Abstract
For manufacturing upper housing product of mechanical control valve, the progressive drawing process was conducted experimental. Then, the center of the product was cut to measure the thickness of the product. As a result, the following conclusions were obtained. By means of a stand-alone pad provided with sufficient pressure, it is possible to prevent the occurrence of wrinkles in the die pad product of the drawing process. As a result of the experiment, it was considered that the flange bottom of the product and the lower edge of the product are made thick in thickness, the top edge and the top surface are thin. It is considered that this is due to the size and roughness of the entrance edge radius of the die in the drawing process, and the inflow of the material by the die pad.