• 제목/요약/키워드: 갈바닉 부식

검색결과 61건 처리시간 0.026초

구리의 내식성에 미치는 어닐링 열처리의 영향 (Effect of Annealing Heat Treatment to Corrosion Resistance of a Copper)

  • 김진경;문경만;이진규
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제29권6호
    • /
    • pp.654-661
    • /
    • 2005
  • Copper is a well known alloying element that is used to improve the resistance to general corrosion of stainless steel And also Cu cation have the anti-fouling effect to inhibit adhesion of the marine algae and shellfish to the surface of heat exchanger cooling pipe or outside wall of the ship, Therefore there are some anti-fouling methods such as anti-fouling Paint mixed with copper oxide or MGPS(Marine Growth Preventing System) by using Cu cation dissolved to the sea wather solution. Cu cation can be dissolved spontaneously by galvanic current due to Potential difference between Cu and cooling pipe of heat exchanger with Ti material, which may be one of the anti-fouling designs. In this study the effect of annealing heat treatment to galvanic current and Polarization behavior was investigated with a electrochemical points of view such as measurement of corrosion Potential, anodic polarization curve. cyclic voltammetric curve, galvanic current etc The grain size of the surface in annealed at $700^{\circ}C$ was the smallest than that of other annealing temperatures. and also the corrosion Potential showed more positive potential than other annealing temperatures. The galvanic current between Ti and Cu with annealed at $700^{\circ}C$ was the largest value in the case of static condition. However its value in the case of flow condition was the smallest than the other temperatures. Therefore in order to increase anti-fouling effect by Cu cation, the optimum annealing temperature in static condition of sea water is $700^{\circ}C$, however non- heat treated specimen in the case of flow condition may be desirable.

선박재료용 SS400강의 내식성에 대한 용접후 열처리효과에 관한 전기화학적 연구 (II) (An Electrochemical Study on the Effect of Post-Weld Heat Treatment about Corrosion Resistance Property of SS400 Steel for Ship`s Materials)

  • 김성종;김진경;문경만
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제24권5호
    • /
    • pp.58-68
    • /
    • 2000
  • When SS400 steel was welded with low hydrogen type and ilmennite type welding, the effect of post-weld heat treatment(PWHT) was investigated with parameters such as micro vickers hardness, corrosion potential, polarization behaviors, galvanic current, Al anode generating current and Al anode weight loss etc. Hardness of each parts(HAZ, BM, WM) by PWHT in case of low hydrogen type and ilmennite type welding was lower than that of each parts by As-welded However hardness of WM area in case of low hydrogen type and ilmennite type welding was the highest among those three parts regardless of PWHT, Whereas in case of ilmennite type welding, WM area was the highest potential among these three parts on galvanic potential series with As-welded while BM area was the highest potential among these three parts by PWHT on the contrary. And in case of low hydrogen type welding, galvanic corrosion and micro cell corrosion of welding parts was decreased with PWHT. However, It was increased with PWHT in case of ilmennite type welding. Moreover Al anode generating current and anode weight loss in case of low hydrogen type was decreased by PWHT compared to As-wedled but, which was increased than that of As-welded in case of ilmennite type welding. Therefore, it is suggested that Corrosion resistance property in case of low hydrogen type welding is increased by PWHT. However its property was devreased with PWHT in case of ilmennite type welding.

  • PDF

다이폴 모델링 기법을 이용한 수중 전기장 신호 특성 예측 기법 연구 (A Study on Prediction Technique for Underwater Electric Field Signature Characteristic using Dipole Modelling Method)

  • 양창섭;정현주;이종주;전재진
    • 한국자기학회지
    • /
    • 제18권6호
    • /
    • pp.221-224
    • /
    • 2008
  • 본 논문에서는 함정 선체의 갈바닉 부식 전류에 의해 발생되는 수중 전기장 신호를 경계요소 해석 도구인 FNREMUS 소프트웨어를 이용하여 예측하고, 예측된 신호로부터 함정 전기장 신호 특성을 특이치 분해(singular value decomposition) 방법을 이용하여 등가적으로 다이폴 모델링하는 방법에 대해 기술하고 있다. 제안된 다이폴 모델링 기법은 30 m 심도에서 예측된 경계요소 해석 결과와의 평균 차이 비교 방법을 통해 타당함이 확인되었다. 본 논문에서 제안된 모델링 기법을 이용하면 함정에서의 다양한 심도 변화에 따른 수중 정 전기장 신호 분포 특성 예측 및 분석이 가능하다.

AL계 희생양극에 의한 2종스테인리스 강축의 음극방식 실용화 연구 (Study of Practical Cathodic Protection of 2nd Class Stainless Steel Shaft by means of Al Sacrificial Anode)

  • 손영태;이명훈;이희준
    • 선박안전
    • /
    • 통권22호
    • /
    • pp.34-53
    • /
    • 2007
  • In the case of hull material. large sized merchant ships are made of steel, on the other hand FRP or wood are used for small sized fishing boats. At present in Korea approximately 88,500 fishing boats are in operation of which 70% are made of FRP In the meantime, stainless steel is frequently used as shaft materials of the small-size FRP fishing boat. Namely, the kinds of shaft materials are STS 304(18Cr-8Ni), STS 316(18Cr-12Ni-2.5Mo steel) and STS 630(17Cr-Ni-Nb steel)etc. Among these things, STS 304 which is the cheapest and having ordinary corrosion resistance is most widely used as 2nd class shaft material. But, using STS 304 for shaft system material of the small-size FRP fishing boat on seawater environments entails a severe corrosion which causes shaft system troubles. Particularly, the corrosions tend to be concentrated of the stern and bow side, propeller shaft surface of inside of stern tube and the boat having no stern cooling pipe line system. As a solution for those problems, research on the ways to mitigate corrosion on the part of 2nd class stainless steel shaft have been undertaken. In the result, not only clarification for the reason of corrosion of the part of stainless steel shaft used mainly for the small-size FRP fishing boat was done, but also most optimal corrosion protection system was developed by experimenting shaft's protection simulation based of the electrochemical cathodic protection principle. In addition, verification through the field test on the optimal cathodic corrosion protection method by means of aluminum sacrificial anode was carried out. In this study, effective and economical shaft's protection system is suggested to the small-size FRP fishing boat operator by substantiating the results obtained from the research on the optimal cathodic protection.

  • PDF

가스 질화를 통한 316L스테인리스강의 내식성 개선 (Improvement of Corrosion Resistance of 316L Stainless Steel by Gas Nitriding)

  • 조현빈;박세림;김지수;이정훈
    • 전기화학회지
    • /
    • 제27권1호
    • /
    • pp.8-14
    • /
    • 2024
  • 오스테나이트계 스테인리스강은 내식성 및 성형성이 양호하여 다양한 분야에 적용되며, 구리계의 합금을 용가재로 하는 브레이징을 통하여 다양한 형상의 제품으로 가공되어 활용되고 있다. 이때, 구리 기반의 용가재와 스테인리스강의 계면에서 갈바닉 셀을 형성하여 부식을 촉진할 수 있으며, 확산을 통해 스테인리스강에 고용 시 형성되는 구리 과다 영역(Cu-rich region)은 공식 발생의 기점이 되어 내식성을 저하시킨다. 본 연구에서는 브레이징이 적용된 스테인리스강의 내식성을 개선하고자, AISI 316L 스테인리스강에 암모니아 가스를 이용한 질화처리를 적용하였다. 질화처리한 시편은 처리 온도가 증가함에 따라 두께가 증가하고 표면 경도가 높아졌다. 동전위분극시험을 통해 내식성을 평가한 결과 질화층 내 고용된 질소의 용출 및 부동태 거동으로 모재대비 내식성이 개선되었지만 처리온도가 높아 크롬질화물(CrN) 분율이 증가하는 경우 내식성이 감소하였다.

선박 해수배관에서 용접봉의 종류에 따라 직류 아크 용접한 용접부위의 부식특성에 관한 전기화학적 평가 (Electrochemical Evaluation of Corrosion Property of Welded Zone of Seawater Pipe by DC Shielded Metal Arc Welding with Types of Electrodes)

  • 이성열;이규환;원창욱;나승수;윤영곤;김윤해;이명훈;문경만;김진경
    • 한국해양공학회지
    • /
    • 제27권3호
    • /
    • pp.79-84
    • /
    • 2013
  • The seawater pipes in the engine rooms of ships are surrounded by severely corrosive environments caused by fast flowing seawater containing chloride ions, high conductivity, etc. Therefore, it has been reported that seawater leakage often occurs at a seawater pipe because of local corrosion. In addition, the leakage area is usually welded using shielded metal arc welding with various electrodes. In this study, when seawater pipes were welded with four types of electrodes(E4311, E4301, E4313, and E4316), the difference between the corrosion resistance values in their welding zones was investigated using an electrochemical method. Although the corrosion potential of a weld metal zone welded with the E4316 electrode showed the lowest value compared to the other electrodes, its corrosion resistance exhibited the best value compared to the other electrodes. In addition, a heat affected zone welded with the E4316 electrode also appeared to have the best corrosion resistance among the electrodes. Furthermore, the corrosion resistance of the weld metal zone and heat affected zone exhibited relatively better properties than that of the base metal zone in all of the cases welded with the four types of electrodes. Furthermore, the hardness values of all the weld metal zones were higher than the base metal zone.

용접재료 별 주강 피스톤 크라운 용접부위의 부식 특성에 대한 평가 (Evaluation of the Corrosion Property on the Welded Zone of Cast Steel Piston Crown with Types of Electrode)

  • 문경만;김윤해;이명훈;백태실;김진경
    • 한국해양공학회지
    • /
    • 제28권4호
    • /
    • pp.356-362
    • /
    • 2014
  • Wear and corrosion of the engine parts surrounded with combustion chamber is more serious compared to the other parts of the engine because temperature of the exhaust gas in a combustion chamber is getting higher and higher with increasing of using the heavy oil of low quality. Therefore, an optimum repair weldment as well as an available choice of the base metal for these parts are very important to prolong their lifetime in a economical point of view. It reported that there was an experimental result for repair weldment on the forged steel which would be generally used with piston crown material, however, it is considered that there is no study for the repair weldment on the cast steel of piston crown material. In this study, four types of electrodes such as 1.25Cr-0.5Mo, 0.5Mo Inconel 625 and 718 were welded with SMAW and GTAW methods on the cast steel which would be generally used with piston crown material. And the corrosion properties of weld metal, heat affected zone and base metal were investigated using electrochemical methods such as measurement of corrosion potential, anodic polarization curves, cyclic voltammogram and impedance etc. in 35% $H_2SO_4$ solution. In the cases of Inconel 625, 718, the weld metals and base metals exhibited the best and worst corrosion resistance respectively, however, 1.25Cr-0.5Mo and 0.5Mo indicated that corrosion resistance of the base metal was better than the weld metal. And the weld metal welded with electrodes of Inconel 625 revealed the best corrosion resistance among the electrodes, and Inconel 718 followed the Inconel 625. Hardness relatively also indicated higher value in the weld metal compared to heat affected zone and base metal. In particular, Inconel 718 indicated the highest value of hardness compared to other electrodes in the heat affected zone.

솔더 조인트 신뢰성 향상을 위한 무전해 니켈-도금의 표면형상 제어 (Study on Surface Morphology Control of Electroless Ni-P for Reliability Improvement of Solder Joints)

  • 이동준;최진원;조승현
    • 마이크로전자및패키징학회지
    • /
    • 제15권3호
    • /
    • pp.27-33
    • /
    • 2008
  • PDA, 핸드폰과 같은 포터블 제품의 사용이 급증함에 따른 전자 제품의 사용 환경의 변화는 제품의 솔더 조인트 신뢰성을 더욱 필요로 하게 되었다. 무전해 니켈/금 도금 표면 처리는 솔더링 특성이 우수하고, 표면처리 두께가 균일하며 패키징 공정에서 사용되는 광학설비에서 인식이 잘되기 때문에 미세피치 SMT 디바이스와 BGA 기판에 폭넓게 사용되고 있다. 그러나 무전해 니켈/금 도금 표면과 솔더 계면에서 발생되는 취성 파괴가 문제점으로 지적되고 있다. 솔더의 취성 파괴는 솔더링시 금속간 화합물과 무전해 니켈층 사이에 형성된 P-rich 영역의 갈바닉 니켈 부식에 의한 black pad 현상에 기인한다. 이론적으로 평탄한 무전해 Ni표면은 무전해 금도금 과정 중 도금액의 균일하게 순환되기 때문에 black pad 발생을 억제하는 장점을 가지고 있다. 그러나 이러한 장점에도 불구하고 무전해 Ni층의 표면형상을 어떻게 제어 할지에 대한 연구는 충분히 이루어 지지 않고 있다. 본 연구에서는 Cu 하지층의 표면 형상이 무전해 Ni층의 표면 형상에 미치는 영향에 대하여 분석하였다. 이를 위해 Cu 에칭액과 Cu에칭 처리 횟수를 변화시켜 Cu 하지층의 표면 형상을 다양하게 변화시켰다.

  • PDF

Mg 중간층 두께에 따른 Zn/Mg/Zn 다층 박막의 내식특성에 관한 연구 (The Study on the Corrosion Property of the Zn/Mg/Zn Multilayer Coatings with Various Mg layer thicknesses)

  • 배기태;라정현;이상율
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2016년도 추계학술대회 논문집
    • /
    • pp.177-177
    • /
    • 2016
  • 우수한 내식성을 가지는 Zn 박막은 자동차, 가전제품, 전자제품 등에 사용되는 철 생산품의 수명 연장을 위하여 널리 사용되어 왔다. 최근 개발된 Zn-Mg 합금 박막은 Zn나 Mg에 비해 우수한 내식성을 나타내는 Zn-Mg 합금상을 형성하기 때문에 순수한 Zn 박막이나 다른 Zn 계 합금 박막에 비해 우수한 내식성을 가진다고 보고된 바 있다. 본 연구에서는 다양한 합금상의 형성을 위해 Mg 중간층 두께를 제어하며 Zn/Mg/Zn 다층 박막들을 합성하였으며 열처리를 통한 합금상의 변화, 그에 따른 박막의 내식성에 관해 연구하였다. Zn/Mg/Zn 다층 박막은 총 $4{\mu}m$의 두께로 Mg 중간층의 두께를 변화하였으며 비대칭 마그네트론 스퍼터링 공정을 이용하여 냉연강판 위에 합성하였다. 합성된 다층 박막은 다양한 Zn-Mg 합금상을 형성하기 위하여 진공로를 이용하여 $200^{\circ}C$에서 1시간 동안 어닐링 열처리를 실시하였다. 열처리 전, 후 Zn/Mg/Zn 다층 박막의 미세조직과 조성은 X선 회절 분석기 (XRD)와 전계방출형 주사전자현미경 (FE-SEM)과 글로우 방전 분광분석기 (GDEOES)를 사용하여 분석하였다. 어닐링 열처리를 통한 Zn-Mg 합금상 형성이 Zn/Mg/Zn 다층 박막의 내식성에 미치는 영향을 평가하기 위하여 동전위 분극시험과 EIS(Electrochemical impedance spectroscopy) 분석 실시하였다. FE-SEM과 GDOES 분석 결과, Zn/Mg/Zn 다층 박막들 각각의 중간층 Mg 두께는 1.5, 2.0, $2.5{\mu}m$ 였으며, 어닐링 열처리 후 중간층의 Mg이 상, 하부의 Zn 층으로 확산되면서 박막을 치밀한 구조로 변화시키는 것으로 확인되었다. XRD 분석 결과, 열처리를 하지 않은 Zn/Mg/Zn 다층 박막들에서는 Mg 상의 피크의 강도 차이만 존재할 뿐 Zn-Mg 합금상은 형성되지 않았다. 그러나 열처리를 후 Zn/Mg/Zn 다층 박막들에서 $MgZn_2$ 합금상이 형성되었으며, 중간층 Mg 두께가 $1.5{\mu}m$ 이하인 박막에서는 Zn 상이, 초과하는 박막에서는 Mg 상이 잔존하는 것을 확인하였다. EIS 분석 결과, 열처리 후 박막의 전하이동저항 값은 증가하며 박막의 어드미턴스 값이 감소하였으며 Bode phase plot을 통해 열처리 후 시정수(time constant)가 높은 주파수 영역에서 형성 되는 것을 확인하였다. 이는 열처리 후 Zn/Mg/Zn 다층 박막이 치밀해지고 내식성이 향상되었음을 나타낸다. 동전위 분극시험 결과에서도 마찬가지로 열처리 한 Zn/Mg/Zn 다층 박막들은 열처리 전 대비 내식성이 향상되는 것을 확인하였다. 열처리를 통한 Zn/Mg/Zn 다층 박막의 내식성의 향상은 우수한 내식성의 합금상의 형성과 박막 미세구조의 치밀화에 기인한다고 판단하였다. 또한 열처리 한 Zn/Mg/Zn 다층 박막들에서는 Zn와 $MgZn_2$ 상들이 공존 할 경우 가장 우수한 내식성을 나타내었으며, 이는 $MgZn_2$와 Zn 사이의 적은 전위 차이로 인해 갈바닉 부식 효과가 감소되었기 때문으로 판단된다.

  • PDF

아말감과 이종(異種)금속의 거리에 따른 부식에 대한 고찰 (A Study on Corrosion according to Distance between Amalgam and Dissimilar Metals)

  • 김주원;정은경
    • 치위생과학회지
    • /
    • 제4권3호
    • /
    • pp.103-109
    • /
    • 2004
  • 본 실험은 제조회사 매뉴얼과 통법에 의해서 Amalgam 합금, Ni-Cr alloy의 Crown용 Verabond, Denture용 Talladium $^{TM}alloy$로 각각 24개의 총 72의 시편을 하악 제1대구치근 원심 치관 폭경과 임상에서의 MOD cavity를 고려하여 제작하였고 인공 타액 80ml를 담은 200ml 용 비이커에 시편을 넣어 0mm, 7mm, 40mm 거리에서 7일 후 갈바닉 부식을 측정하였다. 유리금속은 유도 플라즈마 방출 분광기(Inductively Coupled Plasma - Atomic Emission Spectrometer(ICP-AES, JY-50P, VG Elemental Co. France)로 전해액내의 Cu, Ag, Ni, Cr, Sn, Zn, Hg를 정량 분석했으며 그 결과 다음과 같은 결론을 얻었다. 첫째, Cu, Sn, Ag, Hg, Zn은 아말감이 금 합금과 접촉했을 때가 크라운용 Ni-Cr alloy와 덴쳐용 Talladium alloy 보다 아주 많이 유리 했으며 금 합금이 구강조직과 생체 적합성이 가장 좋다지만 아말감과 함께 있을 때 가장 불리 했슴을 알 수 있었다. 둘째, 아말감이 금 합금과 접촉했을 때, 금 합금의 조성에서 Ni, Cr 같은 중금속이 함유되지 않았기 때문인지 전혀 유리되지 않았으나 Sn은 조성에는 없었지만 $227.1{\pm}18.0035{\mu}g/cm^2$나 유리 되었고 Hg도 유리되었는데 이는 아말감 자체의 유리 물질임을 추측할 수 있었다. 셋째, 아말감 합금과 금 합금 사이에서의 0mm, 7mm, 40mm 거리에서는 Cu, Ag는 유의성이 있었으며 Hg는 유의성이 없었다. 이는 금합금은 절대 아말감과 같이 사용해서 안되며 이종 보철물 사이의 거리에 관계없이 사용을 금해야 하는 것으로 사료된다. 넷째, 아말감합금이 Crown용 Ni-Cr 합금과 접촉했을 때 아말감의 Ag이 유리 되지 않았으며 Zn, Ni, Sn, Hg, Cu의 순으로 유리되었다. 0mm, 7mm, 40mm 거리에 따라서 유의성이 있었다. Hg는 유리 되지 않았지만 중금속인 Ni, Cr은 유리되었고 반대 악궁이나 거리가 떨어져 있으면 접촉보다 Hg의 유리가 적었다. 다섯째, 아말감합금이 Denture용 Talladium alloy 합금과 접촉했을 때 0mm, 7mm, 40mm 거리에서도 유의성이 있었다. 0mm, 7mm, 40mm 거리에 따라서 유의성이 있었다. Hg는 유리 되지 않았지만 중금속인 Ni, Cr은 유리되었고 반대 악궁이나 거리가 떨어져 있으면 접촉보다 Hg의 유리가 적었다. 여섯째, 인공 타액에서 접촉 시 Amalgam alloy와 Gold, Verabond, Talladium alloy의 Cu, Sn, Ag, Hg, Zn, Ni, Cr의 ICPES 검사 결과 Cu, Hg가 유의성을 있었다. 일곱째, 인공타액에서 아말감합금과 두 비귀금속인 Ni-Cr alloy(crown용), Denture용 Talladium alloy가 접촉한 경우 거리에 따른 Hg, Ni, Cr의 유리 부산물에서 유의성을 확인했다.

  • PDF