• 제목/요약/키워드: [2+2] addition

검색결과 48,618건 처리시간 0.066초

La2O3첨가에 따른 무연 Bi(Na,K)TiO3-SrTiO3 세라믹스의 압전 특성 (Piezoelectric Properties of Pb-free Bi(Na,K)TiO3-SrTiO3 Ceramics with the Amount of La2O3 Addition)

  • 류주현;이현석;박창엽;정광현;이덕출;정영호;홍재일
    • 한국전기전자재료학회논문지
    • /
    • 제17권8호
    • /
    • pp.830-834
    • /
    • 2004
  • In this study, lead-free pirzoelectric ceramics were investigated for pressure sensor applications as a function of the amount of ${La}_2{O}_3$ addition at $Bi(Na, K)Ti{O}_3-SrTi{O}_3$system. With increasing the amount of addition, the density and dielectric constant increased up to 0.9 wt% ${La}_2{O}_3$ addition and decreased above 0.9 wt% ${La}_2{O}_3$addition. Electromechanical coupling factor( $K_{P}$) showed the maximum value at 0.2 wt% ${La}_2{O}_3$addition and decreased above 0.2 wt% ${La}_2{O}_3$ addition. Electromechanical coupling $factor{(K)}_P$, density, dielectric constant$(\varepsilon_\Gamma)$, piezoelectric constant$(d_33)$ and curie temperature$(T_C)$ showed optimum value of 0.40, 5.75 g/㎤, 768, 215 pC/N and 320 $^{\circ}C$ at 0.2 wt%${La}_2{O}_3$addition, respectively.

초미립 WC-10%Co 초경합금의 물성에 미치는 타탄화물 첨가의 영향 (Effects of the Addition of Other Carbides on the Properties of Submicron WC-10% Co Cemented Carbides)

  • 이승원
    • 한국분말재료학회지
    • /
    • 제3권2호
    • /
    • pp.86-90
    • /
    • 1996
  • The effects of added VC, Cr$_3$C$_2$ and TaC on the microstructures and properties of submicron WC-10%Co cemented carbides. The relative sintered density of compact was increased by addition of Cr$_3$C$_2$ but decreased oppositely by addition of VC or TaC. The growth of WC grains was significantly suppressed by addition of these carbides. The hardness of these alloys was increased by addition of other carbides and showed a maximum value by simultaneously added VC and Cr$_3$C$_2$. The transverse rupture strength(T.R.S.) was in- creased by addition of Cr$_3$C$_2$, while it was decreased by addition of VC or TaC. The relative sintered density and T.R.S. of these alloys were improved by HIP-treatment. The maximum T.R.S. was 328kg/mm$^2$ in the Wc-10%Co cemented carbide with addition of 0.5%VC.

  • PDF

$CH_4/O_2/N_2$ 화염에서 할로겐 첨가제의 역할 (The Function of Halogen Additive in $CH_4/O_2/N_2$ Flames)

  • 이기용;신성수
    • 한국연소학회:학술대회논문집
    • /
    • 대한연소학회 2003년도 제27회 KOSCO SYMPOSIUM 논문집
    • /
    • pp.209-214
    • /
    • 2003
  • Numerical simulations are performed at atmospheric pressure in order to understand the effect of additives on flame speed, flame temperature, the radical concentration, the NOx formation in freely propagating $CH_4/O_2/N_2$ flames. The additives used are carbon dioxide and hydrogen chloride which have a combination of physical and chemical behavior on hydrocarbon flame. In the flame established with the same mole of methane and additive, $CO_2$ addition significantly contributes toward the reduction of flame speed and flame temperature by the physical effect, whereas addition of HCl mainly does by the chemical effect. The impact of HCl addition on the decrease of the radical concentration is about 1.6-1.8 times as large as $CO_2$ addition. Hydrogen chloride addition is higher on the reduction of EINO than $CO_2$ addition because of the chemical effect of HCl.

  • PDF

$BaB_2B_4$ 첨가에 따른 반도성 $BaTiO_3$ 세라믹스의 소결 및 전기적 특성 (Sintering and Electrical Characteristics of Semiconducting $BaTiO_3$ Ceramics with Addition of $BaB_2O_4$)

  • 허영우;이준형;김정주;김남경;조상희
    • 한국세라믹학회지
    • /
    • 제33권9호
    • /
    • pp.1038-1044
    • /
    • 1996
  • The variations of sintering and electrical characteristics of semiconducting BaTiO3 ceramics with sintering agents added were investigated comparing the case of BaB2O4 addition to BN and TiO2 addition. When BaB2O4 added in BaTiO3 ceramics the densitifcation of specimen could be acheived more easily and recvealed the better PTCR characteristics than BN and TiO2 addition. As increase of addition of BaB2O4 in BaTiO3 spec imens the slope of resistivity jump also increased but the temperature of maximum resistivity decreased, It was supposed that addition of BaB2O4 led to increase of Ns (acceptor state density) value at grain boundaries.

  • PDF

$\textrm{TiO}_2$ 첨가량에 대한 알루미나 세라믹스의 특성에 관한 연구 (A Study on the Properties of Alumina Ceramics as the Amount of $\textrm{TiO}_2$ Addition)

  • 류수착
    • 한국재료학회지
    • /
    • 제9권9호
    • /
    • pp.900-904
    • /
    • 1999
  • TiO$_2$분말을 $Al_2$O$_3$분말에 대하여 무게비로 1,3,5,7,9와 11wt%로 혼합하여 알루미나 세라믹스의 미세조직 및 기계적 물성변화를 관찰하였다. TiO$_2$분말의 첨가량이 증가할수록 부피비중은 3.26에서 2.90g/㎤으로 감소하였으며 기공율은 TiO$_2$분말의 첨가량이 7wt%까지는 감소하였으나 9wt%이상 첨가할 경우 증가하였다. 압축강도 측정 결과 파괴강도는 TiO$_2$분말의 첨가량이 7wt%까지는 증가하였으나 9wt%이상 첨가할 경우 감소하였다. 3점 곡강도를 측정한 결과 최대 파괴 응력 값은 TiO$_2$분말의 첨가량이 증가할수록 감소하였다.

  • PDF

$Nb_2O_5$$V_2O_5$의 첨가가 Lithium Ferrite의 소결현상과 B-H Loop 특성에 미치는 영향 (Effects of $Nb_2O_5$ and $V_2O_5$ Additions on the Sintering Behavior and B-H Loop Properties of Lithium Ferrite)

  • 김현태;임호빈
    • 한국세라믹학회지
    • /
    • 제19권4호
    • /
    • pp.267-274
    • /
    • 1982
  • The sintering behavior and B-H loop properties of $Li_{0.5O4}$ with the addition of $Nb_2O_5$ and $V_2O_5$ have been investigated by observation of microstructures and measurement of semi-static hysteresis loops. The sintering temperature was lowered by the additions of $Nb_2O_5$ and $V_2O_5$ and the effect of $V_2O_5$ addition was greater than that of $Nb_2O_5$. The abnormal grain growth was observed at about 100$0^{\circ}C$(d:4.6g/㎤) and 85$0^{\circ}C$(d:4.5g/㎤) in the specimens with the addition of $Nb_2O_5$ and $V_2O_5$ respectively. The addition of $Nb_2O_5$ retulted in a large and uniform grain size, and the addition of $V_2O_5$ resulted in a uniform grain size but the final density was lower than that of the pure specimen. The squareness was increased and the coercive force was decreased by the addition of $Nb_2O_5$, and the squareness was decreased and the coercive force was increased by the addition of $V_2O_5$. These effects could be explained by a large and uniform grain size, and by a lower final density of specimens with the addition of $Nb_2O_5$ and $V_2O_5$ respectively.

  • PDF

Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3계의 삼방정, 정방정 및 상경계조성에서의 MnO2 첨가에 따른 유전 및 압전특성에 비교 (Comparisons on Dielectric and Peizoelectric Proeprties of Rhombohedral, Tetragonal and Morphotropic Phase Boundary in Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3 System with MnO2 Addition)

  • 전구락;손정호;김정주;조상희
    • 한국세라믹학회지
    • /
    • 제25권5호
    • /
    • pp.488-494
    • /
    • 1988
  • Effects of MnO2 addition on themicrostructure, dielectric and piezoelectric properties of Rhombohedral, Tetragonal and Morphotropic phase boundary(MPB) in Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3 system were investigated and respectively the amount of MnO2 addition was 0, 0.2, 0.5, 1.0, 3.0wt%. In the tetragonal region, compared with the Rhombohedral and Morpotropic phase boundary, Mechanical quality factor(Qm), Curie temperature(Tc) and Dissipation factor were promoted by addition of MnO2. According to the results of the microstructure, dielectric and piezoelectric properties, the solid solution range of MnO2 addition in this system was 0.2-0.5wt%.

  • PDF

$Al_2O_3$의 물리적 성질 및 전기전도도에 미치는 단사정 지르코니아와 정방정 지르코니아의 첨가효과 ((Effect of Monoclinic Zirconia and Tetragonal Zirconia Addition on Physical Properties and Electrical conductivity of $Al_2O_3$))

  • 박재성;어수해
    • 대한전자공학회논문지TE
    • /
    • 제39권1호
    • /
    • pp.1-8
    • /
    • 2002
  • 단사정 ZrO/sub 2/(ZrO2(m)) 또는 Y/sub 2/O/sub 3/를 5.35wt% 첨가한 정방정 ZrO2(ZrO/sub 2/(t))를 A1/sub 2/O/sub 3/에 첨가하여 물리적 및 전기전도도의 영향을 연구하였다. ZrO/sub 2/(m)과 ZrO/sub 2/(t)의 첨가는 A1/sub 2/O/sub 3/의 소결밀도를 증가 시켰다. ZrO2(t)의 첨가함에 따라 비커스 경도 또한 증가했으며, 그 량이 20wt%에서 최대가 되었다. 시편의 경도는 소결밀도에 의존함을 알 수 있었다. A1/sub 2/O/sub 3/-ZrO/sub 2/계의 경도는 ZrO/sub 2/(t)의 첨가에 의해 개선 되었고, ZrO/sub 2/(m)의 첨가가 ZrO/sub 2/(t)의 첨가보다 A1/sub 2/O/sub 3/-ZrO/sub 2/계의 열충격 특성에는 더 많은 영향을 받음을 알 수 있었다. l5wt% 이상의 ZrO/sub 2/(t) 첨가에서 인가전압이 증가 함에 따라 점차로 전기전도도가 증가 하였으나, ZrO/sub 2/(m)의 첨가에서는 영향이 없었다.

$La_2O_3$ 첨가에 따른 무연 BNKT세라믹의 압전 특성 (Piezoelectric properties of Pb-free BNKT ceramics with the amount of $La_2O_3$ addition)

  • 이현석;이창배;류주현;정영호;홍재일;정광현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 춘계학술대회 논문집 반도체 재료 센서 박막재료 전자세라믹스
    • /
    • pp.145-149
    • /
    • 2004
  • In this study, leed-free piezoelectric ceramics were investigated for pressure sensor applications as a function of the amount of $La_2O_3$ addition at BNKT system. With increasing amount of $La_2O_3$ addition, density and dielectric constant were increased up to 0.9wt% addition and decreased after 0.9wt% addition, electromechanical coupling factor$(k_p)$ and mechanical quality factor$(Q_m)$ showed the maximum values at 0.2wt% addition and decreased after 0.2wt% addition. The $k_p$, density, dielectric constant and $Q_m$ were showed the optimum values of 0.40, $5.71g/cm^3$, 768 and 118 at $La_2O_3$ 0.2wt% addition, respectively.

  • PDF

90wt% Cordierite-10wt% Enstatite 총체의 $TiO_2$ 첨가에 의한 결정화 (Crystallization of 90wt% Cordierite-10wt% Enstatite Melt by $TiO_2$ Addition)

  • 이준;한덕현;조동수;전정필
    • 한국세라믹학회지
    • /
    • 제23권5호
    • /
    • pp.9-16
    • /
    • 1986
  • The effect of $TiO_2$ addition to the 90wt% Cordierite-10wt% Enstatite base glass was investi-gated to understand the crystallization behavior of the glass. Glasses with addition of $TiO_2$ less than 7, 5wt% had a tendency of surface crystallization and were cracked when heat treated and in this case the crystalline phase formed was indialite. glasses with addition of $TiO_2$ more than 10wt% to 15wt% were crystallized in bulk when heat treated and were suitable for glass-ceramics. The highest microhardness 1640kg/$mm^2$ was obtained when the glass of 12.5wt% $TiO_2$ addition was heat treated at 762$^{\circ}C$ for 60 minutes for nucleation and at 1135$^{\circ}C$ for 20 minutes for crystal growth and in general higher microhardness was obtained when crystalline phase of magnesium aluminum titanate and $\mu$-cordierite were developed. Avrami equation for crystal growth kinetics was applicable in glasses of less than 7.5 wt% $TiO_2$ addition and in case of glasses of more than 10wt% $TiO_2$ addition it was not applicable because of too fast crystal growth.