Abstract

Weighting of silk fabrics have long been practiced in silk fabric trading based on the primary consideration of price-weight, and secondary one of quality improvement in handle, luster, and drape properties. Recent trend of practicing weighting of silk fabrics is, however, focused on the improvement of the handle, luster, drape, and other properties. During the finishing processes of synthetic fiber, nylon, comprising amide structure, include the use of tannic acid, especially in the dyeing. A multitude of studies are being implemented in terms of improving fastness to washing, fastness to light of dyed nylon product, or the light fastness of nylon 6 itself. In this study, the effects of various tannic acid treatments on the physical properties related to the handle of nylon 6 and silk fabrics are examined and reviewed. The effects of treatment condition of the tannic acid, e.g., the concentration of the aqueous tannic acid solution, treatment time, and temperature were investigated. As the concentration of the aqueous solution of tannic acid increased, the bending rigidity values of the silk and nylon 6 fabrics increased. The treated fabrics felt stiff to the touch. Within the mild conditions of bending employed in the bending measurement of KES, nylon 6 treated fabric specimen exhibited a trend of improvement of bending resiliency within the range of small bending deformation. The weight of treated fabrics have all increased. The air-permeability values decreased as the treatment concentration increased. However, the decrease tendency of air permeability values may be alleviated by adjusting the fabric count during the tentering or expanding processes, either by tension adjustment or heat treatment. Optimum conditions of the treatment for nylon 6 are 1.25% tannic acid concentration, bath temperature of $85^{\circ}C$, pH 3.1, and those for silk fabric treatment are 1.25% tannic acid concentration, bath temperature of $85^{\circ}C$, pH 3.1. The treatment conditions will lead to the improvement in the properties of fabrics for summer.

Keywords

References

  1. Albu, M. G., Ghica, M. V., Giurginca, M., Trandafir, V., Popa, L., & Cotrut, C. (2009). Spectral characteristics and antioxidant properties of tannic acid immobilized on collagen drug-delivery systems. Revista de Chimie -Bucharest- Original Edition- 60(7), 666-672.
  2. Brand, R. H. (1964). Measurement of fabric aesthetics: analysis of aesthetic components. Text. Res. J., 34(9), 791-804. https://doi.org/10.1177/004051756403400909
  3. Burkinshaw, S. M., & Bahojb-Allafan, B. (2004). The development of a metal-free, tannic acid-based aftertreatment for nylon6,6 dyed with acid dyes -part 4: tannic acid. Dyes & Pigments, 62(2), 159-172. https://doi.org/10.1016/j.dyepig.2003.12.001
  4. El-Gabry, L. K., & El-Zawahry, M. M. (2008). Effect of tannic acid on the dyeing process of nylon 6 fabric with cationic dye. Res. J. of Textile and Apparel, 12(4), 21-30. https://doi.org/10.1108/RJTA-12-04-2008-B003
  5. Kawabata, S., & Niwa, M. (1989). Fabric performance in clothing manufacture. Journal Textile Institute, 80(1), 19-50. https://doi.org/10.1080/00405008908659184
  6. Kim, T., Cho., N., Ma, H., Yang, G. W., & Rho, Y. H. (2013). A study on the effect of gallotannin treatment of ceramide-containing fibers on atopic skin diseases. Textile Coloration & Finishing, 25(4), 271-278. https://doi.org/10.5764/TCF.2013.25.4.271
  7. Na, B., Lv, R., Tian, N., Xu, W., Li, Z., & Fu, Q. (2009). Micro-FT-IR study of stretching a single filament: polymorphic transition in nylon 6. J. Polymer Sci., Part B, Polymer Physics, 47(9), 898-902. https://doi.org/10.1002/polb.21696
  8. Pantoja-Castroa, M. A., Gonzalez-Rodrigueza, H. (2011). Study by infrared spectroscopy and thermogravimetric analysis of tannins and tannic Acid. Rev. latinoam. quim, 39(3), 107-112.
  9. Tirpak, G. A., & Sibilia, J. P. (1973). A new fiber-sampling technique for Infrared spectroscopy as applied to nylon 6 and poly(ethylene Terephthalate). J. Appl. Polymer Sci., 17(2), 643-648. https://doi.org/10.1002/app.1973.070170226
  10. Um, I. C., Kweon, H. Y., Park, Y. H., & Hudson, S. (2001). Structural characteristics and properties of the regenerated silk fibroin prepared from formic acid. International Journal of Biological Macromolecules, 29, 91-97. https://doi.org/10.1016/S0141-8130(01)00159-3
  11. Vankar, P. S., Shanker, R., & Verma, A. (2007). Enzymatic natural dyeing of cotton and silk fabrics without metal mordant, J. of Cleaner Production, 15, 1441-1450. https://doi.org/10.1016/j.jclepro.2006.05.004
  12. Wu, Y., Xu, Y., Wang, D., Zhao, Y., Weng, S., Xu, D., & Wu, J. (2004). FT-IR Spectroscopic Investigation on the Interaction Between Nylon 66 and Lithium Salts, J. Appl. Polymer, 91(5), 2869-2895. https://doi.org/10.1002/app.13495

Cited by

  1. 아토피성 피부질환 완화용 세라마이드 함유 3차원 섬유 구조체 디자인 및 평가 vol.55, pp.6, 2016, https://doi.org/10.12772/tse.2018.55.398
  2. Hydrolyzable vs. Condensed Wood Tannins for Bio-based Antioxidant Coatings: Superior Properties of Quebracho Tannins vol.9, pp.9, 2020, https://doi.org/10.3390/antiox9090804
  3. Utilizing a pH-responsive palladium nanocomposite to fabricate adhesion-enhanced and highly reliable copper coating on nylon 6 fabrics vol.15, pp.None, 2021, https://doi.org/10.1016/j.jmrt.2021.10.053