• 제목/요약/키워드: (Bi, Pb)-2223

Search Result 52, Processing Time 0.025 seconds

Formation of the precipitates in the Bi-2223/Ag superconducting tapes by post-heat treatment (Bi-2223 초전도 선재의 후열처리 과정에 의한 석출물의 형성)

  • Lee, Sang-Hee;Kim, Cheol-Jin;Chung, Jun-Ki;Yoo, Jae-Moo;Ko, Jae-Woong
    • 한국초전도학회:학술대회논문집
    • /
    • v.10
    • /
    • pp.262-267
    • /
    • 2000
  • To tap the possibility of exploiting the precipitates as flux-pinning center in the Bi-2223 superconducting system, as-received Bi-2223/Ag tapes with the starting composition of Bi$_{1.8}$Pb$_{0.4}$Sr$_2$Ca$_{2.2}$Cu$_3$O$_8$ were post-annealed at various temperature, oxygen partial pressure, and annealing time. The 2$^{nd}$ phases in the annealed specimen were analysed with XRD, SEM, TEM, and EDS. The size and the distribution of the precipitates such as (Ca,Sr)$_2$(Pb,Bi)O$_4$ and Bi$_{0.5}$Pb$_3$Sr$_2$Ca$_2$CuO$_{12+{\delta}}$ (3221) in the Bi-2223 matrix was controllable by varying heat-treatment condition without breaking the connectivity of the 2223 grains. The nano-size precipitates within the 2223 grains are conjectured as working as flux-pinning sites, resulting in increased J$_c$ value.

  • PDF

Effect of La0.7Sr0.3MnO3 addition on superconducting properties and local structure of (Bi, Pb)-2223 superconductor

  • M. A. Anugrah;R. P. Putra;J. Y. Oh;B. Kang
    • Progress in Superconductivity and Cryogenics
    • /
    • v.25 no.2
    • /
    • pp.5-9
    • /
    • 2023
  • The effect of La0.7Sr0.3MnO3 (LSMO) addition on the superconducting property of Bi1.6Pb0.4Sr2Ca2Cu3O10+δ ((Bi, Pb)-2223) polycrystalline samples was studied. LSMO (0.3 wt.% to 2.0 wt.%) added (Bi, Pb)-2223 samples were prepared by using a solid-state reaction method. The XRD analyses show that as the LSMO addition increases, the volume fraction of the Bi-2223 phase is gradually decreased. The critical temperature (Tc) exhibits a gradual decrease with a single transition as the LSMO amount increases up to 1.0 wt.%, but a further addition of LSMO induces an abrupt decrease of Tc with a dual transition. The analyses on the local structure of the CuO2 plane from the X-ray absorption fine structure (EXAFS) measurements showed that for the samples with low concentration of LSMO up to 1.0 wt.%, the Cu-O bond length and the CuO2 plane ordering do not degrade from the values of pure (Bi, Pb)-2223, while they get worsen with a further increase of LSMO addition. These results open up the possibility of LSMO as artificial pinning centers of the (Bi, Pb)-2223 system for power application.

Properties of Bi-2223/Ag HTS tapes using different content of precursors (조성이 다른 전구체 분말에 따른 Bi-2223/Ag 초전도 테이프의 특성 변화)

  • Ha, Dong-Woo;Yang, Joo-Saeng;Ha, Hong-Soo;Oh, Sang-Soo;Hwang, Sun-Yuk;Lee, Dong-Hoon;Choi, Jung-Kyu;Lee, En-Yong;Kwon, Young-Kil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.05a
    • /
    • pp.69-72
    • /
    • 2003
  • Bi-2223 superconducting wires were fabricated by stacking, drawing process with different precursor powders and different heat-treatment histories. The precursor powders were 2 kinds of Pb content. And a part of the tapes were experienced pre-annealing process which caused tetragonal structure of Bi-2212 phase to orthorhombic structure of it was during drawing process. We confirmed the transformation of Bi-2212 phase from tetragonal structure to orthorhombic structure and reduction of second phases. XRD and DC magnetization analysis were performed in order to investigate the fraction of Bi-2223 phase in Bi-2223/Ag HTS tape. We could achieve best Ic of 70 A class at the Bi-2223/Ag tape using low Pb content of precursor powder and experienced pre-annealing process. DC magnetization analysis was useful to investigate the fraction of Bi-2223 phase in the Bi-2223/Ag tape.

  • PDF

Effect of drawing process parameters on a sausaging in Bi(Pb)-2223 superconductor (Bi(Pb)-2223 초전도 선재에서 소세징에 대한 인발 공정 변수의 영향)

  • 박동인;김병민;오상수;하홍수
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2003.05a
    • /
    • pp.311-314
    • /
    • 2003
  • Superconduction materials possess electrical/electronic and magnetic properties. Because superconduction materials is a ceramic powder, that can not be produced singlehandedly. So Ag sheathed Bi-2223 wire was produced by drawing process using powder-in-tube(PIT) method This superconductor has many difficulties to produce. The main difficulty is that the mechanical properties of the ceramic powder are very different from those of the Ag sheath. Actually, the fabrication of Ag sheathed Bi-2223 superconductor by PIT tends to lead to non-uniformity in the core thickness during drawing process. That is so called “Sausaging”. This study analyzed a sausaging using the finite-element method. Also, Effects of drawing process parameters on a sausaging has been carried out using finite element method. Finally, A way to prevent a sausaging has been discussed.

The Precipitation of Second Phases by Annealing Heat Treatment in the $(Bi,Pb)_2$${Sr_2}{Ca_2}{Cu_3}{O_{10}}$ Superconductor System (BSCCO계 초전도체에서 서냉 열처리에 의한 2차상 석출)

  • 이상희;김철진;유재무
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.12
    • /
    • pp.1212-1220
    • /
    • 2000
  • Bi-2223 초전도체계에서 석출물을 flux-pinning center로 이용할 수 있는지 가능성을 타진하기 위하여 $Bi_{1.8}$P $b_{0.4}$S $r_{2}$C $a_{2.2}$C $u_3$ $O_{8}$ 조성을 가진 Bi-2223/Ag 선재를 반응온도, 산소분압, 시간 등을 변화시키면서 열처리를 행하였다. 열처리 후 석출물들은 XRD, SEM, TEM, EDS로 분석하였다. Bi-2223 모상내의 (Ca, Sr)$_2$(Pb,Bi) $O_4$, B $i_{0.5}$ P $b_3$S $r_2$C $a_2$Cu $O_{12+}$$\delta$/ (3221)와 같은 2차상들의 크기와 분포는 2223 입자들의 연결성을 파괴하지 않고 열처리 조건에 의해서 조절할 수 있었다. 서냉 열처리가 된 시편은 임계전류밀도( $J_{c}$)값이 증가하였는데, 이는 2223 입자내 나노미터 크기로 형성된 석출물들이 flux-pinning sites로 작용한 것으로 추정된다.다.

  • PDF

Properties of Bi-2223/Ag HTS tapes prepared using powders of varying lead content (Pb 함량을 달리한 전구체 분말에서의 Bi-2223/Ag 초전도 테이프의 특성 변화)

  • Ha, Dong-Woo;Yang, Joo-Saeng;Hwang, Sun-Yuk;Ha, Hong-Soo;Oh, Sang-Soo;Lee, En-Yong;Kwon, Young-Kil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.07a
    • /
    • pp.585-588
    • /
    • 2003
  • Bi-2223 superconducting wires were fabricated by stacking, drawing process with different precursor powders and different heat-treatment histories. The precursor powders were 2 kinds of Pb content. And a part of the tapes were experienced pre-annealing process which caused tetragonal structure of Bi-2212 phase to orthorhombic structure of it was during drawing process. We confirmed the transformation of Bi-2212 phase from tetragonal structure to orthorhombic structure and reduction of second phases. AC magnetization analysis were performed in order to investigate the fraction of Bi-2223 phase in Bi-2223/Ag HTS tape. The cross sections of 55 filaments and 61 filaments were investigated after rolled in order to understand deformation mechanism of superconducting cores. We could achieve best Ic of 70 A class at the Bi-2223/Ag tape using low Pb content of precursor powder and experienced pre-annealing process. AC magnetization analysis was useful to investigate the fraction of Bi-2223 phase in the Bi-2223/Ag tape.

  • PDF

Study on fabrication process of long length of Bi-2223/Ag MTS wires for high critical current (Bi-2223/Ag HTS 장선재의 Ic 특성 향상 공정 연구)

  • 하동우;양주생;황선역;이동훈;최정규;하홍수;오상수;권영길
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2003.02a
    • /
    • pp.105-108
    • /
    • 2003
  • Long length of Bi-2223 superconducting wires were fabricated by stacking, drawing process with different precursor owders and different heat-treatment histories. The precursor powders were 2 kinds of Pb content. And a part of the tapes were experienced pre-annealing process which caused tetragonal structure of Bi-2212 phase to orthorhombic structure of it was during drawing process. We confirmed the transformation of Bi-2212 phase from tetragonal structure to orthorhombic structure and reduction of second phases. We designed and made a continuous Ic measurement system for Bi-2223/Ag HTS tape. We could achieve best Ic of 65 A at the Bi-2223/Ag tape using low Pb content of precursor powder and experienced pre-annealing process.

  • PDF

The Effect of Relatively Low Lead Contents on the Phase Formation and Jc values of Bi-2223/Ag Tapes

  • Jiang, C.H.;Yoo, J.M.;Ko, J.W.;Kim, H.D.;Chung, H.S.
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.04a
    • /
    • pp.17-20
    • /
    • 2002
  • The effects of relatively low lead content (0.2~0.3) on the 2223 phase formation and transport property of Bi-2223/Ag tapes have been investigated. The results show that lead contents have great impact on the phase assemblage of precursors, subsequently, on the phase formation and transport property of silver sheathed BSCCO-2223 tapes. Powders containing Pb=0.25 and Pb=0.3 resulted in the nearly identical $J_c$ values in fully processed tapes, but leaded to significant difference on the phase formation process. For the case of Pb=0.2, both low conversion fraction of 2212 to 2223 and low $J_c$ value were obtained in final reacted tape, which was probably due to lack of enough liquid phase to facilitate the phase transformation.

  • PDF

Phase transition of (Bi, Pb)-2223 superconductor induced by Fe3O4 addition

  • Ko, Y.J.;Oh, J.Y.;Song, C.Y.;Yang, D.S.;Tran, D.H.;Kang, B.
    • Progress in Superconductivity and Cryogenics
    • /
    • v.21 no.4
    • /
    • pp.1-5
    • /
    • 2019
  • We investigated the effect of Fe3O4 addition on the critical temperature of (Bi, Pb)-2223 polycrystalline samples. Bi1.6Pb0.4Sr2Ca2Cu3O10+δ + x wt. % Fe3O4 (x = 0.0, 0.2, 0.4, 0.6, and 0.8) samples were prepared by using a solid-state reaction method. The analysis of X-ray diffraction data indicates that as Fe3O4 is added, dominant phase of the sample changes from Bi-2223 to Bi-2212 with an increasing Bi-2201 phase. The transition temperature of the samples drastically decreased with the Fe3O4 addition. The resistance data of samples with x = 0.2 and 0.4 showed a double transition indicating a coexistence of Bi-2223 and Bi-2212 phase while the samples with x = 0.6 and 0.8 showed a single transition with a semiconducting behavior. This phase transition may originate from changes in local structure of the Bi-2223 system by Fe3O4 addition. Analysis of the pair distribution function of the Cu-O pair in the CuO2 plane calculated from extended X-ray absorption fine structure data revealed that the oxygen coordination of copper ion changes from CuO4 planar type (x = 0.0 - 0.4) to CuO5 pyramidal type (x = 0.6, 0.8). The correlated Debye-Waller factor, providing information on the atomic disorder within the CuO2 plane, shows an inverse relation to the coordination number. These results indicate that addition of Fe3O4 changes the oxygen distribution around Cu in the CuO2 plane, causing a phase transition from Bi-2223 to more stable Bi-2212/Bi-2201 phases.

Characterizations of fine Bi-2223 precursor powder by spray pyrolysis process (분무 열분해법으로 제조된 미세 Bi-2223 전구분말의 특성)

  • Kim S. H.;Yoo J. M.;Ko J. W.;Kim Y. K.
    • Progress in Superconductivity
    • /
    • v.6 no.2
    • /
    • pp.124-128
    • /
    • 2005
  • Homogeneous and fine powders for Bi-2223 tape were prepared by ultrasonic spray pyrolysis (SP) method from an aqueous solution of metal nitrates. Bi-2223 precursor powders were synthesized with various solutes concentration and pyrolysis temperature. The synthesized precursor powders had a narrow particle size distribution and an average particle size was $\~{\cal}um$. The reactivity of precursor powder by SP method is very high, attributed to the fine and narrow particle size distribution. Bi-2223/Ag tape was prepared using PIT method and followed by various sintering conditions. The precursor powder by SP method promoted a very quick formation of the Bi-2223 phase for short sintering time while the secondary phase such as large AEC phase and $Ca_2PbO_4$ were minimized for SP tapes.

  • PDF