DOI QR코드

DOI QR Code

Review on The Measurement of Wood Shrinkage

목재수축률 측정에 대한 총설

  • Lee, So Sun (Department of Wood Science and Engineering, Research Institute for Agriculture & Life Sciences, Chonnam National University) ;
  • So, Won-Tek (Department of Wood Science and Engineering, Research Institute for Agriculture & Life Sciences, Chonnam National University) ;
  • Jeong, Gi Young (Department of Wood Science and Engineering, Research Institute for Agriculture & Life Sciences, Chonnam National University)
  • Received : 2015.09.04
  • Accepted : 2015.10.15
  • Published : 2015.11.25

Abstract

The goal of this study was to review the wood shrinkage published in Journal of The Korean Wood Science and Technology from 1976 to 2015. Previous studies reported that shrinkage from Larix kaempferi in the tangential, radial, longitudinal directions ranged from 4.21%-9.79%, 2.09%-4.67%, 0.17%-0.33%, respectively. When different drying methods including closed cylinder drying, oven drying, and room temperature drying were used, volumetric shrinkage of Dipterocarpus grandiflorus was different, ranging from 31.6% to 21.0%. With an increment of the drying temperature of $115^{\circ}C$, $120^{\circ}C$, $125^{\circ}C$, the shrinkage of Larix kaempferi did not show a consistent trend. When sample size of Pinus densiflora was increased from $20{\times}20{\times}20mm$ to $100{\times}100{\times}100mm$, the tangential, radial and volumetric shrinkage decreased 2.61%, 1.32%, 0.80%, respectively. When a caliper having a sensitivity of 0.01 mm was used to measure $20mm^3$ specimen from Cryptomeria japonica, the measurement error occurred 1.97% in the radial direction and 35.7% in the longitudinal direction. From the previous studies, wood shrinkage could be influenced by sample size, drying method and measurement technique.

본 논문에서는 목재 수축률에 관한 1976-2015년도에 발표된 목재공학회지 논문을 정리하였다. 국내산 낙엽송(Larix kaempferi) 수축률을 측정한 연구자들간에 접선방향 수축률은 4.21%-9.79%, 방사방향 수축률은 2.09%-4.67%, 섬유방향 수축률은 0.17%-0.33%로 접선방향 2.3배, 방사방향 2.2배, 섬유방향 1.9배로 연구자들마다 측정 값에 차이가 나타났다. 소나무(Pinus densiflora) 시편 크기가 $20{\times}20{\times}20mm$에서 $100{\times}100{\times}100mm$로 증가함에 따라 접선방향, 방사방향, 부피수축률은 2.61%, 1.32%, 0.80% 감소하였다. 아피통(Dipterocarpus grandiflorus)을 밀폐건조, 오븐건조, 실온건조 하였을 때 부피수축률은 31.6%, 26.5%, 21.0%로 건조방법에 따라 5.5%-10.6% 차이가 나타났으며 건조온도가 $115^{\circ}C$, $120^{\circ}C$, $125^{\circ}C$로 증가함에 따라 낙엽송의 수축률은 일정한 증가, 감소 경향이 보이지 않았다. $20mm^3$ 크기의 삼나무(Cryptomeria japonica) 시편을 한국산업규격(KS F 2203, 2004)에서 제시하는 정밀도 0.01 mm의 길이측정도구로 수축률을 측정하였을 때, 방사, 섬유방향 수축률 측정오차는 1.97%, 35.7%로 크게 나타났다. 목재의 수축률은 시편 크기, 건조방법, 측정방법에 영향을 받는 것으로 나타났다.

Keywords

References

  1. Hwang, K.H., Park, B.S. 2009. Effect of Cross-Sectional Dimension on thd Shrinkage Property of Korean Red-Pine Wood. Journal of the Korean Wood Science and Technology 37(3): 231-238
  2. Hwang, W.J., Kim, N.H. 1999. Utilization of Domestic Small Timbers Shrinkage and Swelling of Alkali-Treated Woods. Journal of Korea forestry energy 18(2): 70-77.
  3. Jeong, S.H., Park, B.S. 2008. Wood properties of the useful tree species grown in Korea. Korea forest research institute. Seoul, Korea.
  4. Jung, H.S., Lee, N.H., Yeo, H.M., Lee, J.H., Yoo, T.K. 1996. Rotary Veneer Peeling of Some Softwoods and Its Veneer Drying. Journal of the Korean Wood Science and Technology 24(1): 34-47.
  5. Jung, H.S., Sim, J.H. 1986. Development of Kiln Drying Schedule of Lesser-Known Species Imported from Solomon. Journal of the Korean Wood Science and Technology 14(1): 45-54.
  6. Kang, C.W., Matsumura, J., Kang, W. 2008. Observation of Shrinkage Features of Cross Sectional Surface of Wood by LV-SEM. Journal of the Korean Wood Science and Technology 36(3): 17-23.
  7. Kang, H.Y. 1994. Shrinkages of Prefrozen or Presteamed Wood. Journal of the Korean Wood Science and Technology 22(1): 66-71.
  8. Kang, H.Y. 1998. Prediction of Microwave Drying Curves for Various Hardwoods and Softwoods. Journal of the Korean Wood Science and Technology 26(4): 34-42.
  9. Kang, H.Y. 2003. Drying Boards of Populus alba x P. glandulosa in Conventional, High-Temperature and Microwave-Vacuum Kilns. Journal of the Korean Wood Science and Technology 31(4): 31-37.
  10. Kim, B.R. 1995. Studies on Variability in Wood Properties in Tree Stems of Pinus koraienses (I) -Differences in Green Moisture Content and Shrinkage between Heartwood and Sapwood-. Journal of the Korean Wood Science and Technology 23(1): 28-34.
  11. Kim, J.H., Lee, W.H. 2002. Physical Properties of Larch (Larix kaemferi Carr.) Treated by High Temperature Steaming -Effect of high temperature steaming on shrinkages of larch block-. Journal of the Korean Wood Science and Technology 30(2): 102-107.
  12. Kim, Y.S., Lee, W.Y. 1976. Study on the shrinkage properties of commercial hardwoods. Journal of the Korean Wood Science and Technology 4(1): 8-14.
  13. Korean Standard F 2203, 2004, Method of shrinkage test for wood, Korean Standard Association, Seoul, Korea.
  14. Lee, J.H., Jung, H.S. 1997. Effects of Drying Temperature on Internal Temperature, Drying Rate and Drying Defects for Japanese Larch in High-Temperature Drying. Journal of the Korean Wood Science and Technology 25(4): 99-107.
  15. Mun, S.H., Cha, J.K. 2002. Effect of Cycle Moisture Content Changes on Shrinkage and Thermal Conductivity in Domestic Quercus acutissima Carr. and Larix Kaempferi Carr. Journal of the Korean Wood Science and Technology 30(4): 41-50.
  16. Park, Y.G., Chang, Y.S., Yang, S.Y., Yeo, H.M., Lee, M.R., Eom, C.D., Kwon, O.K. 2015. Wood Shrinkage Measurement of Using a Flatbed Scanner. Journal of the Korean Wood Science and Technology 43(1): 43-51. https://doi.org/10.5658/WOOD.2015.43.1.43
  17. Park, Y.G., Eom, C.D., Park, J.H., Chang, Y.S., Kim, K.M., Kang, C.W., Yeo, H.M. 2012. Evaluation of Physical Properties of Korean Pine (Pinus koraiensis Siebold & Zucc.) Lumber Heat-Treated by Superheated Steam. Journal of the Korean Wood Science and Technology 40(4): 257-267. https://doi.org/10.5658/WOOD.2012.40.4.257
  18. Yeo, H.M., Jung, H.S. 1994. Distribution Model Based on Computer Simulation for Internal Temperature and Moisture Content in Press Drying of Tree Disks. Journal of the Korean Wood Science and Technology 22(2): 61-70.