Ti-15V-3Al합금의 시효거동과 열처리에 따른 고온 기계적 특성 (Aging Behavior and Effect of Heat Treatment on High Temperature Mechanical Properties in Ti-15V-3AI-3Cr-3Sn)

  • 이재원;이백희;이규환;김영도
    • 한국재료학회지
    • /
    • 제14권1호
    • /
    • pp.13-18
    • /
    • 2004
  • Titanium alloys are the one of promising candidate materials for medium high temperature parts in the aircraft, automobile, petrochemistry and electrochemistry because of their high strength with low density in medium high temperature. In this study, the effects of aging and heat treatments on the mechanical properties of Ti-15-3 alloy in medium high temperature, which was $400^{\circ}C$, were studied. Solid solution treatment was performed at $8000^{\circ}C$ of $\beta$ phase region for 1 h and the alloy was quenched in water. The alloy was aged at $5000^{\circ}C$ of $\alpha$ and $\beta$ two-phase region for 1, 2, 4, 8, ... and 100 h to increase the mechanical property. The $\beta$ single phase was observed at all parts of specimens in Ti-15-3 alloy after ST. As the aging at $500^{\circ}C$, fine precipitates of a phase was generated from matrix of $\beta$ phase and the microstructure was consisted of weaving structure such as Widmanstiitten a phase. The most suitable aging time is 24h in$ 400^{\circ}C$. At this time, strength is 1164 MPa and elongation is about 12%. In room temperature, elongation of Ti-15-3 alloy aged at $500^{\circ}C$ for 16 h is poor (=3%) in spite of high tensile strength (1458 MPa).

Ti-6Al-4Fe 합금의 가공열처리 미세조직 분석 (Microstructural Analysis of Thermo-Mechanical Processed Ti-6Al-4Fe Alloy)

  • 최병학;최원열;심종헌;박찬희;강주희;김승언;현용택
    • 한국재료학회지
    • /
    • 제25권8호
    • /
    • pp.410-416
    • /
    • 2015
  • Microstructural analysis of a (${\alpha}+{\beta}$) Ti alloy was investigated to consider phase transformation in each step of the thermo-mechanical process using by SEM and TEM EDS. The TAF (Ti-6Al-4Fe) alloy was thermo-mechanically treated with solid solution at $880^{\circ}C$, rolling at $880^{\circ}C$ and annealing at $800^{\circ}C$. In the STQ state, the TAF microstructure was composed of a normal hcp ${\alpha}$ and metastable ${\beta}$ phase. In a rolled state, it was composed of fine B2 precipitates in an ${\alpha}$ phase, which had high Fe segregation and a coherent relationship with the ${\beta}$ matrix. Finally, in the annealing state, the fine B2 precipitates had disappeared in the ${\alpha}$ phase and had gone to the boundary of the ${\alpha}$ and ${\beta}$ phase. On the other hand, in a lower rolling temperature of $704^{\circ}C$, the B2 precipitates were more coarse in both the ${\alpha}$ and the boundary of ${\alpha}$ and ${\beta}$ phase. We concluded that microstructural change affects the mechanical properties of formability including rolling defects and cracks.

상압소결 $\beta$-SiC에 있어서 표면부에서의 액상집중과 미세구조의 변화 (Concentration of Liquid-phase in the Surface Region and Microstructural Change in Pressureless Sintered$\beta$-SiC)

  • 이종국;양권승;김환
    • 한국세라믹학회지
    • /
    • 제33권8호
    • /
    • pp.921-927
    • /
    • 1996
  • The liquid-phase concentration from the interior to the surface region and its influence on the microstructural changes were investigated in pressureless sintered $\beta$-SiC Surface reaction-layer was formed by reaction of packing powder and volatile components on the surface during sintering which was induced the concentration of liquid-phase in the surface regions. The microstructural changes between the surface region and the interior were appeared in sintered specimen which was resulted from the difference of liquid-phase content during sintering. Microstructural changes were observd with the depth of about 250${\mu}{\textrm}{m}$ from he surface. The grain size and aspect ratio of SiC in the interior are larger than those in the surface region and the rate of transforma-tion of $\beta$-to $\alpha$-SiC during sintering is higher in the interior than that in the surface region.

  • PDF

탄화규소 소결체의 기계적 특성 및 마찰마모 (The Mechanical and Tribological Properties of Silicon Carbide Bodies)

  • 이승훈;김홍기;김영호;이경희
    • 한국세라믹학회지
    • /
    • 제31권11호
    • /
    • pp.1307-1314
    • /
    • 1994
  • The aim of this work is to show the way of manufacturing the SiC mechanical seal at the low temperature of 130$0^{\circ}C$ using clay and frit as source of secondary phase. $\alpha$-SiC and $\beta$-SiC powder which showed different distribution of particle were used as starting materials, i.e. average particle size of $\alpha$-SiC was larger than that of $\beta$-SiC. The mechanical and tribological properties of two groups of specimen, i.e. one contained mainly larger $\alpha$-SiC powder and the other mainly fine particle $\beta$-SiC, were measured. The specimen consisted of larger $\alpha$-SiC exhibited lower density flexural strength and wear resistance is comparison with these of sample containning mainly $\beta$-SiC . This difference could be originated from the dependence of capillary force on the particle size. For the larger SiC particle, the liquid phase may not fill the whole pores during sintering, due to low capillary force, whereas the liquid phase can infiltrate into the small ores surrounded small $\beta$-SiC particle. Thus, the course of high flexural strength and high wear resistance of specimen prepared using small particles can be explaced from the easy infiltration of liquid phase.

  • PDF

2 상 Ti3Al-xNb 계 금속간 화합물들의 초소성 특성에 미치는 상분율의 영향 (Effects of α2/β Volume Fraction on the Superplastic Deformation)

  • 김지식
    • 소성∙가공
    • /
    • 제11권5호
    • /
    • pp.447-456
    • /
    • 2002
  • A study has been made to investigate the boundary sliding and its accommodation mode with respect to the variation of $\alpha$$_2$/$eta$ volume fraction during superplastic deformation of two-phase Ti$_3$Al-xNb intermetallics. Step strain rate and load relaxation tests have been performed at 950, 970 and 99$0^{\circ}C$ to obtain the flow stress curves and to analyze the deformation characteristics by the theory of inelastic deformation. The results show that the grain matrix deformation and boundary sliding of the three intermetallics containing 21, 50 and 77% in $eta$ volume fractions are well described by the plastic deformation and viscous flow equations. Due to the equal accommodation of both $a^2$ and $\beta$ phases, the accommodation modes for fine-grained materials are in good agreement with the iso-strain rate models. The sliding resistance analyzed for the different boundaries is the lowest in the $\alpha$$_2$/$\alpha$$_2$ boundary, and increases in the order of $\alpha$$_2$/$\alpha$$_2$<< $\alpha$$_2$/$\beta$ = $\beta$/$\beta$, which plays an important role in controlling the superplasticity of the alloys with the various $\alpha$$_2$/$\beta$ phase ratio.

Expression of Cytokines in Radiation Injured Brain at Acute Phase

  • Lee, Jang-Bo;Kim, Min-Ho;Chung, Yong-Gu;Park, Jung-Yul
    • Journal of Korean Neurosurgical Society
    • /
    • 제42권3호
    • /
    • pp.200-204
    • /
    • 2007
  • Objective : Radiation therapy is an important treatment for brain tumor. However, serious complications such as radiation necrosis can occur and it may be secondary to the expression of acute phase genes, like cytokines. In particular, inflammatory cytokines (IL-$1{\beta}$, TNF-${\alpha}$) and other immunomodulatory cytokines (TNF-${\alpha}$, TGF-${\beta}1$) might be changed after irradiation (high single dose irradiation). Although it has been reported that IL-1 level is remarkably elevated within 8 week after the irradiation to the rat brain. the change of cytokines levels at acute phase (within 24 hours) has not been reported. In the present study, we examined TNF-${\alpha}$, TGF-${\beta}1$, and IL-$1{\beta}$ levels in acute phase to clarify the early effect of cytokines on the radiation-induced brain damage. Methods : Fifty Sprague-Dawley rats were used and these were divided into irradiation group and control group. After a burr-hole trephination on the right parietal area using a drill, a single 10Gy was irradiated at the trephined site. Their forebrains were extirpated at 30 min, 2 hr, 8 hr, 12 hr and 24 hr, respectively and examined for the expression of TNF-${\alpha}$, TGF-${\beta}1$, and IL-$1{\beta}$. Results : The expression of TNF-${\alpha}$ and TGF-${\beta}1$ were decreased until 12 hr after irradiation but elevated thereafter. The expression of IL-1 was peak at 8 hr and then decreased until 12 hr but elevated after this time window. The present study indicated that expression of cytokines (TNF-${\alpha}$, TGF-${\beta}1$ and IL-$1{\beta}$) were increased at 24 hr after the irradiation to the rat brain. IL-$1{\beta}$ level, on the other hand. reached peak at 8 hr after radiation injury. Conclusion : These findings indicate that IL-1, among various cytokines, may have a more important role in the inflammatory reaction by radiation injury at acute phase and provide some clues for better understanding of the pathogenesis of radiation injury.

The Influence of Temperature, Ultrasonication and Chiral Mobile Phase Additives on Chiral Separation: Predominant Influence of β-Cyclodextrin Chiral Mobile Phase Additive Under Ultrasonic Irradiation

  • Lee, Jae Hwan;Ryoo, Jae Jeong
    • Bulletin of the Korean Chemical Society
    • /
    • 제33권12호
    • /
    • pp.4141-4144
    • /
    • 2012
  • This paper introduces a technique for resolving amino acids that combines the advantages of the conventional CSP (chiral stationary phase) method with the CMPA (chiral mobile phase additive) method. A commercially available chiral crown ether column, CROWNPAK CR(+), was used as the CSP and three cyclodextrins (${\beta}$-CD, ${\gamma}$-CD, HP-${\beta}$-CD) were used as the mobile phase additives. Chromatographic resolution was performed at $25^{\circ}C$ and $50^{\circ}C$ with or without sonication. A comparison of the chromatographic results under ultrasonic conditions with those under non-ultrasonic conditions showed that ultrasound decreased the elution time and enantioselectivity at all temperatures. In the case of the ${\beta}$-CD mobile phase additive, the elution time and enantioselectivity under ultrasonic condition were significantly higher than under non-sonic condition at all temperatures. Commercially available Chiralpak AD, Whelk-O2 and Pirkle 1-J columns were used as CSPs to examine more meticulously the effects of ultrasonication and temperature on the optical resolution. The optical resolution of some chiral samples analyzed at $25^{\circ}C$ and $50^{\circ}C$ with or without sonication was compared. As in the previous case, the enantioselectivity was lower at $25^{\circ}C$ but similar enantioselectivity was observed at $50^{\circ}C$.

방전플라즈마 소결에 의한 자기 통전식 SiC계 세라믹 발열체 개발 (Development of Electroconductive SiC Ceramic Heater by Spark Plasma Sintering)

  • 신용덕;최원석;고태헌;이정훈;주진영
    • 전기학회논문지
    • /
    • 제58권4호
    • /
    • pp.770-776
    • /
    • 2009
  • The composites were fabricated by adding 0, 15, 30, 45[vol.%] $ZrB_2$ powders as a second phase to SiC matrix. The physical, mechanical and electrical properties of electroconductive SiC ceramic composites by spark plasma sintering(SPS) were investigated. Reactions between ${\beta}$-SiC and $ZrB_2$ were not observed in the XRD and the phase analysis of the electroconductive SiC ceramic composites. The relative density of mono ${\beta}$-SiC, ${\beta}$-SiC+15[vol.%]$ZrB_2$, ${\beta}$-SiC+30[vol.%]$ZrB_2$ and ${\beta}$-SiC+45[vol.%]$ZrB_2$ composites are respectively 99.24[%], 87.53[%], 96.41[%] and 98.11[%] Phase analysis of the electroconductive SiC ceramic composites by XRD revealed mostly of ${\beta}$-SiC, $ZrB_2$ and weakly of $ZrO_2$ phase. The flexural strength showed the lowest of 114.44[MPa] for ${\beta}$-SiC+15[vol.%]$ZrB_2$ powders and showed the highest of 210.75[MPa] for composite no added with $ZrB_2$ powders at room temperature. The trend of the mechanical properties of the electroconductive SiC ceramic composites is accorded with the trend of the relative density. The electrical resistivity of the electroconductive SiC ceramic composites decreased with increased $ZrB_2$ contents. The electrical resistivity of mono ${\beta}$-SiC, ${\beta}$-SiC+15[vol.%]$ZrB_2$, ${\beta}$-SiC+30[vol.%]$ZrB_2$ and ${\beta}$-SiC+45[vol.%]$ZrB_2$ composites are respectively $4.57{\times}10^{-1},\;2.13{\times}10^{-1},\;2.68{\times}10^{-2}\;and\;1.99{\times}10^{-2}[{\Omega}{\cdot}cm]$ at room temperature. The electrical resistivity of mono ${\beta}$-SiC and ${\beta}$-SiC+15[vol.%]$ZrB_2$ are negative temperature coefficient resistance(NTCR) in temperature ranges from $25[^{\circ}C]\;to\; 100[^{\circ}C]$. The electrical resistivity of ${\beta}$-SiC+30[vol.%]$ZrB_2$ and ${\beta}$-SiC+45[vol.%]ZrB_2$ are positive temperature coefficient resistance(PTCR) in temperature ranges from $25[^{\circ}C]\;to\;100[^{\circ}C]$. It is convinced that ${\beta}$-SiC+30[vol.%]$ZrB_2$ composites by SPS for heater or ignitors can be applied.

진공증착법을 이용한 철프탈로시아닌 박막의 합성과 그 특성 (Preparation and Characterization of Iron Phthalocyanine Thin Films by Vacuum Sublimation)

  • 지종기;이재구;황동욱;임윤묵;양현수;류해일;박하선
    • 공업화학
    • /
    • 제10권5호
    • /
    • pp.644-651
    • /
    • 1999
  • 본 연구에서는 진공 증착법을 이용하여 철프탈로시아닌(FePc) 박막을 실리콘 웨이퍼와 알루미나 기판 위에 합성하였으며, 박막의 증착 온도와 두께를 변화시켜 실험한 후 일부의 박막을 열처리하였다. 박막의 두께 변화에 따른 표면 구조 변화, 상전이와 전기 저항 감도 변화를 SEM, XRD, 그리고 전기저항의 측정으로 관찰하였다. 증착 온도가 $370^{\circ}C$에서 $350^{\circ}C$로 감소함에 따라 $\alpha$상의 (200)면, (011)면, (211)면, 그리고 (114)면이 사라지며 $\beta$상의 (100)면의 피크가 나타났다. 전구물질의 양을 달리하며 고속 증착시켜 박막 두께를 조절한 결과, 두께 증가에 따라 결정 크기가 증가하고 또한 $\alpha$상에서 $\beta$상으로의 상 전이가 일어남을 알 수 있었다. 열처리한 박막의 결정성을 측정한 결과 열처리 온도가 증가함에 따라 $150^{\circ}C$으로부터 $\alpha$상에서 $\beta$상으로의 상 전이가 일어나기 시작하여 $350^{\circ}C$에서 완전히 $\beta$상으로 전이되었다. $NO_x$에 대한 철프탈로시아닌 박막의 온도에 따른 전기저항감도를 측정한 결과 박막의 두께가 얇을수록 더 좋고 안정된 전기 저항 감도를 보여주었다. 즉 박막의 표면구조가 조밀하게 성장할수록 전기 저항 감도가 더욱 좋아짐을 확인하였다.

  • PDF

기계적 합금화 Iron Silicide의 열간성형 및 열처리에 의한 상변화 (Phase Transformation During Hot Consolidation and Heat Treatments in Mechanically Alloyed Iron Silicide)

  • 어순철;김일호;황승준;조경원;최재화
    • 한국재료학회지
    • /
    • 제11권12호
    • /
    • pp.1068-1073
    • /
    • 2001
  • An n-type iron$silicide(Fe_{0.98}Co_{0.02}Si_2)$has been produced by mechanical alloying process and consolidated by vacuum hot pressing. Although as-milled powders after 120 hours of milling did not show an alloying progress,${\beta}-FeSi_2$phase transformation was induced by isothermal annealing at$830{\circ}C$for 1 hour, and the fully transformed${\beta}-FeSi_2$phase was obtained after 4 hours of annealing. Near fully dense specimen was obtained after vacuum hot pressing at$ 1100{\circ}C$with a stress of 60MPa. However, as-consolidated iron silicides were consisted of untransformed mixture of ${\Alpha}-Fe_2Si_5$and ${\varepsilon-FeSi$phases. Thus, isothermal annealing has been carried out to induce the transformation to a thermoelectric semiconducting${\beta}-FeSi_2$phase. The condition for${\beta}-FeSi_2$transformation was investigated by utilizing DTA, SEM, and XRD analysis. The phase transformation was shown to be taken place by a vacuum isothermal annealing at$830{\circ}C$and the transformation behaviour was investigated as a function of annealing time. The mechanical properties of${\beta}-FeSi_2$materials before and after isothermal annealing were characterized in this study.

  • PDF