Effects of Low-Temperature Sintering on Varistor Properties and Stability of VMCDNB-Doped Zinc Oxide Ceramics

  • Nahm, Choon-W.
    • Journal of the Korean Ceramic Society
    • /
    • v.56 no.1
    • /
    • pp.84-90
    • /
    • 2019
  • The varistor properties and stability against dc-accelerated stress of $V_2O_5-Mn_3O_4-Co_3O_4-Dy_2O_3-Nb_2O_5-Bi_2O_3$ (VMCDNB)-doped zinc oxide ceramics sintered at $850-925^{\circ}C$ were investigated. Increasing the sintering temperature increased the average grain size from 4.6 to 8.7 mm and decreased the density of the sintered pellet density from 5.54 to $5.42g/cm^3$. The breakdown field decreased from 5919 to 1465 V/cm because of the increase in the average grain size. Zinc oxide ceramics sintered at $875^{\circ}C$ showed the highest nonlinear coefficient (43.6) and the highest potential barrier height (0.96 eV). Zinc oxide ceramics sintered at $850^{\circ}C$ showed the highest stability: the variation rate of the breakdown field was -2.0% and the variation rate of the nonlinear coefficient was -23.3%, after application of the specified stress (applied voltage/temperature/time).

Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PMN-PNN-PZT Ceramics with the amount of PNN substitution (PNN 변화에 따른 저온소결 PMN-PNN-PZT 세라믹스의 유전 및 압전특성)

  • Kim, Kook-Jin;Lee, Gap-Soo;Kim, Do-Hyung;Yoo, Ju-Hyun
    • Proceedings of the KIEE Conference
    • /
    • 2007.07a
    • /
    • pp.1337-1338
    • /
    • 2007
  • In this study, in order to develop low temperature sintering ceramics for multilayer piezoelectric actuator, 0.07Pb$(Mn_{1/3}Nb_{2/3})O_{3}-xPb(Ni_{1/3}Nb_{2/3})O_{3}-(0.93-x)Pb(Zr,Ti)O_{3}$ ceramics system were fabricated using $Li_{2}CO_{3}-Bi_{2}O_{3}$-CuO sintering aids and the specimens were sintered at $930^{\circ}C$. Thereafter their piezoelectric and dielectric characteristics were investigated with the amount of PNN substitution. At 9[mol%] PNN substitution, electromechanical coupling factor (kp), mechanical quality factor (Qm) and piezoelectric constant ($d_{33}$) showed the optimum value of 0.60, 1323 and 387pC/N, respectively.

  • PDF

Element Dispersion by the Wallrock Alteration of Daehyun Gold-silver Deposit (대현 금-은광상의 모암변질에 따른 원소분산)

  • Yoo, Bong Chul
    • Economic and Environmental Geology
    • /
    • v.46 no.2
    • /
    • pp.199-206
    • /
    • 2013
  • The Daehyun gold-silver deposit consists of two hydrothermal quartz veins that fill NE-trending fractures in the Cambro-Ordovician calcitic marble. I have sampled wallrock, hydrothermaly-altered rock and gold-silver ore vein to study the element dispersion and element gain/loss during wallrock alteration. The hydrothermal alteration doesn't remarkably recognized at this deposit and consists of mainly calcite, dolomite, quartz and minor epidote. The ore minerals composed of arsenopyrite, pyrrhotite, pyrite, sphalerite, stannite, chalcopyrite, galena, electrum, native bismuth and silver-bearing mineral. Based on analyzed data, the chemical composition of wallrock consists of mainly $SiO_2$, CaO, $CO_2$ with amounts of $Al_2O_3$, $Fe_2O_3(T)$ and MgO. The contents of $SiO_2$, $Fe_2O_3(T)$, MgO, CaO and $CO_2$ vary significantly with distance from ore vein. The element dispersion doesn't remarkably recognized during wallrock alteration and only occurs near the ore vein margin because of physical and chemical properties of wallrock. Remarkable gain elements during wallrock alteration are $Fe_2O_3(T)$, total S, Ag, As, Bi, Cd, Cu, Ni, Pb, Sb, Sn, W and Zn. Remarkable loss elements are $SiO_2$, MnO, MgO, CaO. $CO_2$ and Sr. Therefore, Our result may be used when geochemical exploration carry out at deposits hosted calcitic marble in the Hwanggangri metallogenic district.

A study on the relationship of various characterizations for undoped ZnO thin films (Undoped ZnO 박막의 다양한 특성의 상관관계에 대한 연구)

  • Baek, Kyung-Hyun;Park, Hyeong-Sik;Jang, Kyung-Soo;Jung, Sung-Wook;Ryu, Kyung-Yul;Yun, Eui-Jung;Yi, J.
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2010.06a
    • /
    • pp.147-147
    • /
    • 2010
  • PTC Thermistors specimens were fabricated by added $MnO_2$ as donors, and $Nb_2O_5$ as acceptors and sintered $1250^{\circ}C$/2hrs. Average grain size decreased with increased in added $MnO_2$, and increased with added in $Nb_2O_5$. But, appeared liquid phase as $Bi_2O_3$ and $TiO_2$, affect to grain growth. XRD result, peak strength waslowed then crystallization not well, but, secondary phase were not showed all specimens. All specimens resistance were so high, about $40M{\Omega}$ over, couldn't measured to those resistance and doesn't appear PTCR effect.

  • PDF

A Study on the Effects of $TiO_2$ and $Al(OH)_3$ for ZnO Ceramic Varistor (ZnO Ceramic Varistor에 미치는 $TiO_2$$Al(OH)_3$의 영향)

  • 안영필;김복희
    • Journal of the Korean Ceramic Society
    • /
    • v.19 no.4
    • /
    • pp.287-292
    • /
    • 1982
  • Nonohmic properties of ZnO ceramics with various small amounts of additives were studied in relation to experimental methods, additive contant and sintaring temperature. The kinds of additives used to following chemicals were basic additives ($0.5Bi_2O_3$, $0.3BaCO_3$, $0.5MnCO_3$, $0.5Cr_2O_3$, $0.1KNO_3$), $TiO_2$ and $Al(OH)_3$. Expecially, this study has focused on the effectsof $TiO_2$ and $Al(OH)_3$ in ZnO ceramics with the basic additives. SEM studies indicated that the addition of TiO2 promoted grain growth but retarded grain growth with the addition of $Al(OH)_3$. Also, in the case of calcination of ZnO with $TiO_2$ and ZnO with $Al(OH)_3$ previously, grain size of ZnO with $TiO_2$ was larger and that of ZnO with Al(OH)3 was smaller in comparison to the case with out calcination. From the viewpoint of nonohmic exponent and nonohimic resistance, electrical characteristics of ZnO, $TiO_2$ and the basic additives was more effective than that of ZnO, $Al(OH)_3$ and the basic additives. Nonohmic exponent and nonohmic resistance of ZnO, $TiO_2$ and the basic additives was 11-13 and 40-65 respectively.

  • PDF

The Microstructure and Electrical Characteristics of High Voltage ZnO Varistors with $Sb_2O_3$Additive ($Sb_2O_3$가 첨가된 고전압 ZnO 바리스터의 미세 구조 및 전기적 특성)

  • Oh, Soo-Hong;Jung, Woo-Sung;Hong, Kyung-Jin;Lee, Jin;Kim, Tae-Sung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.369-372
    • /
    • 2000
  • ZnO varistor is studied to sintering condition and mixing condition for the improvement to non linear of electrical characteristics. In this paper, ZnO varistor, ZnO-Bi$_2$O$_3$-Y$_2$O$_3$-MnO-Cr$_2$O$_3$-Sb$_2$O$_3$series, is fabricated with Sb$_2$O$_3$mol ratio(0.5~4[mol%]) and sintered at 1250[$^{\circ}C$] for 2 hours. The grain size to Sb$_2$O$_3$moi ratio was measured by fractal mathematics. The ZnO varistors that Sb$_2$O$_3$mot ratio is 1[mol%] were shown small grain size because of spinel phase. The fractal dimension were increased with increasing of Sb$_2$O$_3$mo ratios. The capacitance of ZnO varistors with increasing of Sb$_2$O$_3$additive in voltage-capacitance characteristics was decreased by small grain size.

  • PDF

Microstructure of High Voltage ZnO Varistors by Various Addition. (다양한 첨가물에 의한 고전압 ZnO 바리스터의 미세구조)

  • O, Su-Hong;Gi, Hyeon-Cheol;Jang, Dong-Hwan;Hong, Gyeong-Jin;Kim, Tae-Seong
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.05b
    • /
    • pp.185-189
    • /
    • 2000
  • ZnO varistor has many merits as compared with SiC varistor. But, because of leakage current and non-linear coefficient, it has unstable function properties. For the purpose of improvement of ZnO varistor properties, ZnO varistor is studied according to sintering condition and mixing condition. ZnO varistor, $ZnO-Bi_2O_2-Y_2O_3-MnO-Cr_2O_3-Sb_2O_3$ series, is fabricated with $Sb_2O_3$ mol ratio(0.5-4[mol%]) and sintered at $1250[^{\circ}C]$ In accordance with $Sb_2O_3$ mol ratio and sintering temperature, grain size and non-linear coefficient are measured. The specimen, $Sb_2O_3$ mol ratio is 1[mol%], has small grain size. It has best properties because of its liquid phase shape. When $Sb_2O_3$ mol ratio is 1[mol%], grain size is decreased.