• Title/Summary/Keyword: +5X

Search Result 16,361, Processing Time 0.044 seconds

Prediction of Physical Properties in the Design of Mono-Acetate Filter Cigarette by Response Surface Methodology (반응표면 실험 계획법에 의한 Mono-Acetate 필터담배 설계의 물리성 예측)

  • 김영호;이영택;김성한;김윤동;임광수;김용태
    • Journal of the Korean Society of Tobacco Science
    • /
    • v.16 no.1
    • /
    • pp.3-13
    • /
    • 1994
  • To minimize the time ordinarily spent in mono filter cigarette design, we studied the relationship between major seven independant variables ; filament(X1) and total denier(X2), porosity of the aller plug wrap(X3), filter length(X4), Porosity of the tip paper(X5) and cigarette paper(X6) and net weight of the reference cut tobacco(X7). Ninty trial numbers were obtained as a results of using rotatable central composite design and it is analyzed by the multiple regression analysis with stepwise in SAS/pc under restricted conditions. That is, UPD (Y1) = 82.96 - 3.80X1 + 2.50X2 - 3.29X3 - 3.15X5 - 0.83X22 + 1.88X5X6 - 1.38 X5X7(R2: 0.63), EPD(Y2) : 120.91 - 5.70X1 + 3.60X2 + 4.23X4 - 0.93X6 + 4.06X7 (R2=0.84), TVR(Y3) = 49.70 - 0.78X1 + 3.60X3 + 2.00X4 + 4.20X5 - 0.93X6 + 2.64X7 - 1.07X1X2 + 1.0IX1 X3 + 1.05X2X6 + 0.45X22 - 0.64X42 + 1.29X4X6 - 0.97X4X7 - 1.28X5X6 + 1.53X5X7 + 1.39X6X7(R2=0.65), and EVR(Y4) : 3.24-0.21X3-0.20X4 -0.24X5+0.67X6+0.26X4X7 (R2=0.55), where EPD : encapsulated pressure drop, VPD : unencapsulated pressure drop, TVR ; tip ventilation rate, and En : envelope ventilation rate. All variables in the model are significant at the 0.05 level.

  • PDF

Composition-Some Properties Relationships of Non-Alkali Multi-component La2O3-Al2O3-SiO2 Glasses (무알칼리 다성분 La2O3-Al2O3-SiO2 유리의 조성과 몇 가지 물성의 관계)

  • Kang, Eun-Tae;Yang, Tae-Young;Hwang, Jong-Hee
    • Journal of the Korean Ceramic Society
    • /
    • v.48 no.2
    • /
    • pp.127-133
    • /
    • 2011
  • Non-Alkali multicomponent $La_2O_3-Al_2O_3-SiO_2$ glasses has been designed and analyzed on the basis of a mixture design experiment with constraints. Fitted models for thermal expansion coefficient, glass transition temperature, Young's modulus, Shear modulus and density are as follows: ${\alpha}(/^{\circ}C)=8.41{\times}10^{-8}x_1+5.72{\times}10^{-7}x_2+2.13{\times}10^{-7}x_3+1.09{\times}10^{-7}x_4+1.10{\times}10^{-7}x_5+1.15{\times}10^{-7}x_6+2.72{\times}10^{-8}x_7+2.41{\times}10^{-7}x_8-1.08{\times}10^{-8}x_1x_2+4.28{\times}10^{-8}x_3x_7-2.02{\times}10^{-8}x_3x_8-1.60{\times}10^{-8}x_4x_5-2.71{\times}10^{-9}x_4x_8-2.19{\times}10^{-8}x_5x_6-3.89{\times}10^{-8}x_5x_7$ $T_g(^{\circ}C)=7.36x_1+15.35x_2+20.14x_3+8.97x_4+13.85x_5+4.22x_6+28.21x_7-1.44x_8-0.84x_2x_3-0.45x_2x_5-1.64x_2x_7+0.93x_3x_8-1.04x_5x_8-0.48x_6x_8$ $E(GPa)=2.04x_1+14.26x_2-1.22x_3-0.80x_4-2.26x_5-1.67x_6-1.27x_7+3.63x_8-0.24x_1x_2-0.07x_2x_8+0.14x_3x_6-0.68x_3x_8+0.29x_4x_5+1.28x_5x_8$ $G(GPa)=0.35x_1+1.78x_2+1.35x_3+1.87x_4+9.72x_5+29.16x_6-0.99x_7+3.60x_8-0.48x_1x_6-0.50x_2x_5+0.08x_3x_7-0.66x_3x_8+0.94x_5x_8$ ${\rho}(g/cm^3)=0.09x_1+0.51x_2-4.94{\times}10^{-3}x_3-0.03x_4+0.45x_5-0.07x_6-0.10x_7+0.07x_8-9.60{\times}10^{-3}x_1x_2-8.20{\times}10^{-3}x_1x_5+2.17{\times}10^{-3}x_3x_7-0.03x_3x_8+0.05x_5x_8$ The optimal glass composition similar to the thermal expansion coefficient of Si based on these fitted models is $65.53SiO_2{\cdot}25.00Al_2O_3{\cdot}5.00La_2O_3{\cdot}2.07ZrO_2{\cdot}0.70MgO{\cdot}1.70SrO$.

Surface Photovoltage Characteristics of ${In_{0.5}}({Ga_{1-x}}{Al_x})_{0.5}P$/GaAs Double Heterostructures (${In_{0.5}}({Ga_{1-x}}{Al_x})_{0.5}P$/GaAs 이중 이종접합 구조에 대한 표면 광전압 특성)

  • Kim, Ki-Hong;Choi, Sang-Soo;Bae, In-Ho;Kim, I n-Soo;Park, Sung-Bae
    • Korean Journal of Materials Research
    • /
    • v.11 no.8
    • /
    • pp.655-660
    • /
    • 2001
  • Surface photovoltage spectroscopy was used to study $In_{0.5}(Ga_{1-x}Al_x)_{0.5}P/GaAs$ grown by metalorganic chemical vapor deposition(MOCVD). Energy gap related transition in GaAs and $In_{0.5}(Ga_{1-x}Al_x)_{0.5}P$ were observed. By measuring the frequency dependence of $In_{0.5}(Ga_{1-x}Al_x)_{0.5}P/GaAs$, we observed that SPV line shape does not chance, whereas the amplitude change. This results is due to the difference in the lifetimes of the photocarriers in GaAs and in $In_{0.5}(Ga_{1-x}Al_x)_{0.5}P$. We also have evaluated the parameters that describe the temperature dependences of the band gap.

  • PDF

A study on the Degradation and By-products Formation of NDMA by the Photolysis with UV: Setup of Reaction Models and Assessment of Decomposition Characteristics by the Statistical Design of Experiment (DOE) based on the Box-Behnken Technique (UV 공정을 이용한 N-Nitrosodimethylamine (NDMA) 광분해 및 부산물 생성에 관한 연구: 박스-벤켄법 실험계획법을 이용한 통계학적 분해특성평가 및 반응모델 수립)

  • Chang, Soon-Woong;Lee, Si-Jin;Cho, Il-Hyoung
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.32 no.1
    • /
    • pp.33-46
    • /
    • 2010
  • We investigated and estimated at the characteristics of decomposition and by-products of N-Nitrosodimethylamine (NDMA) using a design of experiment (DOE) based on the Box-Behken design in an UV process, and also the main factors (variables) with UV intensity($X_2$) (range: $1.5{\sim}4.5\;mW/cm^2$), NDMA concentration ($X_2$) (range: 100~300 uM) and pH ($X_2$) (rang: 3~9) which consisted of 3 levels in each factor and 4 responses ($Y_1$ (% of NDMA removal), $Y_2$ (dimethylamine (DMA) reformation (uM)), $Y_3$ (dimethylformamide (DMF) reformation (uM), $Y_4$ ($NO_2$-N reformation (uM)) were set up to estimate the prediction model and the optimization conditions. The results of prediction model and optimization point using the canonical analysis in order to obtain the optimal operation conditions were $Y_1$ [% of NDMA removal] = $117+21X_1-0.3X_2-17.2X_3+{2.43X_1}^2+{0.001X_2}^2+{3.2X_3}^2-0.08X_1X_2-1.6X_1X_3-0.05X_2X_3$ ($R^2$= 96%, Adjusted $R^2$ = 88%) and 99.3% ($X_1:\;4.5\;mW/cm^2$, $X_2:\;190\;uM$, $X_3:\;3.2$), $Y_2$ [DMA conc] = $-101+18.5X_1+0.4X_2+21X_3-{3.3X_1}^2-{0.01X_2}^2-{1.5X_3}^2-0.01X_1X_2+0.07X_1X_3-0.01X_2X_3$ ($R^2$= 99.4%, 수정 $R^2$ = 95.7%) and 35.2 uM ($X_1$: 3 $mW/cm^2$, $X_2$: 220 uM, $X_3$: 6.3), $Y_3$ [DMF conc] = $-6.2+0.2X_1+0.02X_2+2X_3-0.26X_1^2-0.01X_2^2-0.2X_3^2-0.004X_1X_2+0.1X_1X_3-0.02X_2X_3$ ($R^2$= 98%, Adjusted $R^2$ = 94.4%) and 3.7 uM ($X_1:\;4.5\;$mW/cm^2$, $X_2:\;290\;uM$, $X_3:\;6.2$) and $Y_4$ [$NO_2$-N conc] = $-25+12.2X_1+0.15X_2+7.8X_3+{1.1X_1}^2+{0.001X_2}^2-{0.34X_3}^2+0.01X_1X_2+0.08X_1X_3-3.4X_2X_3$ ($R^2$= 98.5%, Adjusted $R^2$ = 95.7%) and 74.5 uM ($X_1:\;4.5\;mW/cm^2$, $X_2:\;220\;uM$, $X_3:\;3.1$). This study has demonstrated that the response surface methodology and the Box-Behnken statistical experiment design can provide statistically reliable results for decomposition and by-products of NDMA by the UV photolysis and also for determination of optimum conditions. Predictions obtained from the response functions were in good agreement with the experimental results indicating the reliability of the methodology used.

Investigation on the Structural, Electrical and Magnetic Properties of Layered Perovskite Manganite La0.5Sr1.5Mn0.5Cr0.5-xFexO4 (x=0.15, 0.3) System (층상 페로브스카이트 구조인 La0.5Sr1.5Mn0.5Cr0.5-xFexO4 (x=0.15, 0.3) 망가나이트의 구조적, 전기적, 자기적 특성의 연구)

  • Singh, Devinder
    • Journal of the Korean Chemical Society
    • /
    • v.55 no.4
    • /
    • pp.697-702
    • /
    • 2011
  • The new layered perovskite manganites $La_{0.5}Sr_{1.5}Mn_{0.5}Cr_{0.5-x}Fe_xO_4$ (x=0.15, 0.3) have been prepared by standard ceramic method. The powder X-ray diffraction studies show that the phases crystallize with tetragonal unit cell in the space group I4/mmm. The electrical transport properties suggest that the phases show insulating behaviour and the electrical conduction in the phases occurs by a 3D variable range hopping mechanism. The magnetic properties suggest that both the phases are antiferromagnetic.

Properties of $Y_{2-x}SiO_{5}:Ce_{x}^{3+}$ Phosphor Powder Prepared by Sol-gel Process (Sol-gel법에 의한 $Y_{2-x}SiO_{5}:Ce_{x}^{3+}$ 형광체 제조와 그 특성)

  • Kim, Sang-Mun;Kang, Kyoung-Tae;Kim, Tae-Ok
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.9
    • /
    • pp.794-798
    • /
    • 2001
  • $Y_{2-x}SiO_5:Ce_x^{3+}$(x=0.002∼0.04) phosphors were prepared by sol-gel process, amorphous crystal phase was observed in calcining dry gel at 800$^{\circ}$C, but pure $X_2$ type of type $Y_2SiO_5$ phase appeared from heat treatment above 1000$^{\circ}$C. Light absorption of tye $Y_2SiO_5$ host lattice occurred at 230∼360nm, and light absorption of the $Y_{2-x}SiO_5:Ce_x^{3+}$ phosphors was observed at 300∼400nm in adding $Ce^{3+}$. $Y_{2-x}SiO_5:Ce_x^{3+}$ phosphors showed maximum emission shoulder at 436nm. Maximum CL intensities of $Y_{2-x}SiO_5:Ce_x^{3+}$ were observed in adding 0.025 $Ce^{3+}$ and the phosphor showed x=0.161, y=0.124 in color coordinate of CIE1931.

  • PDF

Synthesis and Superconductivity in $(Ru_{0.8}Nb_{0.2})Sr_2(Gd_{1.5-x}Nd_xCe_{0.5})Cu_2O_z$ System ($(Ru_{0.8}Nb_{0.2})Sr_2(Gd_{1.5-x}Nd_xCe_{0.5})Cu_2O_z$ 계의 합성 및 초전도 특성)

  • Lee, H.K.;Bae, S.M.
    • Progress in Superconductivity
    • /
    • v.10 no.2
    • /
    • pp.128-132
    • /
    • 2009
  • Polycrystalline samples of $(Ru_{0.8}Nb_{0.2})Sr_2(Gd_{1.5-x}Nd_xCe_{0.5})Cu_2O_z$($ 0{\leq}x{\leq}1.25$) have been synthesized by a solid-state reaction route. The X-ray diffraction data revealed that the Nd solubility limit can be placed between x=0.5 and x=0.75. The superconducting transition temperature decreased with increasing Nd content, confirming that Nd entered the lattice. Room-temperature thermoelectric power measurements showed that all the samples are in the underdoped state and the partial substitution of Nd for Gd resulted in a decrease in the carrier density on the superconducting layers.

  • PDF

Crystallographic and Mossbauer Studies of Magnetic Garnet $Y_{3-x}Bi_xFe_5O_{12}$ by a Sol-Gel Method (Sol-gel 합성에 의한 자성 garnet $Y_{3-x}Bi_xFe_5O_{12}$의 결정학적 및 Mossbauer 분광학 연구)

  • 엄영란;김철성;이재광
    • Journal of the Korean Magnetics Society
    • /
    • v.8 no.4
    • /
    • pp.203-209
    • /
    • 1998
  • Crystallographic and magnetic properties of single phase garnet $Y_{3-x}Bi_xFe_5O_{12}$ (x=0.0, 0.25, 0.5, 0.75, 1.0) were studied by using x-ray diffraction, Mossbauer spectroscopy and vibrating sample magnetometer (VSM). Ultra-fine polycrystalline cubic samples have been prepared by sol-gel method. The lattice constant increase linearly with increasing an amount of Bi. Annealing temperature was larger than 800 $^{\circ}C$ for the growth of a single-phase garnet powder. The second phase of garnet, $(BiFeO_3)$, was at 1000 $^{\circ}C$ for x=0.75, and 950 $^{\circ}C$ for x=1.00. From Mossbauer spectroscopy and VSM measurements, the magnetization and the coercivity were decreased and the Curie temperature $Y_{3-x}Bi_xFe_5O_{12}$(x=0.0, 0.25, 0.5, 0.75, 1.0) was slightly increased as increasing the Bi content.

  • PDF

Mossbauer Studies of Perovskite $Gd_{1-x}Sr_xFeO_{3-y}$ (X = 0.0, 0.5) (Perovskite $Gd_{1-x}Sr_xFeO_{3-y}$ (X = 0.0, 0.5)의 Mossbauer연구)

  • 엄영랑;김철성;서정철;오영제
    • Journal of the Korean Magnetics Society
    • /
    • v.8 no.2
    • /
    • pp.67-73
    • /
    • 1998
  • Crystallographic and magnetic properties of perovskite $Gd_{1-x}Sr_xFeO_{3-y}$ (x=0.0, 0.5) substituted $Sr^{2+}$ having larger inoic radius than $Gd^{3+}$ at GdFeO$_3$have been studied by x-ary diffraction, M$\ "{o}$ssbauer spectroscopy, and VSM. The cystal structures are found to be orthorhombic with the lattice parameters : $a_o=5.53\;{\AA},\;b_o=5.608\;{AA},\;C_o=7.724\;{\AA}$ for $Gd_{0.5}Sr_{0.5}FeO_{3-y}$ (x=0.0, 0.5) have been investigated over temperature range from 4.2 to 690 K using the M$\ "{o}$ssbauer technique. The Neel temperatuer of $Gd_{1-x}Sr_xFeO_{3-y}$ system is 690 K with x value of 0.0 and 515 K with x value of 0.5. Analysis of M$\ "{o}$ssbauer spectra Mohr's salt analysis for $Gd_{1-x}Sr_xFeO_{3-y}$ demonstrated the existence of the mixed valence states of iron and the coordination state of $Fe^{3+}$ and $Fe^{4+}$ ions. The Corresponding hyperfine parameters for GdFeO$_3$ are compatible with S=5/2 $Fe^{3+}$ in octahedral cooedination.l cooedination.

  • PDF

Molybdenum(Ⅴ)-Oxo Complexes with Oxygen, Nitrogen and Sulfur Donors. Synthesis, Spectral and Electrochemical Properties (산소, 질소, 그리고 황 주개 원자의 몰리브덴(Ⅴ)-산소 착물 합성과 분광학적 및 전기화학적 성질)

  • Kim, Hee-Jung;Koo, Bon-Kweon
    • Journal of the Korean Chemical Society
    • /
    • v.39 no.6
    • /
    • pp.434-439
    • /
    • 1995
  • Six-coordinate molybdenum(Ⅴ)-oxo complexes, (R4N)[MoO(NCS)2L](R=CH3, C2H5, n-C4, H9) with S-methyl-3-(2-hydroxy-x-phenyl)methylenedithiocarbazate(L1: x=5-H) and its derivatives (L2:x=5-CH3, L3: x=3-CH3O, L4: x=5,6-C4H4 and L5: x=5-NO2) have been synthesized and the structural, spectral and electrochemical properties of the complexes have been characterized by elemental analysis, molar conductivity, UV-Vis, IR, 1H NMR, and CV (cyclic voltammetry).

  • PDF