• Title/Summary/Keyword: $Bi_2Sr_2CaCu_2O_y$

Search Result 231, Processing Time 0.024 seconds

Phase Equilibria for the Formation of Superconducting Phases in the Bi-Sr-Ca-O System (Bi-Sr-Ca-O계에서 초전도상의 형성에 관한 상평형)

  • Kim, Cheol-Jin
    • Korean Journal of Materials Research
    • /
    • v.3 no.4
    • /
    • pp.410-421
    • /
    • 1993
  • Phase equilibria and reaction paths of the superconducting phases and other compatible phases at $850^{\circ}C$ in the Bi-Sr-Ca-Cu-O system were studied. $Bi_2O_3$ was added to $Sr_2CaCu_2O_x$ by 5% up to 40 mole% Bi in the pseudo-binary $Bi_2O_3-(Sr_2CaCu_2O_x)$ system and the heat treated samples were analysed using XRD. SEM, EDS. and DT A. When Bi contents were greater than 35 mole% Bi, liquid phase was formed which was compatible with $Bi_2Sr_2CaCu_2O_8$ phase. The m.p. of $Bi_2Sr_2CaCu_2O_8$ phase decreased as the content of (Sr+Ca)decreased. $Bi_{2+x}Sr_2CaCu_2O_8$ phase first segregated out of liquid phase around $Bi_2Sr_2CaCu_2O_8$ phase during cooling of liquid phase.

  • PDF

Enhancement of $Bi_2Sr_2Ca_2Cu_3O_{10}$ Formation using $Bi_2Sr_2CuO_6$ and $(Ca_{0.91}Sr_{0.09})CuO_2$ Precursors ($Bi_2Sr_2CuO_6$$(Ca_{0.91}Sr_{0.09})CuO_2$를 이용한 $Bi_2Sr_2Ca_2Cu_3O_{10}$ 고온초전도체의 합성촉진)

  • Lee, Hwa-Sung;Park, Min-Soo;Ahn, Byung-Tae
    • Korean Journal of Materials Research
    • /
    • v.6 no.7
    • /
    • pp.684-691
    • /
    • 1996
  • To enhance the formation of Bi,Sr,Ca,Cu,O,(Bi-2223) single phase in a shorter reaction time, the intermediate compounds such as Bi,Sr,CuO,(Bi-2201). BizSr,CaCuz08(Bi-2212) and (Ca, Sr,, ,9)CuOz in the Bi-Sr-Ca-Cu-0 system were used as the precursors. The formation of Bi-2223 was enhanced in the mixture of Bi-2201 and (Ca, ,,Sr, 119)C~eOsZpe,c ially from the mixture with (Ca, 9I Sr, ,,)CuO,-rich composition compared to Bi, iPb, 4Sr2Ca,Cu3010-cxo mposition. The formation of Bi- 2223 essentially completed within 60h at 860$^{\circ}$C and 870$^{\circ}$C. However, a small amount of the remnant Bi-2212 phase did not disappear even after a prolonged reaction at 870'C. The merit of the proposed synthetic method using the intermediate precusors can be summarized as a shorter reaction time for the formation of Bi-2223 phase, in addition to a smaller amount of second phases compared to the conventional solid-state reaction method.

  • PDF

Float Zone Growth of Superconduction $Bi_2Sr_2CaCu_2O_8$ Fiber with Halogen Lamp (할로겐 램프 열원을 이용한 초전도성 $Bi_2Sr_2CaCu_2O_8$ Fiber의 Float Zone 성장)

  • 김철진;정준기
    • Korean Journal of Crystallography
    • /
    • v.7 no.2
    • /
    • pp.147-155
    • /
    • 1996
  • Floating Zone Image furnace with halogen lamps as heat source has been made and applied to the growth of high-Tc superconductor Bi2Sr2CaCu2O8. The manufactured crystal growth equipment is composed of holder unit for setting the halogen lamps at the focal point of the elliptical mirror, image furnace with maximum temperature of 1800℃ with 1kW halogen lamps, cooling unit, feeding unit for supplying source material to the molten zone, pulling unit for crystal growth, and the control unit in the range of 2mm/hr -40 mm/hr vertical movement and 15rpm - 12rpm rotation. Bi2Sr2CaCu2O8 fibers have been grown with 300W halogen lamps and characterized with XRD, SEM and EDS. The growth condition was air atmosphere, growth speed 3∼4mm/hr, rotation speed of upper and lower part 20∼25 rpm. The fiber was composed of 20∼25 rpm matrix phase and secondary phases such as (Sr,Ca)CuO2 and (Sr,Ca)2CuO3.

  • PDF

Bi(Pb)SrCaCuO superconductor fabricated by interdiffusion of SrCaCuO and BiPbCuO double layers (SrCaCuO와 BiPbCuO 이중층의 상호확산에 의해 제조된 Bi(Pb)SrCaCuO 초전도체)

  • 최효상;이중근;정동철;한병성
    • Electrical & Electronic Materials
    • /
    • v.9 no.7
    • /
    • pp.680-689
    • /
    • 1996
  • SrCaCuO와 BiPbCuO 화합물로 이루어진 이중층시료가 만들어 졌으며, 소결과정에서 나타나는 확산과 입자간의 상호작용으로 108K의 임계온도를 나타내었다. 이 시료는 820.deg. C에서 0-210 시간동안 소결되었다. 초전도체의 생성, 성장메카니즘과 임계온도의 관계가 연구되었으며, 최적조건은 820.deg. C에서 210시간 소결하고 SrCaCuO와 BiPbCuO의 도포비가 1:0.6인 시편에서 나타났다. 또한 이중층시료에서 가장 좋은 조성비는 S $r_{2}$C $a_{2}$C $u_{2}$ $O_{x}$와 B $i_{1.9}$P $b_{0.5}$C $u_{3}$ $O_{y}$ 이었다.다.

  • PDF

The mechanism of Bi$_{0.5}Pb_3Sr_2Ca_2CuO_{\delta}$ and (Ca,Sr)$_2$(BiPb)O$_4$ phase as a flux-pinning center in (Bi,Pb)$_2Sr_2Ca_2CuO_{10}$ superconductor ((Bi,Pb)$_2Sr_2Ca_2CuO_{10}$ 초전도체에l서 flux-pinning center로서 Bi$_{0.5}Pb_3Sr_2Ca_2CuO_{\delta}$ 및 (Ca,Sr)$_2$(BiPb)O$_4$ 상의도입 기구)

  • Chung, Jun-Ki;Kim, Cheol-Jin;Lee, Sang-Hee;Yoo, Jae-Moo;Kim, Hae-Doo;Koh, Jae-Woong
    • 한국초전도학회:학술대회논문집
    • /
    • v.9
    • /
    • pp.300-304
    • /
    • 1999
  • To tap the feasibility of exploiting the 2$^{nd}$ phases as flux-pinning centers in the (Bi,Pb)$_2Sr_2Ca_2CuO_{10}$ superconductor, the size and the distribution of the precipitates have been controlled by changing reaction temperature and time, oxygen partial pressure Po$_2$ and annealing condition. Various annealing heat treatments were also conducted on the as-received 61 filament Bi-2223 tapes with Bi$_{1.8}Pb_{0.4}Sr_2Ca_{2.2}Cu_3O_8$ starting composition and annealed specimen were analyzed with XRD, SEM, EDS and TEM.. The grain size of (Ca,Sr)$_2$(BiPb)O$_4$ or Bi$_{0.5}Pb_3Sr_2Ca_2CuO_{\delta}$ was controllable by optimizing the heat treatment condition and critical current density (J$_c$) showed dependence on the size of the 2$^{nd}$ phases.

  • PDF

Fabrication of $Bi_{2}Sr_{2}CaCu_{2}O_{8}$ Superconducting Films by the LiReac-PreCu Method (급속반응공정에 의한 동 테이프 $Bi_{2}Sr_{2}CaCu_{2}O_{8}$)

  • 성현태;한상철;한영희;이준성;최희락
    • Progress in Superconductivity and Cryogenics
    • /
    • v.1 no.1
    • /
    • pp.7-14
    • /
    • 1999
  • Wekk oriented $Bi_{2} Sr_{2} CaCu_{2} O_{8}$ suppercondcting thick films were fabricared on copper tape by LiReac-PreCu (liquid reaction between a Cu-free precousor and Cu tape) method. Cu-free precursor power which is composed of $Bi_{2}Sr_{2}Ca_{5}$ was printed on a copper tape by screen printing and was heat-treated. The speciment were partially in a molten state at the heat treatment temperature (85$0^{\circ}C$~87$0^{\circ}C$). The heat heat treatments for the reaction were performed in air or low oxygen pressure in several stages. XRD analyses of the resulting Bi2Sr2CaCu2O8 superconducting tapes show that the $Bi_{2} Sr_{2} CaCu_{2} O_{8}$ phase is dominant and a small amount of $Bi_{2} Sr_{2} Cu_{2} O_{6}$ phase is detected. Both phases are aligned in the c-axis direction.

  • PDF

Superconducting Phase Formation and Properties in the Bi-Sr-Ca-Cu-O System (Bi-Sr-Ca-Cu-O 계에서 초전도체 상형성 및 특성)

  • Nam, Gung-Chan;Lee, Sang-Yun
    • Korean Journal of Materials Research
    • /
    • v.6 no.6
    • /
    • pp.543-554
    • /
    • 1996
  • Bi-Sr-Ca-Cu-O 계에서 상형성에 관해 연구하였다. 임계온도가 80K인 초전도체는 Bi-Sr-Ca-Cu의 몰비율이 2:2:1:2의 성분으로부터 solid state synthesis의 방법으로 합성하였다. 이때 이상에 대한 x-ray diffraction pattern은 모두 색인하였다. 2:2:1를 기본으로한 solid solution의 형성을 Bi2Sr2-xCa1+yCu2O8+$\delta$으로 단일상(single phase)을 형성하고 있으며, 이때 x와 y의 범위는 0

  • PDF

Studies of the Crystallization through Volume Change from Bi-Sr-(Ca, Cd)-Cu-O Amorphous Materials (Bi-Sr-(Ca, Cd)-Cu-O 비정질체의 체적변화에 따른 결정화 과정 연구)

  • 한영희;성태현;한상철;이준성;정상진
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 1999.02a
    • /
    • pp.51-53
    • /
    • 1999
  • The crystallization mechanism of an amorphous $Bi_{2}$$Sr_{2}$$Ca_{2 x}$$Cd_{x}$$Cu_{3}$$O_{y}$ phase were studied from the relations between crystallization and volume changes by dilatometry. Further, the effect of addition of CdO on the crystallization mechanism and superconductivity was discussed. The shrinkage of the amorphous $Bi_{2}$$Sr_{2}$$Ca_{2 x}$$Cd_{x}$$Cu_{3}$$O_{y}$ occurred with the crystallization of $Bi_{2}$$Sr_{2}$Cu$O_{6}$ phase decrease with increasing CdO content with a minimum at x=0.4. Better superconductivity was obtained in the specimens formation less amount of the$Bi_{2}$$Sr_{2}$Cu$O_{6}$ phase during the crystallization process.

  • PDF

The Effects of CdO Addition on the Orientation Process of Bi-Sr-Ca-Cu-O Supercoducting Thick Film (Bi계 초전도 후막의 배향과정에 CdO 첨가의 영향)

  • 한영희;성태현;한상철;이준성;정상진
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 1999.02a
    • /
    • pp.47-50
    • /
    • 1999
  • The orientation mechanism of an amorphous $Bi_{2}$$Sr_{2}$$Ca_{2 x}$$Cd_{x}$$Cu_{3}$$O_{y}$ phase were studied by using the dilatometry. The amorphous $Bi_{2}$$Sr_{2}$$Ca_{2 x}$$Cd_{x}$$Cu_{3}$$O_{y}$ samples brought about a volume shrinkage at the onset of the crystallization of a $Bi_{2}$$Sr_{2}$$CaCu_{2}$$O_{6}$phase around $400^{\circ}C$. The random crystal growth of $Bi_{2}$$Sr_{2}$$CaCu_{2}$$O_{8}$ phase around $800^{\circ}C$. yielded a rapid volume expansion and after then samples shrinmed, accompanied with the crystal orientation. The$Bi_{2}$$Sr_{2}$$Ca_{2 x}$$Cd_{x}$$Cu_{3}$$O_{y}$ (x=0.4) sample exhibited the best-oriented structure because the liquid phase formed seemed to have the lowest viscosity which would contributed to the easy collapse of the card-house structure.

  • PDF

Influence of Carbon Content on Superconductivity of $Bi_{2}Sr_{2}CaCu_{2}O_{x}$ HTS

  • Jeon, Yong-Woo;Soh, Dea-Wha;Fan, Zhanguo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.11a
    • /
    • pp.276-279
    • /
    • 2002
  • $Bi_{2}Sr_{2}CaCu_{2}O_{x}$ was prepared by the conventional method of solid state reaction and SHS method. The samples were annealed in different atmosphere in order to examine the influence of atmospheres on the carbon contents in the $Bi_{2}Sr_{2}CaCu_{2}O_{x}$ compound. The lowest carbon content in $Bi_{2}Sr_{2}CaCu_{2}O_{x}$ could be attended when the sample was annealed in $O_{2}$ at $800^{\circ}C$ for 100 hours. The $CO_{2}$ in air pollute the samples and increase the carbon content in the sintering process. The critical current density of the $Bi_{2}Sr_{2}CaCu_{2}O_{x}$ samples will decrease with the increasing carbon contents in the samples. The impurity carbon will deposit in the grain boundary, which makes critical current density lower.

  • PDF