• 제목/요약/키워드: $LiCoO_{2}$

검색결과 700건 처리시간 0.026초

공침법을 통하여 합성된 코어-쉘 구조를 가지는 하이 니켈 양극 소재 안정화 (Stabilization of High Nickel Cathode Materials with Core-Shell Structure via Co-precipitation Method)

  • 김민정;홍순현;전형권;구자훈;이희상;최규석;김천중
    • 한국재료학회지
    • /
    • 제32권4호
    • /
    • pp.216-222
    • /
    • 2022
  • The capacity of high nickel Li(NixCoyMn1-x-y)O2 (NCM, x ≥ 0.8) cathodes is known to rapidly decline, a serious problem that needs to be solved in a timely manner. It was reported that cathode materials with the {010} plane exposed toward the outside, i.e., a radial structure, can provide facile Li+ diffusion paths and stress buffer during repeated cycles. In addition, cathodes with a core-shell composition gradient are of great interest. For example, a stable surface structure can be achieved using relatively low nickel content on the surface. In this study, precursors of the high-nickel NCM were synthesized by coprecipitation in ambient atmosphere. Then, a transition metal solution for coprecipitation was replaced with a low nickel content and the coprecipitation reaction proceeded for the desired time. The electrochemical analysis of the core-shell cathode showed a capacity retention of 94 % after 100 cycles, compared to the initial discharge capacity of 184.74 mA h/g. The rate capability test also confirmed that the core-shell cathode had enhanced kinetics during charging and discharging at 1 A/g.

ESS용 NCM계 LIB의 설계인자별 성능분석 및 열화특성 연구 (Performance Analysis and Degradation Characteristics of NCM LIB for ESS)

  • 권순종;박은영;임지훈;최진혁;김종훈
    • 전력전자학회:학술대회논문집
    • /
    • 전력전자학회 2018년도 전력전자학술대회
    • /
    • pp.219-221
    • /
    • 2018
  • ESS용 NCM계 $LIB(Li[Ni_xCo_yMn_z]O_2)$의 양극 전이금속 설계인자 조성비(x:y:z)를 5:2:3, 6:2:2로 달리하여 제작한 전지를 사용하여 C-rate별 방전시험을 통한 기본성능평가를 진행하였고, 가속열화 시험을 통한 수명특성을 분석하였다. EIS(Electrochemical Impedance Spectroscopy) 실험을 통하여 전지의 임피던스를 확인하였고, 열화되지 않은(Fresh) 전지와 열화된(Aging) 전지의 SOC(State-of-Charge)별 임피던스 특성을 비교 분석하였다.

  • PDF

5-Amino-2H-1,2,4-thiadiazoline-3-one의 토토머화 현상과 알킬화 반응 (Tautomerism and Alkylation of 5-Amino-2H-1,2,4-thiadiazoline-3-one)

  • 조남숙;박영철;라도영;강성권
    • 대한화학회지
    • /
    • 제39권7호
    • /
    • pp.564-571
    • /
    • 1995
  • NaOH 수용액에서 과산화수소로 2-thiobiuret를 산화성 고리화 반응시켜 5-amion-2H-1, 2, 4-thiadiazoline-3-one을 합성하였다. 이 화합물에 대한 토오토머화 현상을 IR, $^1H$ NMR, $^13C$ NMR 등의 분광학적인 방법으로 고찰하고 분자괘도함수에 의한 이론적 계산 결과와 비교 검토하였다. 이 결과 5-Amion-2H-1, 2, 4-thiadiazoline-3-one는 락팀형보다는 락탐형으로 존재한다. 알킬화 반응을 여러 염기로 DMF 용매와 이상용매계 $H_2O$-THF에서 시도한 결과 N-2 위치에서 알킬화 반응이 일어남을 알 수 있었다. 알킬화 반응은 할로켄화 알칸을 $Li_2CO_3$/DMF의 조건하에서 반응시켰을 때 가장 수율이 좋았다. N-2 위치에서 알킬화 반응 생성물의 확인은 IR, $^1H$ NMR과 $^13C$ NMR 등의 분광학적인 방법과 5-methyl-2-thiobiuret를 thiobiuret와 같이 산화성 고리화 반응을 통하여 5-amino-2-methyl-1,2,4-thiadiazolidine-3-one 표준 시료를 합성하여 알킬화 반응 생성물과 비교 확인하였다.

  • PDF

Piezoelectric and Dielectric Properties of Low Temperature Sintered Pb(Mn1/3Nb2/3)0.02(Ni1/3Nb2/30.12(ZrxTi1-x)0.86O3 System Ceramics

  • Yoo, Ju-Hyun;Lee, Sang-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • 제10권4호
    • /
    • pp.121-124
    • /
    • 2009
  • In this study, in order to develop compositions of ceramics suitable for piezoelectric actuator and ultrasonic vibrator applications using low temperature sintering, multilayer, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3$ and $Na_2CO_3$ as sintering aids. Their structural, piezoelectric and dielectric characteristics were investigated according to the Zr/Ti ratio. As the Zr/Ti ratio increased, the electromechanical coupling factor $k_p$, and piezoelectric constant $d_{33}$ and the mechanical quality factor $Q_m$ all increased with Zr/Ti ratio and then decreased after the ratio exceeded 50/50. At the ratio of Zr/Ti =49/51 and sintering temperature of $900^{\circ}C$; the density, electromechanical coupling factor $k_p$, dielectric constant ${\varepsilon}_r$ piezoelectric $d_{33}$ constant and mechanical quality factor $Q_m$ all showed the optimum values of 7.900 $g/cm^3$, 0.576, 856, 312 pC/N, 1,326, respectively. These property values are very suitable for multilayer ceramics actuator applications.

냉매 열교환기 구성방법에 따른 제 2종 흡수식 히트펌프의 성능 특성 변화에 관한 연구 (Performance Characteristics of Type II LiBr-H2O Absorption Heat Pump in Accordance with the Refrigerant Heat Exchanger Configuration)

  • 이창현;윤준성;김인관;권오경;차동안;배경진;김민수;박찬우
    • 설비공학논문집
    • /
    • 제29권7호
    • /
    • pp.373-384
    • /
    • 2017
  • The objective of this study was to determine the effect of refrigerant heat exchanger on the performance of type II absorption heat pump performance using numerical analysis. Two heat exchange installation methods were used: solution to refrigerant and waste hot water to refrigerant. These methods were compared to the standard model of hot water flow without using refrigerant heat exchanger. When waste hot waters were bypassed to refrigerant heat exchanger, COP was not affected. However, steam mass generation rates were increased compared to those of the standard model. When solutions were bypassed to the refrigerant heat exchanger, results were different depending on the place where the solution rejoined. COP and steam mass generation rates were lower compared to those when waste heat water was passed to refrigerant heat exchanger. Thus, it is possible to obtain higher steam mass generation rates by using waste water and installing refrigerant heat exchanger.

하소온도가 저온소결 PMN-PZN-PZT 세라믹스의 압전특성에 미치는 영향 (Effect of Calcination Temperature on the Piezoelectric Characteristics of Low Temperature Sintering PMN-PZN-PZT ceramics)

  • 이일하;이상호;류주현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.214-216
    • /
    • 2006
  • In this study, in order to develop the composition ceramics for low loss and low temperature sintering multilayer piezoelectric actuator, PMN-PZN-PZT ceramics were fabricated using two stage calcination method and $Li_2CO_3$, $Bi_2O_3$ and CuO as sintering aids and their piezoelectric characteristics were investigated according to the 2nd calcination and sintering temperature. At the calcination temperature of $750^{\circ}C$ and sintering temperature of $930^{\circ}C$, density, electromechanical coupling factor ($k_p$), mechanical quality factor ($Q_m$), Dielectric constant (${\varepsilon}_r$) and piezoelectric constant ($d_{33}$) of specimen showed the optimum value of $7.94g/cm^2$ 0.581, 1554, 1555 and 356pC/N, respectively for multilayer piezoelectric actuator application.

  • PDF

저온소결 PMN-PZT 압전세라믹의 소성시간에 따른 미세구조 및 압전특성 (Microstructural and Piezoelectric Properties of Low Temperature Sintering PMN-PZT Ceramics with the Variations of Sintering Times)

  • 류주현;이창배;이상호;백동수;정영호;임인호
    • 한국전기전자재료학회논문지
    • /
    • 제18권3호
    • /
    • pp.237-242
    • /
    • 2005
  • In this paper, in order to develop the low temperature sintering ceramics for multilayer piezoelectric transformer, PMN-PZT ceramics were manufactured with the variations of sintering times, and their microstructural, piezoelectric and dielectric properties were investigated. Li$_2$CO$_3$ and Bi$_2$O$_3$ were used as sintering aids and the specimens were sintered during 30, 60, 90, 120, 150, and 180 minutes, respectively. At the specimen sintered during 90 minute, mechanical quality factor(Qm), electro-mechanical coupling factor(kp) and dielectric constant were showed the optimum values of 2,356, 0.504 and 1,266, respectively.

Effect of Tris(trimethylsilyl) Phosphate Additive on the Electrochemical Performance of Nickel-rich Cathode Materials at High Temperature

  • Jang, Seol Heui;Mun, Junyoung;Kang, Dong-Ku;Yim, Taeeun
    • Journal of Electrochemical Science and Technology
    • /
    • 제8권2호
    • /
    • pp.162-168
    • /
    • 2017
  • $LiNi_xCo_yMn_zO_2$ cathode materials have been the focus of much attention because of their high specific capacity. However, because of the poor interfacial stability between cathodes and electrolytes, the cycling performance of these materials fades rapidly, especially at high temperatures. In the present paper, we propose the use of tris(trimethylsilyl) phosphate (TMSPO), which contains phosphate and silyl functional groups, as a functional additive in electrolytes. The addition of TMSPO resulted in the formation of cathode electrolyte interphase (CEI) layers on the surfaces of the cathodes and effectively suppressed electrolyte decomposition reactions, even at high temperatures. As a result, cells cycled with TMSPO exhibited remarkable capacity, which remained after 50 cycles (82.0%), compared to cells cycled without TMSPO (64.6%).

저온소결 8/65/35 PLZT 세라믹의 전기열량 효과 (Electrocaloric Effect of 8/65/35 PLZT Ceramics Sintered at Low Temperature)

  • 최승훈;라철민;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제28권10호
    • /
    • pp.615-619
    • /
    • 2015
  • In this study, in order to develop the composition ceramics with the excellent electrocaloric properties, 8/65/35 PLZT ceramics were fabricated by the conventional solid-state method with the addition of $Bi_2O_3$, CuO, $Li_2CO_3$ and the variation of sintering temperature from $930^{\circ}C$ to $990^{\circ}C$. The XRD pattern of all specimens indicated general perovskite structure and the rhombohedral phase were observed. Curie temperature ($T_c$) of all specimens was observed in the vicinity of about $190^{\circ}C$. Density, coercive field and remnant polarization of the specimen sintered at $950^{\circ}C$ was $7.55g/cm^3$, 8.895 kV/cm, $11.22{\mu}C/cm^2$, respectively. EC effect of PLZT ceramics was measured by indirect method and the temperature change ${\Delta}T$ due to the electrocaloric effect was calculated by Maxwell's relations. ${\Delta}T$ of ceramic sintered at $950^{\circ}C$ was $0.21^{\circ}C$ under application of 40 kV/cm at $190^{\circ}C$.

소결첨가제에 따른 적층 PTCR 세라믹스의 미세구조와 전기적 특성 (Microstructures and Electrical properties of Multilayer PTCR ceramics as a function of Sintering Additives)

  • 명성재;박명성;전명표;조정호;남중희;김병익
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.180-181
    • /
    • 2008
  • 화학양론적 $BaTiO_3$의 소결은 고온의 에너지를 필요로 하며, 내부전극과 세라믹충의 동시소성과정에서 Ni이 세라믹층으로의 확산이 발생되어 PTC의 물성저하를 초래한다. 본 연구에서는 저온에서 액상을 형성하여 소결온도를 낮추는 것으로 알려진 산화물 및 비산화물계 소결첨가제가 적층 PTC 세라믹스의 미세구조 및 전기적 특성에 미치는 영향에 대하여 고찰하였다. 소결과정에서 분해되어 기체를 형성하는 BN, $Li_2CO_3$, LiF의 경우 기공율을 증가시켜 산소의 이동경로를 형성하였으며, 이는 입계의 재산화를 용이하게 하여 PTC 효과를 보였다.

  • PDF