Comparative Study on the Bond Strength between Direct Tensile Test and Indirect Tensile Test for Bonded Concrete Overlay (직접인장 및 간접인장 실험방법에 따른 접착식 콘크리트 덧씌우기의 부착강도 비교 고찰)

  • Kim, Young Kyu;Lee, Seung Woo
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.33 no.3
    • /
    • pp.1153-1163
    • /
    • 2013
  • Bonded concrete overlay is a favorable maintenance method since the material properties are similar to existing concrete pavements. In addition, bonded concrete overlay has advantage of structural performance based on being bonded together, both for the overlay layer and the existing pavement which perform as one monolithic layer. Therefore, it is important to have a suitable bond strength criteria for long term performance of bonded concrete overlay. This study aimed to investigate the affecting of bond strength on various bond characteristics, and to compare the bond strength between direct tensile test and indirect tensile test due to various conditions such as overlay materials, compressive and flexure strength of existing pavement, and deterioration status of existing pavement. As a result of this study, bond strength occurred by both of direct and indirect tensile test due to monotonic load is highly correlated such as coefficient of determination of 0.75 and P-value of 0.002. However, bond strength by indirect tensile test was relatively higher than bond strength by direct tensile test. It was known that correlation between direct and indirect tensile test was possible to use the characteristics analysis of bond fatigue behavior based on bond strength due to cyclic load which can simulate real field behavior of bonded concrete overlay.

Cleavage Dependent Indirect Tensile Strength of Pocheon Granite Based on Experiments and DEM Simulation (포천화강암의 결에 따른 간접인장강도 특성에 대한 실험 및 개별요소 수치해석)

  • Zhuang, Li;Diaz, Melvin B.;Jung, Sung Gyu;Kim, Kwang Yeom
    • Tunnel and Underground Space
    • /
    • v.26 no.4
    • /
    • pp.316-326
    • /
    • 2016
  • The purpose of this study is to investigate the influence of cleavages on indirect tensile strength (ITS) of the granite. Brazilian disc tests and ring tests with three different hole sizes were performed. 2D DEM (Discrete Element Method) simulation was employed to further understand the failure process during the tests and the mechanism behind. Results show that ITS decreases across hardway, grain and rift cleavage. Measured average ITS from ring tests is about 2.5 ~ 6.4 times of those measured from Brazilian disc tests, and it decreases with increasing ratio of diameters of inner hole and specimen. Failure pattern in ring tests is influenced by both hole size and relative positions of cleavages parallel and perpendicular to the loading direction.

Characterization of Tensile Strength of Anisotropic Rock Using the Indirect Tensile Strength Test (간접인장강도시험을 통한 이방성 암석의 인장강도 특성)

  • 김영수;정성관;최정호
    • Journal of the Korean Geotechnical Society
    • /
    • v.18 no.5
    • /
    • pp.133-141
    • /
    • 2002
  • Isotropic rock and anisotropic rock have different tensile strength which has the greatest influence on rock failure. In this study, elastic modulus of anisotropic rock is obtained through uniaxial compression test, and tensile strength and tension failure behavior are analyzed through indirect tensile strength test. Stress concentration factor of a specimen at the center is obtained from anisotropic elastic modulus and strain by indirect tensile strength test. Theoretical solutions for tensile strength of isotropic and anisotropic rock are compared. Stress concentration factor of anisotropic rock is either higher or lower than isotropic rock depending on the inclination angle of bedding plane. The use of stress concentration factor of isotropic rock resulted in overestimation or underestimation of tensile strength.

Laboratory Performance Characteristics of Cold-Mixed Reclaimed Asphalt Pavement(RAP) (상온재생공법활용 회수아스팔트 혼합물의 실험적 공용특성)

  • Kim, Nak-Seok;Jo, Myoung-Hwan;Im, Jung-Soon
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.3 no.1 s.8
    • /
    • pp.133-140
    • /
    • 2003
  • The research was performed to evaluate the cracking resistance characteristics of cold-mixed reclaimed asphalt pavement (RAP) using indirect tensile strength test and fatigue tests. Indirect tensile tests were conducted to estimate the indirect tensile strength at variable temperatures($10^{\circ}C\;and\;20^{\circ}C$). Fatigue tests were also carried out using 500kgf, 400kgf, and 300kgf of dynamic loads, and the fatigue life (Nf) for each mixture was measured. Indirect tensile strength of cold-mixed reclaimed asphalt pavement was about 90% of conventional 13mm dense-graded asphalt mixture. Fatigue life of cold-mixed reclaimed asphalt mixture was 70%, 55%, 30% (for 500kgf, 400kgf, 300kgf of load level, respectively) of the conventional one.

Effects of filler addition to bonding agents on shear bond strength (FILLER함량이 BONDING AGENT의 전단접착강도에 미치는 영향)

  • Oh, Young;Oh, Myung-Hwan;Cho, Byeong-Hoon;Son, Ho-Hyun;Kwon, Hyuk-Choon;Um, Chung-Moon
    • Restorative Dentistry and Endodontics
    • /
    • v.27 no.1
    • /
    • pp.44-53
    • /
    • 2002
  • 목적 : 최근 개발된 bonding agent 중 일부는 다양한 함량의 filler를 포함하고 있으며 filler의 첨가는 bonding agent의 기계적인 물성을 향상시킴으로써 접착력의 향상에 기여한다는 주장이 있다. 본 연구에서는 다양한 함량의 filler를 포함한 adhesive를 실험적으로 만들어, filler의 함량이 전단접착강도에 미치는 영향을 살펴보고 임상적으로 가장 적절한 filler의 함량을 알아보고자 하였다. 또 adhesive의 간접인장강도를 측정하여 adhesive의 기계적인 물성과 접착력과의 상관관계를 알아보았다. 방법 : 발거된 건전한 70개의 대구치를 투명 레진에 매몰하고 상아질면을 노출시켰다. 3M사의 Scotchbond Multipurpose의 etchant와 primer를 제조사의 지시대로 적용하고 1$\mu\textrm{m}$크기의 barium glass filler를 0, 5, 10, 15, 20, 30, 45wt% 포함하도록 실험적으로 제작한 adhesive를 도포한 후 레진을 충전하여 시편을 완성하였다. Instron으로 0.5mm/min의 속도에서 전단접착강도를 측정하고 그 단면을 입체현미경으로 관찰하여 파절의 양상을 확인하였다. Filler함량에 따른 adhesive의 후경을 측정하기 위해 상기한 방법으로 시편을 제작하여 주사 전자현미경으로 관찰한 후 Sigmascan을 이용하여 그 후경을 측정하였다. 또, 지름 4mm 높이 6mm의 원통형 시편을 제작하여 Instron로 간접인장강도의 측정을 시행하였다. 얻어진 결과는 Kruskal-Wallis test와 Mann-Whitney test를 시행하여 분석하였으며, 상관관계를 분석을 위해 Pearson Product Moment Correlation Coefficient를 구하였다. 결과 : 1) Filler함유량에 따라 전단접착강도는 유의할 만한 차이를 보였다(p<0.05). 2) Filler함량의 증가에 따라 전단접착강도는 유의하게 증가하여 15% 수준에서 가장 높은 갈(19.9$\pm$1.38Mpa)을 보였으며 20% 이상의 수준에서는 유의하게 감소하였다(p<0.05). 3) Adhesive의 간접인장강도는 20% 수준까지는 증가하는 양상을 보였으나 통계적 유의성은 없었으며(p>0.05), 30% 이상에서는 유의할 만한 감소를 보였다(p<0.05). 4) Adhesive의 후경은 0% 수준에서 5.97$\pm$1.23$\mu\textrm{m}$부터 45%수준에서 73.37$\pm$11.7$\mu\textrm{m}$까지 유의하게 증가하였다(p<0.05). 5) Filler함량에 따른 Adhesive의 간접인장강도와 전단접착강도는 상관관계가 없었다.

Evaluation of mechanical properties of several dual-cure resin cements by curing modes (중합방법에 따른 여러 이중중합 레진 시멘트의 기계적 성질 평가)

  • Kim, Soo-Yeon;Park, Se-Hee;Kim, Jin-Woo;Cho, Kyung-Mo
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.31 no.1
    • /
    • pp.1-9
    • /
    • 2015
  • Purpose: The purpose of this study was to evaluate the mechanical properties of several dual-cure cements by different curing modes. Materials and Methods: One resin-modified glass ionomer cement (FujiCEM 2), two conventional dual-cure resin cements (RelyX ARC, Multilink N), and two dual-cure self-adhesive resin cements (RelyX U200, G-CEM LinkAce) were used. To evaluate the influence of the curing methods, each cements divided into four conditions (n = 20); Condition 1: self-curing for 10 minutes, Condition 2: immediate after 20 seconds light-curing, Condition 3: 24 hours after self-curing, Condition 4: 24 hours after light-curing. The compressive strength and diametral tensile strength were measured with a universal testing machine. All data were statistically analyzed using t-test, one-way ANOVA and Scheffe's test. Results: The results showed the compressive strength and diametral tensile strength after 24 hours in all curing modes were higher than immediate except RelyX ARC light-cured and Multilink N light-cured. The FujiCEM 2 showed lowest values (P < 0.05). Conclusion: The outcome was cement-depend, but there is no significant difference about compressive strength and diametral tensile strength between dual-cure self-adhesive resin cements and conventional resin cements. And this result will be used as a base line data selecting resin cement for favorable long-term prognosis.

Evaluation of Laboratory Performance Characteristics of Fiber-Reinforced Asphalt Concrete (섬유활용 아스팔트 콘크리트의 실험적 공용특성평가)

  • Kim, Nak-Seok
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.2 no.2 s.5
    • /
    • pp.61-72
    • /
    • 2002
  • The optimum fiber and asphalt binder contents were decided on the base of the Mashall mix design method. To compare the mechanical characteristics between the conventional(dense-graded 20) and the fiber-reinforced mixtures, indirect tension tests were conducted under three temperatures(5, 20, 60$^{\circ}C$). In particular, the wheel tracking tests were performed to evaluate the rutting resistances of the mixtures. Test results showed that the indirect tensile strength of fiber-reinforced asphalt concrete was higher than that of conventional one. The toughness of fiber-reinforced mixture was 1.27 to 1.97 times higher than that of conventional one, depending upon the temperature. In addition, the results of wheel tracking tests and the retained indirect splitting tension tests conducted at $60^{\circ}C$ revealed that the resistance to permanent deformation of fiber-reinforced mixture was stronger than that of the conventional one.

Experimental Performance Characteristics of Crumb Rubber-Modified(CRM) Asphalt Concrete (폐타이어활용 아스팔트 콘크리트의 실험적 공용특성)

  • Kim, Nak-Seok
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.3 no.2 s.9
    • /
    • pp.89-97
    • /
    • 2003
  • Indirect tensile strength(IDT) test and resilient modulus(Mr) test were performed to evaluate experimental performance characteristics for the conventional and crumb rubber-modified(CRM) asphalt concrete using dry and wet processes asphalt. The IDT test was conducted under three temperatures(5, 10, 20$^{\circ}C$). According to the test results, it was shown that indirect tensile strength of CRM asphalt concrete was lower than that of the conventional one. However, toughness and maximum vortical strain of the CRM asphalt concrete were higher than those of the conventional one. The results of Mr test were presented that Mr of CRM asphalt concrete was higher than that of the conventional one. In addition, it was revealed that the overall laboratory performance characteristics of the wet-processed CRM asphalt concrete was better than those of the dry-processed one.

Characteristics of the Warm-Mix Asphalt Mixtures Using the Modified Sulfur Binder (개질 유황결합재를 사용한 중온아스팔트 혼합물의 특성)

  • Kim, Se-Won;Park, Hung-Suck;Kim, Jong-Kyu;Jung, Yong-Wook
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.4
    • /
    • pp.489-495
    • /
    • 2016
  • In this study, the Warm-Mix Asphalt was prepared using a modified Sulfur Binder mixed with an additive of a polymer component in sulfur, which is an industrial by-product generated in the crude oil refining process. The dynamic stability and durability characteristics of the prepared Warm-Mix Asphalt was evaluated by the indirect tensile strength, the tensile strength ratio before and after water immersion and freezing-thawing, and the dynamic stability by wheel tracking test. The Warm-Mix Asphalt Mixtures using Modified Sulfur Binder has a tensile strength ratio before and after water immersion of 0.88, which is about 1.13 times that of the Warm-Mix formed modified Asphalt, and the tensile strength ration before and after freezing-thawing is also 0.82, thus, all tensile strength ratios satisfied the KS quality standard value of 0.75 or more. The indirect tensile strength was 1.6MPa which was twice the KS quality standard value of 0.8MPa, and about 1.24 times higher than that of normal heated asphalt 1.29MPa. In addition, the dynamic stability by the wheel tracking test was 14,075 times/mm, which was about 15 times higher than that of normal heated asphalt and about 3 times higher than that of the Warm-Mix formed modified Asphalt, showing excellent resistance to plastic deformation such as fatigue cracks.

An Indirect Experimental Method for the Determination of Mechanical Properties of Ion-nitrided Layer and Residual Stress Distribution (이온질화층의 기계적 성질과 잔류응력 분포를 위한 간접 실험법)

  • 곽병만;길영준
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.9 no.2
    • /
    • pp.240-249
    • /
    • 1985
  • 여러 가지 조건하에서 한쪽면만 이온질화 처리된 SCM4 의 평판을 모델로 하여 질화층의 기계적 성질과 잔류응력을 연구하였다. 질화층에서의 재료의 성질은 질소함량분포에 비례하여 변할 것이 라는 가정하에 외팔보의 굽힘과 온도-곡률의 관계를 구하는 이론적 모델을 정립하고 이에 따른 간접적 실험방법을 제시하였다. 질화층 표면에서의 선팽창 계수는 질화되지 않은 코어의 값에 비 해 2내지 12% 증가를 보였고 탄성계수는 50내지 700%증가를 보였다. 질화로 인한 축방향 팽창은 변형도로 약 0.002를 얻었다. 상온에서의 코어의 최대인장 잔류응력은 2내지 25Kg/mm$^{2}$이 며, 질화층표면에서 일어나는 최대압축잔류응력은 질화조건에 따라 50내지 300Kg/mm$^{2}$을 얻었다.