Microwave dielectric properties of $La_2O_3-ZnO-B_2O_3$ glass-added alumina ($La_2O_3-ZnO-B_2O_3$계 유리 첨가 알루미나 복합체의 유전특성)

  • Hong, Seung-Hyuk;Jung, Eun-Hee;Shin, Hyun-Ho;Oh, Chang-Yong;Lim, Wook
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.06a
    • /
    • pp.324-324
    • /
    • 2007
  • Influence of $La_2O_3$ addition to $ZnO-B_2O_3$-based glass on the water leaching resistance of the glass was first investigated. The optimized $La_2O_3-ZnO-B_2O_3$ (LZB) glass was ball milled for varying time, followed by mixing with $Al_2O_3$ crystalline phase to form $Al_2O_3$-LZB glass composites at $875^{\circ}C$ for lh. Microwave dielectric properties of the composites were investigated as a function of the ball milling time of the LZB glass. Dielectric constant and quality factor of the composites were 6.01 and 11676 GHz, respectively, when the LZB glass was ball milled for 2h prior to mixing with $Al_2O_3$.

  • PDF

Minimizing the Water Leaching of Zincborate Glass by La2O3 Addition for LTCC Applications

  • Hong, Seung-Hyuk;Jung, Eun-Hee;Oh, Chang-Yong;Kim, Shin;Shin, Hyun-Ho
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.3
    • /
    • pp.157-160
    • /
    • 2008
  • A series of $La_2O_3$-added zincborosilicate glasses was fabricated by systematically varying $La_2O_3$ addition up to 15mol% under the constraint of a ZnO:$B_2O_3$ ratio of 1:2. The degree of water leaching after ball milling of the prepared glasses in water medium was relatively quantified by the change in zinc peak intensity in energy dispersive spectroscopy. 8mol% of $La_2O_3$ was the most efficient addition in inhibiting the glass leaching by water. The role of $La_2O_3$ in inhibiting the leaching was explained in terms of change of structural units in the glass network. When the optimum 8mol% $La_2O_3$-added ZnO-$B_2O_3$ glass was used as sintering aid for $Al_2O_3$, the fabricated alumina-glass composite at $875^{\circ}C$ demonstrated dielectric constant of 6.11 and quality factor of 15470 GHz, indicating the potential of leaching-minimized $La_2O_3-ZnO-B_2O_3$ glass for application to low temperature co-firing ceramic technology.

The Properties of Optical Glass of B2O3-SiO2-La2O3 System with Li2O (Li2O가 포함된 B2O3-SiO2-La2O3계 광학 유리 특성)

  • Ji-Sun Lee;Sae-Hoon Kim;Jinho Kim
    • Korean Journal of Materials Research
    • /
    • v.32 no.12
    • /
    • pp.560-564
    • /
    • 2022
  • In this study, lanthanum boron silicate glasses were prepared with a composition of x Li2O-(60-x)B2O3-5CaO-5BaO-7ZnO-10SiO2-10La2O3-3Y2O3 where x = 1,3,5,7, and 9 mol%. Each composition was melted in a platinum crucible under atmospheric conditions at 1,400 ℃ for 2 h. Clear glasses with a transmittance exceeding 85 % were fabricated. Their optical, thermal, and physical properties, such as refractive index, Abbe number, density, glass transition (Tg) and Knoop hardness were studied. The results demonstrated that refractive index was between 1.6859 and 1.6953 at 589.3 nm. The Abbe number was calculated using an equation for 589.3 nm (nd), 656.3 nm (nf) and 486.1 nm (nc) and was observed to be in the range from 57.5 to 62.6. As the Li2O content increased, the glass transition temperature of the optical glass decreased from 608 ℃ to 564 ℃. If glass mold pressing is performed using a material with a low transition temperature and high mechanical strength, then the optical glasses developed in this study can be completely commercialized.

A study on the development of SRM for XRF analysis of PZT[$Pb(ZrTi)O_3$] (PZT[$Pb(ZrTi)O_3$]의 XRF 분석용 SRM 개발에 관한 연구)

  • Kim, Young Man;Jeong, Chan Yee;Lim, Chang Ho;Choi, Beom Suk
    • Analytical Science and Technology
    • /
    • v.10 no.6
    • /
    • pp.439-444
    • /
    • 1997
  • Twelve kinds (1set) standard materials of chemical ingredients of lead zirconate titanate[$Pb(ZrTi)O_3$] have been developed in order to determine fast and accurate measurement of X-ray fluorescence spectrometry. Especially, we used diluted(ahout sixteen times) filling compound($Li_2B_4O_7/LiBO_2=4/1$) to consider removal effect of matrix, storage convenience, and homogenous characteristics. As a result from the four different laboratories, we obtained extremly good agreement about the standard curve on twelve standard materials which containing eleven elements, PbO, $ZrO_2$, $TiO_2$, SrO, $WO_3$, $La_2O_3$, $Cr_2O_3$, MgO, $Nb_2O_5$, and $MnO_2$. The correlation factor of standard curve was over 0.998. However, ZnO has relatively low correlation factor, 0.977, because the concentration was 10ppm lower than other original materials. This analysis reveals that ZnO has shown the poor linearity as well as low fluorescence intensity. In present work, XRF standard materials are useful for determining a rapid and accurate results for major and minor elements concentration among PZT.

  • PDF

A study on development of CRM by means of XRF analysis for fine ceramic ($BaTiO_3$) (티탄산바륨 소재의 XRF 분석용 CRM 개발에 관한 연구)

  • Kim, Young Man;Jeong, Chan Yee;Lim, Chang Ho;Song, Taek Yong;Lee, Dong Soo
    • Analytical Science and Technology
    • /
    • v.9 no.4
    • /
    • pp.382-391
    • /
    • 1996
  • In this study, 12 different chemical species of fine ceramic($BaTiO_3$) were synthesized as the standard materials for the fast and accurate measurements of X-ray fluorescence spectrometry. Samples were diluted to sixteen times with the filling compound ($Li_2B_4O_7+LiBO_2$) in order to remove the matrix effect, and to get the convenient storage and homogeneity of ingredients. The matrix effects among the ingredients were corrected by the empirical coefficient method based on the Lucas-Tooth and Price model. The standard curve on 12 standard materials containing 15 elements were obtained by using X-ray fluorescence spectrometry at three different laboratories. The correlation factors of BaO, PbO, SrO, $Fe_2O_3$, $La_2O_3$, $SnO_2$, ZnO, $ZrO_2$, CaO indicated the relati vely good agreement over 0.995 among the three different laboratories. $SiO_2$ and $Al_2O_3$ showed the poor linearity because of their low fluorescence intensities.