Sintered alumina ceramics were joined by 2 kinds of SiO$_2$-CaO-A1$_2$O$_3$ glass solders having a similar expansivity as alumina. Wetting of glass/alumina was examined by sessile drop method. The observation of interface and bending strength related to alumina/glass/alumina systems were investigated by means of SEM/EDX and 4-point bending test. the result are summarized as follow: (1) Wetting of glass solders on alumina was good at temperatures higher than 145$0^{\circ}C$. (2) When the joining temperature wan high, diffusion and/or reactions between solder md alumina took place at the interface. These diffusions and reactions occurring at the interface greatly affected the bending strength of joining body. (3) Highest strength corresponding to 80% that of alumina was obtained by the solder of 35SiO$_2$-35CaO-30A1$_2$O$_3$(wt%) glass.
The monolithic dry gels of the Li2O-Al2O3-TiO2-SiO2 system were prepared by the sol-gel technique using metal alkoxides as starting materials to obtain monolithic glass-ceramics at low temperature without melting. Activation energy for the crystal growth of the gel with 6.05% TiO2, nucleating ageng, for the preparation of Li2O-Al2O3-TiO2-SiO2 system glass-ceramic was 101.14kcal/mol. As a result of the analysis of DTA & XRD, it was confirmed that the crytallization of Li2O-Al2O3-TiO2-SiO2 system glass-ceramic was the most efficient when 6.05% TiO2, nucleating agent, was added. $\beta$-eucryptite solid solution crystals and $\beta$-spodumene solid solution crystals were detected in the sample heat treated above 85$0^{\circ}C$. The sintered gel heat treated at 85$0^{\circ}C$ had the specific surface area of 185$m^2$/g, the pore volume of 0.19cc/g and the average pore radius of 20.8$\AA$. This shows that the sintered gel is also comparatively porous material. In temperature range of 25~85$0^{\circ}C$ thermal expansion coefficient of the specimen which was crystallized for 10hrs at 85$0^{\circ}C$ was 6.7$\times$10-7/$^{\circ}C$, which indicated that the crystallized specimen was turned out to be the glass-ceramic with low thermal expansion.
Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
/
2001.06a
/
pp.313-318
/
2001
The sliding wear behavior of Plasma-Sprayed Al$_2$O$_3$-TiO$_2$ Coating against Cemented Carbide were Investigated using a pin on disk type tester. The experiment was conducted using Al$_2$O$_3$-TiO$_2$ Coaling as pin material and Cemented Carbide as disk material and different operating conditions, at room temperature under a dry conditions. The results showed that the type B(250kw power) appeared average wear rate Is lowed than type A(80kw power). The specific wear rate of Specimen A1 Increased with normal load. But The specific wear rate of Specimen B1 decreased with normal load. Average wear rate of specimen A3, B3 are lowed than other but the sliding wear mechanism of edge were rough.
Several combinations of ozone based advanced oxidation processes were tested for the treatment of red water (RW) containing recalcitrant chemical pollutants produced from 2,4,6-trinitrotoluene (TNT) manufacturing process. $O_3$, $UV/O_3$, $UV/O_3/H_2O_2$, $UV/O_3/H_2O_2/Fe^{2+}$ processes were tested for the treatment of RW. The order of organic and color removal efficiency was found to be : $O_3{\leq}UV/O_3$ < $UV/O_3/H_2O_2$ < $UV/O_3/H_2O_2/Fe^{2+}$. The optimum conditions for the removal of organic and color in the $UV/O_3/H_2O_2/Fe^{2+}$ process were 0.053 g/min of ozone flow rate, 10 mM of $H_2O_2$ concentration and 0.1 mM of $FeSO_4$ concentration. Organic and color removal efficiencies were 96 and 100 % respectively in the $UV/O_3/H_2O_2/Fe^{2+}$ process. tert-butyl alcohol (t-buOH) was used as the hydroxyl radical scavenger. Enhancement of hydroxyl radical production was achieved by the combination of ozone with several oxidants such as UV, $H_2O_2$, $Fe^{2+}$.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.11
no.2
/
pp.111-120
/
1998
In this paper, the $(SrPb)(CaMg)TiO_3$ ceramics with paraelectric properties were fabricated by the mixed oxide method. It was investigated that which the variation of contents of $Bi_2O_3{\cdot}3TiO_2$ effects on structural, dielectrical and electrical properties of specimens. As a result, the grain size were grown with increasing the contents of $Bi_2O_3{\cdot}3TiO_2$. The relative dielectric constants were increased up to 4[mol%] of $Bi_2O_3{\cdot}3TiO_2$, and decreased more or less at a low temperature in the specimens which had more than. But the temperature coefficient. of capacitance were showed ${\pm}25$[%]. The dielectric loss were less than 0.05 in all specimens which had more than 4[mol%] of $Bi_2O_3{\cdot}3TiO_2$. In order to investigate the behavior of charged particles, the characteristics of electrical conduction were measured. As a result, the conduction current was divided into the three steps as a function of DC electric field. The first step was Ohmic region due to ionic conduction, below 15[kV/cm]. The second step was showed a saturation which seems to be related to a depolarizing field occuring in field-enforced ferroelectric phase, between 15[kV/cm] and 40[kV/cm]. The third step was attributed to Child's law related to space charge which injected from electrode, above 40[kV/cm].
The electrochemical behaviors of polycrystalline silver electrodes in 8M KOH solutions containing $Bi_2O_3$ were studied under various conditions by cyclic voltammetry, potentiostatic and galvanostatic techniques as well as the morphology of the silver oxide structures by SEM. It was found that three new compounds comprising silver, bismuth, and oxygen as well as $Bi_2O_3$, $Ag_2O$ and AgO were formed during the electrochemical oxidation of silver. In addition, the potentiostatic current transients were characterized by the appearances of the first current peaks corresponding to the formation of silver oxides, and the second current peaks corresponding to the Ag-Bi-O compounds, indicating the presence of the nucleation and 3D growth mechanism, in the potential regions of $Ag_2O$ and AgO, respectively. Microscopic examinations showed that two types of silver (I) oxide morphologies are formed in the potential region of $Ag_2O$.
Diffusion coupling experiment was done to study expansion of body and soild reaction in BaCO3-TiO2 system. Specimen of BaCO3 and TiO2 was formed with Pt-mark's method. Each specimen was fired at interval of 25℃ from 900℃ to 1000℃ for 2hrs. After that, specimen was fixed with resin and polished. Product layers of specimen were observed with SEM and EDS. The result were following; 1. Diffusion component is Ba2+, which diffuse toward TiO2. 2. Large crack between layer of BaCO3 and Ba2TiO4 was generated because of difference of thermal expansion coefficient. 3. Ba2TiO4 is formed to TiO2 body by the reaction of BaTiO3 and BaO and its structure is very porous. 4. BaTiO3 changes immediately to Ba2TiO4 by the reaction of BaO. But BaTiO3 which formed by the reaction of TiO2 and Ba2TiO4 exsists as layer because the diffusion distance of Ba2+ is far.
The microwave dielectric materials of the BaO-Nd$_2$O$_3$-TiO$_2$and BaO-(Sm, Nd)$_2$O$_3$-TiO$_2$system were synthesized by conventional ceramic processing and sintered 1220 to 140$0^{\circ}C$ for 2 hours respectively. Their crystallization and dielectric properties were examined. In the BaO-Nd$_2$O$_3$-TiO$_2$ and BaO-(Sm, Nd)$_2$O$_3$-TiO$_2$system. Nd$_2$Ti$_2$O$_{7}$ and (Sm, Nd)$_2$Ti$_2$O$_{7}$ were observed as a second phase respectively. The maximum relative dielectric constant were 79,99 for the BaO-Nd$_2$O$_3$-TiO$_2$system and 105.07 for the BaO-(Sm,Nd)$_2$O$_3$-TiO$_2$system and their Q-value were over 2000 at 3GHz.GHz.
High-voltage dielectric discharges are an emerging technique in environmental pollutant degradation, which that are characterized by the production of hydroxyl radicals as the primary degradation species. The initiation and propagation of the electrical discharges depends on several physical, chemical, and electrical parameters such as 1st and 2nd voltage of power, gas supply, conductivity and pH. These parameters also influence the physical and chemical characteristics of the discharges, including the production of reactive species such as OH, $H_2O_2$ and $O_3$. The experimental results showed that the optimum 1st voltage and air flow rate for RNO (N-Dimethyl-4-nitrosoaniline, indicator of the generation of OH radical) degradation were 160 V (2nd voltage of is 15 kV) and 4 L/min, respectively. As the increased of the 2nd voltage (4 kV to 15 kV), RNO degradation, $H_2O_2$ and $O_3$ generation were increased. The conductivity of the solution was not influencing the RNO degradation and $H_2O_2$ and $O_3$ generation. The effects pH was not high on RNO degradation. However, the lower pH and the conductivity, the higher $H_2O_2$ and $O_3$ generation were observed.
The effects of the addition of either monoclinic $ZrO_2(pure)$ or tetragonal $ZrO_2$ containing 5.35wt% $Y_2O_3(Y-TZP)$ on the mechanical properties and thermal shock resistance of $Al_2O_3$ ceramics were investigated. The addition of $ZrO_2$(m) and Y-TZP increased sintered density of $Al_2O_3$. The Vickers hardness also increased as the volume fraction of Y-TZP increased going through a maximum at 20wt%. The hardness of the specimens was found to be dependent on the sintered density. The higher volume fraction of either $ZrO_2(m)$ or Y-TZP resulted in the higher fracture toughness of the composite was. This result may be taken as evidence that toughening of $Al_2O_3$ can be achieved by not only the transformation toughening but microcrack toughening of $ZrO_2$. The thermal shock property for $Al_2O_3-ZrO_2$ composites was improved by increasing the volume fraction of monoclinic $ZrO_2(pure)$. The grain size increased as the volume fraction of $ZrO_2$ did.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.