DOI QR코드

DOI QR Code

A Method of Measuring Wood Failure Percentage of Wood Specimens Bonded with Melamine-Urea-Formaldehyde Resins Using I mage Analysis

  • KIM, Minseok (Department of Wood and Paper Science, Kyungpook National University) ;
  • PARK, Byung-Dae (Department of Wood and Paper Science, Kyungpook National University)
  • Received : 2021.02.04
  • Accepted : 2021.05.20
  • Published : 2021.05.25

Abstract

Transparent and colorless melamine-urea-formaldehyde (MUF) resins make it difficult to identify the area of wood failure percentage (WFP) in the fracture surface of bonded wood specimens. Therefore, in this study, we develop a method of measuring WFP after the adhesion strength measurement of MUF resins under shear stress. The fractured wood surface of b lock shear strength (BSS) specimens bonded with cold-setting MUF resins at three melamine contents (20%, 30%, and 40%) was marked black, and then, WFP was accurately measured via image analysis. WFP values measured using this method consistently increased with BSS as the melamine content increased, showing the reliability of this new method. The results suggested that this new method is useful and reliable for measuring the WFP of the fracture surface of wood specimens bonded with colorless adhesives such as urea-formaldehyde, MUF, and melamine-formaldehyde resins.

Keywords

Acknowledgement

This work is supported by the Korea Forestry Promotion Institute (Grant No. 2019143D10-1921-AB01)

References

  1. Aydin, I. 2004. Activation of wood surfaces for glue bonds by mechanical pre-treatment and its effects on some properties of veneer surfaces and plywood panels. Applied Surface Science. 233(1-4): 268-274. https://doi.org/10.1016/j.apsusc.2004.03.230
  2. Baxter GE. Kreibich RE. 1973. A fast curing phenolic adhesive system. Forest Products Journal 23: 17-22.
  3. Cameron, F.A. Pizzi, A. 1985. Effect of excessive pretreatment of pine timber with CCA wood preservatives on the bond quality of PRF and TRF wood adhesives. European Journal of Wood and Wood Products 43(4): 149-151. https://doi.org/10.1007/BF02619403
  4. Choi, G.W., Yang, S.M., Lee, H.J., Kim, J.H., Choi, K. H., Kang, S.G. 2020. A Study on the Block Shear Strength according to the Layer Composition of an d Adhesive Type of Ply-Lam CLT. Journal of the Ko rean Wood Science and Technology 48(6): 791-806. https://doi.org/10.5658/WOOD.2020.48.6.791
  5. Clauss, S., Joscak, M., Niemz, P. 2011. Thermal stability of glued wood joints measured by shear tests. European Journal of Wood and Wood Products. 69(1): 101-111. https://doi.org/10.1007/s00107-010-0411-4
  6. Collett, B.M. 1972. A review of surface and interfacial adhesion in wood science and related fields. Wood Science and Technolgy. 6: 1-42. https://doi.org/10.1007/BF00351806
  7. Dunky, M. 1998. Urea-formaldehyde (UF) adhesive resins for wood. International Journal of Adhesion and Adhesives 18(2): 95-107. https://doi.org/10.1016/S0143-7496(97)00054-7
  8. Ellis, S. 1995. Correlation of waferboard internal bond and wood failure as measured by image analysis. Wood and Fiber Science 27(1): 79-83.
  9. Frihart, C.R., Brandon, R., Ibach, R. 2004. Selectivity of Bonding for Modified Wood. The Adhesion Society 7: 329-332.
  10. Frihart, C.R., Hunt, C.G. 2010. Adhesives with wood materials-bond formation and performance. Wood Handbook. 1: 10.1-10.24. General Technical Report FPL-GTR-190 Chapter 10.
  11. Galih, N.M.G., Yang, S.M., Yu, S.M., Kang, S.G. 2020. Study on the Mechanical Properties of Tropical Hybrid Cross Laminated Timber Using Bamboo Laminated Board as Core Layer. Journal of the Korean Wood Science and Technology 48(2): 245-252. https://doi.org/10.5658/WOOD.2020.48.2.245
  12. Glavinic, I.U., Boko, I., Toric, N., Vrankovic, J.L. 2020. Application of hardwood for glued laminated timber in Europe. Journal of the Croation Association of Civil Enginners 72(7): 607-616. https://doi.org/10.14256/JCE.2741.2019
  13. Hendrik, J., Hadi, Y.S., Massijaya, M.Y., Santoso, A., Pizzi, A. 2019, Properties of Glued Laminated Timber Made from Fast-growing Species with Mangium Tannin and Phenol Resorcinol Formaldehyde Adhesives. Journal of the Korean Wood Science and Technology 47(3): 253-264. https://doi.org/10.5658/WOOD.2019.47.3.253
  14. Hong, M.K., Park, B.D. 2017. Performance of Melamine-Urea-Formaldehyde Resin Adhesives at Various Melamine Contents for Bonding Glued Laminated Timber under High Frequency Heating. Journal of the Korean Wood Science and Technology 45(4): 409-18. https://doi.org/10.5658/WOOD.2017.45.4.409
  15. Hse, C.Y. 1972. Wettability of southern pine veneer by phenol formaldehyde wood adhesives. Forest Products Journal 22(1): 51-56.
  16. Jeong, B., Park, B.D. 2019. Performance of Urea-Formaldehyde Resins Synthesized at Two Different Low Molar Ratios with Different Numbers of Urea Addition, Journal of the Korean Wood Science and Technology 47(2): 221-228. https://doi.org/10.5658/WOOD.2019.47.2.221
  17. Jeong, B., Park, B.D., Causin, V. 2019. Influence of synthesis method and melamine content of urea-melamine-formaldehyde resins to their features in cohesion, interphase, and adhesion performance. Journal of Industrial and Engineering Chemistry 79: 87-96. https://doi.org/10.1016/j.jiec.2019.05.017
  18. Jeong, B., Park, B.D., Causin, V. 2020. Effects of Storage Time on Molecular Weights and Properties of Melamine-Urea-Formaldehyde Resins. Journal of the Korean Wood Science and Technology 48(3): 291-302. https://doi.org/10.5658/WOOD.2020.48.3.291
  19. Kamke, F.A., Lee, J.N. 2007. Adhesive penetration in wood - A review. Wood and Fiber Science 39(2): 205-220.
  20. Kenai, S. 2011. Effect of curing time on shear strength of cohesive soils stabilized with combination of lime and natural pozzolana. International Journal of Civil Engineering 9(2): 90-96
  21. Kunniger, T. 2008. A semi-automatic method to determine the wood failure percentage on shear test specimens. European Journal of Wood and Wood Products 66(3): 229-232. https://doi.org/10.1007/s00107-008-0236-6
  22. KS F 3021. 2018. Structural glued laminated timber. Korean Standards Association, 1-33
  23. KS M 3705. 2015. General Testing Methods for Adhesives. Korean Standards Association, 1-32
  24. Lhelihe, K. 2016. Cold-setting MUF resins adhesive prepared with concentrated fomaldehyde. Journal of Zhejian A & F University 33(2): 300-305.
  25. Lim, H., Tripathi, S., Sachin, Li., Minghao. 2020. Rolling shear modulus and strength of cross-laminated timber treated with micronized copper azole type C (MCA-C). Construction and Building Materials 259: 120419. https://doi.org/10.1016/j.conbuildmat.2020.120419
  26. Lim, H., Tripathi, S., Tang, J.D. 2020. Bonding performance of adhesive systems for cross-laminated timber treated with micronized copper azole type C (MCA-C). Construction and Building Materials 232(1): 117208. https://doi.org/10.1016/j.conbuildmat.2019.117208
  27. Lin, L., He, S., Fu, F., Wang, X. 2015. Detection of wood failure by image processing method: influence of algorithm, adhesive and wood species. European Journal of Wood and Wood Products 73(4): 485-491. https://doi.org/10.1007/s00107-015-0907-z
  28. Lubis, M.A.R., Park, B.D. 2020. Influence of initial molar ratios on the performance of low molar ratio urea-formaldehyde resin adhesives. Journal of the Korean Wood Science and Technology 48(2): 136-153. https://doi.org/10.5658/WOOD.2020.48.2.136
  29. Lubis, M.A.R., Park, B.D., Lee, S.-M. 2019, Performance of Hybrid Adhesives of Blocked-pMDI/Melamine-Urea-Formaldehyde Resins for the Surface Lamination on Plywood. Journal of the Korean Wood Science and Technology 47(2): 200-209. https://doi.org/10.5658/WOOD.2019.47.2.200
  30. Lubis, M.A.R., Jeong, B., Park, B.D., Lee, S.-M., Kang, E.-C. 2019. Effect of Synthesis Method and Melamine Content of Melamine-Urea-Formaldehyde Resins on Bond-Line Features in Plywood. Journal of the Korean Wood Science and Technology 47(5): 579-586. https://doi.org/10.5658/wood.2019.47.5.579
  31. Mansouri, H.R., Pizzi, A., Fredon, E. 2009. Honeymoon fast-set adhesives for glulam and fingerjoints of higher natural materials content. European Journal of Wood and Wood Products 67(2): 207-210. https://doi.org/10.1007/s00107-009-0312-6
  32. Marshall, S.J., Bayne, S.C., Baier, R., Tomsia, A.P., Marshall, G.W. 2010. A review of adhesion science. Dental Materilas 26(2): 11-16.
  33. Paris, J.L., Kamke, F. 2014. Wood-Adhesive Bondline Analyses with Micro X-ray Computed Tomography. Wood Science and Materials Science PhD: 302.
  34. Park, H.-M., Gong, D.-M., Shin, M.-G., Byeon, H.-S. 2020. Bending Creep Properties of Cross-Laminated Wood Panels Made with Tropical Hardwood and Domestic Temperate Wood. Journal of the Korean Wood Science and Technology 48(5): 608-617. https://doi.org/10.5658/WOOD.2020.48.5.608
  35. Park, J., Kim, K., Hong, S. 2004. The Bending Strength and Adhesive Properties of PRF and MUF Glulam. Journal of the Korea Furniture Society 15(2): 19-27.
  36. Pizzi, A. 2003. Melamine-Formaldehyde Adhesives. Taylor & Francis Group 32: 1-28.
  37. Properzi, M., Pizzi, A., Uzielli, L. 2001. Honeymoon MUF adhesives for exterior grade glulam. Holzforschung 59: 413-421. https://doi.org/10.1515/HF.2005.067
  38. Roh, J.K., Kim, Y.G. 2018. Bonding Properties and Resin Exudation Characteristics of Pitch Pine, Journal of Korean Wood Science and Technology 46(3): 213-220. https://doi.org/10.5658/WOOD.2018.46.3.213
  39. Sauget, A., Pizzi, A., Guillot, A., Godart, S., Apolit, R., Mezzina, M. 2014. Performance of MUF honeymoon adhesive for glulam. European Journal of Wood and Wood Products 72(5): 697-698. https://doi.org/10.1007/s00107-014-0819-3
  40. Steiger, R., Gehri, E., Richter, K. 2010. Quality control of glulam: Shear testing of bondlines. Eur. J. European Journal of Wood and Wood Products 68(3): 243-256. https://doi.org/10.1007/s00107-010-0456-4
  41. Tohmura, S.I., Inoue, A., Sahari, S.H. 2001. Influence of the melamine content in melamine-urea-formaldehyde resins on formaldehyde emission and cured resin structure. Journal of Wood Science 47(6): 451-457. https://doi.org/10.1007/BF00767897
  42. Wen, M.-Y., Zhu, J.-Z, Zhu, M., Sun, Y.-X., Park, H.-J., Shi, J. 2020, Research on Flame Retardant Formaldehyde-Free Plywood Glued by Aqueous Polymer Isocyanate Adhesive. Journal of the Korean Wood Science and Technology 48(5): 755-764. https://doi.org/10.5658/WOOD.2020.48.5.755
  43. Zanetti, M., Pizzi, A. 2001. Low addition of melamine salts for improved melamine-urea-formaldehyde adhesive water resistance. Journal of Applied Polymer Science 88: 287-292. https://doi.org/10.1002/app.11687
  44. Zhou, J., Yue, K., Lu, W., Li, M., Chen, Z., Cheng, X., Liu, W., Jia, C., Tang, L. 2018. Effect of CMC formic acid solution on bonding performance of muf for interior grade glulam. Cellulose Chemistry and Technology 52: 239-245.
  45. Zink, A.G., Kartunova, E. 1998. Wood failure in plywood shear samples measured with image analysis. Forest Products Journal 48(4): 69-74.