Abstract
Recently, structures such as large retailers, outlets and warehouses have been increasing in accordance with changes in consumption patterns. Since these structures include ultra-flat slab members, they are thoroughly managed to control slab cracking by the plastic and drying shrinkage. In order to control the cracking of the slab member, a chemical crack reduction method is used. In particular, the use of the shrinkage reducing agent has been examined. However, domestic research results are limited. In this study, the shrinkage properties of concrete using shrinkage reducing agent and the drying shrinkage properties according to the mixing factors were investigated. The performance of domestic shrinkage reducing agent was appeared similar to that of overseas high-grade shrinkage reducing agent. As the shrinkage reducing agent usage increased, the drying shrinkage reduction effect increased. At the age of 100 days, the dry shrinkage rate of specimen with the shrinkage reducing agent of 1.5%was shown about half that of the specimen without the shrinkage reducing agent. The shrinkage reducing agent was gound to have no specific performance change for the use of the admixture.
최근 소비패턴의 변화에 따라 대형마트, 아울렛 및 물류창고 등과 같은 구조물들이 증가하고 있다. 이와 같은 구조물들은 초평탄 바닥부재를 포함하고 있기 때문에 소성 및 건조수축에 의한 슬래브 부재의 균열 억제 관리를 철저하게 실시한다. 슬래브 부재의 균열을 억제하기 위한 방안으로 화학적 균열저감 방법을 사용하고 있으며, 특히 수축저감제에 대한 사용검토가 증가하고 있다. 그러나 이에 대한 국내 연구결과는 부족한 상황이다. 본 연구에서는 수축저감제를 사용한 콘크리트의 수축특성과 배합요인 변동에 따른 건조수축 특성을 검토하였다. 국내 수축저감제는 해외 고급형 수축저감제와 성능이 유사한 것으로 나타났으며, 수축저감제 사용량이 증가할수록 건조수축 억제 효과는 높아지는 것으로 나타났다. 수축저감제 1.5%를 사용한 시험체는 재령 100일에서 수축저감제를 사용하지 않은 시험체에 비해 건조수축량이 약 절반으로 나타났다. 또한, 혼화재료 사용에 대해 특별한 성능변화는 없는 것으로 확인되었다.