소성 온도가 (Na,K,Li)(Nb,Sb,Ta)O3 세라믹스의 유전 및 압전 특성에 미치는 영향 (Effect of Sintering Temperature on the Dielectric and Piezoelectric Properties of (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics)

  • 김유석;류주현;홍재일;이지영
    • 한국전기전자재료학회논문지
    • /
    • 제26권11호
    • /
    • pp.806-809
    • /
    • 2013
  • In this study, $(Na_{0.525}K_{0.443}Li_{0.037})(Nb_{0.883}Sb_{0.08}Ta_{0.037})O_3+0.10\;wt%Bi_2O_3+0.35\;wt%B_2O_3$ ceramics were prepared by conventional soild-state sintering process. The specimens were sintered at temperature range from $1,060^{\circ}C$ to $1,100^{\circ}C$. XRD (X-ray diffractron), SEM (scanning electron microscope) were used to analyze the crystal structure and microstructural sproperties of specimens. And also, $T_{O-T}$, TC were observed by the mesurement of temperature dependence of dielectric constant. Excellect physical properties of the piezoelectric constant $d_{33}$= 170 pC/N, electromechanical coupling factor kp= 0.312, Tc= $315^{\circ}C$ were obtained, respectively, from the specimen sintered at $1,080^{\circ}C$.

A promising new piezoelectric material -Langasite and its related compounds-

  • Kawanaka, Hiroyuki;Takeda, Hiroaki;Shimamura, Kiyoshi;Onozato, Norio;Fukuda, Tsuguo
    • 한국결정성장학회:학술대회논문집
    • /
    • 한국결정성장학회 1997년도 Proceedings of the 12th KACG Technical Meeting and the 4th Korea-Japan EMGS (Electronic Materials Growth Symposium)
    • /
    • pp.145-145
    • /
    • 1997
  • Recent progress of electric technology requires new piezoelectric crystals having superior properties such as zero temperature coefficients and large electromechanical coupling factors. We have developed a series of new leading chandidates, La$_3$Ga5SiO14(langasite, LGS), La3Nb0.5Ga5.5O14(LNG), La3Ta0.5O14(LTG), to satisfy those requirements. High quality LGS, LNG and LTG single crystals, with dimensions of 2 inches in diameter, were successfully grown by the Czochralski method at a pulling rate of 1mm/h. Since no variation of chemical composition was observed when whole melt in a crucible was crystallized, congruency of these compositions was confirmed. Physical constants such as elastic constants, dielectric constants and piezoelectric constants were measured. Filters and oscillators made of grown LGS, LNG and LTG single crystals showed superior properties such as three times wider passband than that of quartz, low insertion loss and easy processing, Langasite family crystals were shown to be superior materials to other known materials such as quartz, LiTaO$_3$, $\alpha$-AlPO$_4$ and Li$_2$B$_4$O7.

  • PDF

$LiTaO_3$ crystal의 dynamic 초전특성과 그 주파수의 의존성 (Dynamic Pyroelectric Properties and Their Frequency Dependences of $LiTaO_3$ Crystal)

  • 이원재;강성준;정양희;윤영섭
    • 대한전자공학회논문지SD
    • /
    • 제37권8호
    • /
    • pp.35-41
    • /
    • 2000
  • $LiTaO_3$ 단결정 시료의 초전특성에 대한 주파수 의존성을 dynamic 방법을 이용하여 조사하였다. 2 ~ 1000Hz 주파수 범위에서 $LiTaO_3$ 단결정 시료의 전압응답을 부하 저항의 크기에 따라 초전전압영역 ($U_{PV},\;R_L=17.3G{\Omega}$) 과 초전전류영역 ($U_{PV},\;R_L=1M{\Omega}$) 으로 분류하여 측정하였다. 초전전류영역의 전압응답에 의존하는 초전계수는 40 Hz에서 최대값 $1.56{\times}10^{-8}C/cm^2{\cdot}K$를 나타내었고, 전압감도와 검출능을 위한 재료평가지수는 각각 최대값 $10.8{\times}10^{-11}C{\cdot}cm/J$$13{\times}10^{-7}C{\cdot}cm/J$을 나타내었다. 전압감도는 초전전압영역의 전압응답에 의존하여 2 Hz에서 488V/W 의 최대값을 나타내었다. 잡음등가전력과 비검출능은 40 Hz에서 각각 최소값 $3.95{\times}10^{-10}W/{\sqrt}Hz$와 최대값 $5.6{\times}10^8cm{\cdot}{\sqrt}Hz/W$이었다.

  • PDF

GROWTH AND CHARACTERIZATIONS OF $La_3Ga_5SiO_{14}$ SINGLE CRYSTALS AND SINTERED BODY FOR THE APPLICATIONS OF FILER AND RESONATOR

  • Jung, Il-Hyoung;Kyung Joo;Shim, Kwang-Bo;Auh, Keun-Ho
    • 한국결정성장학회:학술대회논문집
    • /
    • 한국결정성장학회 1998년도 PROCEEDINGS OF THE 15TH KACG TECHNICAL MEETING-PACIFIC RIM 3 SATELLITE SYMPOSIUM SESSION 4, HOTEL HYUNDAI, KYONGJU, SEPTEMBER 20-23, 1998
    • /
    • pp.73-77
    • /
    • 1998
  • Langasite(La3Ga5SiO14) is a new piezoelectric material which is similar to quartz, LN(LiNbO3) and LT(LiTaO3) in its acoustic behavior. In this study, pure Langasite and Langasite family groups were synthesized by the solid state reactions in air. For the synthesis process, diffusion species were investigated and sintered body of synthesized powders were studied on dielectric property according to surface microstructures.

  • PDF

압전응용을 위한 Langasite(La$_3$Ga$_5$SiO$_{14}$) 단결정의 성장 및 특성 (Growth and Characteristics of Langasite(La$_3$Ga$_5$SiO$_{14}$) Single Crystal for the Piezoelectric Applicatons)

  • 정일형;오근호
    • 한국세라믹학회지
    • /
    • 제36권6호
    • /
    • pp.640-645
    • /
    • 1999
  • Recently rapid progress of electronic and telecommunication technology requires the development of new piezoelectric materials and cellular communication is more and more used in various fields. Langasite(La3Ga5SiO14) is suitable for new piezoelectric properties. Langastie can be applied as communication devices due to intermediate piezoelectric properties which are similar to those of quartz and LiTaO3 in its acoustic characteristics. So in this study Langastie(La3Ga5SiO14) single crystal with 47 mm in diameter and 25mm in length were sucessfully grown by using self-designed Czochralski system. In addition optimum growth conditions for the piezoelectric applications throughout estimation of crystal quality and frequency characteristics were investigated.

  • PDF

Strain characteristics and electrical properties of [Li0.055(K0.5Na0.5)0.945](Nb1-xTax)O3 ceramics

  • Lee, Jong-Kyu;Cho, Jeng-Ho;Kim, Byung-Ik;Kim, Eung Soo
    • Journal of Ceramic Processing Research
    • /
    • 제13권spc2호
    • /
    • pp.341-345
    • /
    • 2012
  • [Li0.055(K0.5Na0.5)0.945](Nb1-xTax)O3 (0.05 ≤ x ≤ 0.25) ceramics were prepared by the partial sol-gel (PSG) method to improve the microstructure homogeneity of Ta5+ ion and were compared to those prepared by the conventional mixed oxide (CMO) method. For the PSG method, Ta(OC2H5)5 was directly reacted with calcined [Li0.055(K0.5Na0.5)0.945]NbO3 powders and the specimens sintered at 1100 ℃ for 5 hrs showed a single phase with a perovskite structure. Compared to the specimens prepared by conventional mixed oxide powders, the relative ratio of tetragonal phase to orthorhombic phase of the sintered specimens prepared by Ta(OC2H5)5 was larger than that of the sintered specimens prepared by Ta2O5. The electromechanical coupling factor (kp), piezoelectric constant (d33) and dielectric constant (εr) of the sintered specimens were increased with Ta5+ content. These results could be attributed to the decrease of the orthorhombic-tetragonal polymorphic phase transition temperature (To-t), which could be evaluated by oxygen octahedral distortion. Strain of the sintered specimens prepared by the PSG method was higher than that of specimens prepared by the CMO method due to the increase of relative density. The effects of crystal structure on the strain characteristics of the specimens were also discussed.

MnO2 첨가량에 따른 비납계 (Na,K,Li)(Nb,Sb,Ta)O3 세라믹스의 전기적특성 (Electrical Properties of lead free (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics with MnO2 Addition)

  • 이승환;남성필;이동현;이성갑;이상철;이영희
    • 전기학회논문지
    • /
    • 제60권4호
    • /
    • pp.801-804
    • /
    • 2011
  • Electrical properties and microstructure were investigated on the effects of $MnO_2$ and the lead-free $(Na_{0.44}K_{0.52}Li_{0.04})(Nb_{0.83}Sb_{0.07}Ta_{0.1})O_3$ ceramics with the addition of $MnO_2$ were fabricated by a conventional mixed oxide method. A gradual change in the crystal and microstructure was observed with the increase of $MnO_2$ addition. For the NKN-LST-xmol%$MnO_2$ sintered at $1100^{\circ}C$, bulk density increased with the addition of $MnO_2$ and showed maximum value at addition 1.0mol% of $MnO_2$. Curie temperature of the NKN-LST ceramics slightly decreased with adding $MnO_2$. The dielectric constant, piezoelectric constant ($d_{33}$) and electromechanical coupling factor ($k_p$) increased below 0.25mol% of $MnO_2$ addition, which might be due to the increase in density. The high piezoelectric properties = 145 pC/N, electromechanical coupling factor = 0.421 and dielectric constant = 2883 were obtained for the NKN-LST-0.25mol%$MnO_2$ sintered at $1100^{\circ}C$ for 4h.

인가주파수에 따른 결합형 광변조기 특성변화 (Characterization of coupling optical modulator to the applied frequency)

  • 강기성
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제9권6호
    • /
    • pp.584-592
    • /
    • 1996
  • Coupling optical modulator which on the $LiTaO_3$ substrate is fabricated by using proton exchange method and self-aligned method. Proton exchange of proton diffusion method was applied to pattern a waveguide on $LiTaO_3$ substrate. The annealing at >$400^{\circ}C$ was carded out to control waveguide width and depth. The depths of the two annealed optical waveguides, which were measured by using .alpha.-step, were 1.435 K.angs. and 1.380 K.angs. Using .alpha.-step facility, we examined that the width of waveguides is increased from 5.mu.m to 6.45 .mu.m and 6.3.mu.m due to the annealing effects. The process of proton exchange was done at 150.deg. C for 120 min, >$200^{\circ}C$ for 60 min and annealing process was done at >$400^{\circ}C$ for 90 min, >$400^{\circ}C$ for 60 min. The high speed coupling optical modulator has very good figures of merits; the measured high frequency power were achieved.

  • PDF

$MnO_2$ 첨가량에 따른 비납계 (Na,K,Li)(Nb,Sb,Ta)$O_3$ 세라믹스의 전기적특성 (Electrical properties of lead free (Na,K,Li)(Nb,Sb,Ta)$O_3$ ceramics with $MnO_2$ addition)

  • 이승환;남성필;이성갑;신동진;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2011년도 제42회 하계학술대회
    • /
    • pp.1487-1488
    • /
    • 2011
  • Electrical properties and microstructure were investigated on the effects of $MnO_2$ and the lead-free $(Na_{0.44}K_{0.52}Li_{0.04})(Nb_{0.83}Sb_{0.07}Ta_{0.1})O_3$ ceramics with the addition of $MnO_2$ were fabricated by a conventional mixed oxide method. A gradual change in the crystal and microstructure was observed with the increase of $MnO_2$ addition. For the NKN-LST-xmol%$MnO_2$ sintered at $1100^{\circ}C$, bulk density increased with the addition of $MnO_2$ and showed maximum value at addition 1.0mol% of $MnO_2$. Curie temperature of the NKN-LST ceramics slightly decreased with adding $MnO_2$. The dielectric constant, piezoelectric constant ($d_{33}$) and electromechanical coupling factor ($k_p$) increased below 0.25mol% of $MnO_2$ addition, which might be due to the increase in density. The high piezoelectric properties = 145 pC/N, electromechanical coupling factor = 0.421 and dielectric constant = 2883 were obtained for the NKN-LST-0.25mol%$MnO_2$ sintered at $1100^{\circ}C$ for 4h.

  • PDF