Property Evaluation of the Concrete Replacing 5-13mm Recycled Coarse Aggregates (5~13mm 입도분급 순환 굵은 골재 혼합사용에 따른 콘크리트의 특성평가)

  • Han, Min-Cheol;Song, Young-Wo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.17 no.1
    • /
    • pp.55-61
    • /
    • 2017
  • This paper is to investigate experimentally the effect of substitution of recycled coarse aggregate(RCA) under 13mm on the engineering properties of the concrete using gap graded coarse aggregates. Concretes with 0.4 of water to cement ratio(W/C) were fabricated to achieve 30MPa of design strength with coarse aggregate over 13mm in size with the maximum size of 25mm. RCA was substituted for coarse aggregate over 13mm from 10% to 50% and crushed coarse aggregate under 13mm was also substituted for coarse aggregate over 13mm from 20% to 40%, respectively. Test results indicated that the replacement of RCA up to 20% resulted in an increase of fluidity and strength. It also caused a decrease in the drying shrinkage due to dense packing effect by achieving continuous grading of mixed aggregates. For practical application of RCA, when properly substituted, the use of RCA enabled the concrete to reduce water contents and sand to aggregate ratio in mixing design stage of the concrete. And, it can also enhance the compressive strength of the concrete.

Effect of the Replacement of Recycled Coarse Aggregates Under 13mm on Engineering Properties of the Concrete (13mm 이하 순환굵은골재 치환이 콘크리트의 공학적 특성에 미치는 영향)

  • Han, Min-Cheol;Kang, Byeong-Heo
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.1
    • /
    • pp.43-49
    • /
    • 2015
  • The objective of this paper is to investigate experimentally the effect of the substitution of recycled aggregates under 13mm on the properties of the concrete using coarse aggregate with size of 13~25mm. Recycled aggregate under 13mm were substituted to the concrete ranged from 10% to 100%. To compare the properties with the case of recycled aggregate, crushed stone with smaller than 13mm was also substituted to the concrete by 20% and 40%. Test results showed that increase of recycled aggregate under 13mm resulted in the increase of slump and compressive strength compared with plain mixture, which was made with only aggregate with 13~25mm size. This is due to the dense gradation of aggregate in association with addition of relatively small particle. It is thought that the use of recycled aggregate under 13mm along with 30% contributes to the quality improvement of the concrete made with only 13~25mm aggregate.