Dielectric Properties in the Pb1-3x/2Lax[(Mg1/3Ta2/3)0.66Zr0.34]O3 Systems

  • Kim, Yeon Jung
    • Applied Science and Convergence Technology
    • /
    • v.26 no.4
    • /
    • pp.70-73
    • /
    • 2017
  • The dielectric constant and loss of poling/non-poling was measured in the $Pb_{1-3x/2}La_x[(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ samples. The addition of $La^{3+}$ to the $Pb_{1-3x/2}La_x[(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ did not cause a large change in grain size. But the addition of $La^{3+}$ did show transition temperature, which shifted toward low temperature in the $Pb[(Mg_{1/3}Ta_{2/3})Zr]O_3$ systems. In addition, the dielectric and pyroelectric properties (${\varepsilon}{\sim}20000$, $p{\sim}0.03C/m^2K$) of this system using $La^{3+}$ have been greatly improved. Pyroelectrics $Pb_{0.97}La_{0.02}(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ system was found to have a relatively high ferroelectric FOMs ($F_V{\sim}0.035m^2/C$, $F_D{\sim}0.52{\times}10^{-4}Pa^{-1/2}$) at room temperature. Spontaneous polarization showed a value of $0.27{\sim}0.35C/m^2$ in the composition added to $La^{3+}$. The piezoelectric constant ($d_{33}=350{\sim}490pC/N$) and electromechanical coupling factor ($k_P=0.25{\sim}0.35$) are obtained in $Pb_{1-3x/2}La_x[(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ compositions with $La^{3+}$ dopant.

Synthesis and Conductivity Properties of $LaNiO_3$ Ceramic Conductors ($LaNiO_3$전도성 세라믹의 합성과 도전특성)

  • Cho, Jung-Ho;Cho, Joo-Hun;Kim, Kang-Eun;Chung, Su-Tae
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.406-409
    • /
    • 2001
  • The conductivity properties and synthesis of $LaNiO_{3}$ ceramics from $La_{1+\delta}NiO_{3}(\delta=-0.06,0,0.06)$ were investigated. A single perovskite phase was realized at $800^{\circ}C$. $La_{2}NiO_{4}$ and other unexpected oxide were observed at $1000^{\circ}C$. The Microstructure was showed clearly that it is a low density porous material. $LaNiO_3$ ceramic showed a metallic conductivity. The conductivity of La rich samples had a higher value than the La poor samples.

  • PDF

Synthesis and Conductivity Properties of LaNiO$_3$ Ceramic Conductors (LaNiO$_3$전도성 세라믹의 합성과 도전특성)

  • 조정호;조주현;김강언;정수태
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.406-409
    • /
    • 2001
  • The conductivity properties and synthesis of LaNiO$_3$ ceramics from La$\sub$1+$\delta$/NiO$_3$($\delta$=--0.06, 0, 0.06) were investigated. A single perovskite phase was realized at 800$^{\circ}C$. La$_2$NiO$_4$ and other unexpected oxide were observed at 1000$^{\circ}C$. The Microstructure was showed clearly that it is a low density porous material. LaNiO$_3$ ceramic showed a metallic conductivity. The conductivity of La rich samples had a higher value than the La poor samples.

  • PDF

Development of Pd/TiO2 Catalysts with La2O3 Addition and Study on the Performance Improvement of H2 Oxidation at Room Temperature (La2O3가 첨가된 Pd/TiO2 촉매의 개발 및 H2 상온산화 반응에서의 성능 향상 연구)

  • Lee, Dong Yoon;Kim, Sung Chul;Lee, Sang Moon;Kim, Sung Su
    • Applied Chemistry for Engineering
    • /
    • v.31 no.6
    • /
    • pp.674-678
    • /
    • 2020
  • In this study, a Pd/TiO2 catalyst which oxidized H2 at room temperature without an additional energy source was prepared. And a specific surface area of TiO2 as a support was not proportional to H2 oxidation reaction performance of Pd/TiO2 catalyst. In addition La2O3 was added to Pd/TiO2 catalyst in order to evaluate the performance effect due to the change of catalysts physical properties. A Pd/La2O3-TiO2 was prepared by adding different amounts of La2O3 to TiO2 and CO chemisorption analysis was performed. Compared to the conversion rate (14% at 0.5% H2) of the Pd/TiO2(G) catalyst, the Pd/La2O3-TiO2 catalyst showed 74% which was improved by more than five times. It was found that the larger the metal dispersion of Pd as an active metal is, the more favorable to H2 oxidation reaction is. However, when the added La2O3 amount exceeded 10%, the catalyst performance decreased again. Finally, it was concluded that the physical properties of the Pd/La2O3-TiO2 catalyst have a dominant influence on the catalytic activity until 0.3~0.5% of injected H2 concentrations and the catalyst reaction rate was controlled by substance transfer from 1% or more concentrations of H2.

GROWTH AND ELECTRICAL PROPERTIES OF (La,Sr)CoO$_3$/Pb(Zr,Ti)O$_3$/(La,Sr)CoO$_3$ HETEROSTRUCTURES FOR FIELD EFFECT TRANSISTOR

  • Lee, J.;Kim, S.W.
    • Journal of the Korean institute of surface engineering
    • /
    • v.29 no.6
    • /
    • pp.839-846
    • /
    • 1996
  • Epitaxial (La, Sr)$CoO_3/Pb(Zr,\;Ti)O_3/(La,\;Sr)CoO_3$by pulsed laser deposition for ferroelectric field effect transistor. Epitaxial $LaCoO_3/Pb(Zr,\;Ti)O_3/(La,\;Sr)CoO_3$ heterostructures exhibited 70$\mu C/cm^2$ and 17 $\mu C/cm^2$at a positively and negatively poled states, respectively. On the other hand, epitaxial (La, Sr)$CoO_3/Pb(Zr,\;Ti)O_3/LaCoO_3$heterostructures show the remnant polarization states opposite to the $LaCoO_3/Pb(Zr,\;Ti)O_3/(La,\;Sr)CoO_3$ heterostructures. This indicates that the interface between (La, Sr)$CoO_3$ (LSCO) and $Pb(Zr, Ti)O_3(PZT)$ layers affects the asymmetric polarization remanence through electrochemical nature. The resistivity of $LaCoO_3$ (LCO) layer was found to be dependent on an ambient oxygen, primarily the ambient oxygen pressure during deposition. The resistivity of the LCO layer varied in the range of 0.1-100 $\Omega$cm. It is suggested that, with an appropriate resistivity of the LCO layer, the LCO/PZT/LSCO heterostructure can be used as the ferroelectric field effect transistor.

  • PDF

Preparation and Characterization of LaAlO3 Ceramics from High Energy Ball Milling Powders (고에너지 볼 밀에 의한 LaAlO3 세라믹스의 제조와 특성)

  • 최상수;서병준;여기호;정수태
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.17 no.1
    • /
    • pp.39-45
    • /
    • 2004
  • Fine LaAlO$_3$ powders wore successfully synthesized from La$_2$O$_3$ and ${\gamma}$ $Al_2$O$_3$ powders milling for 10∼50 hours via the high energy milling technique (mechanochemical method) in room temperature and air. The particle size of LaAlO$_3$ powder were estimated from XRD patterns and SEM images to be 160∼180 nm. The LaAlO$_3$ ceramics arc derived for the synthesized powders (milling for 10, 30 and 50 hours) by sintering at 140$0^{\circ}C$ and 150$0^{\circ}C$. The micrographs of grains showed an agglomeration and the degree of agglomeration increased with the milling time. The LaAlO$_3$ made from synthesized powders milling for 50 hours can be sintered to 99.5% of theoretical density at 150$0^{\circ}C$ for 1 hour. These ceramics exhibits a dielectric constant of 20, a dielectric loss of 0.0003 and a temperature coefficient of capacitance of 15 ppm/$^{\circ}C$ at 1 MHz.

Hydrothermal synthesis of PLT[$(Pb,La)TiO_3$] powders (수열법에 의한 PLT[$(Pb,La)TiO_3$ 분말의 합성)

  • 김판채;최종건
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.8 no.1
    • /
    • pp.42-48
    • /
    • 1998
  • Synthesis of PLT($Pb_{1-X}La_{2X/3}TiO_3$, x=0.1~0.3) powders was carried out by hydrothermal method. Optimal conditions for synthesis were $250^{\circ}C$ of reaction temperature, 8M-KOH solution of hydrothermal solvent and 12 hrs reaction time, and the monolithic $Pb_{1-X}La_{2X/3}TiO_3$ particles were obtained with the composition of x$\leq$0.2. The tetragonality(c/a) and the phase transition temperature were decreased by the increment of the $La_2O_3$ contents in PLT solid solutions, and the Curie temperature of the $Pb_{1-X}La_{2X/3}TiO_3$(x=0.2) was $400^{\circ}C$. The shape of the synthesized particles were nearly spherical and the size was in the 20~200 nm range.

  • PDF

Variations in the Properties of LSGM System Electrolyte with Sr and Mg Addition and Sintering Conditions (Sr과 Mg 첨가량 및 소결조건에 따른 LSGM계 전해질의 특성 변화)

  • Lee, Mi-Jai;Park, Sang-Sun;Choi, Byung-Hyun
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.4
    • /
    • pp.352-358
    • /
    • 2002
  • The variations of the properties of Sr and Mg added $LaGaO_3$ system electrolyte with the amount of the additive and the sintering condition were studied. Main phase was (La$_{1-x}Sr_x)(Ga_{1-y}Mg_y)O_{3-\delta}$ phase for each compositions and the single phases $(La_{0.85}Sr_{0.15})(Ga_{0.85}Mg_{0.15})O_{3-\delta},(La_{0.85}Sr_{0.15})(Ga_{0.8}Mg_{0.2})O_{3-\delta}$ and $(La_{0.8}Sr_{0.2})(Ga_{0.8}Mg_{0.2})O{3-\delta}$ were obtained with the decrease in the sintering temperature and Mg addition. Thermal expansion coefficient of the $(La_{0.8}Sr_{0.2})(Ga_{0.8}Mg_{0.2})O_{3-\delta}$ decreased with the increase in the sintering temperature. Electric conductivity of electrolyte sintered at $1500^{circ}C$ for 1h was 0.14 S/cm at $800^{circ}C$ with 1 mA.

Structural Changes and Dielectric Properties of$Pb(Mg_{1}{3}Nb_{2}{3})O_3$Ceramics Substituted by$Na^+/La^{3+}$Ions ($Na^+/La^{3+}$이온으로 치환된$Pb(Mg_{1}{3}Nb_{2}{3})O_3$의 구조 변화 및 유전 성질)

  • Hong, Young-Sik;Park, Hyu-Bum;Ahn, Tae-Ho;Kim, Si-Joong
    • Journal of the Korean Chemical Society
    • /
    • v.40 no.9
    • /
    • pp.607-614
    • /
    • 1996
  • The structural changes and dielectric properties of Pb1-x(Na1/2La1/2)x(Mg1/3Nb2/3)O3 compounds substituted by 0∼50 mol.% of Na+/La3+ mixed ions were investigated by X-ray diffraction method, IR and Raman spectroscopy, and LCR meter. The amount of perovskite phase increased with the increases of Na+/La3+ substituents and sintering temperatures. Although the superlattice lines due to 1:1 ordering were not detected by X-ray diffraction method, it was found, from the Raman spectroscopy and the increase of diffuseness coefficient, that the ordering behavior was related to the decrease of A site ion size. Dielectric properties in Pb1-x(Na1/2La1/2)x(Mg1/3Nb2/3)O3 were affected by the amount of perovskite phase, grain size, and density. The phase transitions were broadened and phase transition temperatures were lowered by the increase of Na+/La3+ ions.

  • PDF

Electrical and Dielectric Properties, and Accelerated Aging Characteristics of Lanthania Doped Zinc Oxide Varistors

  • Nahm, Choon-Woo
    • Transactions on Electrical and Electronic Materials
    • /
    • v.7 no.4
    • /
    • pp.189-195
    • /
    • 2006
  • The microstructure, electrical and dielectric properties, and stability against DC accelerated aging stress of the varistors, which are composed of quaternary system $ZnO-Pr_6O_{11}CoO-Cr_2O_3-based$ ceramics, were investigated for different $La_2O_3$ contents. The increase of $La_2O_3$ content led to more densified ceramics, whereas abruptly decreased the nonlinear properties by incorporating beyond 1.0mol%. The highest nonlinearity was obtained from 0.5mol% $La_2O_3$, with the nonlinear coefficient of 81.6 and the leakage current of $0.1{\mu}A$. The varistors doped with 0.5mol% $La_2O_3$ exhibited high stability, in which the variation rates of breakdown voltage, nonlinear coefficient, leakage current, dielectric constant, and dissipation factor were -1.1%, -3.7%, +100%, +1.4%, and +8.2%, respectively, for stressing state of $0.95V_{1mA}/150^{\circ}C/24h$.