Corrosion of Containment Alloys in Molten Salt Reactors and the Prospect of Online Monitoring

  • Received : 2021.07.27
  • Accepted : 2021.09.23
  • Published : 2022.03.30

Abstract

The aim of this review is to communicate some essential knowledge of the underlying mechanism of the corrosion of structural containment alloys during molten salt reactor operation in the context of prospective online monitoring in future MSR installations. The formation of metal halide species and the progression of their concentration in the molten salt do reflect containment corrosion, tracing the depletion of alloying metals at the alloy salt interface will assure safe conditions during reactor operation. Even though the progress of alloying metal halides concentrations in the molten salt do strongly understate actual corrosion rates, their prospective 1st order kinetics followed by near-linearly increase is attributed to homogeneous matrix corrosion. The service life of the structural containment alloy is derived from homogeneous matrix corrosion and near-surface void formation but less so from intergranular cracking (IGC) and pitting corrosion. Online monitoring of corrosion species is of particular interest for molten chloride systems since besides the expected formation of chromium chloride species CrCl2 and CrCl3, other metal chloride species such as FeCl2, FeCl3, MoCl2, MnCl2 and NiCl2 will form, depending on the selected structural alloy. The metal chloride concentrations should follow, after an incubation period of about 10,000 hours, a linear projection with a positive slope and a steady increase of < 1 ppm per day. During the incubation period, metal concentration show 1st order kinetics and increasing linearly with time1/2. Ideally, a linear increase reflects homogeneous matrix corrosion, while a sharp increase in the metal chloride concentration could set a warning flag for potential material failure within the projected service life, e.g. as result of intergranular cracking or pitting corrosion. Continuous monitoring of metal chloride concentrations can therefore provide direct information about the mechanism of the ongoing corrosion scenario and offer valuable information for a timely warning of prospective material failure.

Keywords

Acknowledgement

Pacific Northwest National Laboratory is operated by Battelle Memorial Institute for the U.S. Department of Energy under Contract No. DE-AC05-76RL01830. This work was supported by the U.S. Department of Energy, Office of Nuclear Energy.

References

  1. E.S. Bettis, R.W. Schroeder, G.A. Cristy, H.W. Savage, R.G. Affel, and L.F. Hemphill, "The Aircraft Reactor Experiment-Design and Construction", Nucl. Sci. Eng., 2, 804-825 (1957). https://doi.org/10.13182/NSE57-A35495
  2. W.D. Manly, G.W. Adams, J.H. Coobs, J.H. DeVan, D.A. Douglas, E.E. Hoffman, and P. Patriarca. Aircraft Reactor Experiment - Metallurgical Aspects, Oak Ridge National Laboratory Report, 29, ORNL-2349 (1957).
  3. W.D. Manly, J.H. Coobs, and J.H. DeVan, "Metallurgical Problems in Molten Fluoride Systems", Prog. Nucl. Energy, 2, 4 (1960).
  4. J.H. DeVan and R.B. Evans. Corrosion Behavior of Reactor Materials in Fluoride Salt Mixtures, Oak Ridge National Laboratory Technical Report, ORNL/TM-328 (1962).
  5. V. Ignatiev and A. Surenkov, "5.10-Material Performance in Molten Salts", in: Comprehensive Nuclear Materials, R.J.M. Konings, eds., 221-250, Elsevier, Amsterdam (2012).
  6. J.R. DiStefano, J.H. DeVan, J.R. Keiser, R.L. Klueh, and W.P. Eathery, "Materials Consideration for Molten Salt Accelerator-based Plutonium Conversion Systems", Oak Ridge National Laboratory Report, Oak Ridge National Laboratory, ORLN/TM-12925 (1995).
  7. Elysium Industries. "The Molten Chloride Salt Fast Reactor." Elysium Industries. Accessed Apr. 08 2021. Available from: http://www.elysiumindustries.com/technology.
  8. TerraPower LLC. "TerraPower's Molten Chloride Fast Reactor Technology: Retooling Nuclear for a Changing Energy Sector." TerraPower LLC. Accessed Apr. 08 2021. Available from: https://www.terrapower.com/wp-content/uploads/2020/08/TP_2020_MCFR_Technology_082020.pdf.
  9. Moltex Energy. "Moltex's Stable Salt Reactor - Waste-burner (SSR-W) Uses the Nuclear Waste From Past and Present Operations as Fuel, Significantly Reducing Waste Stockpiles." Moltex Energy. Accessed Apr. 08 2021. Available from: https://www.moltexenergy.com/reduces-waste/.
  10. D.E. Holcomb, G.F. Flanagan, B.W. Patton, J.C. Gehin, R.L. Howard, and T.J. Harrison. Fast Spectrum Molten Salt Reactor Options, Oak Ridge National Laboratory Report, ORNL/TM-2011/105 (2011).
  11. O. Benes and R.J.M. Konings, "Thermodynamic Evaluation of NaCl-MgCl2-UCl3-PuCl3 System", J. Nucl. Mater., 375(2), 202-208 (2008). https://doi.org/10.1016/j.jnucmat.2008.01.007
  12. R.E. Thoma. Phase Diagrams of Nuclear Reactor Materials, Oak Ridge National Laboratory Technical Report, ORNL 2548 (1959).
  13. J.W. Koger. Alloy Compatibility With LiF-BeF2 Salts Containing ThF4 and UF4, Oak Ridge National Laboratory Report, ORNL/TM-4286 (1972).
  14. J.A. Lane, H.G. MacPherson, and F. Maslan, Fluid Fuel Reactors, Addison-Wesley Publishing Company Inc., Massachusetts (1958).
  15. J. Busby, L.M. Garrison, L. Lin, S.S. Raiman, S. Sham, C. Silva, H. Wang, R. Iyengar, and G. Tartal. Technical Gap Assessment for Materials in Component Integrity Issues for Molten Salt Reactors, Oak Ridge National Laboratory Technical Report, ORNL/SPR-2019/1089 (2019).
  16. Australian Stainless Steel Development Association. "304: The Place to Start." ASSDA. Accessed Apr. 08 2021. Available from: https://www.assda.asn.au/technical-info/grade-selection/304-the-place-to-start.
  17. Australian Stainless Steel Development Association. "316: The First Step up." ASSDA. Accessed Jul. 30 2020. Available from: https://www.assda.asn.au/technical-info/grade-selection/316-the-first-step-up.
  18. J.R. Keiser, J.H. Devan, and E.J. Lawrence, "Compatibility of Molten Salts With Type 316 Stainless Steel and Lithium", J. Nucl. Mater., 85-86, 295-298 (1979). https://doi.org/10.1016/0022-3115(79)90505-1
  19. C.F. Baes, "The Chemistry and Thermodynamics of Molten Salt Reactor Fuels", J. Nucl. Mater., 51(1), 149-162 (1974). https://doi.org/10.1016/0022-3115(74)90124-X
  20. J.A. Plambeck, "Electromotive Force Series in Molten Salts", J. Chem. Eng. Data, 12(1), 77-82 (1967). https://doi.org/10.1021/je60032a023
  21. S. Guo, J. Zhang, W. Wu, and W. Zhou, "Corrosion in the Molten Fluoride and Chloride Salts and Materials Development for Nuclear Applications", Prog. Mater. Sci., 97, 448-487 (2018). https://doi.org/10.1016/j.pmatsci.2018.05.003
  22. J.W. Koger. Evaluation of Hastelloy N Alloys After Nine Years Exposure to Both a Molten Fluoride Salt and air at Temperatures From 700 to 560℃, Oak Ridge National Laboratory Report, ORNL/TM-4189 (1972).
  23. R.B. Evans, J.H. DeVan, and G.M. Watson. Self-diffusion in Nickel-base Alloys, Oak Ridge National Laboratory Report, ORNL-2982 (1961).
  24. Z. Tokei, K. Hennesen, H. Viefhaus, and H.J. Grabke, "Diffusion of Chromium in Ferritic and Austenitic 9-20wt% Chromium Steels", Mater. Sci. Technol., 16(10), 1129-1138 (2000). https://doi.org/10.1179/026708300101507055
  25. L.G. Harrison, "Influence of Dislocations on Diffusion Kinetics in Solid With Particular Reference to the Alkali Halides", Trans. Faraday Soc., 57, 1191-1199 (1961). https://doi.org/10.1039/TF9615701191
  26. M. Mizouchi, Y. Yamazaki, Y. Iijima, and K. Arioka, "Low Temperature Grain Boundary Diffusion of Chromium in SUS316 and 316L Stainless Steel", Mater. Trans., 45(10), 2945-2950 (2004). https://doi.org/10.2320/matertrans.45.2945
  27. T. Suzuoka, "Lattice and Grain Boundary Diffusion in Polycrystals", Trans. Jpn. Inst. Met., 2(1), 25-32 (1961). https://doi.org/10.2320/matertrans1960.2.25
  28. G.B. Gibbs, "Grain Boundary Impurity Diffusion", Phys. Status Solidi B, 16(1), K27-K29 (1966). https://doi.org/10.1002/pssb.19660160143
  29. R.A. Perkins, R.A. Padgett, and N.K. Tunali, "Tracer Diffusion of 59Fe and 51Cr in Fe-17 wt Pct Cr-12 wt Pct Ni Austenitic Alloy", Metall. Mater. Trans. B, 4, 2535-2540 (1973). https://doi.org/10.1007/BF02644255
  30. A.F. Smith, "The Diffusion of Chromium in Type 316 Stainless Steel", Met. Sci., 9(1), 375-378 (1975). https://doi.org/10.1179/030634575790444270
  31. J. Cermak, "Grain Boundary Self-diffusion of 51Cr in Fe-Cr-Ni Alloys", Z. Metallkd., 81(3), 193-195 (1990).
  32. A.P. Sutton and R.W. Balluffi, Interfaces in Crystalline Materials, Clarendon Press, Oxford (1995).
  33. S.S. Raimanm and S. Lee, "Aggregation and Data Analysis of Corrosion Studies in Molten Chloride and Fluoride Salts", J. Nucl. Mater., 511, 523-535 (2018). https://doi.org/10.1016/j.jnucmat.2018.07.036
  34. J.R. Keiser, D.L. Manning, and R.E. Clausing, "Corrosion Resistance of Some Nickel-Based Alloys in Molten Fluoride Salts Containing UF4 and Tellurium", Proc. of the 1st Int. Symp. On Molten Salts, vol.1976-6, 315-328, The Electrochemical Society, New York (1976).
  35. J.R. Keiser. Compatibility Studies of Potential Molten-Salt Breeder Reactor Materials in Molten Fluoride Salts, Oak Ridge National Laboratory Report, ORNL/TM-5783 (1977).
  36. G.S. Was, J. Busby, and P.L. Andresen, "Effect of Irradiation on Stress-Corrosion Cracking and Corrosion in Light Water Reactors", in: Corrosion: Environments and Industries, S.D. Cramer and B.S. Covino, eds., vol. 13C, 386-414, ASM International, Ohio (2006).
  37. T.R. Allen and J.T. Busby, "Radiation Damage Concerns for Extended Light Water Reactor Service", JOM, 61(7), 29-34 (2009). https://doi.org/10.1007/s11837-009-0099-2
  38. F.A. Garner, "Irradiation Performance of Cladding and Structural Steels in Liquid Metal Reactors", in: Materials Science and Technology - A Comprehensive Treatment, R.W. Cahn, P. Haasen, and E.J. Kramer, eds., 419-543, VCH Publishers Inc., New York (1994).