• Title/Summary/Keyword: $Al_2O_3-SiO_2$

Search Result 2,270, Processing Time 0.032 seconds

Fabrication of $Al_2O_3$/SiC Hybrid-Composite ($Al_2O_3$/SiC Hybrid-Composite의 제조)

  • Lee, Su-Yeong;Im, Gyeong-Ho;Jeon, Byeong-Se
    • 연구논문집
    • /
    • s.26
    • /
    • pp.103-112
    • /
    • 1996
  • $Al_2O_3/SiC$ Hybrid-Composite has been fabricated by conventional powder process. The addition of $\alpha-Al_2O_3$ as seed particles in the transformation of $\gamma-Al_2O_3 to $\alpha-Al_2O_3$ provided a homogeneity of the microstructure, resulting in increase of mechanical properties. The grain growth of $Al_2O_3$ are significantly surpressed by the addition of nano-sized. SiC particles, increasing in fracture strength. The addition of SiC plates to $Al_2O_3$ nano-composite decreased the fracture strength, but increased the fracture toughness. Coated SiC plates with nitrides such as BN and /SiC$Si_3N_4$ enhanced fracture toughness much more than uncoated SiC plates by inducing crack deflection.

  • PDF

Influences of the Molar Ratio of $Mo/MoO_3$ on Characteristics of $MoSi_2-Al_2O_3$ composites by SHS Methods (연소합성법에 의한 $MoSi_2-Al_2O_3$ 복합재료의 특성에 미치는 $Mo/MoO_3$ 몰비의 영향)

  • 장윤식;이윤복;김용백;김인술;박흥채;오기동
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.11
    • /
    • pp.1209-1216
    • /
    • 1996
  • MoSi2-Al2O3 composites were prepared by thermal explosion mode of self-propagating high temperature syn-thesis (SHS) using element powders of MoO3 Mo Si and Al. The combustion products of MoSi2 which have 10, 20, 30 and 40 wt% Al2O3 showed the molten state in the range of Mo to MoO3 6:1-9.5:1, 2:1-8:1, 1:1-5:1, and 1:1-3:1 (molar ratio) respectively. The combustion products which made least seperation the molten phase from the slag phase were in Mo/MoO3=9, 5:1, 8:1, 5:1 and 3:1 (molar ratio) respectively. Particles size of MoSi2 and Al2O3 in the combustion product were decreased as the molar ratio of Mo to MoO3 increase. By XRD analysis only MoSi2 and $\alpha$-Al2O3 peaks were identified in the combusion products, In case of MoSi2 containing 20wt% Al2O3 5.1wt% Al existed into MoSi2 grains and 30.7wt% Si and 7.7wt% Mo existed into Al2O3 grains. The relative density of MoSi2 containing 10, 20, 30 and 40 wt% Al2O3 were 82.7, 85.2, and 81.9% respectively. The fracture strength of MoSi2-Al2O3 composites increased with increasing Al2O3 and that of MoSi2-20wt% Al2O3 composite was 195 MPa.

  • PDF

Study on the Properties of $B_2O_3$-$SiO_2$and $Al_2O_3$-$SiO_2$Coating Films by the Sol-Gel Method (Sol-Gel법으로 제조한 $B_2O_3$-$SiO_2$$Al_2O_3$-$SiO_2$ 박막의 특성에 관한 연구)

  • 황규석;김병훈;최석진
    • Journal of the Korean Ceramic Society
    • /
    • v.27 no.5
    • /
    • pp.583-588
    • /
    • 1990
  • Glass films in the binary system B2O3-SiO2 and Al2O3-SiO2 were prepared on soda-lime-silica slide glass by the dip-coating technique from TEOS and boric acid or aluminum nitrate. Thickness of the films varying with viscosity and withdrawal speed were measured and effect of composition and firing temperature on the properties such as transmittance and refractive index were investigated. nM2O3.(100-n)SiO2(M=B or Al) films containing up to 20mol% B2O3 and 40mol% Al2O3 were transparent. Maximum transmittance at visible range were obtained for the sample containing 15mol% Ba2O3 and 32.5mol% Al2O3 and heat-treated at 50$0^{\circ}C$, respectively. Refractive index of the film containing 15mol% B2O3 was mininum in the B2O3-SiO2 binary system and minimal refractive index was appeared at the film containing 32.5mol% Al2O3. In IP spectra, addition of B2O3 were increased absorption peak intensity of B-O and Si-O-B bond and addition of Al2O3 were decreased absorption peak intensity of Si-O bond, respectively.

  • PDF

Fabrication of $Al_2O_3/SiC$ Composite Through Oxidation of SiC (SiC의 산화에 의한 $Al_2O_3/SiC$ 복합체의 제조)

  • 김경환;이홍림;이형민;홍기곤
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.5
    • /
    • pp.535-543
    • /
    • 1997
  • The surface of SiC particles were partially oxidized to produce SiO2 layers on the SiC particles to prepare Al2O3/SiC composite by formation of mullite bonds between the grains of Al2O3 and SiC during sintering at 1$600^{\circ}C$. This process is considered to enable the sintering of Al2O3/SiC composite at lower temperature and also to relieve the stress, produced by thermal expansion mismatch between Al2O3 and SiC. In fact, Al2O3/SiC composite prepared by oxidation of SiC was observed to be more effectively sintered and densified at lower temperature. Maximum density, flexural strength and microhardness were obtained with 5.65 vol% of mullite content in Al2O3/SiC composite.

  • PDF

Solid-state reaction kinetics for the formation of mullite($3Al_2O_3{\cdot}2SiO_2$) from amorphous $SiO_2$ and ${alpha}-Al_2O_3$ (비정질 $SiO_2$${alpha}-Al_2O_3$부터 Mullite를 합성하기 위한 고체상태 반응속도)

  • 김익진;곽효섭;고영신
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.8 no.2
    • /
    • pp.332-341
    • /
    • 1998
  • Reaction kinetics for the solid - state reaction of ${\alpha}-Al_2O_3$with amorphous $SiO_2$to produce mullite ($3Al_2O_3;{cdot};2SiO_2$) was studied in the temperature range of 1450~$1480^{\circ}C$. Rate of kinetic reaction were determined by using $SiO_2$- coated $Al_2O_3$ compact containing 28.16 wt.% $SiO_2$and heating the reactant mixtures in MgO at definite temperature for various times. Amount of products and unreacted reactants were determined by X-ray diffractometry. Data from the volume fraction and ratio of peak intensities of mullite indicated that the reaction of ${\alpha}-;Al_2O_3$ with $SiO_2$to form $3Al_2O_3\;{\cdot}\;2SiO_2$ start between 1450 and $1480^{\circ}C$. The activation energy for solid-state reaction was determined by using the Arrhenius equation; The activation energy was 31.9 kJ/mol.

  • PDF

The effect of the addition of TiO2 in the preparation of (Al2O3-SiC)- SiC composite powder by SHS Process (SHS법을 이용한 복합분말(Al2O3-SiC) 제조시 TiO2첨가의 영향)

  • Yun, Gi-Seok;Yang, Beom-Seok;Lee, Jong-Hyeon;Won, Chang-Hwan
    • Korean Journal of Materials Research
    • /
    • v.12 no.1
    • /
    • pp.48-53
    • /
    • 2002
  • $Al_2O_3-SiC$ and $Al_2O_3-SiC$-TiC composite powders were prepared by SHS process using $SiO_2,\;TiO_2$, Al and C as raw materials. Aluminum powder was used as reducing agent of $SiO_2,\;TiO_2$ and activated charcoal was used as carbon source. In the preparations of $Al_2O_3-SiC$, the effect of the molar ratio in raw materials, compaction pressure, preheating temperature and atmosphere were investigated. The most important variable affecting the synthesis of $Al_2O_3-SiC$ was the molar ratio of carbon. Unreactants remained in the product among all conditions without compaction. The optimum condition in this reaction was $SiO_2$: Al: C=3: 5: 5.5, 80MPa compaction pressure under Preheating of $400^{\circ}C$ with Ar atmosphere. However there remains cabon in the optimum condition. The effect of $TiO_2$ as additive was investigated in the preparations of $Al_2O_3-SiC$. As a result of $TiO_2$ addition, $Al_2O_3-SiC$-TiC composite powder was prepared. The $Al_2O_3$ powder showed an angular type with 8 to $15{\mu}m$, and the particle size of SiC powder were 5~$10{\mu}m$ and TiC powder were 2 to $5{\mu}m$.

A Study on the Transparent Glass-Ceramics On Al2O3-SiO2 System (투명 결정화 유리에 관한 연구 - $Al_2O_3-SiO_2$계에 관하여)

  • 박용완;김용욱
    • Journal of the Korean Ceramic Society
    • /
    • v.29 no.3
    • /
    • pp.223-231
    • /
    • 1992
  • CaO and ZnO were added to Al2O3-SiO2 binary system respectively as flux, then ZrO2 and TiO2 were applied as nucleating agent to these CaO-Al2O3-SiO2 and ZnO-Al2O3-SiO2 ternary system glass. The transparency could not be kept in CaO-Al2O3-SiO2 system glass, whereas the transparent glass-ceramics were prepared in ZnO-Al2O3-SiO2 system glass containing ZrO2 as the nucleating agent. At this time the optimum heating temperatures for the nucleation and the crystal growth were 78$0^{\circ}C$ and 97$0^{\circ}C$. The sizes of the precipitated crystals in the transparent glass-ceramics were below 0.1 ${\mu}{\textrm}{m}$, and their light transmissibilities were more than 80%.

  • PDF

R-Curve Behavior and Mechanical Properties of Al2O3 Composites Containing SiC and TiC Particles (SiC와 TiC 입자를 함유하는 Al2O3 입자복합체의 균열저항거동과 기계적 성질)

  • Na, Sang-Woong;Lee, Jae-Hyung
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.4
    • /
    • pp.413-419
    • /
    • 2002
  • Particulate composites of $Al_2O_3$/TiC/SiC, $Al_2O_3$/TiC and $Al_2O_3$/SiC have been fabricated by hot pressing and their R-curve behaviors and mechanical properties were investigated. $Al_2O_3$ containing 30 vol% TiC particles showed higher toughness by 8% than that for monolithic alumina and its fracture strength was increased significantly by approximately 30%. On the other hand, the addition of 30 vol% SiC of $3{\mu}m$ in $Al_2O_3$ decreased the fracture strength slightly but induced a rising R-curve behavior owing to the strong crack bridging of SiC particles. In case of $Al_2O_3$/TiC/SiC, arising R-curve behavior was also observed and the fracture toughness reached 6.6 MPa${\cdot}\sqrt{m}$ at the crack length of $1000{\mu}m$, which was lower than that of $Al_2O_3$/SiC, however, while the fracture strength was higher by about 20%. The fracture toughness seemed to be decreased as smaller TiC particles roughened the SiC interface and pullout of the SiC particles for crack bridging became less active.

A Study on the Thermal Stability of an Al2O3/SiON Stack Structure for c-Si Solar Cell Passivation Application (결정질 실리콘 태양전지의 패시베이션 적용을 위한 Al2O3/SiON 적층구조의 열적 안정성에 대한 연구)

  • Cho, Kuk-Hyun;Chang, Hyo Sik
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.3
    • /
    • pp.197-200
    • /
    • 2014
  • We investigated the influence of blistering on $Al_2O_3$/SiON stacks and $Al_2O_3$/SiNx:H stacks passivation layers. $Al_2O_3$ film provides outstanding Si surface passivation quality. $Al_2O_3$ film as the rear passivation layer of a p-type Si solar cell is usually stacked with a capping layer, such as $SiO_2$, SiNx, and SiON films. These capping layers protect the thin $Al_2O_3$ layer from an Al electrode during the annealing process. We compared $Al_2O_3$/SiON stacks and $Al_2O_3$/SiNx:H stacks through surface morphology and minority carrier lifetime after annealing processes at $450^{\circ}C$ and $850^{\circ}C$. As a result, the $Al_2O_3$/SiON stacks were observed to produce less blister phenomenon than $Al_2O_3$/SiNx:H stacks. This can be explained by the differences in the H species content. In the process of depositing SiNx film, the rich H species in $NH_3$ source are diffused to the $Al_2O_3$ film. On the other hand, less hydrogen diffusion occurs in SiON film as it contains less H species than SiNx film. This blister phenomenon leads to an increase insurface defect density. Consequently, the $Al_2O_3$/SiON stacks had a higher minority carrier lifetime than the $Al_2O_3$/SiNx:H stacks.

Study on the R-curve Behaviour in $Al_2O_3-ZrO_2-SiC$ Whisker Comosite ($Al_2O_3-ZrO_2-SiC$ Whisker 복합재료에서의 R-curve 거동에 관한 연구)

  • Kim, Hyun-Ha;Park, Hyun;Choi,Sung-Churl
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.9
    • /
    • pp.731-739
    • /
    • 1993
  • R-curve measurements were performed on Al2O3(matrix)-ZrO2-SiC whisker composite and Al2O3-ZrO2, Al2O3-SiC whisker composites in the favor of comparing the effect of ZrO2 and SiC whisker, as a second phase, to Al2O3 matrix. Al2O3-SiC whisker and Al2O3-ZrO2-SiC whisker were fabricated by hot pressing at 1$700^{\circ}C$, 15MPa and Al2O3-ZrO2 by pressureless sintering at 1$600^{\circ}C$. A controlled flaw/strength technique was utilized to determine fracture resistance as a function of crack extension and R-curve behaviour was determined from the relationship which is KR=K0(Δa)m. R-curveresults were KR=6.173$\times$Δa0.031 for Al2O3-ZrO2, KR=18.796$\times$Δa0.172 for Al2O3-SiC whisker and KR=11.96$\times$Δa0.110 for Al2O3-ZrO2-SiC whisker composite. From the analysis of R-curve and expeirmental data above three composites, it is found that R-curve behaviour of Al2O3-ZrO2-SiC whisker composite was dominated initially by the strengthening effect of ZrO2 and after, some extended crack were influenced by the effect of SiC whisker. Analysis of SEM and X-ray data revealed that whisker bridging in the crack wake and whisker pull-out mechanisms were the main mechanism for the R-curve behaviour.

  • PDF