    • /
    • pp.327-333
    • /
    • 1995
  • 전자소자의 축소화에 따라 박막배선에서의 electromigration은 점차 극소전자 디바이스의 주요 결함원인으로 부각되고 있다. 본 실험에서는 현재 박막 배선 재료로 가장 널리 사용되고 있는 AI-1%Si 금속박막배선의 electromigration에 대한 온도 및 배선길이의 의존성에 관하여 연구하였다. PSG($8000AA$)/SiO2(1000$\AA$)/AI-1%Si(7000$\AA$)/SiO2(5000$\AA$)/p-Si(100)의 보호막처리되지 않은 시편 등을 standard photolithography 공정을 이용하여 각각 제작하였다. 선폭 3$\mu$m, 길이 100, 400, 800, $\1600mu$m등의 AI-1%Si 배막배선구조를 사용하였다. 가속화실험을 위해 인가된 d.c.전류밀도는 4.5X106A/$ extrm{cm}^2$이었고 실온에서 $100^{\circ}C$까지의 분위기 온도에서 electromigration test를 진행하였다. 박막배선의 길에에 따른 MTF(Mean-Time-to-Failure)는 임계길이 이상에서 포화되는 경향을 보이며 이는 보호막층의 유무에 관계없이 나타난다. 선폭 $3\mu$m인 AI-1%Si 박막배선에서 임계길이는, 보호막처리된 시편은 $800\mu$m, 보호막처리되지 않은 시편은 $400\mu$m 배선길이에서 나타난다. 이러한 포화의 경향은 낮은 온도에서 더욱 명확해지는 특성을 보인다. 각 시편에서 electromigration에 대한 활성화에너지도 MTF의 특성과 유사하게 임계길이 이상에서 포화되는 특성을 보인다.

  • PDF