SiC계 세라믹 절삭공구의 절삭특성 평가 Part 1: SiC계 절삭공구의 미세구조와 기계적 특성 (Cutting Characteristics of SiC-based Ceramic Cutting Tools Part 1: Microstructure and Mechanical Properties of SiC-based Ceramic Cutting Tools)

  • 박준석;김경재;심완희;권원태;김영욱
    • 한국정밀공학회지
    • /
    • 제18권9호
    • /
    • pp.82-88
    • /
    • 2001
  • In order to fulfil the requirements of the various performance profiles of ceramic cutting tools, six different SiC-based ceramics have been fabricated by hot-pressing (SiC--${Si}_3 {N}_4$composites) or by hot-pressing and subsequent annealing (monolithic SiC and SiC-TiC composites). Correlation between the annealing time and the corresponding microstructure and the mechanical properties of resulting ceramics have been investigated. The grain size of both ${Si}_3 {N}_4$and SiC in SiC-${Si}_3 {N}_4$composites increased with the annealing time. Monolithic SiC has the highest hardness, SiC-TiC composite the highest toughness, and the SiC-${Si}_3 {N}_4$composite the highest strength among the ceramics investigated. The hardness of SiC-${Si}_3 {N}_4$composites was relatively independent of the grain size, but dependent on the sintered density. The cutting performance of the newly developed SiC-based ceramic cutting tools will be described in Part 2 of this paper.

  • PDF

SiO2 콜로이달에 의한 Si3N4 복합 세라믹스의 상온굽힘강도 및 균열치유 현상 (Room Temperature Strength and Crack Healing Morphology of Si3N4 Composite Ceramics with SiO2 Colloidal)

  • 남기우;김종순;이희방
    • 대한기계학회논문집A
    • /
    • 제33권7호
    • /
    • pp.652-657
    • /
    • 2009
  • Strength characteristics of $Si_3N_4$ composite ceramics has been studied as functions of heat-treatment temperature and additive $SiO_2$. $SiO_2$ colloidal could significantly increase the bending strength. Crack healing temperature decreased 300 K by additive $TiO_2$. Bending strength of specimen added $SiO_2$ is higher than that of non-added $SiO_2$. Moreover, bending strength of specimen with $SiO_2$ colloidal coating is much higher that of non-coated specimen. In in-situ observation, crack-healed specimen at 1,573 K shows phenomenon like a fog on the surface. By SPM, both crack-healed specimen, non-coating and coating of $SiO_2$ colloidal, at 1,273 K were healed completely but both of 1,573 K exist crack. This was made by evaporation of $SiO_2$ at high temperature. Crack-healing materials of $Si_3N_4$ composite ceramics is crystallized $Y_2Si_2O_7$, $Y_2Ti_2O_7$ and $SiO_2$. A large amount of Si and O, and little C were detected by EPMA. Si and O increase but C decreases according to heat treatment temperature. Specimens with additive $SiO_2$ were more detected Si and O than that of non-additive $SiO_2$. Specimen with $SiO_2$ colloidal coatings were much more detected O.

Development of CNT-dispersed Si3N4 Ceramics by Adding Lower Temperature Sintering Aids

  • Matsuoka, Mitsuaki;Yoshio, Sara;Tatami, Junichi;Wakihara, Toru;Komeya, Katsutoshi;Meguro, Takeshi
    • 한국세라믹학회지
    • /
    • 제49권4호
    • /
    • pp.333-336
    • /
    • 2012
  • The study to give electrical conductivity by dispersing carbon nanotubes (CNT) into silicon nitride ($Si_3N_4$) ceramics has been carried out in recent years. However, the density and the strength of $Si_3N_4$ ceramics were degraded and CNTs disappeared after firing at high temperatures because CNTs prevent $Si_3N_4$ from densification and there is a possibility that CNTs react with $Si_3N_4$ or $SiO_2$. In order to suppress the reaction and the disappearance of CNTs, lower temperature densification is needed. In this study, $HfO_2$ and $TiO_2$ was added to $Si_3N_4-Y_2O_3-Al_2O_3$-AlN system to fabricate CNT-dispersed $Si_3N_4$ ceramics at lower temperatures. $HfO_2$ promotes the densification of $Si_3N_4$ and prevents CNT from disappearance. As a result, the sample by adding $HfO_2$ and $TiO_2$ fired at lower temperatures showed higher electrical conductivity and higher bending strength. It was also shown that the mechanical and electrical properties depended on the quantity of the added CNTs.

반도성 $BaTiO_3$ 세라믹스의 미세구조 및 PTCR 특성에 미치는 $Si_3N_4$ 첨가효과 (Effect of $Si_3N_4$ Addition on the Microstructure and PTCR Characteristics in Semiconducting $BaTiO_3$ Ceramics)

  • 김준수;정윤해;이병하
    • 한국세라믹학회지
    • /
    • 제31권10호
    • /
    • pp.1089-1098
    • /
    • 1994
  • The effect of Si3N4 addition on the microstructure and PTCR characteristics of BaTiO3 was studied. When 0.1 mol% Sb2O3-doped BaTiO3 codoped with Si3N4 (0.1, 0.25, 0.5, 0.75, and 1 wt%, respectively) were sintered, their microstructures were changed by the amount of the liquid phase as a result of eutectic reaction at 126$0^{\circ}C$. By these microstructural changes, the specific resistivity ratio($\rho$max/$\rho$min) with Si3N4 content variation of 0.1 mol% Sb2O3-doped BaTiO3 ceramics sintered at 130$0^{\circ}C$ for 1 hour varied between 3.70$\times$102(0.1 wt% Si3N4) to 1.16$\times$103 (1wt% Si3N4).

  • PDF

Si3N4 세라믹스의 균열 치유와 굽힘 강도 특성 (Cracked-Healing and Bending Strength of Si3N4 Ceramics)

  • 남기우;박승원;도재윤;안석환
    • 대한기계학회논문집A
    • /
    • 제32권11호
    • /
    • pp.957-962
    • /
    • 2008
  • Crack-healing behavior of $Si_3N_4$ composite ceramics has been studied as functions of heat-treatment temperature and amount of additive $SiO_2$ colloidal. Results showed that optimum amount of additive $SiO_2$ colloidal and coating of $SiO_2$ colloidal on crack could significantly increase the bending strength. The heat-treatment temperature has a profound influence on the extent of crack healing and the degree of strength recovery. The optimum heat-treatment temperature depends on the amount of additive $SiO_2$ colloidal. Crack healing strength was far the better cracked specimen with $SiO_2$ colloidal coating on crack surface. After heat treatment at the temperature 1,273 K in air, the crack morphology almost entirely disappeared by scanning prob microscope. At optimum healing temperature 1,273 K, the bending strength with additive $SiO_2$ colloidal 0.0 wt.% without $SiO_2$ colloidal coating recovered to the value of the smooth specimens at room temperature for the investigated crack sizes $100\;{\mu}m$. But that with $SiO_2$ colloidal coating increase up to 140 %. The amount of optimum additive $SiO_2$ colloidal was 1.3 wt.% and crack healed bending strength with $SiO_2$ colloidal coating increase up to 160 % to smooth specimen of additive $SiO_2$ colloidal 0.0 wt.%. Crack closure and rebonding of the crack due to oxidation of cracked surfaces were suggested as a dominant healing mechanism operating in $Si_3N_4$ composite ceramics.

파우더 블라스팅에 의한 $Si_3N_4$-hBN계 머시너블 세라믹스의 미세패턴 가공성 평가 (Micro-Pattern Machining Characteristics Evaluation of $Si_3N_4$-hBN based Machinable Ceramics Using Powder Blasting Process)

  • 박동삼;조명우;김동우;조원승
    • 한국공작기계학회논문집
    • /
    • 제13권2호
    • /
    • pp.33-39
    • /
    • 2004
  • Sandblasting has recently been developed into a powder blasting technique for brittle materials. In this study, the machinability of $Si_3N_4$-hBN based machinable ceramics are evaluated for micro - pattern making processes using powder blasting. Material properties of the developed machinable ceramics according to the variation of h-BN contents give a good machinability to the ceramics. The effect of scanning times, the size of patterns and variation of BN contents on the erosion depth of samples without mask and samples with different mask patterns in powder blasting of $Si_3N_4$-hBN ceramics are investigated. The Parameters are the impact angle of $90^{\circ}$, the scanning times of nozzle up to 40, and the stand-off distances of 100mm The widths of masked pattern are 0.1mm 0.5mm and 1mm. The powder used is Alumina particles, WA#600. and the blasting pressure of powder is 0.2MPa. Through required experiments, the results are investigated and analyzed. As the results, the machinability of the developed ceramics increases as the BN contents in the ceramics.

Properties of Powders and Sintered Bodies of Sialon $Si_3N_4$ and SiC Prepared from Korean Raw Materials

  • 이홍림
    • 한국세라믹학회:학술대회논문집
    • /
    • 한국세라믹학회 1986년도 Priceedings Of The Third Korea-Japan Seminar On New Ceramics
    • /
    • pp.156-161
    • /
    • 1986
  • Sialon $Si_3N_4$ and SiC powders and ceramics were prepared from Korean natural resources. The properties of the powders and sintered ceramics obtained in this work are considered to be comparable to those of foreign articles.

  • PDF

SiO2 나노 콜로이달 첨가량에 따른 Si3N4의 고온강도 특성 (Characterization of High Temperature Strength of Si3N4 Composite Ceramics According to the Amount of SiO2 Nano Colloidal Added)

  • 남기우;이건찬
    • 대한기계학회논문집A
    • /
    • 제33권11호
    • /
    • pp.1233-1238
    • /
    • 2009
  • This study analyzed the characterization of high temperature strength of $Si_3N_4$ composite ceramics additive based on variations in the amount of nano colloidal $SiO_2$ added. Semi-elliptical cracks about 100 ${\mu}m$ length were obtained from a Vickers indenter using a load of 24.5 N. The results showed that the heat-treated smooth specimens with $SiO_2$ nano colloidal coating exhibited the highest bending strength at 0.0 wt% $SiO_2$ nano colloidal added, which is amounted to a 187 % increase over that of smooth specimen. Limiting temperature for bending strength of crack-healed zone for bending strength was about 1273 K. However, the bending strength of SSTS-3 and SSTS-4 was considerably increased while that of SSTS-1 and SSTS-2 was decreased at a temperature of 1,573K.

Characterization of Subsurface Damage in Si3N4 Ceramics with Static and Dynamic Indentation

  • Kim, Jong-Ho;Kim, Young-Gu;Kim, Do-Kyung
    • 한국세라믹학회지
    • /
    • 제42권8호
    • /
    • pp.537-541
    • /
    • 2005
  • Silicon nitride is one of the most successful engineering ceramics, owing to a favorable combination of properties, including high strength, high hardness, low thermal expansion coefficient, and high fracture toughness. However, the impact damage behavior of $Si_3N_4$ ceramics has not been widely characterized. In this study, sphere and explosive indentations were used to characterize the static and dynamic damage behavior of $Si_3N_4$ ceramics with different microstructures. Three grades of $Si_3N_4$ with different grain size and shape, fine-equiaxed, medium, and coarse-elongated, were prepared. In order to observe the subsurface damaged zone, a bonded-interface technique was adopted. Subsurface damage evolution of the specimens was then characterized extensively using optical and electron microscopy. It was found that the damage response depends strongly on the microstructure of the ceramics, particularly on the glassy grain boundary phase. In the case of static indentation, examination of subsurface damage revealed competition between brittle and ductile damage modes. In contrast to static indentation results, dynamic indentation induces a massive subsurface yield zone that contains severe micro-failures. In this study, it is suggested that the weak glassy grain boundary phase plays an important role in the resistance to dynamic fracture.

Microstructure, Mechanical and Wear Properties of Hot-pressed $Si_3N_4-TiC$ Composites

  • Hyun Jin Kim;Soo Whon Lee;Tadachika Nakayama;Koichi Niihara
    • The Korean Journal of Ceramics
    • /
    • 제5권4호
    • /
    • pp.317-323
    • /
    • 1999
  • Si3N4-TiC composites have been known as electrically conductive ceramics. $Si_3N_4-TiC$ composites with 2 wt% $Al_2O_3$ and 4 wt% $Y_2O_3$ were hot pressed in $N_2$ environment. The mechanical properties including hardness, fracture toughness, and flexural strength and tribological properties were investigated as a function of TiC content. $Si_3N_4-40$ vol% TiC composite was hot pressed at $1,750^{\circ}C$, $1,800^{\circ}C$, and $1,850^{\circ}C$ for 1, 3 and 5 hours in $N_2$ gas. Mechanical and tribolgical properties depended on microstructures, which were controlled by hte TiC content, hot press temperature, and hot press holding time. However, mechanical properties and tribological behaviors were degraded by the chemical reaction between TiC and N. The chemically reacted products such as TiCN, SiC, and $SiO_2$ were detered by the X-ray diffraction analysis.

  • PDF