Effect of storage time on chemical structure of a single-bottle and a two-bottle experimental ceramic primer and micro-shear bond strength of composite to ceramic

  • Armaghan Naghili (Department of Operative Dentistry, Faculty of Dentistry, Tabriz Medical Sciences, Islamic Azad University) ;
  • Amirparsa Ghasemi (Department of Biological Sciences, University of Maryland) ;
  • Amir Ghasemi (Dental Research Center, Research Institute of Dental Sciences, School of Dentistry, Shahid Beheshti University of Medical Sciences) ;
  • Narges Panahandeh (Dental Research Center, Research Institute of Dental Sciences, School of Dentistry, Shahid Beheshti University of Medical Sciences)
  • Received : 2023.11.28
  • Accepted : 2024.06.14
  • Published : 2024.06.30

Abstract

PURPOSE. This study assessed the effect of storage time on chemical structure of a single-bottle and a two-bottle experimental ceramic primer and micro-shear bond strength (µSBS) of composite to ceramic. MATERIALS AND METHODS. This study was conducted on 60 sintered zirconia and 60 feldspathic porcelain blocks. Half of the specimens (n = 30) were subjected to surface treatment with the single-bottle Clearfil ceramic primer (n = 15) and two-bottle experimental primer (n = 15) after 24 hours. The remaining half received the same surface treatments after 6 months storage in distilled water. Composite cylinders were bonded to the ceramics, and they were then subjected to µSBS test. Also, the primers underwent Fourier-transform infrared spectroscopy (FTIR) after 24 hours and 6 months to assess their chemical structure. Data were analyzed with 3-way ANOVA and adjusted Bonferroni test (alpha = 0.05). RESULTS. The µSBS of both ceramics significantly decreased at 6 months in one-bottle ceramic primer group (P = .001), but it was not significantly different from the two-bottle experimental primer group (P = .635). FTIR showed hydrolysis of single-bottle primer, cleavage of silane and 10-MDP bonds, and formation of siloxane bonds after 6 months. CONCLUSION. Six months of storage caused significant degradation of single-bottle ceramic primer, and consequently had an adverse effect on µSBS.

Keywords

References

  1. Ikemura K, Tanaka H, Fujii T, Deguchi M, Endo T, Kadoma Y. Development of a new single-bottle multi-purpose primer for bonding to dental porcelain, alumina, zirconia, and dental gold alloy. Dent Mater J 2011;30:478-84.  https://doi.org/10.4012/dmj.2010-182
  2. Mohammadi N, Shakur Shahabi M, Kimyai S, Pournagi Azar F, Ebrahimi Chaharom ME. Shear bond strengths of methacrylate- and silorane-based composite resins to feldspathic porcelain using different adhesive systems. J Dent Res Dent Clin Dent Prospects 2015;9:181-7.  https://doi.org/10.15171/joddd.2015.033
  3. Keul C, Liebermann A, Roos M, Uhrenbacher J, Stawarczyk B. The effect of ceramic primer on shear bond strength of resin composite cement to zirconia: a function of water storage and thermal cycling. J Am Dent Assoc 2013;144:1261-71.  https://doi.org/10.14219/jada.archive.2013.0055
  4. Hooshmand T, van Noort R, Keshvad A. Storage effect of a pre-activated silane on the resin to ceramic bond. Dent Mater 2004;20:635-42.  https://doi.org/10.1016/j.dental.2003.08.005
  5. Yazdi FM, Moosavi H, Atai M, Zeynali M. Dentin bond strength and degree of conversion evaluation of experimental self-etch adhesive systems. J Clin Exp Dent 2015;7:e243-9.  https://doi.org/10.4317/jced.51842
  6. Lung CY, Matinlinna JP. Aspects of silane coupling agents and surface conditioning in dentistry: an overview. Dent Mater 2012;28:467-77.  https://doi.org/10.1016/j.dental.2012.02.009
  7. Yoshihara K, Nagaoka N, Sonoda A, Maruo Y, Makita Y, Okihara T, Irie M, Yoshida Y, Van Meerbeek B. Effectiveness and stability of silane coupling agent incorporated in 'universal' adhesives. Dent Mater 2016;32:1218-25.  https://doi.org/10.1016/j.dental.2016.07.002
  8. Nishiyama N, Asakura T, Horie K. Condensation behavior of a sulane coupling agent in the presence of colloidal silica studied by 29Si and 13C NMR. J Colloid Interface Sci 1988;124:14-21.  https://doi.org/10.1016/0021-9797(88)90319-0
  9. Hooshmand T, van Noort R, Keshvad A. Bond durability of the resin-bonded and silane treated ceramic surface. Dent Mater 2002;18:179-88.  https://doi.org/10.1016/S0109-5641(01)00047-1
  10. Lung CY, Botelho MG, Heinonen M, Matinlinna JP. Resin zirconia bonding promotion with some novel coupling agents. Dent Mater 2012;28:863-72.  https://doi.org/10.1016/j.dental.2012.04.023
  11. Feitosa VP, Ogliari FA, Van Meerbeek B, Watson TF, Yoshihara K, Ogliari AO, Sinhoreti MA, Correr AB, Cama G, Sauro S. Can the hydrophilicity of functional monomers affect chemical interaction? J Dent Res 2014;93:201-6.  https://doi.org/10.1177/0022034513514587
  12. Aida M, Wakami M, Watanabe T, Omura Y, Nishiyama N. Effects from applying adhesive agents onto silanated porcelain surface on the resin bond durability. Dent Mater J 2008;27:427-32.  https://doi.org/10.4012/dmj.27.427
  13. Nihei T. Dental applications for silane coupling agents. J Oral Sci 2016;58:151-5.  https://doi.org/10.2334/josnusd.16-0035
  14. Li R. Development of a ceramic primer with higher bond durability for resin cement. J Oral Rehabil 2010;37:560-8.  https://doi.org/10.1111/j.1365-2842.2010.02060.x
  15. Luhrs AK, Pongprueksa P, De Munck J, Geurtsen W, Van Meerbeek B. Curing mode affects bond strength of adhesively luted composite CAD/CAM restorations to dentin. Dent Mater 2014;30:281-91.  https://doi.org/10.1016/j.dental.2013.11.016
  16. Kim RJ, Woo JS, Lee IB, Yi YA, Hwang JY, Seo DG. Performance of universal adhesives on bonding to leucite-reinforced ceramic. Biomater Res 2015;19:1-6.  https://doi.org/10.1186/s40824-014-0026-7
  17. Kalavacharla VK, Lawson NC, Ramp LC, Burgess JO. Influence of etching protocol and silane treatment with a universal adhesive on lithium disilicate bond strength. Oper Dent 2015;40:372-8.  https://doi.org/10.2341/14-116-L
  18. Passia N, Lehmann F, Freitag-Wolf S, Kern M. Tensile bond strength of different universal adhesive systems to lithium disilicate ceramic. J Am Dent Assoc 2015;146:729-34.  https://doi.org/10.1016/j.adaj.2015.04.008
  19. Ghasemi A, Sadr A, Pourhashemi A. Effect of storage time of a ceramic primer on microshear bond strength to zirconia. J Dent (Tehran) 2018;15:375-81.  https://doi.org/10.18502/jdt.v15i6.331
  20. Anagnostopoulos T, Eliades G, Palaghias G. Composition, reactivity and surface interactions of three dental silane primers. Dent Mater 1993;9:182-90.  https://doi.org/10.1016/0109-5641(93)90118-A
  21. de Rosatto CM, Roscoe MG, Novais VR, Menezes Mde S, Soares CJ. Effect of silane type and air-drying temperature on bonding fiber post to composite core and resin cement. Braz Dent J 2014;25:217-24.  https://doi.org/10.1590/0103-6440201300005
  22. Matsumura H, Kato H, Atsuta M. Shear bond strength to feldspathic porcelain of two luting cements in combination with three surface treatments. J Prosthet Dent 1997;78:511-7.  https://doi.org/10.1016/S0022-3913(97)70068-4
  23. Ozcan M, Valandro LF, Amaral R, Leite F, Bottino MA. Bond strength durability of a resin composite on a reinforced ceramic using various repair systems. Dent Mater 2009;25:1477-83.  https://doi.org/10.1016/j.dental.2009.06.020
  24. Aoki N, Kimoto S, Tanimura H, Nishiyama N, Aida M. Effects of degree of dissociation of acid used on hydrolytic durability of ceramic primer. Dent Mater J 2014;33:614-20.  https://doi.org/10.4012/dmj.2013-319
  25. Goto H. Aging effect of one bottle-type ceramic primer on bonding efficacy of resin cement. Nihon Hotetsu Shika Gakkai Zasshi 2008;52:107-16.  https://doi.org/10.2186/jjps.52.107
  26. Teshima I. Degradation of 10-methacryloyloxydecyl dihydrogen phosphate. J Dent Res 2010;89:1281-6. https://doi.org/10.1177/0022034510379018