Single crystal growth of ZnWO4 by the Czochralski method and characterization (Czochralski법에 의한 ZnWO4 단결정 성장 및 특성분석)

  • Lim, Chang-Sung
    • Analytical Science and Technology
    • /
    • v.23 no.2
    • /
    • pp.103-108
    • /
    • 2010
  • Single crystals of $ZnWO_4$ with [100], [010] and [001] directions were successfully grown by the Czochralski method. The seed crystals for the single crystal growth of $ZnWO_4$ could be induced by the crystal growth using platinum wires applied by the capillary action from the melt. The growth conditions in each direction were investigated in terms of the variations of rotation speed, pulling rate and diameter of the grown crystals. The formation of cracking in the grown crystals during the cooling process could be prevented by annealing effect. The growth directions of the grown crystals were determined using Laue back reflection. The microscopic characteristics of the grown crystals in each direction were discussed, and their physical properties were evaluated for hardness, thermal expansion coefficients and dielectric constants.

Growth parameters and formation of slip plane in ZnWO4 single crystals by the Czochralski method

  • Lim, Chang-Sung
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.20 no.5
    • /
    • pp.202-206
    • /
    • 2010
  • Single crystals of $ZnWO_4$ were grown successfully in the [100], [010] and [001] directions using the Czochralski method. The growth parameters and the formation of slip plane in $ZnWO_4$ crystals were studied. $ZnWO_4$ crystals had a cleavage plane of (010). The dislocation density on the (010) plane at the center of the crystal was lower than that of the edge region. It was inferred that the high density at the edge of the crystals was caused by the thermal gradient during crystal growth. The etch pit arrangement revealed the (100) slip plane to be most active during crystal growth.

The Growth of Defects $ZnWO_4$ Single Crystals ($ZnWO_4$ 단결정 성장과 결함)

  • 조병곤;오근호
    • Journal of the Korean Ceramic Society
    • /
    • v.27 no.4
    • /
    • pp.447-456
    • /
    • 1990
  • ZnWO4 single crystals were grown by Czochralski method. And the orientation of grown crystals were determined by Laue back reflection, and the crystals were siliced at (100), (010), (001) face before polishing. The morphologys and distribution of etch pits on each face were observed by optical microscopy. In the present study, we understood that dislocation distributjioon rely on shape of solid-liquid interface, and secondary phase acts on the dislocation source. We also observed dislocation trace(etch pits) of (100) slip plane on (010) cleavage plane.

  • PDF

Preparation and characterization of ZnWO4 nanocrystallines and single crystals

  • Lim, Chang-Sung
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.20 no.5
    • /
    • pp.197-201
    • /
    • 2010
  • $ZnWO_4$ nanocrystallines were prepared from polymeric complex method using microwave irradiation. The average nanocrystalline sizes were 18~25 nm showing an ordinary tendency to increase with the temperatures from 400 to $600^{\circ}C$. Bulk type single crystals of $ZnWO_4$ were grown successfully in the [100], [010] and [001] directions using the Czochralski method. The effect of the growth parameters, such as the rotation speed, pulling rate and diameter of the grown crystals, were examined. The hardness, thermal expansion coefficients and dielectric constants of the crystals were evaluated.

$ZnWO_4$ Single Crystal Growth ($ZnWO_4$ 단결정 성장)

  • 임창성;오권한
    • Journal of the Korean Ceramic Society
    • /
    • v.23 no.4
    • /
    • pp.69-77
    • /
    • 1986
  • Single crystals of zinc tungstates were grown by the Czochralski method. To obtain the seed crystals various methods were employed including 4 points platinum wirse which dipped the melt and the capillary action from the melt led the 3 differently oriented seeds such as [100], [010] and [001] directions. Optimum growing conditions were observed as neck diameter 2mm rotation speed 50-60 rpm maximum diameter 15mm and pulling rate 0-10 mm/hr. Dendrites covered on the olidified surface in a platinum crucible were turned out to be [001] direction because obviously this crystal has the strong [001] preferential growth habit. The (100) and (010) planes of single crystals showed the slip planes and the (010) plane showed the perfect cleavage surface.

  • PDF