• Title/Summary/Keyword: $WO_3/TiO_2$

Search Result 144, Processing Time 0.025 seconds

Characteristics of SCR-Catalytic with de-NOx System in Thermal Power plants (화력발전소 NOx 제거를 위한 SCR 촉매 특성)

  • Ko, Seung-Jae;Kim, Ji-Hyun;Kim, Mi-Joung;Cho, Yeon-Bae;Park, Young-Koo
    • Journal of the Korean Applied Science and Technology
    • /
    • v.30 no.3
    • /
    • pp.451-460
    • /
    • 2013
  • NOx from the thermal power plants are NO and $NO_2$. This work investigated the chemical/physical characteristics and SCR efficiency of newly prepared catalysts including tungsten ($WO_3$), molybdenum ($MoO_3$) and antimony ($SbO_3$) based on vanadia($V_2O_5$) over titania($TiO_2$). As a result of the examination, the surface area of the catalysts promoted with additional metals was larger and the de-NOx efficiency also was enhanced with temperature. The most efficient catalytst was $V_2O_5/TiO_2-WO_3$(10%) at $200^{\circ}C$. Such a high efficiency could contribute to reduce the ammonia slip.

A Study on the Regeneration Effects of Commercial $V_2O_5-WO_3/TiO_2$ SCR Catalyst for the Reduction of NOx (질소산화물 제거용 상용 $V_2O_5-WO_3/TiO_2$ SCR 폐 촉매의 재생 효과 고찰)

  • Park, Hea-Kyung
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.27 no.8
    • /
    • pp.859-869
    • /
    • 2005
  • The commercial $V_2O_5-WO_3/TiO_2$ catalysts which had been exposed to the off gas from incinerator for a long time were regenerated by physical and chemical treatment. The catalytic properties and NOx conversion reactivity of those catalysts were examined by analysis equipment and NOx conversion experiment. The characterization of the catalysts were performed by XRD(x-ray diffractometer), BET, POROSIMETER, EDX(energy dispersive x-ray spectrometer), ICP(inductively coupled plasma), TGA(thermogravimetric analyzer) and SEM (scanning electron microscopy). NOx conversion experiment were performed with simulated off gas of the incinerator and $NH_3$ was used as a reductant of SCR reaction. Among the regeneration treatment methods which were applied to regenerate the aged catalysts in this study, it showed that the heat treatment method had excellent regeneration effect on the catalytic performance for NOx conversion. The catalytic performance of the regenerated catalysts with heat treatment method were recovered over than 95% of that of fresh catalyst. For the regenerated catalysts with the acid solution(pH 5) and the alkali solution(pH 12), the catalytic performance were recovered over than 90% of that of fresh catalyst. From the characterization results of the regenerated catalysts, the specific surface area was recovered in the range of $85{\sim}95%$ of that of fresh catalyst. S and Ca element, which are well known as the deactivation materials for the SCR catalysts, accumulated on the aged catalyst surface were removed up to maximum 99%. Among the P, Cr, Zn and Pb elements accumulated on the aged catalyst surface, P, Cr and Zn element were removed up to 95%. But the Pb element were removed in the range of $10{\sim}30%$ of that of fresh catalyst.

Effect of calcination temperature on the Coloring of $TiO_2-WO_3$-NiO Pigments ($TiO_2-WO_3$-NiO 안료의 발색특성에 대한 소결온도의 영향)

  • Chun, Myuong-Pyo;Kang, Kyung-Min;Cho, Jeong-Ho;Kim, Byung-Ik;Kwon, Myon-Joo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2010.06a
    • /
    • pp.274-274
    • /
    • 2010
  • 안료의 색상은 출발원료의 조성, 입자크기 및 소결온도에 의한 결정구조 등에 의존한다. 본 연구에서는 Rutile구조를 갖는 세라믹안료인 $TiO_2-WO_3$-NiO의 합성에서 소결온도를 결정하기 위해 소결전 출발원료를 습식법에 의하여 Jar Mill에서 0.7-0.9um로 혼합분쇄한 후 $100^{\circ}C$에서 24시간 건조하였다. 건조후 $1100-1280^{\circ}C$에서 5구간을 선정하여 소결한 시료를 Jar Mill에서 0.8-1um로 분쇄한 후, 다시 $100^{\circ}C$에서 24시간 건조하였다. 이렇게 얻어진 시료를 XRD로 상합성 정도를 조사하고, 색상 및 착색력을 spectrophotometer를 분석하였다. 색상은 1150와 $1250^{\circ}C$에서 가장 좋은 Yellow 색상이 관찰되었으며, XRD에 의한 결정성의 분석결과와 비교적 일치하고 있다. Rutile구조를 갖는 세라믹안료의 색상은 소결시의 결정화도에 따라 민감하게 변화되고 있음을 알 수 있다.

  • PDF

Microstructure and Dielectric Properties in $30Pb(Mg_{1/3}Nb_{2/3})O_3-20PbTiO_3-50Pb(Mg_{1/2}W_{1/2})O_3$ Ceramics with Excess MgO Addition (MgO가 과잉첨가된 $30Pb(Mg_{1/3}Nb_{2/3})O_3-20PbTiO_3-50Pb(Mg_{1/2}W_{1/2})O_3$계 세라믹스의 미세구조와 유전특성)

  • 길영배;이응상
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.1
    • /
    • pp.31-36
    • /
    • 1997
  • The effects of 0 to 10mol% excess MgO addition on the microstructure and dielectric properties in 30Pb(Mg1/3Nb2/3)O3-20PbTiO3-50Pb(Mg1/2W1/2)O3 ternary system were investigated. Samples were prepared by mixed oxide and precursor methods to compare the role of excess MgO. Excess MgO enhanced grain growth and increased dielectric constant. The dielectric constant and tesmperature dependence of dielectric constant of the sample sintered at 100$0^{\circ}C$ with 5mol% MgO were above 5,000 and +25% to -50% from - 55$^{\circ}C$ to 1$25^{\circ}C$, respectively. For these specimens the phases percent were mainly perovskite and Pb2WO5, which was confirmed by XRD analysis. Also the amount of cubic pyrochlore Pb3Nb4O13 and PbWO4 were de-creased with sintering temperature and MgO addition. BSE image showed the chemical inhomogeneous dis-tribution. Crystal phase formed at each sintering temperature and the chemical inhomogeneous distribution caused the decrease of the temperature dependence of dielectric constant.

  • PDF

Remanufacturing of Commercial $V_2O_5-WO_3/TiO_2$ Catalyst used in the SCR Process of Incinerator (소각장 SCR 공정에서 사용되는 상용 $V_2O_5-WO_3/TiO_2$ 촉매의 재제조에 관한 연구)

  • Yoon, Goan-Gu;Yoo, Man-Sik;Lim, Jong-Sun;Kim, Tae-Won;Park, Hea-Kyung
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.27 no.9
    • /
    • pp.970-977
    • /
    • 2005
  • The commercial $V_2O_5-WO_3/TiO_2$ catalysts which had been exposed to the off gas from incinerator for a long time were remanufactured by washing with distilled water and arid solution and reimpregnation with catalytic active components($V_2O_5-WO_3$). The catalytic properties and NOx conversion reactivity of those catalysts were examined by analysis equipment and NOx conversion experiment. Under the experimental condition used in this study, the remanufactured catalysts activated by distilled water ultra sonic cleaning, the catalytic activity was recovered in the range of $66{\sim}93%$ of that of the fresh and the maximum activity was showed when the ultra sonic cleaning time was more than 3 minutes. The remanufactured catalysts by acid solution ultra sonic cleaning, the catalytic activity was recovered in the range of $81{\sim}97%$ of that of the fresh catalyst and the maximum catalytic activity was shooed when the pH of the acid solution was 5. The remanufactured catalysts by reimpregnation with $V_2O_5$ and $WO_3$, the catalytic activity was recovered in the range of $87{\sim}100%$ of that of the fresh catalyst. Maximum catalytic activity was showed when the $V_2O_5$ was reimpregnated more than 1.0 wt %. In this case, the catalytic activity was recovered 97% of that of the fresh catalyst especially at the $150^{\circ}C$ of the experimental temperature.

Photoinduced Superhydrophilicity in TiO2 Thin Films Modified with WO3

  • Hwang, Young-Kyu;Patil, Kashinath Rangu;Kim, Hye-Kyung;Dattatraya Sathaye, Shivaram;Hwang, Jin-Soo;Park, Sang-Eon;Chang, Jong-San
    • Bulletin of the Korean Chemical Society
    • /
    • v.26 no.10
    • /
    • pp.1515-1519
    • /
    • 2005
  • Tungsten oxide-modified TiO2 thin films were formed on a glass substrate by sol-gel and dip coating processes using acetyl acetone as a chelating agent. The hydrophilic properties of the thin films were investigated with illumination of UV light. The dependence of water contact angle on material composition and morphology of the film is established with SEM image and AFM profile. The surface morphology was controlled with the change of precursor concentration. 0.01 M of tungsten oxide-modified Ti$O_2$ have shown the highest hydrophilicity after UV-irradiation. The effect of composition on photoinduced hydrophilicity of the W$O_3$-Ti$O_2$ films was also investigated. The films were characterized by XRD, SEM, AFM and XPS.

Dielectric properties 40Pb$(Mg_{1/3}Nb_{2/3})O_3-30PbTiO_3-30Pb(Mg_{1/2}W_{1/2})O_3$ ceramics (40Pb$(Mg_{1/3}Nb_{2/3})O_3-30PbTiO_3-30Pb(Mg_{1/2}W_{1/2})O_3$ 세라믹스의 유전특성)

  • 길영배;임대영
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.10 no.2
    • /
    • pp.134-139
    • /
    • 2000
  • Ternary system of 40PMN-30PT-30PMW was prepared by using different reaction process. The PMN-PT was synthesized firstly, then it reacted to $PbWO_4$ as PbO and $WO_3$ sources. The dielectric constants were dependent on the density of sintered body and decreased with sintering temperature above $950^{\circ}C$. The highest dielectric constant was 24,000 in a sample sintered at $950^{\circ}C$ with the dielectric loss of 3 %. The temperature dependence of the dielectric constant were decreased with the increase of sintering temperature due to the appearance of double peak maxima. The lowest change in dielectric constant was -37-0 % from -55 to $125^{\circ}C$in a sample sintered at $1150^{\circ}C$ with dielectric constant of 9,900 at room temperature.

  • PDF

Microwave Dielectric Properties of (Zr, Sn)$TiO_4$ ceramics according to Sn and Additives ((Zr, Sn)$TiO_4$ 세라믹스의 Sn 및 첨가제 양에 따른 고주파 유전 특성)

  • Yun, Jung-Rag;Kim, Kyung-Yong
    • Proceedings of the KIEE Conference
    • /
    • 1993.11a
    • /
    • pp.181-184
    • /
    • 1993
  • Microwave characteristics of the system (Zr, Sn)$TiO_4$, ceramics within composition range X between 0.2 and 0.35 were investigated at 8GHz. For the improvement properties of (Zr, Sn)$TiO_4$, system, $Ta_2O_5$ and $WO_3$ addition in the range of 0.5 to 2.0wt% were investigated.

  • PDF

The Effect of Promoters Addition on NOx Removal by $NH_3$ over V$V_2O_5/TiO_2$

  • Lee, Keon-Joo
    • Journal of Korean Society for Atmospheric Environment
    • /
    • v.18 no.E1
    • /
    • pp.29-36
    • /
    • 2002
  • The selective catalytic reduction (SCR) reaction of promoter catalysts was investigated in this study. A pure anatase type of TiO$_2$ was used as support. Activation measurement of prepared catalysts was practiced on a fixed reactor packing by the glass bead after filling up catalysts in 1/4 inch stainless tube. The reaction temperature was measured by K-type thermocouple and catalyst was heated by electric furnace. The standard compositions of the simulated flue gas mixture in this study were as follows: NO 1,780ppm, NH$_3$1,780ppm, $O_2$1% and $N_2$ as balance gas. In this study, gas analyzer was used to measure the outgassing gas. Catalyst bed was handled for 1hr at 45$0^{\circ}C$, and the reactivity of the various catalyst was determined in a wide temperature range. Conversion of NH$_3$/NO ratio and of $O_2$ concentration was practiced at 1,1.5 and 2, respectively. The respective space velocity were as follows . 10,000, 15,000 and 17,000 hr-1. It was found that the maximum conversion temperature range was in a 5$0^{\circ}C$. It was also found toi be very sensitive at space velocity, $O_2$ concentration, and NH$_3$/NO ratio. We also noticed that the maximum conversion temperature of (W, Mo, Sn) -V$_2$O$_{5}$/TiO$_2$ catalysts was broad. Specially WO$_3$-V$_2$O$_{5}$TiO$_2$2 catalyst appeared nearly 100% conversion at not only above 30$0^{\circ}C$ ut also below 25$0^{\circ}C$. At over 30$0^{\circ}C$, NH$_3$ oxidation decreased with decrease of surface excess oxygen. In addition, WO$_3$-V$_2$O$_{5}$TiO$_2$ catalyst did not appear to affect space velocity, $O_2$ concentration, and NH$_3$/NO ratio.ratio.