Abstract

The paper presents a research project on the tensile properties of RPC mixed with both steel and polypropylene fibers after exposure to $20-900^{\circ}C$. The direct and the indirect tensile strength (in bending) were measured through tensile experiment on dog-bone specimens and bending experiment on $40{\times}40{\times}160mm$ prisms. RPC microstructure was analyzed using scanning electron microscope. The results indicate that, steel fibers can significantly improve the tensile performance of hybrid fiber-reinforced RPC, whereas polypropylene fibers have no obvious effect on the tensile performance. With increasing temperature, the flexural and axial tensile strength of hybrid fiber-reinforced RPC substantially decrease linearly, which attributes to the deteriorating microstructure. Based on the experimental results, equations are established to express the decay of the flexural and tensile strength with increasing temperature.

Keywords

References

  1. Bayard, O., & Ple, O. (2003). Fracture mechanics of reactive powder concrete: material modelling and experimental investigations. Engineering Fracture Mechanics, 70, 839-851. https://doi.org/10.1016/S0013-7944(02)00153-4
  2. Chang, Y.-F., Chen, Y.-H., Sheu, M.-S., et al. (2006). Residual stress-strain relationship for concrete after exposure to high temperatures. Cement and Concrete Research, 36, 1999-2005. https://doi.org/10.1016/j.cemconres.2006.05.029
  3. Chen, B., & Liu, J.-Y. (2004). Residual strength of hybrid-fiberreinforced high-strength concrete after exposure to high temperatures. Cement and Concrete Research, 34(6), 1065-1069. https://doi.org/10.1016/j.cemconres.2003.11.010
  4. Cheyrezy, M., Maret, V., & Frouin, L. (1995). Microstructural analysis of RPC (reactive powder concrete). Cement and Concrete Research, 25, 1491-1500. https://doi.org/10.1016/0008-8846(95)00143-Z
  5. EN 1992-1-2: 2004. (2004). Eurocode 2: Design of concrete structures-Part 1-2: General rules-Structural fire design. European Committee for Standardization.
  6. GB/T 17671-1999. (1999). Method of testing cements-Determination of strength. Quality and Technical Supervision of People's Republic of China.
  7. Han, C.-G., Hwang, Y.-S., Yangb, S.-H., et al. (2005). Performance of spalling resistance of high performance concrete with polypropylene fiber contents and lateral confinement. Cement and Concrete Research, 35(9), 1747-1753. https://doi.org/10.1016/j.cemconres.2004.11.013
  8. Husem, M. (2006). The effects of high temperature on compressive and flexural strengths of ordinary and high-performance concrete. Fire Safety Journal, 41, 155-163. https://doi.org/10.1016/j.firesaf.2005.12.002
  9. Kalifa, P., Chene, G., & Galle, C. (2001). High-temperature behaviour of HPC with polypropylene fibres from spalling to microstructure. Cement and Concrete Research, 31(10), 1487-1499. https://doi.org/10.1016/S0008-8846(01)00596-8
  10. Kalifa, P., Menneteau, F.-D., & Quenard, D. (2000). Spalling and pore pressure in HPC at high temperatures. Cement and Concrete Research, 30, 1915-1927. https://doi.org/10.1016/S0008-8846(00)00384-7
  11. Kang, S.-T., Lee, Y., Park, Y.-D., et al. (2010). Tensile fracture properties of an ultra high performance fiber reinforced concrete (UHPFRC) with steel fiber. Composite Structures, 92(1), 61-71. https://doi.org/10.1016/j.compstruct.2009.06.012
  12. Khalig, W., & Kodur, V. K. R. (2011). Effect of high temperature on tensile strength of different types of high-strength concrete. ACI Materials Journal, 108(4), 394-402.
  13. Kodur, V. K. R. (2000). Spalling in high strength concrete exposed to fire-concerns, causes, critical parameters and cures (pp. 1-8). USA: ASCE structures congress proceedings, Philadelphia, PA.
  14. Li, H.-Y., Wang, Y., Xie, H.-Y., et al. (2012). Microstructure analysis of reactive powder concrete after exposed to high temperature. Journal of Huazhong University of Science and Technology (Natural Science Edition), 40(5), 71-75. (in Chinese).
  15. Li, L., Zheng, W.-Z., & Lu, S.-S. (2010). Experimental study on mechanical properties of reactive powder concrete. Journal of Harbin Institute of Technology (New Series), 17, 795-800.
  16. Pliya, P., Beaucour, A.-L., & Noumowe, A. (2011). Contribution of cocktail of polypropylene and steel fibers in improving the behaviour of high strength concrete subjected to high temperature. Construction and Building Materials, 25(4), 1926-1934. https://doi.org/10.1016/j.conbuildmat.2010.11.064
  17. Rashad, A. M., Saleem, H. E.-D. H., & Shaheen, A. F. (2013). Effect of silica fume and slag on compressive strength and abrasion resistance of HVFA concrete. International Journal of Concrete Structures and Materials, 8(1), 69-81. https://doi.org/10.1007/s40069-013-0051-2
  18. Richard, P., & Cheyrezy, M. (1995). Composition of reactive powder concretes. Cement and Concrete Research, 25, 1501-1511. https://doi.org/10.1016/0008-8846(95)00144-2
  19. SL 352-2006. (2006). Test code for hydraulic concrete. Water Resources Ministry of People's Republic of China.
  20. Song, P.-S., & Wang, S.-H. (2004). Mechanical properties of high-strength steel fiber-reinforced concrete. Construction and Building Materials, 18(9), 669-673. https://doi.org/10.1016/j.conbuildmat.2004.04.027
  21. Tai, Y.-S., Pan, H.-H., & Kung, Y.-N. (2011). Mechanical properties of steel fiber reinforced reactive powder concrete following exposure to high temperature reaching $800^{\circ}C$. Nuclear Engineering and Design, 241, 2416-2424. https://doi.org/10.1016/j.nucengdes.2011.04.008
  22. Vance, K., Aguayo, M., Dakhane, A., Jain, J., & Neithalath, N. (2014). Microstructural, mechanical, and durability related similarities in concretes based on OPC and alkali-activated slag binders. International Journal of Concrete Structures and Materials, 8(4), 289-299. https://doi.org/10.1007/s40069-014-0082-3
  23. Xiao, J.-Z., & Falkner, H. (2006). On residual strength of highperformance concrete with and without polypropylene fibers at elevated temperatures. Fire Safety Journal, 41(2), 115-121. https://doi.org/10.1016/j.firesaf.2005.11.004
  24. Xiao, J.-Z. H., Ren, H.-M., & Wang, P. (2006). Study on residual flexural strength of high performance concrete at elevated temperature. Journal of Tongji University (Natural Science), 34(5), 580-585 (in Chinese).
  25. Yazici, H., Yardimci, M.-Y., Yigiter, H., Ayidin, S., & Turkel, S. (2010). Mechanical properties of reactive powder concrete containing high volumes of ground granulated blast furnace slag. Cement & Concrete Composites, 32, 639-648. https://doi.org/10.1016/j.cemconcomp.2010.07.005
  26. Zheng, W.-Z., Li, H.-Y., Wang, Y., & Xie, H.-Y. (2012a). Tensile properties of steel fiber-reinforced reactive powder concrete after high temperature. In The 2nd international conference on materials science and engineering applications (Vol. 413, pp. 270-276).
  27. Zheng, W.-Z., Li, H.-Y., & Wang, Y. (2012b). Compressive behaviour of hybrid fiber-reinforced reactive powder concrete after high temperature. Materials and Design, 41(C), 403-409. https://doi.org/10.1016/j.matdes.2012.05.026
  28. Zheng, W.-Z., Li, H.-Y., & Wang, Y. (2012c). Mechanical properties of reactive powder concrete with different dosage of polypropylene fiber after high temperature. Journal of Building Structures, 33(9), 119-126 (in Chinese).
  29. Zhou, Y. (2000). Materials analysis method. Beijing, China Machinery Industry Press (in Chinese).

Cited by

  1. A Review on Structural Behavior, Design, and Application of Ultra-High-Performance Fiber-Reinforced Concrete vol.10, pp.2, 2016, https://doi.org/10.1007/s40069-016-0143-x
  2. Effect of Elevated Temperature on Mechanical Properties of Limestone, Quartzite and Granite Concrete vol.11, pp.1, 2016, https://doi.org/10.1007/s40069-016-0175-2
  3. Pull-Out Behaviour of Hooked End Steel Fibres Embedded in Ultra-high Performance Mortar with Various W/B Ratios vol.11, pp.2, 2016, https://doi.org/10.1007/s40069-017-0193-8
  4. Effect of Fiber Hybridization on Durability Related Properties of Ultra-High Performance Concrete vol.11, pp.2, 2017, https://doi.org/10.1007/s40069-017-0195-6
  5. Evaluation of Fire-Damaged Concrete: An Experimental Analysis based on Destructive and Nondestructive Methods vol.11, pp.3, 2016, https://doi.org/10.1007/s40069-017-0211-x
  6. Quality Evaluation Tests for Tensile Strength of Reactive Powder Concrete vol.30, pp.5, 2016, https://doi.org/10.1061/(asce)mt.1943-5533.0002257
  7. Effect of Fibers on High-Temperature Mechanical Behavior and Microstructure of Reactive Powder Concrete vol.12, pp.2, 2016, https://doi.org/10.3390/ma12020329
  8. Study of Toughness and Macro/Micro-Crack Development of Fibre-Reinforced Ultra-High Performance Concrete After Exposure to Elevated Temperature vol.12, pp.8, 2016, https://doi.org/10.3390/ma12081210
  9. Experimental and numerical study on damage evaluation of hybrid fiber-reinforced concrete vol.20, pp.5, 2016, https://doi.org/10.1007/s42107-019-00141-1
  10. Comparisons Between Pull-Out Behaviour of Various Hooked-End Fibres in Normal-High Strength Concretes vol.13, pp.1, 2016, https://doi.org/10.1186/s40069-019-0337-0
  11. The Tensile Strength and Damage Characteristic of Two Types of Concrete and Their Interface vol.13, pp.1, 2016, https://doi.org/10.3390/ma13010016
  12. Thermal Properties of Hybrid Fiber-Reinforced Reactive Powder Concrete at High Temperature vol.32, pp.3, 2016, https://doi.org/10.1061/(asce)mt.1943-5533.0003053
  13. Mechanical Properties of Hybrid Steel-Glass Fiber-Reinforced Reactive Powder Concrete After Exposure to Elevated Temperatures vol.45, pp.5, 2016, https://doi.org/10.1007/s13369-020-04435-4
  14. Elevated Temperature Performance of Reactive Powder Concrete Containing Recycled Fine Aggregates vol.13, pp.17, 2020, https://doi.org/10.3390/ma13173748
  15. Shear strength of fibre-reinforced reactive powder concrete I-shaped beam without stirrups vol.72, pp.21, 2020, https://doi.org/10.1680/jmacr.18.00525
  16. Effect of Elevated Temperature on the Bond Strength of Prestressing Reinforcement in UHPC vol.13, pp.21, 2020, https://doi.org/10.3390/ma13214990
  17. A review study on sustainable development of ultra high-performance concrete vol.9, pp.1, 2016, https://doi.org/10.3934/matersci.2022002
  18. Thermal effects of steel-fibre-reinforced reactive powder concrete at elevated temperatures vol.73, pp.3, 2016, https://doi.org/10.1680/jmacr.19.00105
  19. Uniaxial Tensile Behavior, Flexural Properties, Empirical Calculation and Microstructure of Multi-Scale Fiber Reinforced Cement-Based Material at Elevated Temperature vol.14, pp.8, 2016, https://doi.org/10.3390/ma14081827
  20. Three-dimensional meso-scale modelling of failure of steel fiber reinforced concrete at room and elevated temperatures vol.278, pp.None, 2021, https://doi.org/10.1016/j.conbuildmat.2021.122368
  21. Compressive behavior of hybrid steel-polyvinyl alcohol fiber-reinforced concrete containing fly ash and slag powder: experiments and an artificial neural network model vol.22, pp.9, 2016, https://doi.org/10.1631/jzus.a2000379
  22. Investigation on the Mechanical Properties and Microstructure of Eco-friendly Mortar Containing WGP at Elevated Temperature vol.15, pp.1, 2016, https://doi.org/10.1186/s40069-020-00434-9
  23. Post-fire optimum mechanical properties of self-compacting mortar using Taguchi method and analysis of variance vol.315, pp.None, 2016, https://doi.org/10.1016/j.conbuildmat.2021.125642
  24. ECCs/UHPFRCCs with and without FRP reinforcement for structural strengthening/repairing: A state-of-the-art review vol.316, pp.None, 2016, https://doi.org/10.1016/j.conbuildmat.2021.125824
  25. Design-oriented assessment of the residual post-fire bearing capacity of precast fiber reinforced concrete tunnel linings vol.127, pp.None, 2016, https://doi.org/10.1016/j.firesaf.2021.103503