Y2O3 첨가량에 의한 Al2O3 복합재 세라믹스의 균열 치유와 고온 굴힘강도 특성 (Cracked-Healing and Elevated Temperature Bending Strength of Al2O3 Composite Ceramics by an Amount of Y2O3)

  • 남기우;김해숙;손창석;김성광;안석환
    • 대한기계학회논문집A
    • /
    • 제31권11호
    • /
    • pp.1108-1114
    • /
    • 2007
  • The low kinds of $Al_2O_3$ composite ceramics were prepared using a mixture of 85 wt.% $Al_2O_3$ (mean size $0.5\;{\mu}m$), 15 wt.% SiC Powder with $Y_2O_3$, as an additive powder (0, 1, 3 and 5 wt.%). The crack-healing strengths were studied as functions of crack-healing temperature and amount of $Y_2O_3$. The in-situ crack-healing behavior was observed at 1,573 K for 1 h in the air. The heat treated specimen with 3 wt.% of $Y_2O_3$ showed better crack-healing ability than specimen with 1 or 5 wt.% of $Y_2O_3$. In case of specimen with 3 wt.% of $Y_2O_3$, the bending strength of the crack-healed specimen at 1,473 K was recovered to the bending strength of smooth specimen treated at 1573 K. The heat-resistance limit temperature of $Al_2O_3$ composite ceramics was 1,073 K, 1,373 K, 873 K for the specimen with 1, 3, 5 wt.% of $Y_2O_3$.

SiC세라믹스 동종재 접합재의 전단강도 특성 평가 (Characteristics of Shear Strength for joined SiC-SiC Ceramics)

  • 윤한기;정헌채
    • 대한기계학회논문집A
    • /
    • 제38권5호
    • /
    • pp.483-487
    • /
    • 2014
  • SiC/SiC복합재료는 뛰어난 고온특성, 내산화성 및 크립(Creep)에 대한 저항성이 우수하고 또한 중성자에 의한 조사 손상이 다른 세라믹스에 비해서 적게 받는다는 장점으로 인하여 핵융합로의 블랑켓(Blanket), 제1벽(First-wall) 및 다이버터(Di-vertor)등의 후보재료로 적용이 기대되고 있다. SiC/SiC복합재료 제조시 가장 큰 문제점은 높은 소결온도와 압력으로 인하여 탄화규소 섬유가 손상되어 복합재료의 특성이 저하되는 것이므로 이들 재료의 전단강도 특성 평가는 매우 중요하다, 본 연구에서는 SiC제조특성과 소결온도에 대한 전단강도 특성의 평가한다.