  • The $PbTiO_3$is well known materials having remarkable ferroelectric piezoelectric and pyro-electric properties. Thin films of the lead titanite has been successfully fabricated by Chemical Vapor Deposition on the borosilicate glass and titanium substrate. The $PbTiO_3$ thin film deposited on the borosilicate glass using the $PbCl_2$, $TiCl_4$ dry oxygen and wet oxygen at different temperatures (50$0^{\circ}C$-$700^{\circ}C$) grows along the (001) preferred orientation. On the other hand the $PbTiO_3$ thin film deposited on the titanium substrate using the PbO grows along the (101) preferred orientation. Growth orientation of deposited $PbTiO_3$ depends on the reaction species irrespective of substrate materials. Maximum dielectic constant and loss tangent of the $PbTiO_3$ thin film deposited on the titanium substrate are about 90 and 0.02 respectively, . Deposition rates of $PbTiO_3$ deposited on the borosilicate glass and titanium substrate are 10-15 ${\mu}{\textrm}{m}$/hr. Titanium dioxide interlayer formed be-tween $PbTiO_3$ film and titanium substrate material, It improved the adhesion of the film.

  • PDF

Growth of lead-based functional crystals by the vertical bridgman method

  • Xu Jiayue
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.16 no.1
    • /
    • pp.1-7
    • /
    • 2006
  • Some lead-based crystals show excellent ferroelectric, piezoelectric or scintillation properties and have attracted much attention in recent years. However, the erosion of the high temperature solution on platinum crucible and the evaporation of PbO component are the main problems often encountered during the crystal growth. In this paper, we reported recent progress on the Bridgman growth of lead-based functional crystals, such as novel relaxor ferroelectric crystals (PZNT and PMNT), scintillation crystals $(PbWO_4,\;PbF_2\;and\;PbClF)$ and piezoelectric crystals $(Pb_5Ge_3O_{11}\;and\;Pb_2KNb_5O_{15}),$ in Shanghai Institute of Ceramics, Chinese Academy of Sciences. The vertical Bridgman method has been modified to grow PZNT crystals from high temperature solution and as-grown crystals have been characterized. Large size lead-based scintillators, $PbWO_4\;and\;PbF_2$ crystals, have been mass-produced by the vertical Bridgman method in the multi-crucible fumace. These crystals have been supplied to CERN and other laboratories for high-energy physics experiments. The Bridgman growth of piezoelectric crystals $Pb_5Ge_3O_{11}\;and\;Pb_2KNb_5O_{15}$ are discussed also.

Effects of Sintering Additives and Atmospheres on the Piezoelectric and Sintering Properties of $Pb_{0.98}Cd_{0.02}Zr_{0.36}Ti_{0.39}Ni_{0.083}Nb_{0.167}O_3$ (소결첨가제와 분위기가 $Pb_{0.98}Cd_{0.02}Zr_{0.36}Ti_{0.39}Ni_{0.083}Nb_{0.167}O_3$의 소결 및 압전 특성에 미치는 영향)

  • 문종하;박진성;박현수
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.11
    • /
    • pp.1260-1266
    • /
    • 1996
  • The effects of SiO2 MnO2 and sintering atmospheres (O2, N2) on the piezoelectric properties and densification behaviors of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 were investigated. The addition of SiO2 to the system enhanced the rate of densification but supressed the rate of grain growth. On the other hand the addition of MnO2 to the system did not nearly affect the rate of densification but increased slightly the rate of grain growth The densification of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 was promoted with increasing the partial pressure of O2. The relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 sintered under O2 atmosphere were higher than under N2 atmosphere. Whereas the mechanical quality factor (Qm) of specimens sintered under O2 atmosphere were lower than under N2 atmosphere. Thus the sintering atmosphere of O2 and N2 in Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 acted as donor and acceptor respectively. As the amount of SiO2 increased the relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 but the mechanical quality factor (Qm) did not nearly change, In the case of the addition of MnO2 to the system the relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 sintered under O2 atmosphere decreased rapidly with increasing the amount of MnO2 but they were unchanged with increasing the amount of MnO2 under N2 sintering atmosphere. Therefore the differences of the relative dielect-ric constant ($\varepsilon$r) and piezoelectric constant (d33) due to sintering atmosphere were diminished as the amount of MnO2 increased.

  • PDF

Sol-Gel Template Synthesis and Characterization of PT, PZ and PZT Nanotubes (PT, PZ와 PZT나노튜브의 졸-겔 형판합성과 특성)

  • Jang, Gi Seok;Bernadette A. Hernandez;Ellen R. Fisher;Peter K. Dorhout
    • Journal of the Korean Chemical Society
    • /
    • v.46 no.3
    • /
    • pp.242-251
    • /
    • 2002
  • We report the synthesis and characterization of the perovskite nanotubes made by sol-gel template syn-thesis.Both lead titanate (PbTiO3 : PT), lead zirconate (PbZrO3 : PZ) and lead zirconium titanate (PbZrO3 -PbTiO3 : PZT) solid solution nanotubes were prepared with a chelate sol-gel of titanium isopropoxide (Ti(OPri)4 ), zirconium tet-rabutoxide (Zr(OBu)4 ) and the respective lead acetate (Pb(OAc)2 -3H2O). WhatmanRanodisc membranes, with a 200nm pore size, served as the template. After the removal of the template in the 6M-NaOH, scanning electron microscopy shows that the shapes formed are 200 nm outer diameter tubes with 50mm lengths. Transmission electron microscopy and electron diffraction reveal that the tubes are polycrystalline. The PT nanotubes so far have shown an anomalous transition temperature, 234.4$^{\circ}C$ as measured by DSC with a small particle size, 15.4 nm determined by X-ray analysis with the aid of Scherrer's equation.

Characteristice Study of Ancient Northeast Asian Lead Glass and Green Glaze Based on Analysis Results (분석자료를 기초한 고대 납유리와 녹유의 특성 연구)

  • Lee, Jihee;Kim, Hyunjeong
    • Conservation Science in Museum
    • /
    • v.24
    • /
    • pp.99-116
    • /
    • 2020
  • This study examines the results of analyses of the lead isotope ratio and chemical composition of lead glass and green glaze from ancient Northeast Asia in order to suggest their production sites and reveal further characteristics. The comparison of the lead isotope ratio of lead glass and green glaze from two Baekje remains in Iksan-the Wanggung-ri Site and Mireuksa Temple Site-suggests that they were produced to the west of the South Gyeonggi Massif (Zone 4) using lead extracted from the same area. With a few exceptions, it has proved difficult to identify the production sites of most of the green-glazed roof tiles from Unified Silla-period Buddhist temples across Northeast Asia. The major component of the lead glass from Baekje, Silla, China, and Japan during the seventh century is PbO, SiO2, Al2O3, CuO, and Fe2O3, with a ratio of PbO and SiO2 of 70 and 30 wt.%, respectively. The green-glazed roof tiles excavated from a temple from the Unified Silla period have a high proportion of lead, ranging from 64 to 90 wt.%. Green-glazed lozenge tiles excavated from the Sacheonwangsa Temple site in Gyeongju were shown to contain PbO, SiO2, Al2O3, and CuO, a similar composition with lead glass. An experiment was conducted to reproduce a glaze according to the production method mentioned in the Zō hotokesho sakumotsu-chō (Buddhist statue workshop crop book) in the Shosoin Repository. In this experiment, an identical ratio of PbO was observed for Japanese green-glazed ceramics from the eighth to eleventh century as that found in Chinese lead-glazed ceramics excavated from kilns operated from the seventh to tenth century in Henan. This indicates that production methods for lead glass and glaze were shared across Northeast Asia.

Calcination Condition of CsPbBr3-SiO2 Composite Nanoparticles (CsPbBr3-SiO2 복합 나노입자의 소결 조건 연구)

  • Jeon, Min-Gi;Kabir, Rezaul MD;Kirakosyan, Artavazd;Choi, Jihoon
    • Composites Research
    • /
    • v.35 no.4
    • /
    • pp.298-302
    • /
    • 2022
  • Owing to the superior optoelectronic properties, halide perovskites have emerged as next-generation materials for display application. In this study, we reported a novel route for CsPbBr3 calcination into porous SiO2 nanoparticles to overcome the stability issues of halide perovskite via a spatial confinement of crystal growth within SiO2 pores. The resulting CsPbBr3-SiO2 nanoparticles exhibited the photoluminescence (PL) emission peak at 515 nm under optimal calcination condition. In several polar solvents, PL properties of CsPbBr3-SiO2 nanoparticles was maintained owing to the enclosed pores during calcination process, suggesting their promising application for display color conversion film.

Anomalous Enrichment of $Pb^+$Ions by Crossed Beam Scattering of a Pb($Zr_xTil_{1-x}O_3$) Plume and an $O_2$ Jet

  • Park, Seong Min;Mun, Ji Yun
    • Bulletin of the Korean Chemical Society
    • /
    • v.21 no.8
    • /
    • pp.801-804
    • /
    • 2000
  • A crossed beam scattering of a $Pb(ZrxTi1-x)O_3plume$ and an oxygen jetwas studied by using a time-of-flight quadrupole mass spectroscopy. Both simple collisions and reactive scatterings had significant effects on the transportand energetics of ions in the plume. Relative enrichment of metal and metal oxide ions was also changed with the oxygen pulse because of the differences in the mass and chemical properties of the ions. In particular, an anomalous increase ofPb+ ions was observed as the oxygen jet crossed the plume at high laserfluences, while the signal magnitudes of alI other ions were reduced. This originates from the fact that PbO+ ions dissociate easily to liberate Pb+ ions inthe plume since the bond energy of PbO+ is as low as 2.2 eV.

Variations of Ferroelectric Properties by Unit Cell Distortion of Pb(Zr, Ti)O3-Pb(Co, Nb)O3 Solid Solution in Morphotropic Phase Boundary (Morphotropic Phase Boundary 영역의 Pb(Zr, Ti)O3-Pb(Co, Nb)O3계 고용체의 격자변형에 따른 강유전 특성 변화)

  • 이전국;정형진
    • Journal of the Korean Ceramic Society
    • /
    • v.25 no.6
    • /
    • pp.694-698
    • /
    • 1988
  • Pb(Zr, Ti)O3-Pb(Co, Nb)O3 systems were investigated by x-ray diffraction method. System contains rhombohedral, tetragonal, and pseudocubic structures at room temperature. Crystal symmetry was changed from 4-fold symmetry to 3-fold symmetry by substituting Pb(Co1/3, Nb2/3)O3 ; PCN, to Pb(Zr0.52, Ti0.48)O3 ; PZT. As the substituted PCN concentration was increased, an increase in a-axis direction and a decrease in c-axis in the perovskite structure were occurred simultaneously, so that the crystal symmetry was changed into such way. In the higher sinteringtemperatures, the unit cell distortions occurred rather in the lower substitution range of PCN. The ferroelectric properties were maximized at the region that tetragonal and rhombohedral or pseudocubic structures were coexist.

  • PDF

Piezoelectric and Dielectric Properties of Low Temperature Sintering Pb(Zn1/2W1/2)O3-Pb(Mn1/3Nb2/3)O3-Pb(Zr,Ti)O3 Ceramics

  • Yoo, Ju-Hyun;Lee, Kab-Soo;Lee, Su-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • v.9 no.3
    • /
    • pp.91-95
    • /
    • 2008
  • In this study, in order to develop the composition ceramics for low loss multilayer piezoelectric actuator application, $Pb(Zn_{1/2}W_{1/2})O_3-Pb(Mn_{1/3}Nb_{2/3})O_3-Pb(Zr,Ti)O_3$ (abbreviated as PZW-PMN-PZT)ceramics according to the amount of $MnO_2$ addition were fabricated using two-stage calcinations method. And also, their dielectric and piezoelectric properties were investigated. At the 0.2 wt% $MnO_2$ added PZW-PMN-PZT ceramics sintered at $930^{\circ}C$, density, electromechanical coupling factor $k_p$, dielectric constant ${\varepsilon}_r$, piezoelectric $d_{33}$ constant and mechanical quality factor $Q_m$ showed the optimum value of $7.84g/cm^3$, 0.543, 1,392, 318.7 pC/N, 1,536, respectively for low loss multilayer ceramics actuator application.