• 제목/요약/키워드: $B_2O_3$/$ZrO_2$

검색결과 182건 처리시간 0.024초

침전법으로 제조한 $Al_2O_3$-$ZrO_2$계 세라믹스의 미세구조 및 기계적 특성 (Microstructures and Mechanical Properties of $Al_2O_3$-$ZrO_2$ Ceramics Prepared by a Precipitation Method)

  • 홍기곤;이홍림
    • 한국세라믹학회지
    • /
    • 제27권8호
    • /
    • pp.991-1003
    • /
    • 1990
  • A precipitation method, one of the most effective liquid phase reaction methods, was adopted in order to prepare high-tech Al2O3/ZrO2 composite ceramics. Al2(SO4)3.18H2O, ZrOCl2.8H2O and YCl3.6H2O were used as starting materials and NH4OH as a precipitation agent, various types of metal hydroxides were obtained by single precipitation(series A) and co-precipitation(series B) method at the pH condition between 7 and 11. Fine Al2O3-ZrO2 powders were prepared at optimum calcination condition and the effects of ZrO2 on microstructures and mechanical properties of Al2O3 were investigated. The composition of Al2O3/ZrO2 composites wax fixed as Al2O3-15 v/o ZrO2(+3m/o Y2O3). ZrO2 limited the grain growth of Al2O3 and increased grain size homogeneity of Al2O3 more effectively than MgO.Flexural strength values in Al2O3 and Al2O3/ZrO2 composites were 340-430 MPa and 540-820 MPa, respectively, and the effect of strength improvement showed 20-50% by adding ZrO2 to Al2O3. Fracture toughness of Al2O3/ZrO2 composites was improved by stress-induced phase transformation of tetragonal ZrO2 and toughening effect by microcrack was not observed. Also, ZrO2 particles located at Al2O3 grain junction contributed to toughening, while spherical ZrO2 particles located within Al2O3 grain did not contribute to toughening. Weibull moduli of Al2O3 ceramics and Al2O3/ZrO2 composites of series A and series B were 4.34, 5.17 and 9.06, respectively. Above 0.5 of failure probability, strength values in Al2O3 ceramics and Al2O3/ZrO3 composites of series A and series B were above 400 MPa, 700 MPa and 650 MPa, respectively.

  • PDF

침전법으로 제조한 Al2O3-15v/o ZrO2(+3m/o Y2O3)계 세라믹스의 소결거동 (Sintering Behavior of Al2O3-15v/o ZrO2(+3m/o Y2O3) Ceramics Prepared by Precipitation Method)

  • 홍기곤;이홍림
    • 한국세라믹학회지
    • /
    • 제26권3호
    • /
    • pp.423-437
    • /
    • 1989
  • Al2O3/ZrO2 composites were prepared by precipitation method using Al2(SO4)3.18H2O, ZrOCl2.8H2O and YCl3.6H2O as starting materials and NH4OH as a precipitation agent. Al2O3/ZrO2 composites(series A) were prepared by mixing Al2O3 powder obtained by single precipitation method with ZrO2(+3m/o Y2O3) powder obtained by co-predipitation method. Al2O3/ZrO2 composites (series B) were prepared by co-precipitation method using the three starting materials. In all cases, the composition was controlled as Al2O3-15v/o ZrO2(+3m/o Y2O3). The composites of series A showed higher final relative densities than those of series B and tetagonal ZrO2 in all cases was retained to about 95% at room temperature. ZrO2 particles were coalesced more rapidly in grain boundary of Al2O3 than within Al2O3 grain. ZrO2 particles were located at 3-and 4-grain junction of Al2O3 and limited the grain growth of Al2O3. It was observed that MgO contributed to densification of Al2O3 but limited grain growth of Al2O3 by MgO was not remarkable. In all Al2O3/ZrO2 composites, exaggerated grain growth of Al2O3 was not observed and Al2O3/ZrO2 composites were found to have homogeneous microstructures.

  • PDF

$ZnO-{B_2}{O_3}-{SiO_2}-PbO$계 유리와 $ZrB_2$분말의 소결체의 특성 (Characteristics of Sintered Composites for $ZnO-{B_2}{O_3}-{SiO_2}-PbO$ Glass and $ZrB_2$Powders)

  • 송현진;이병철;류봉기
    • 한국재료학회지
    • /
    • 제11권7호
    • /
    • pp.562-568
    • /
    • 2001
  • 60ZnO-20B$_2$O$_3$-10SiO$_2$-10PbO의 조성을 가진 결정성 봉착용 유리분말과 ZrB$_2$분말을 출발물질로 사용하여 Na분위기 하에서 소결한 복합소결체를 저항체 후막으로써 사용가능성을 검토하였다. 도전성입자 ZrB$_2$는 소결중 매우 민감한 산화특성을 나타내었으며, 이것은 로내 또는 시편내에 잔류된 미량의 산소 및 유리성분 중 B$_2$O$_3$의 반응에 의한 배위수 변화과정에서 유리되는 산소가 원인으로 될 수 있다는 것을 시편의 밀도 및 부피변화 등을 통해 확인되었다. 각 혼합물의 소결온도와 혼합비 변화에 따라 내부조직의 변화와 함께 10~$10^{5}{\Omega}/cm^2$정도의 제어 가능한 저항값을 얻을 수 있었다. 이러한 결과들로부터 유리기지 중에서 ZrB$_2$입자들의 치밀화 경향을 갖는 복합소성시편들에 대한 거시적인 관점에서 도전성경로형성 및 도전기구를 설명하였다.

  • PDF

침전법으로 제조한 $Al_2O_3$-$ZrO_2$계 세라믹스의 열충격 거동 (Thermal Shock Behavior of $Al_2O_3$-$ZrO_2$ Ceramics Prepared by a Precipitation Method)

  • 홍기곤;이홍림
    • 한국세라믹학회지
    • /
    • 제28권1호
    • /
    • pp.11-18
    • /
    • 1991
  • A precipitation method, one of the most effective liquid phase reaction methods, was adopted in order to prepare high-tech Al2O3/ZrO2 composite ceramics, and the effects of stress-induced phase transformation of ZrO2 on thermal shock behavior of Al2O3-ZrO2 ceramics were investigated. Al2(SO4)3.18H2O, ZrOCl2.8H2O and YCl3.6H2O were used as starting materials and NH4OH as a precipitation agent. Metal hydroxides were obtained by single precipitation(process A) and co-precipitation(process B) method at the condition of pH=7, and the composition of Al2O3-ZrO2 composites was fixed as Al2O3-15v/o ZrO2(+3m/o Y2O3). Critical temperature difference showing rapid strength degradation by thermal shock showed higher value in Al2O3/ZrO2 composites(process A : 20$0^{\circ}C$, process B : 215$^{\circ}C$) than in Al2O3(175$^{\circ}C$). The improvement of thermal shock property for Al2O3/ZrO2 composites was mainly due to the increase of strength at room temperature by adding ZrO2. The strength degradation was more severe for the sample with higher strength at room temperature. Crack initiation energies by thermal shock showed higher values in Al2O3/ZrO2 composites than in Al2O3 ceramics due to increase of fracture toughness by ZrO2.

  • PDF

Electrical Resistivity and Fracture Toughness of SiC-ZrB2

  • Shin, Yong-Deok;Ju, Jin-Young;Kwon, Ju-Sung
    • The Korean Journal of Ceramics
    • /
    • 제5권4호
    • /
    • pp.400-403
    • /
    • 1999
  • The mechanical and electrical properties of hot-pressed and annelaed $\beta$-SiC+39vol.% $ZrB_2$ electroconductive ceramic composites were investigated as a function of the liquid forming additives of $Al_2O_3+Y_2O_3$(6:4 wt%). In this microstructures, no reactions and elongated $\alpha$-SiC grains with equiaxed $ZrB_2$ grains were observed between $\beta$-SiC and $ZrB_2$. The properties of the $\beta$-SiC+39vol.%$ZrB_2$ composites with 4wt% $Al_2O_3+Y_2O_3$ at R.T. are as follows: fracture toughness is 6.37 MPa.m1/2, electical resistivity is $1.51\times10^{-4}\Omega \cdot\textrm{cm}$ and the relative density is 98.6% of the theoretical density. The fracture toughness of the $\beta$-SiC+39 vol.% $ZrB_2$ composites were weakly decreased with increasing amount of $Al_2O_3+Y_2O_3$ additives. Internal stresses due to the difference of $\beta$-SiC and $ZrB_2$ thermal expansion coefficient and elastic modulus mismatch appeared to contribute to fracture toughening in $\beta$-SiC+39vol.%$ZrB_2$ electroconductive ceramic composites.

  • PDF

$Al_{2}O_{3}+Y_{2}O_{3}$를 첨가한 $\beta$-SiC-$ZrB_2$ 복합체의 특성 (Properties of the $\beta$-SiC-$ZrB_2$ Composites with $Al_{2}O_{3}+Y_{2}O_{3}$ additives)

  • 신용덕;주진영
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 추계학술대회 논문집 학회본부 C
    • /
    • pp.853-855
    • /
    • 1998
  • The electrical resistivity and mechanical properties of the hot-pressed and annealed ${\beta}$-SiC+39vol.%$ZrB_2$ electroconductive ceramic composites were investigated as a function of the liquid forming additives of $Al_{2}O_{3}+Y_{2}O_{3}$(6:4wt%). In this microstructures. no reactions were observed between $\beta$-SiC and $ZrB_2$, and the relative density is over 97.6% of the theoretical density. Phase analysis of composites by XRD revealed mostly of a $\alpha$-SiC(6H, 4H), $ZrB_2$ and weakly $\beta$-SiC(15R) phase. The fracture toughness decreased with increased $Al_{2}O_{3}+Y_{2}O_{3}$ contents and showed the highest for composite added with 4wt% $Al_{2}O_{3}+Y_{2}O_{3}$ additives. The electrical resistivity increased with increased $Al_{2}O_{3}+Y_{2}O_{3}$ contents because of the increasing tendency of pore formation according to amount of liquid forming additives $Al_{2}O_{3}+Y_{2}O_{3}$. The electrical resistivity of composites is all positive temperature coefficient resistance(PTCR) against temperature up to $700^{\circ}C$.

  • PDF

Ni-Mn 산화물 NTC 서미스터의 미세구조와 전기적 특성에 미치는 ZrO2첨가의 효과 (Effect of ZrO2 Addition on the Microstructure and Electrical Properties of Ni-Mn Oxide NTC Thermistors)

  • 박경순;방대영;윤성진;최병현
    • 한국세라믹학회지
    • /
    • 제40권1호
    • /
    • pp.11-17
    • /
    • 2003
  • Ni-Mn 산화물 NTC 서미스터의 미세구조와 전기적 특성에 미치는 Zr $O_2$ 첨가의 효과를 연구하였다. Zr $O_2$를 포함하는 Ni-Mn-Zr 산화물 소결체의 주요 상은 입방정 스피넬 구조를 가지는 NiO-Mn$_3$ $O_4$-Zr $O_2$의 고용체와 정방정 결정구조를 가지는 Zr $O_2$ 상이였다. Zr $O_2$의 첨가량이 증가함에 따라 Ni-Mn-Zr산화물의 고용체를 형성하지 못하고 생성된 Zr $O_2$의 양이 증가하였다. NiO-Mn$_3$ $O_4$-Zr $O_2$ NTC 서미스터에 있어서 절대온도 역수(l/T)에 대한 로그 비저항(log $ho$)은 직선적인 관계가 있었고, 비저항, B$_{140}$320/정수 및 활성화 에너지는 Zr $O_2$ 함량이 증가함에 따라 크게 증가하였다.

Ni3Al-7.8%Cr-1.3%Zr-0.8%Mo-0.025%B 합금의 고온산화막분석 (Characterization of Oxide Scales Formed on Ni3Al-7.8%Cr-1.3%Zr-0.8%Mo-0.025%B)

  • 김기영;이동복
    • 한국재료학회지
    • /
    • 제12권3호
    • /
    • pp.220-224
    • /
    • 2002
  • The oxide scales formed on $Ni_3Al$-7.8%Cr-1.3%Zr-0.8%Mo-0.025%B after oxidation at 900, 1000 and 110$0^{\circ}C$ in air were studied using XRD, SEM, EPMA and TEM. The oxide scales consisted primarily of $NiO,\; NiAl_2O_4,\;{\alpha}-Al_2O_3,\; monoclinic-ZrO_2,\; and \;tetragonal-ZrO_2$. The outer layer of the oxide scale was rich in Ni-oxides, whereas the internal oxide stringers were rich in Al-oxides and $ZrO_2$. Within the above oxide scales, Cr and Mo tended to exist as dissolved ions.

액장 소결에 의한 $\beta-SiC-ZrB_2$ 복합체의 제조와 특성 (Properties and Manufacture of the $\beta-SiC-ZrB_2$ Composited Densified by Liquid-Phase Sintering.)

  • 신용덕;주진영
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제48권2호
    • /
    • pp.92-97
    • /
    • 1999
  • The mechanical and electrical properties of the hot-pressed and annealed $\beta-Sic$+39vol.%$ZrB_2$ electroconductive ceramic composites were investigated as a function of the liquid forming additives of $Al_2O_3+Y_2O_3(6:4wt%)$. In this microstructures, no reactions and elongated $\alpha$-SiC grains with equiaxed $ZrB_2$, gains were observed between $\beta-SiC$ and $ZrB_2$, and the relative density was over 97.6% of the theoretical density. Phase analysis of the composites by XRD revealedmostly of $\alpha$-SiC(6H, 4H), $ZrB_2$, and weakly $\beta-SiC$(15R) phase. The fracture toughness decreased with increasing $Al_2O_3+Y_2O_3$ contents and showed the highest of $6.37MPa.m^{\fraction ane-half}$ for composite added with 4wt% $Al_2O_3+Y_2O_3$ additives at room temperature. The electrical resistivity increased with increasing $Al_2O_3+Y_2O_3$contents and showed the lowest of $1.51\times10^{-4}\Omega.cm$ for composite added with $Al_2O_3+Y_2O_3$ additives at $25^{\circ}C$. This reason is the increasing tendency of pore formation according to amount of liquid forming additives $Al_2O_3+Y_2O_3$. The electrical resistivity of the composites was all positive temperature coefficient resistance(PTCR) against temperature up to $700^{\circ}C$.

  • PDF

$B_2O_3$ 첨가에 의한 적색 축광성 형광체의 발광특성에 관한 연구 (A study on the luminescence characterization of red long persistent phosphors by the $B_2O_3$ addition)

  • 황구현;최종건
    • 한국결정성장학회지
    • /
    • 제18권1호
    • /
    • pp.22-26
    • /
    • 2008
  • [ $CaCO_3$ ]와 $ZrO_2$를 모체결정으로 하고 Pr을 부활제로, 융제로 $B_2O_3$을 사용하였으며 고상반응법으로 합성하여 $CaZrO_3$ : Pr 적색 축광성 형광체를 제조하였다. XRD 분석을 통하여 시료의 결정상을 확인하였고, PL 검사를 통하여 $480{\sim}570nm$영역과 $590{\sim}700nm$ 영역의 발광 스펙트럼을 관찰하였다. 융제로서 $B_2O_3$을 각각 1%, 5%, 10%를 첨가하여 고상반응법으로 합성하였을 때, 494 nm 에서 발광은 $B_2O_3$의 농도가 1%일 때 가장 높은 강도를 나타냈다. 적색을 나타내는 620 nm에서의 Peak는 $B_2O_3$의 농도가 10%일 때 가장 높은 강도를 나타내었다.